Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “high temperature hydrogen”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 19 records

Microstructural evolution of Mo-UO 2 cermets under high temperature hydrogen environments

Ceramic-metallic (cermet) materials show promise for use in nuclear thermal propulsion applications due to attractive thermophysical properties including high temperature stability and high thermal conductivity. In this work, molybdenum-uranium dioxide (Mo-UO 2 ) cermet fuel elements were fabricated by means of spark plasma sintering (SPS) and were subsequently exposed to hydrogen at high temperatures (2500 K). Mo-UO 2 samples pre- and post-exposure were characterized by means of optical microscopy, scanning electron microscopy, and X-ray diffraction (XRD). Microscopy analyses of the as-produced material displayed microscopic cracking on the interior of the spherical UO 2 fuel particles but confirmed that the fuel particles were fully encapsulated in the Mo matrix. The results further showed mass loss, macroscopic swelling, and cracking in the cermet samples which occurred during high temperature hydrogen testing. Nanoscale swelling was evidenced by XRD in the Mo matrix and UO 2 fuel structure due to the incorporation of defects and accompanied microstrain.

36 MATERIALS SCIENCE↗

A mechanistic interpretation of Nelson curves for PVP failures under high temperature hydrogen attack

As an empirically established design criterion, Nelson curves that relate the service temperature and the allowable hydrogen partial pressure have been developed and utilized for more than sixty years in pressure vessels and piping (PVP) safety design. Despite a relatively clear thermodynamic understanding of the high-temperature-hydrogen-attack (HTHA) problem, the detailed fracture process on the microstructural length scales, however, remains elusive, and a quantitative assessment of the PVP lifetime under HTHA from the available creep fracture dataset is still not possible. This work develops a microstructure-informed and micromechanics-based model by incorporating a synergy between hydrogen transport and intergranular-cavity-based fracture process. Based on the available creep lifetime data of C-0.5Mo steels, we are able to calibrate material constitutive parameters, and then conduct nonlinear finite element simulations that reveal a real-time stress-induced hydrogen diffusional transport along grain boundaries, coupled with a microstructure-explicit failure process, from which Nelson curves can be computed. Such failure analyses allow us to delineate two distinct regimes on the Nelson curves, i.e., dislocation-creep-controlled or grain boundary diffusion-assisted cavity growth. More importantly, we found that a small change of the pipe thickness and applied stresses can significantly shift these lifetime curves. However, these two parameters are usually not provided in Nelson curves, thus limiting their usage in material selection and safety design. In conclusion, this discrepancy can clearly be mitigated by extensive parametric studies from our micromechanical modeling/simulation framework.

36 MATERIALS SCIENCE↗

Hydrogen Safety Review for Gas Turbines, SOFC, and High Temperature Hydrogen Production

This report presents an introduction and summary on hydrogen safety issues, as they relate to hydrogen production, storage, and use in the energy sector, primarily as related to electricity generation by gas turbines, and solid oxide fuel cells (SOFC), and hydrogen production from gasification and steam methane reforming processes. The impetus behind this effort is the U.S. DOE goal for decarbonization of the power generation sector by the year 2035. In many cases, hydrogen is expected to replace natural gas as the primary fuel source (or form of energy storage) to achieve this goal. Advanced technologies for large-scale energy production using hydrogen as a fuel source which can be deployed over the next 5–10 years will be required. However, to develop and mature these hydrogen-based technologies, it will be critical to identify the safety issues related to widespread use of hydrogen as a fuel source, so that they may be addressed prior to widespread deployment.

08 HYDROGEN↗

Effects of a refractory metal protective barrier on uranium carbonitride ceramic–metallic composites exposed to a high temperature hydrogen environment

Uranium nitride has been under consideration at NASA and the Department of Energy for nuclear thermal propulsion applications intended for deep space exploration vehicles. It is critical to the success of the technology development that the behavior of the fuel system is properly characterized in operational environments. This body of work fabricated ceramic metal composites consisting of uranium ceramic fuel in a molybdenum and molybdenum–tungsten metal matrix, both with and without an exterior molybdenum barrier. Specimens were introduced to a high temperature hydrogen environment and characterized through x-ray diffraction, scanning electron microscopy, and energy dispersive spectroscopy to identify characteristic changes. A portion of the specimens was fabricated with a 1.27 mm thick molybdenum barrier in order to isolate the material from the hydrogen environment. Instability of the uranium nitride occurred as low as 2073 K, leading to aggressive instability approaching 2658 K. Carbon reactions with the metal matrix were observed as well as alloying between the uranium and metal matrix constituents. The liquid uranium resulting from the instability of the uranium nitride was observed to attack the grain boundaries of the refractory metal, resulting in the formation of a liquid uranium molybdenum eutectic melt. Specimens encased in a barrier experienced similar results. The authors conclude this is a significant challenge to applications of this cermet at these temperatures. Alternate configurations with resilient hermetic seals or lower temperature applications such as power reactors may have more success.

