At least 19 records

Mechanistic insight into the effects of A-site doping in perovskite nanorods on interfacial Li-ion and Na-ion transport in polymer–perovskite composite electrolytes

Composite polymer electrolytes (CPEs) offer a promising pathway to safer and higher energy density electrochemical energy storage yet optimizing interfacial ion transport remains a critical challenge due to high resistances and a lack of understanding of the complex interfacial electrostatic interactions. This work investigates the mechanistic origins of the interfacial ion transport enhancement in single-ion conducting (SIC) polymer electrolytes filled with A-site disordered perovskite LaxMyTiOz (LMTO) (M = Li, Na, K) nanorods. By integrating Density Functional Theory (DFT) with broadband dielectric spectroscopy (BDS) and pulsed-field-gradient NMR (PFG-NMR), we analyze the ion transport behavior in Li-based and Na-based SIC systems containing compositionally distinct LMTO fillers (LMTO800 and LMTO900). Specifically, we introduce the site-to-site energy difference (ΔE) descriptor, which extends beyond single-site descriptors such as adsorption energy and ion binding energies. We demonstrate that ΔE together with ion binding energies provide a more comprehensive picture of the energy landscape at the polymer–ceramic interface. The combined DFT and experimental results show that A-site doping in the ceramic filler can effectively modulate ΔE and ion binding energies, creating a favorable potential energy landscape that promotes enhanced ion transport along the interface. This comprehensive study illustrates the impact of ceramic compositional tuning on interfacial ion transport and provides materials design rules towards real-world applications.

B shepard, Lauren [Pennsylvania State University]↗

Localized High Concentration Electrolytes for High Voltage Lithium-Metal Batteries: Correlation between the Electrolyte Composition and Its Reductive/Oxidative Stability

We demonstrate a first-principles screening methodology as an effective tool to explore electrolyte formulations for the new generation of high energy density rechargeable batteries. We study the liquid structure and electronic properties in dilute electrolytes, high concentration electrolytes (HCE), and localized high concentration electrolytes (LHCE), with focus on electrolyte formulations based on lithium bis(fluorosulfonyl)imide (LiFSI), dimethyl carbonate (DMC), and bis(2,2,2-trifluoroethyl) ether (BTFE) as a diluent. We describe the solvation complexes in the dilute electrolyte and explore structural changes triggered by the increase in lithium salt concentration for HCEs and the diluent effects in LHCEs. In HCE formulations, there is a 4-fold coordination environment of lithium-ions as in the dilute electrolyte, but the number of lithium-ion interactions with O atoms from FSI- anions dominates. In these solutions, the ability of the FSI- anions to interact with multiple lithium-ions allows complex 3D network formation and influences the reductive/oxidative behavior of the electrolyte. Interestingly, in LHCEs, the BTFE diluent molecules do not change the 3D solution structure when diluting the HCE formulation from 5.49 to 3.83 M. However, there is a composition threshold where the structural and electronic behavior may change. We show that diluting the HCE electrolyte with BTFE down to 1.77 M breaks the three-dimensional solution structure into an island-like solvation complex. We relate these structural changes to the electronic properties of the electrolytes finding a causal relationship between the reductive/oxidative behavior and the lithium-oxygen interaction mechanisms in the solvated complexes. The coordination with lithium-ions lowers the electrolyte LUMO and HOMO levels: the higher is the number of interactions with lithium-ions, the more likely the solvent molecule, FSI- anion, or diluent molecule is to be reduced and the less likely it is to become oxidized. The evolution of the solvated ion structure in HCE and LHCE suggests a close connection to a corresponding change in the lithium-ion transport mechanisms for these electrolytes.

anions, molecules, oxygen, solvents, electrolytes↗

Effect of Background Electrolyte Composition on the Interfacial Formation of Th(IV) Nanoparticles on the Muscovite (001) Basal Plane

