At least 19 records

Cation Vacancies Enable Anion Redox in Li Cathodes

Conventional Li-ion battery intercalation cathodes leverage charge compensation that is formally associated with redox on the transition metal. Employing the anions in the charge compensation mechanism, so-called anion redox, can yield higher capacities beyond the traditional limitations of intercalation chemistry. Here, we aim to understand the structural considerations that enable anion oxidation and focus on processes that result in structural changes, such as the formation of persulfide bonds. Using a Li-rich metal sulfide as a model system, we present both first-principles simulations and experimental data that show that cation vacancies are required for anion oxidation. First-principles simulations show that the oxidation of sulfide to persulfide only occurs when a neighboring vacancy is present. To experimentally probe the role of vacancies in anion redox processes, we introduce vacancies into the Li 2 TiS 3 phase while maintaining a high valency of Ti. When the cation sublattice is fully occupied and no vacancies can be formed through transition metal oxidation, the material is electrochemically inert. Upon introduction of vacancies, the material can support high degrees of anion redox, even in the absence of transition metal oxidation. The model system offers fundamental insights to deepen our understanding of structure–property relationships that govern reversible anion redox in sulfides and demonstrates that cation vacancies are required for anion oxidation, in which persulfides are formed.

25 ENERGY STORAGE↗

Short Range Order in Disordered Spinel and the Impact on Cation Vacancy Transport

Spinels are important complex oxides for use in radiation damage environments and resulting from the corrosion of steels. It is known that, in these environments, normal spinels exist with some concentration of antisite cation pairs known as inversion. In this work we show that even in highly disordered states characterized by high levels of inversion, spinel still shows some short range order (SRO) that manifests itself in antisite chains. The propensity to form these antisite chains is confirmed through Monte Carlo simulations which find that the length of chains which can form depend on the spinel chemistry. We also consider the effect of antisite chains on the diffusivity of cation vacancies and find the effect strongly depends on the spinel chemistry. At the extremes, chains in FeCr2O4 significantly increase vacancy transport but in MgAl2O4 chains have the inverse effect of drastically reducing vacancy mobility. The explanation of these dramatically different effects results from the assessment of the thermodynamic stability of the antisite chains and contrasting attractive/repulsive interactions of vacancies with the chains.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Embedding Reverse Electron Transfer Between Stably Bare Cu Nanoparticles and Cation‐Vacancy CuWO 4

Cu nanoparticles (NPs) have attracted widespread attention in electronics, energy, and catalysis. However, conventionally synthesized Cu NPs face some challenges such as surface passivation and agglomeration in applications, which impairs their functionalities in the physicochemical properties. Here, the issues above by engineering an embedded interface of stably bare Cu NPs on the cation-vacancy CuWO 4 support is addressed, which induces the strong metal-support interactions and reverse electron transfer. Various atomic-scale analyses directly demonstrate the unique electronic structure of the embedded Cu NPs with negative charge and anion oxygen protective layer, which mitigates the typical degradation pathways such as oxidation in ambient air, high-temperature agglomeration, and CO poisoning adsorption. Kinetics and in situ spectroscopic studies unveil that the embedded electron-enriched Cu NPs follow the typical Eley-Rideal mechanism in CO oxidation, contrasting the Langmuir-Hinshelwood mechanism on the traditional Cu NPs. This mechanistic shift is driven by the Coulombic repulsion in anion oxygen layer, enabling its direct reaction with gaseous CO to form the easily desorbed monodentate carbonate.

Cu nanoparticles↗

Pressure-induced cation and vacancy disorder-order transition and near-zero τ f in deficient hexagonal perovskite Ba 8 ZnTa 6 O 24 dielectrics

