Engineering PapersSearch

SEARCH · Engineering Papers

Results for “nanoindentation”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

Investigation of Lunar-Inspired Geopolymer Concrete Formulations Mixed and Cured in Microgravity on the International Space Station (ISS)

The research outlined in this presentation investigates the use of various lunar regolith simulants in geopolymer lunar concrete mixes mixed and cured on the International Space Station (ISS). The motivation for this work is to study the effects of gravity on the microstructure of alkali-activated materials cured with heat, and to develop materials for the construction of long-term infrastructure on the lunar surface with in-situ resource utilization (ISRU). ISRU for construction materials reduces the cost and mass of payloads related to lunar construction. The advantage of geopolymer concrete as opposed to traditional portland cement concrete is that water acts as a medium for the polymerization reaction and leaves the system throughout the process, reducing its demand. Twelve samples of lunar regolith simulant and a solution composed of sodium hydroxide and sodium silicate were sent to the ISS. The three simulants were OPRH2N, OPRL2N, and JSC-1AF, using only particles less than 53 µm in diameter to increase reactivity of the simulant. Simulant to solution ratios were determined by workability while mixing. The simulant and solution were sealed Burst Pouches® along with 2 other sealed bags to prevent material from leaking. Crew member F-14 conducted testing on the ISS by introducing the solution to the simulant in the Burst Pouch®, mixing the sample with a spatula, and then clamping the specimen in the fresh state to prevent flow inside the Burst Pouch®. These specimens were then put in a thermos heated to 80C via sealed drinking water bags to cure for 24 hours with a temperature logger. The cured specimens remained in microgravity for at least 28 days and were returned from the ISS in February 2025. The specimens were then brought to the NASA Marshall Space Flight Center (MSFC) to analyze. Material characterization consisted of conducting Micro-CT tests of entire samples in their sealed apparatus to a resolution of 25µm. 2D image slices were saved in each orthogonal direction of each specimen at a 0.03 mm step size from the 3D model to conduct analytical porosity calculations. Representative samples from each specimen were sampled to perform helium gas pycnometery and were then mounted in resin for SEM imaging, EDS, and nanoindentation. Porosity was analyzed analytically using micromechanics modelling with the assistance of the NASA Multiscale Analysis Tool (NASMAT), as well as the NASA Advanced Supercomputing (NAS) servers (V. Saseendran & N. Yamamoto, 2024). Density was measured using helium gas pycnometery and was then compared to the theoretical density for experimental porosity calculation. Due to the samples’ non-uniform shape being cured in a pouch, traditional compression and tensile strength testing could not be performed. Nanoindentation was conducted at Clarkson University to determine the microhardness and reduced modulus of elasticity. Results from flight samples can be compared to ground samples currently in DLR’s possession to determine the effect on microstructure from being mixed and cured in microgravity. This study gives further insight and understanding of geopolymer lunar concrete and its viability as a lunar construction material with ISRU.

Adam Johnson

The Shape Effect: Influence of 1D and 2D Boron Nitride Nanostructures on the Radiation Shielding, Thermal, and Damping Properties of High-Temperature Epoxy Composites

In space exploration, lightweight multifunctional materials capable of shielding neutron radiation, dissipating heat, and providing damping are essential. Polymer composites reinforced with boron nitride (BN) nanomaterials—specifically one-dimensional boron nitride nanotubes (BNNTs) and two-dimensional boron nitride nanoplatelets (BNNPs)—offer promising solutions. This study investigates how BN nanomaterial morphology influences the performance of high-temperature (HT) epoxy composites. We developed ultralightweight, three-dimensional BN foams comprising 1D BNNTs, 2D BNNPs, and hybrid 1D BNNT/2D BNNP structures via freeze-drying, then infiltrated them with HT epoxy to form dense composites. The BNNT foam exhibited the highest neutron radiation shielding, with a mass absorption coefficient of 26.64 cm2 g −1 , outperforming the hybrid foam (18.18 cm 2 g −1 ) and the BNNP foam (11.12 cm 2 g −1 ). A similar trend was observed in the HT epoxy composites; incorporating these foams at least doubled the mass absorption coefficient compared to the neat polymer. In terms of thermal conductivity, the BNNT/BNNP foam-epoxy composite achieved the highest value of 0.34 W m −1 K −1 , a 2.13-fold increase over neat HT epoxy. The BNNT/BNNP foam-epoxy composites also improved by 1.88 and 1.75 times, respectively. Mechanical testing revealed that BNNP foams withstood the highest loads during nanoindentation (3.53 kN), followed by BNNT/BNNP foams (1.93 kN) and BNNT foams (1.56 kN). All BN foam-epoxy composites exhibited enhanced damping properties, with tan δ increasing by at least 30 % compared to neat HT epoxy. These findings elucidate the impact of BN nanomaterial morphology on the multifunctional performance of HT epoxy composites, offering insights for developing high-performance, tailorable materials for demanding environments.

Kazue Orikasa