Understanding the impact of actinide nanoparticle (NP) formation is important to assess radionuclide mobility in the environment. We combined surface X-ray diffraction (SXRD) and in situ AFM to investigate the previously reported unusual electrolyte effects on Th uptake on mica. At low [Th] (0.1 mM), interfacial structures show a broad Th electron density (~50 Å). A linear decrease of Th uptake with decreasing hydration enthalpy of the electrolyte cation (Li+, K+, NH4+, and Cs+) indicates a competitive effect between Th and the electrolyte cation. Na+ is a clear outlier from this trend. In situ AFM imaging confirms the results. Particles show a vertical size of ~1–2 nm and larger lateral dimensions of ~10–20 nm, which is typical for particles formed at interfaces (heterogeneous nucleation). At high [Th] = 1 and 3 mM, all investigated electrolytes (ACl, A = Li+, Na+, K+) show similar Th uptake, indicating a much smaller impact of electrolyte composition. The interfacial structures are dominated by a high Th loading at a distinct distance (~6.5 Å) from the surface. Therefore, the main retention mechanism at high [Th] is suggested to be the sorption of Th NPs aggregated from Th oligomers present in solution (homogeneous nucleation).

Neumann, J↗

Solid-state rigid-rod polymer composite electrolytes with nanocrystalline lithium ion pathways

A critical challenge for next-generation lithium-based batteries lies in development of electrolytes that enable thermal safety along with use of high-energy-density electrodes. We describe molecular ionic composite (MIC) electrolytes based on an aligned liquid crystalline polymer combined with ionic liquids and concentrated Li salt. This high strength (200 MPa) and non-flammable solid electrolyte possesses outstanding Li + conductivity (1 mS cm -1 at 25 °C) and electrochemical stability (5.6 V vs Li|Li + ) while suppressing dendrite growth and exhibiting low interfacial resistance (32 Ω cm 2 ) and overpotentials (≤ 120 mV @ 1 mA cm -2 ) during Li symmetric cell cycling. A heterogeneous salt doping process modifies a locally ordered polymer-ion assembly to incorporate an inter-grain network filled with defective LiFSI & LiBF 4 nanocrystals, strongly enhancing Li + conduction. Furthermore, this modular material fabrication platform shows promise for safe and high-energy-density energy storage and conversion applications, incorporating the fast transport of ceramic-like conductors with the superior flexibility of polymer electrolytes.

25 ENERGY STORAGE↗

Room Temperature to 150 °C Lithium Metal Batteries Enabled by a Rigid Molecular Ionic Composite Electrolyte

Molecular ionic composites (MICs), made from ionic liquids and a rigid-rod polymer poly(2,2'-disulfonyl-4,4'-benzidine terephthalamide) (PBDT), are a new type of rigid gel electrolyte that combine fast ion transport with high thermal stability and mechanical strength. In this work, a MIC electrolyte membrane is prepared that is composed of PBDT, lithium bis(trifluoromethylsulfonyl)imide (LiTFSI), and 1-butyl-1-methylpyrrolidinium bis(trifluoromethylsulfonyl)imide (Pyr 14 TFSI) in a mass ratio of 10:10:80. The ionic conductivity at 25 °C is 0.56 mS cm –1 with no added flammable/volatile components. Although the polymer content is only 10 wt%, this MIC membrane is rigid with a tensile modulus of 410 MPa at room temperature. The MIC membrane remains stable and rigid at 200 °C with the shear storage modulus (G') only slightly decreasing by 35%. Li/MIC/LiFePO 4 cells demonstrate stable cycling performance over a wide temperature range from 23 to 150 °C. The specific discharge capacity at 100 and 150 °C at 1 C rate exceeds 160 mAh g –1 . The discharge capacity retention is 99% after 50 cycles at 150 °C. Furthermore, this stable battery performance shows that this low polymer content MIC membrane qualifies for use as a solid electrolyte in lithium metal batteries operating over a wide temperature range.