Pressure applications can enable the tuning of atomic/defect ordering and provide access to new functional materials. Here, in this study, we report that pressure-induced structural transformation featuring disorder-order transition of both cations and vacancies in the 8-layer deficient hexagonal perovskite tantalate dielectrics Ba 8 ZnTa 6 O 24 , which transformed the structure from twin to shift and remarkably lowered the temperature coefficient of resonant frequency τ f down to near zero (∼0.56 ppm/°C) from 38 ppm/°C for the twinned precursor. The atomic scale STEM-HAADF and EDS results confirm the ordering of Zn in the Ta host at the nanometer scale in the shifted material featuring well-ordered Ba 8 ZnTa 6 O 24 slabs intergrown with Ba 3 ZnTa 2 O 9 and Ba 5 Ta 4 O 15 monolayers and anti-phase grain boundaries as planar defects. The pressure-induced twin-shift structural transformation of Ba 8 ZnTa 6 O 24 features the rare constant concentration of the hexagonal stacked layers, which is allowed by the vacancy ordering at the central layers of face-shared octahedral (FSO) trimers avoiding the FSO B-B repulsion, and remarkably the faster cationic ordering kinetics compared with the 2:1 ordered complex perovskites. Although the inclusion of numerous planar defects and the oxidizable atomic defects led to significant p-type conduction and inhomogeneous electrical microstructures, resulting in an extraordinarily high extrinsic dielectric loss for the high-pressure shifted Ba 8 ZnTa 6 O 24 pellet, the intrinsically near-zero τ f could make the shifted Ba 8 ZnTa 6 O 24 perovskite an ideal microwave dielectric resonator candidate if the defects could be eliminated.

high pressure↗

Defect Generation and Evolution in Irradiated Epitaxial Films and Heterostructures of Fe 3 O 4 and Cr 2 O 3

Abstract The functionality of nuclear structural materials, sensors, and microelectronics in harsh environments such as radiation relies on understanding defect generation and evolution processes in oxide layers. The initial radiation response of epitaxial thin films of Fe 3 O 4 (111), Cr 2 O 3 (0001), and Fe 3 O 4 (111)/Cr 2 O 3 (0001) heterostructures deposited on Al 2 O 3 (0001) by oxygen‐assisted molecular beam epitaxy and irradiated with 200 keV He + is characterized. X‐ray diffraction and X‐ray absorption near edge spectroscopy showed that the Cr 2 O 3 layers underwent significant lattice expansion and disordering under irradiation, whereas the Fe 3 O 4 layers do not exhibit noticeable changes. In contrast, positron annihilation spectroscopy revealed an evolution of cation vacancy point defects in the Fe 3 O 4 layers into larger vacancy clusters with increasing irradiation, while the cation vacancies in Cr 2 O 3 remained primarily as single vacancies and small clusters. The results suggest that the Fe 3 O 4 lattice can utilize the free volume of the larger vacancy clusters to relax but the small vacancies in the Cr 2 O 3 lattice do not facilitate relaxation. Comparing defect concentrations in the single layer films versus the heterostructure suggests that point defects may cross the interface from Fe 3 O 4 into Cr 2 O 3 . Together, these results enhance the understanding of the initial defect evolution mechanisms in oxide layers in harsh irradiation environments.

36 MATERIALS SCIENCE↗

Electrochemical and Chemical Reactivities of Titanium Oxide-Based Materials with a Chloroaluminate Ionic Liquid Electrolyte for Aluminum Batteries

Here, by selecting three different types of electrode materials, we intended to better understand the Al 3+ intercalation chemistry of titanium oxide-based frameworks with an acidic chloroaluminate electrolyte. In agreement with previous reports, we confirmed that the native interstitial sites of anatase TiO 2 are less prone to accommodate Al 3 + than Li + or Na + ions, while introducing cationic vacancies largely increases the electrochemical storage capacity. Upon the first cycle, the highest reversible capacity, up to 277 mAh/g, was obtained for a hydrated layered structure featuring cationic vacancies. Total scattering data showed that the insertion of Al 3+ ions induced a strong distortion of the framework. In addition, combined 27 Al MAS NMR and DFT calculations revealed that in oxy-hydroxylated vacant sites, the coordination mode of Al 3+ ions depends on the arrangement of anions around vacancies inducing the occurrence of 4-, 5-, and 6-fold coordination modes. Further cycling experiments revealed a progressive capacity fading for all electrode materials. Using cyclic voltammetry on the used electrolyte, we evidenced that a partial dissolution has occurred, which is more pronounced for the layered hydrate compound, and that solubilized species are electrochemically active, giving rise to specific signatures in both CVs and galvanostatic experiments. Raman spectroscopy enabled us to characterize these species, which are derived from the Ti-Cl system. The solubilized species, however, eventually precipitated, as shown by a purple deposit observed on the separator and tentatively assigned to TiCl 3 , known to be insoluble in this medium. By providing further information on the Al 3+ intercalation chemistry and a better understanding of the electrochemical and chemical reactivities of electrode materials, this work will enable progress to be made in the development of aluminum-ion batteries.