36 MATERIALS SCIENCE↗

Intergranular corrosion of Ni-30Cr in high-temperature hydrogenated water after removing surface passivating film

Abstract High-resolution transmission electron microscopy and atom probe tomography are used to characterize the initial passivation and subsequent intergranular corrosion of degraded grain boundaries in a model Ni-30Cr alloy exposed to 360 °C hydrogenated water. Upon initial exposure for 1000 h, the alloy surface directly above the grain boundary forms a thin passivating film of Cr 2 O 3 , protecting the underlying grain boundary from intergranular corrosion. However, the metal grain boundary experiences severe Cr depletion and grain boundary migration during this initial exposure. To understand how Cr depletion affects further corrosion, the local protective film was sputtered away using a glancing angle focused ion beam. Upon further exposure, the surface fails to repassivate, and intergranular corrosion is observed through the Cr-depleted region. Through this combination of high-resolution microscopy and localized passive film removal, we show that, although high-Cr alloys are resistant to intergranular attack and stress corrosion cracking, degradation-induced changes in the underlying metal at grain boundaries make the material more susceptible once the initial passive film is breached.

(S)TEM↗

Exceptional radiation resistance of hardened amorphous SiC under high-temperature hydrogen ion implantation

This study provides a compelling comparison of the structural and mechanical responses of single-crystal silicon carbide (sc-SiC), nanocrystalline silicon carbide (nc-SiC), and amorphous silicon carbide (am-SiC) to hydrogen ion implantation at 650 °C across three distinct fluences: low, medium, and high (LF, MF, HF). While both sc-SiC and nc-SiC exhibit blistering, microcracking, and exfoliation, am-SiC remains free of blisters, demonstrating superior resilience. Notably, nc-SiC, with its high density of stacking faults (SFs), requires a higher fluence to initiate blistering compared to sc-SiC. At high fluences, hydrogen accumulation at grain boundaries (GBs) in nc-SiC elevates internal gas pressure, intensifying exfoliation. In sc-SiC, blistering leads to increased hardness, whereas in nc-SiC, the degradation of the SF structure results in a reduction in hardness. In contrast, am-SiC undergoes structural relaxation during irradiation, resulting in a significant increase in hardness while maintaining its structural integrity, with only the formation of nano-sized spherical bubbles observed. Furthermore, these findings highlight the exceptional suitability of am-SiC for nuclear applications, where resistance to radiation-induced microcracking is critical.

36 MATERIALS SCIENCE↗

Dynamic Modeling of a Solar-To-Hydrogen Flexible High Temperature Steam Electrolysis Plant

Sustainble hydrogen production for use as a renewable combustible fuel and clean chemical feedstock is an important objective as the world moves towards a renewable energy future. High temperature steam electrolysis is a promising hydrogen production technology due to its reduced electric input that is offset by heat input into steam generation and steam superheating. An option to provide this heat is to use concentrating solar thermal technology that can sustainably provide heat input while renewable electricity is used for the electrolysis reaction. In this work, a solar-to-hydrogen high temperature steam electrolysis plant is designed and dynamically modeled, showing continuous hydrogen production by utilizing supplemental heating and efficient recuperative heating from the electrolysis product streams. Through this design, over 90% of the required heat input for the process can by met by a combination of solar and recuperative heat. Additionally, the plant can flexibility operate by ramping down hydrogen production and through flexible heat integration, which intelligently integrates solar heat based on solar conditions. Smooth operation with flexible hydrogen production is demonstrated which decreases electrical input during on-peak grid times and also decreases the total supplemental heat load over the course of a day from 26.1% to 24.5%. In addition, by using flexible heat integration, the plant can increase its solar heat usage by 4.1% relative to a base case. Both options for flexibility show efficient use of solar thermal energy to sustainably and continuously produce hydrogen.