25 ENERGY STORAGE↗

Transport and mechanical behavior in PEO-LLZO composite electrolytes

Abstract Composite solid electrolytes (CEs), wherein ion-conducting polymer and ceramic/glass is mixed, are promising candidates for all-solid-state batteries due to their promise of acceptable ionic conductivity and mechanical properties compared to their individual constituents. While numerous studies have focused on improving the performance of CEs, it is still unclear what the material targets are that can result in improved macroscopic performance especially in light of the coupled needs for high transport and high mechanical strength in these materials. In this study, a two-dimensional (2D) mathematical model is developed to investigate electrochemical and mechanical characteristics of CEs. The model is compared to CEs consisting of poly-ethylene-oxide (PEO) polymer and lithium lanthanum zirconium oxide (LLZO) ceramic material with examination of the impact of varying LLZO volume fractions. The potential drop at the PEO-LLZO interface is evaluated using the junction potential theory. Using experimental data from the literature, the model estimates the ionic conductivity, effective transference number, and mechanical stiffness of the CEs. While the mechanical stiffness improves with increasing volume fraction of LLZO, the impact on conductivity and transference number depends on interfacial resistance at the interface. Finally, the study reports CE’s potential to enhance Li-ion transport and mechanical properties to inhibit lithium (Li) dendrite growth.

25 ENERGY STORAGE↗

Role of Scaffold Architecture and Excess Surface Polymer Layers in a 3D-Interconnected Ceramic/Polymer Composite Electrolyte

3D-interconnected ceramic/polymer composite electrolytes offer promise to combine the benefits of both ceramic and polymer electrolytes. However, an in-depth understanding of the role of the ceramic scaffold's architecture, and the associated polymer/ceramic interfaces on the electrochemical properties of such composite electrolytes is still incomplete. Here, these factors are systematically evaluated using an interconnected composite electrolyte with a tunable and well-defined architecture. The ionic conductivity of the ceramic scaffold is strongly dependent on its porosity and tortuosity, as demonstrated experimentally and via theoretical modeling. The connectivity of the ceramic framework avoids the high interfacial impedance at the polymer/ceramic electrolyte interface within the composite. However, this work discovers that the interfacial impedance between the bulk composite and excess surface polymer layers of the composite membrane dominates the overall impedance, resulting in a 1–2 order drop of ionic conductivity compared to the ceramic scaffold. Despite the high impedance interfaces, an improved Li + transference number is found compared to the neat polymer (0.29 vs 0.05), attributed to the ceramic phase's contributions toward ion transport. Further, this leads to flatter overpotentials in lithium symmetric cell cycling. These results are expected to guide future research directions toward scalable manufacturing of composite electrolytes with optimized architecture and interfaces.

25 ENERGY STORAGE↗

Particle‐Size‐Dependent Lithium‐Ion Transport in PEO/LLZO Composite Electrolytes

Lithium-metal batteries with solid electrolytes can deliver higher energy density and improved safety than conventional Li-ion batteries. Among solid electrolyte candidates, polymer/ceramic composite electrolytes are attractive because they combine polymer flexibility with the high ionic conductivity of ceramics. However, whether ceramic fillers synergistically reduce polarization losses in the polymer matrix remains unclear. A central unknown is the critical polymer/ceramic interfacial resistance (Rint,crit), below which adding ceramics lowers electrolyte overpotential. Here, we present the first macroscale model framework to quantify R int,crit for composite electrolytes based on polyethylene oxide (PEO) and Ta-doped Li 7 La 3 Zr 2 O 12 (LLZO). A 1D model for DC-polarization of tri-layer cells (PEO-LiTFSI/LLZO/PEO-LiTFSI) shows that LLZO surface functionalization reduces the PEO/LLZO interfacial resistance, consistent with electrochemical impedance measurements. Extending to a 2D composite model, we show notably that Rint,crit scales linearly with LLZO particle diameter and shifts toward experimentally accessible values (e.g., 28.8 Ωcm 2 ) as particle size increases. At fixed ceramic volume fraction, larger LLZO particles reduce the number of interfacial crossings, driving more current through the ceramic phase and lowering concentration polarization. In contrast, R int,crit is largely independent of ceramic volume fraction. These results demonstrate that ceramic filler-size engineering can enable synergistic, energy-efficient transport in polymer/ceramic composite electrolytes.

25 ENERGY STORAGE↗

Chemical Heterogeneity in PAN/LLZTO Composite Electrolytes by Synchrotron Imaging

Solid polymer/ceramic composite electrolytes are promising for batteries due to their attractive thermal stability and mechanical properties. Chemical heterogeneity in solid composite electrolytes, such as the inhomogeneity in the ceramic phase and salt distribution at the polymer/ceramic interface, is critical to the performance of solid composite electrolytes. However, such heterogeneity has not been well understood yet. In this work, we use Synchrotron-based X-ray fluorescence imaging (XRF) and Transmission X-ray Microscope (TXM) to image nanoscale chemical heterogeneity in polyacrylamide/Li 7+x La 3 Zr 2–x Ta x O 12 (LLZTO) composite electrolytes and investigate the effects of lithium salt, salt concentration, and plasticizer. We find that LLZTO particles show strong inter- and intra-particles chemical heterogeneities, and the off-stoichiometry of Zr in an LLZTO particle is unlikely to be only balanced by Ta substitution. Moreover, statistical analysis suggests that LiI tends to accumulate at the ceramic/polymer interface at a low concentration of 5 wt%, but no such tendency was observed in samples with 10 wt% LiI. However, composite electrolytes with LiTFSI show interfacial accumulation at both 5 wt% and 10 wt%. Furthermore, this report provides insight into element distributions in solid composite electrolytes, and we hope further researches can shed light on the connections between chemical heterogeneity and ionic transport pathway inside.

36 MATERIALS SCIENCE↗

Gel electrolyte composite including ionic liquid and zwitterionic polymer scaffold

A gel electrolyte composite containing a nonvolatile electrolyte and a zwitterionic polymer scaffold in which the non-volatile electrolyte is a non-lithium-containing ionic liquid, a sodium-containing ionic liquid, or a lithium-containing ionic liquid and the zwitterionic polymer scaffold is formed from one or more zwitterionic monomers only or both one or more zwitterionic monomers and one or more non-zwitterionic monomers. The zwitterionic polymer scaffold contains 8 mol % or higher of zwitterions relative to the total content of the gel electrolyte composite when the nonvolatile electrolyte is a non-lithium-containing ionic liquid, and contains 1 mol % or higher of zwitterions relative to the total content of the gel electrolyte composite when the nonvolatile electrolyte is a sodium-containing ionic liquid or a lithium-containing ionic liquid. Also disclosed are a method of preparing the above-described gel electrolyte composite and an electrochemical energy storage device containing same.

D'Angelo, Anthony J.↗

Methods of enhancing conductivity of a polymer-ceramic composite electrolyte

Methods for enhancing conductivity of polymer-ceramic composite electrolytes are provided which include forming a polymer-ceramic composite electrolyte film by a melt casting technique and uniaxially stretching the film from about 5 to 15% in length. The polymer-ceramic composite electrolyte is also preferably annealed after stretching such that it has a room temperature conductivity of from 10.sup.-4 S cm.sup.-1 to 10.sup.-3 S cm.sup.-1. The polymer-ceramic composite electrolyte formed by the methods of the present invention may be used in lithium rechargeable batteries.

Kumar, Binod↗

SEI formation mechanisms and Li + dissolution in lithium metal anodes: Impact of the electrolyte composition and the electrolyte-to-anode ratio

The lithium metal battery is one of today's most promising high-energy-density storage devices. Its full-scale implementation depends on solving operational and safety issues intrinsic to the Li metal high reactivity leading to uncontrolled electrolyte decomposition and uneven Li deposition. In this work, we study the spontaneous formation of the solid electrolyte interphase (SEI) upon contact of Li metal with the electrolyte and describe the heterogeneous SEI morphological features. Multiple electrolyte formulations based on lithium bis(fluorosulfonyl)imide (LiFSI), dimethoxyethane (DME), dimethyl carbonate (DMC), 1,2,2-tetrafluoroethyl-2,2,3,3-tetrafluoropropyl ether (TTE) and bis(2,2,2-trifluoroethyl) ether (BTFE) are used. Findings include the description of the SEI evolution from dispersed LiO, LiS, LiN, and LiF clusters to a continuous and compact inorganic phase in which the LiO and LiF content depend on the presence of fluorine diluents. Further, the role of the DME ether solvent helping the growth of a “wet-SEI” is compared to that of the highly unstable carbonate DMC, which decomposes into complex radical oligomers that might contribute to further electrolyte decomposition. The impact of the electrolyte-to-anode ratio on LiFSI decomposition is highlighted. Finally, we suggest the existence of a critical LiFSI concentration and electrolyte-to-anode ratio that could potentially balance the rate of electrolyte depletion and lithium consumption.