Immonen, Jake (ORCID:0000000341231625)↗

Magnetic field screening in hydrogen-rich high-temperature superconductors

In the last few years, the superconducting transition temperature, T c , of hydrogen-rich compounds has increased dramatically, and is now approaching room temperature. However, the pressures at which these materials are stable exceed one million atmospheres and limit the number of available experimental studies. Superconductivity in hydrides has been primarily explored by electrical transport measurements, whereas magnetic properties, one of the most important characteristic of a superconductor, have not been satisfactory defined. Here, we develop SQUID magnetometry under extreme high-pressure conditions and report characteristic superconducting parameters for Im-3m-H 3 S and Fm-3m-LaH 10 —the representative members of two families of high-temperature superconducting hydrides. We determine a lower critical field H c1 of ~0.82 T and ~0.55 T, and a London penetration depth λ L of ~20 nm and ~30 nm in H 3 S and LaH 10 , respectively. The small values of λ L indicate a high superfluid density in both hydrides. These compounds have the values of the Ginzburg-Landau parameter κ ~12–20 and belong to the group of “moderate” type II superconductors, rather than being hard superconductors as would be intuitively expected from their high T c s.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

A High-Temperature Multipoint Hydrogen Sensor Using an Intrinsic Fabry–Perot Interferometer in Optical Fiber

This paper presents a multiplexable fiber optic chemical sensor with the capability of monitoring hydrogen gas concentration at high temperatures up to 750 °C. The Pd-nanoparticle infused TiO 2 films coated on intrinsic Fabry–Perot interferometer (IFPI) array were used as sensory films. Strains induced upon exposure to hydrogen with varied concentrations can be monitored by IFPI sensors. The fiber sensor shows a repetitive and reversible response when exposed to a low level (1–6%) of hydrogen gas. Uniform sensory behavior across all the sensing cavities is demonstrated and reported in this paper.

47 OTHER INSTRUMENTATION↗

Probabilistic Risk Assessment of a Light Water Reactor Coupled with a High-Temperature Electrolysis Hydrogen Production Plant

This paper presents recent updates on the Level 1 Probabilistic Risk Assessment (PRA) of Light Water Reactors (LWRs) coupled with a hydrogen production plant. It provides the overview of past results on the PRA for Pressurized Water Reactors (PWRs) and Boiling Water Reactors (BWRs) coupled to a 1150 MW High Temperature Electrolysis Facility (HTEF), as well as the latest research results for a smaller 100 MW HTEF facility. Differences between the two HTEF designs are listed. Key differences include the amount and quality of diverted LWR steam, complexity of the Heat Extraction System (HES), and the electrical power source for the HTEF plant. A Failure Mode and Effect Analysis (FMEA) was conducted for the new HTEF design, and the LWR PRA models were modified in the SAPHIRE risk assessment tool to account for the newly identified risk contributors. These include the steam loss event at the HES system, the electrical overcurrent event at the HTEF facility and at the transmission line from the LWR plant, and the hydrogen detonation event at the HTEF facility. The coupling of LWRs with a 100 MW HTEF increases the frequency of several initiating events. For the reference PWR, the largest frequency increase is for the steam line break event at 5.5%. While for the reference BWR, the largest frequency increase is for the switchyard-related Loss of Offsite Power (LOOP) event at 0.11%. The overall plant risk increases by 6.56% and 0.03% for PWR and BWR reference plants respectively. It is found that these risk metrics satisfy the safety criteria of both 10 CFR 50.59 and Regulatory Guide 1.174 licensing pathways.

08 HYDROGEN↗

Probabilistic Risk Assessment of a Light-Water Reactor Coupled with a High-Temperature Electrolysis Hydrogen Production Plant

This report details an expansion of the original two generic probabilistic risk assessments (PRAs) for the addition of a heat extraction system (HES) to a light-water reactor, one for a pressurized-water reactor and one for a boiling-water reactor. The new material in this revision includes a new HES design, direct electrical coupling of the nuclear power plant to the High-Temperature Electrolysis Facility (HTEF), and a smaller 100-MWt HTEF analysis. The results investigate the applicability of the potential licensing approaches, which do not require a full United States Nuclear Regulatory Commission licensing review. The PRAs are generic and include some assumptions. We eliminated many conservative assumptions from the preliminary pressurized-water reactor PRA report using design data for both the HES and HTEF. The PRA results indicate that the 10 CFR 50.59 licensing approach is justified due to the minimal increase in initiating event frequencies for all design basis accidents, with none exceeding 5.6%. The PRA results for core damage frequency and large early release frequency support the use of RG 1.174 as further risk information that supports a change without a full licensing amendment review. Further insights provided through hazard analyses and sensitivity studies confirm with high confidence that the safety case for licensing an HES addition and an HTEF sited 1.0 km from the nuclear power plant is strong and that the placement of a HTEF at 0.5 km is also a viable case. Site-specific information can alter these conclusions.