25 ENERGY STORAGE↗

Electrolyte compositions comprising ionic liquids and metal hydride batteries comprising same

Electrolyte compositions comprising a) an ionic liquid and b) a protic acid and/or an organic solvent are suitable for use in electrochemical cells, e.g. metal hydride batteries. The electrolyte compositions may replace the currently employed 30% by weight aqueous KOH. Suitable protic acids include carboxylic acids, mineral acids, sulfonic acids and the like. Suitable organic solvents include organic carbonates, ethers, glymes, ortho esters, polyalkylene glycols, esters, lactones, glycols, formates, sulfones, sulfoxides, amides, alcohols, ketones, nitro solvents, nitrile solvents and combinations thereof. Present batteries may achieve a nominal open-circuit voltage of >1.2 V (volts) and up to about 6 V. The electrolyte compositions allow enlargement of the electrochemical window, thus allowing the use of further cathode active materials. Further cathode active materials include transition metals and their oxides, hydroxides and fluorides; for example, Sc, Ti, V, Cr, Mn, Fe, Co, Ni, Cu, Zn, Y, Zr, Nb, Mo, Tc, Ru, Rh, Pd, Ag, Cd, Lu, Hf, Ta, W, Re, Os, Ir, Pt and Au and their oxides, hydroxides, oxide/hydroxides and fluorides.

25 ENERGY STORAGE↗

Polymer–Ceramic Composite Electrolytes for Lithium Batteries: A Comparison between the Single-Ion-Conducting Polymer Matrix and Its Counterpart

Single-ion-conducting polymer electrolytes are attractive to use in lithium batteries as the transference number of the lithium cation approaches unity. This helps prevent concentration gradients across the electrolyte, which can result in dendrite formation. The addition of ceramic particles to polymer electrolytes at high loadings can increase the mechanical strength of the polymer, which can also help suppress dendrite formation. Here, a single-ion-conducting polymer electrolyte is blended with lithium-conducting oxide ceramic particles to make a composite electrolyte. This electrolyte is studied in comparison to a composite electrolyte containing freely dissolved lithium salt. It is found that the addition of ceramic particles to the single-ion-conducting polymer can result in increased cation dissociation and consequent increased ionic conductivity. The electrolytes are cycled in lithium symmetrical cells, and it is found that the ceramic-containing electrolytes show increased interfacial stability with the lithium metal compared to the pristine polymer electrolytes. Our findings shed light on how to optimize the polymer host chemistry to form composite electrolytes that can meet the challenging requirements to stabilize the lithium metal anode.

25 ENERGY STORAGE↗

Critical role of polymer-ceramic ion exchange for high conductivity composite electrolytes

Polymer-ceramic composites offer a path to enhance the transport and mechanical properties of solid electrolytes. However, an in-depth understanding of the extent and role of ion transport along and across polymer-ceramic interfaces in these systems is lacking. We have recently shown that Li-conducting Li 0.11 Na 0.24 K 0.02 La 0.43 TiO 2.82 (LMTO) nanorods can be prepared by a molten flux method, and the addition of 30–50 weight (wt.)% LMTO to a bis[(trifluoromethyl)sulfonyl]imide-vinyl ethylene carbonate-based single-ion conducting (SIC) polymer electrolyte leads to a two-fold enhancement in Li-ion conductivity, from 1.4 to 3.0 × 10 −5 S/cm at 30 °C. In the present study, we use NMR methods to identify the Li-ion transport pathways and determine the timescale of chemical exchange between the SIC polymer and LMTO ceramic components. Tracer exchange NMR indicates preferential transport through the polymer or polymer-interfacial regions, and exchange spectroscopy (EXSY) and a new isotope exchange method reveal negligible Li exchange between the SIC polymer and LMTO ceramic up to several days. Here, LMTO nanorods act as a passive filler. Our results further highlight that significant (e.g., 10- or 100-fold) conductivity enhancements in composite electrolytes can only be achieved 1) with ionically-conductive fillers, and 2) when both the ceramic and polymer components actively participate in long-range transport. For this, fast interfacial ion exchange is needed. In conclusion, this leads us to introduce a critical interfacial ion exchange time to evaluate whether a filler actively contributes to conduction in a composite electrolyte, and screen for promising polymer-ceramic pairings to accelerate the development of high conductivity solid electrolytes.

Battery, Solid electrolyte↗

Structural effects of composition tuning in A-site disordered perovskite La0.5Li0.5−xMxTiO3 (M = Na, K) nanorods for fast interfacial transport for solid composite electrolyte design

Polymer-ceramic composite electrolytes (CPE) have emerged as promising replacements for currently used liquid organic electrolytes, which pose as safety hazards, in Li-ion batteries. Limits in conductivity enhancement in CPEs is often attributed to a high resistance for Li-ion transport along the interface due to the incompatibility of the polymer and ceramic phases. A clear understanding of the interfacial structure and how this impacts interfacial Li-ion transport is needed in order to efficiently design a CPE with optimal ionic conductivity. In this study, density functional theory (DFT) calculations, in conjunction with scanning transmission electron microscopy (STEM) and electron energy loss spectroscopy (EELS), are used to unveil the bulk and surface structure of La0.5Li0.5−xMxTiO3 (M = Na, K) (LMTO) nanorods, a newly-reported ceramic system with promising applications in CPEs, and the LMTO interactions with the poly(lithium sulfonyl (trifluoromethane sulfonyl)imide methacrylate) (p(MTFSILi)) polymerized ionic liquid. Substitution of lithium for sodium and potassium onto the A-site perovskite lattice is shown to increase the stability of the preferred pseudocubic perovskite phase because of their increased cation size which allows them to reduce the TiO6 octahedral rotations in the bulk and at the surface. STEM and EELS results show that LMTO nanorods with differing compositions have Ti-enriched (110)-oriented surfaces. Increased sodium and potassium compositions in LMTO is also shown using the DFT calculations to weaken the binding of the lithium atom to the MTFSI unit when LiMTFSI is adsorbed to the LMTO surface. This weakening of lithium binding to the polymer at the LMTO interface indicates that the lithium mobility is increased, correlating to an increase in interfacial Li-ion transport. Overall, this work provides insights into how to tune the interfacial interactions between the polymer (p(MTFSI)) and ceramic (LMTO) for optimal CPE design.

Shepard, Lauren B [Pennsylvania State University, ↗

Polymer-ceramic composite electrolytes for all-solid-state lithium batteries: Ionic conductivity and chemical interaction enhanced by oxygen vacancy in ceramic nanofibers

Perovskite Li 3x La 2/3-x TiO3 (LLTO) nanofibers have been heat-treated in the hydrogen-containing atmosphere and then incorporated with the poly(vinylidene fluoride)-co-hexafluoropropylene (PVDF-HFP) polymer to form a composite electrolyte. Hydrogen treatment has created oxygen vacancies in the LLTO nanofibers, which has reduced the activation energy of Li ion transport along intra-grains and inter-grains, leading to improvement in the ion conductivity of LLTO nanofibers. Hydrogen treatment of the LLTO nanofibers has also enhanced the chemical interaction between the LLTO nanofibers and the polymer matrix in the composite electrolyte, and favored the Li ion transport at the nanofiber/polymer interface, improving the ion conductivity of the composite electrolyte to 3.4×10- 4 S/cm at room temperature. As a result, the Li|composite-electrolyte|Li half-cell exhibits good stability during lithium plating/stripping cycling at room temperature, showing an overpotential of ~91 mV at a constant current density of 0.5 mA/cm 2 . Finally, the full-cell battery with the composite electrolyte, lithium metal anode and lithium iron phosphate cathode shows excellent rate capacity and cycling performance.

25 ENERGY STORAGE↗