08 HYDROGEN↗

Probabilistic Risk Assessment of a Light Water Reactor Coupled with a High Temperature Electrolysis Hydrogen Production Plant

Two generic probabilistic risk assessments (PRA) for the addition of a heat extraction system (HES) addition to a light water reactor (LWR) are performed, one for a pressurized water reactor (PWR) and one for a boiling water reactor (BWR). The results investigate the applicability of the potential licensing approaches which do not require a full U.S. Nuclear Regulatory Commission (NRC) licensing review. The PRAs are generic, and some assumptions are made. Many conservative assumptions from a the preliminary PWR PRA report were eliminated using design data for both the HES and the high temperature electrolysis facility (HTEF). The results of the PRA indicate that the 10 CFR 50.59 licensing approach is justified due to the minimal increase in initiating event frequencies for all DBAs, none exceeding 5.6%. The PRA results for CDF and LERF support the use of RG 1.174 as further risk information that supports a change without a full LAR. Further insights provided through hazard analysis and sensitivity studies confirm with high confidence that the safety case for licensing an HES addition and a HTEF sited at 1.0 km from the NPP is strong and that the placement of a HTEF at 0.5 km is a viable case. Site specific information can alter these conclusions.

29 ENERGY PLANNING, POLICY, AND ECONOMY↗

Developing a low-cost renewable supply of hydrogen with high-temperature electrochemistry

Abstract Producing inexpensive hydrogen using electricity to split water or to extract hydrogen from hydrocarbon compounds is a two-sided coin: one side is obtaining and exploiting low-cost, emissions-free energy sources while the opposite side is establishing low-cost robust, durable, and efficient materials for the conversion processes. This article explores the materials needed for water splitting electrolysis, electrochemical abstraction of hydrogen from light alkanes, and looping thermal-chemical reaction processes that typically form and then dissociate an acid compound in a two- or three-step process. The focus is on the R&D needs of materials that are used for high-temperature electrochemistry, focusing on solid-oxide, ion-conducting cell materials sets (SOECs). To exploit the availability of low-cost electricity, these materials must stand up to cyclic operations. They also must be durable for years of service to reduce operating and maintenance costs, and they must achieve high conversion efficiencies to avoid large, energy-intensive recycle loops. Graphical abstract

Boardman, Richard D.↗

A scaling law of the neutral penetration length and Balmer- α wing shape in high-temperature plasmas

Hydrogen atoms penetrating deep inside high-temperature magnetically confined plasmas by repetitive charge-exchange collisions result in a particle source of the plasma, which affects the plasma transport significantly. In this paper, we present an approximate solution of the fluid equations for neutral transport and an analytical representation of the neutral penetration length, in a simplified plasma geometry. This analysis predicts a power-law decay in the Balmer-α line wings which reflects the velocity distribution of the neutral atoms, with the power-law exponent analytically represented as well. These scaling laws are compared with a simple Monte–Carlo simulation and spectroscopic observations of Large Helical Device plasmas. Since the Balmer-α line wings are experimentally accessible, our formulation opens the possibility to quickly estimate the neutral penetration length from spectroscopic observations.

neutral opacity↗

Stoichiometric effects on grain growth in zirconium carbide coatings for high-temperature nuclear fuel

Interest in coated particle fuel for space nuclear propulsion (SNP) has expanded in recent years due to successful demonstrations of the resiliency of the coatings to extreme environments. For SNP applications, the coating layer for the particle design needs to be able to withstand exposure to high temperature hydrogen during operating conditions. ZrC has been proposed as a protective layer, however, it is important to understand the high temperature behavior to ensure adequate protection to this fuel. In this study, surrogate ZrC coated particles were heat treated at 1900 °C up to 300 min, to examine how the microstructure evolves when exposed to high temperature. Scanning electron microscopy and electron backscatter diffraction (EBSD) were conducted to determine grain size and grain boundary character and orientation to determine the degree of change in the ZrC layer post heat treatment. Raman spectroscopy provided insight to understand how the as-fabricated stoichiometry of each sample contributed to the differences in grain growth behavior. Despite the as-fabricated samples showing a similar initial grain size and grain boundary character, the samples with a higher amount of excess carbon exhibited smaller grain areas and slower growth rates when exposed to 1900 °C. In conclusion, this investigation details the as-fabricated microstructure of the ZrC layer, specifically grain size, evolved under high temperature as this can impact the performance of the fuel under operating conditions.

EBSD↗