Al3+-ion insertion chemistry↗

Native point defects in HgCdTe infrared detector material: Identifying deep centers from first principles

We investigate the native point defects in the long-wavelength infrared (LWIR) detector material Hg0.75Cd0.25Te using a dielectric-dependent hybrid density functional combined with spin–orbit coupling. Characterizing these point defects is essential as they are responsible for intrinsic doping and nonradiative recombination centers in the detector material. The dielectric-dependent hybrid functional allows for an accurate description of the bandgap (Eg) for Hg1−xCdxTe (MCT) over the entire compositional range, a level of accuracy challenging with standard hybrid functionals. Our comprehensive examination of the native point defects confirms that cation vacancies VHg(Cd) are the primary sources of p-type conductivity in the LWIR material given their low defect formation energies and the presence of a shallow acceptor level (−/0) near the valence-band maximum. In addition to the shallow acceptor level, the cation vacancies exhibit a deep charge transition level (2−/−) situated near the midgap, characteristic of nonradiative recombination centers. Our results indicate that Hg interstitial could also be a deep center in the LWIR MCT through a metastable configuration under the Hg-rich growth conditions. While an isolated Te antisite does not show deep levels, the formation of VHg–TeHg defect complex introduces a deep acceptor level within the bandgap.

Physics↗

Dopant effect of yttrium and the growth and adherence of alumina on nickel-aluminum alloys

The atom superposition and electron delocalization molecular orbital theory and large cluster models have been employed to study cation vacancy diffusion in alpha-Al2O3 and the bonding of alpha-Al2O3 to nickel, aluminum, and yttrium surfaces. Al(3+) diffusion barriers in alpha-Al2O3 by the vacancy mechanism are in reasonable agreement with experiment. The barrier to Y(3+) diffusion is predicted to be much higher. Since addition of yttrium to transition metal alloys is known to reduce the growth rate and stress convolutions in protective alumina scales, this result suggests the rate-limiting step in scale growth is cation vacancy diffusion. This may partially explain the beneficial effect of yttrium dopants on scale adhesion. The theory also predicts a very strong bonding between alumina and yttrium at the surface of the alloy. This may also be important to the adhesion phenomenon. It is also found that aluminum and yttrium atoms bond very strongly to nickel because of charge transfer from their higher lying valence orbitals to the lower lying nickel s-d band.

Anderson, A. B.↗

Optimizing Li‐Excess Cation‐Disordered Rocksalt Cathode Design Through Partial Li Deficiency

Li-excess disordered rocksalts (DRXs) are emerging as promising cathode materials for Li-ion batteries due to their ability to use earth-abundant transition metals. In this work, a new strategy based on partial Li deficiency engineering is introduced to optimize the overall electrochemical performance of DRX cathodes. Specifically, by using Mn-based DRX as a proof-of-concept, it is demonstrated that the introduction of cation vacancies during synthesis (e.g., Li 1.3-x Mn 2+ 0.4-x Mn 3+ x Nb 0.3 O 1.6 F 0.4 , x = 0, 0.2, and 0.4) improves both the discharge capacity and rate performance due to the more favored short-range order in the presence of Mn3+. Density functional theory calculations and Monte Carlo simulations, in combination with spectroscopic tools, reveal that introducing 10% vacancies (Li 1.1 Mn 2+ 0.2 Mn 3+ 0.2 Nb 0.3 O 1.6 F 0.4 ) enables both Mn 2+ /Mn 3+ redox and excellent Li percolation. However, a more aggressive vacancy doping (e.g., 20% vacancies in Li 0.9 Mn 3+ 0.4 Nb 0.3 O 1.6 F 0.4 ) impairs performance because it induces phase separation between an Mn-rich and a Li-rich phase.

25 ENERGY STORAGE↗

Ionic conductivity and thermoelectric power of pure and Al2O3-dispersed AgI

Ionic and electronic conductivities, and thermoelectric power have been measured for AgI and AgI containing a dispersion of submicron size Al2O3 particles. While the dispersion of Al2O3 enhances the ionic conductivity significantly, it does not affect the electronic properties of the matrix. The enhancement is a strong function of the size and concentration of the dispersoid. Various models have been tested to account for the enhanced conduction. However, the complex behavior of the present results points out the need for more sophisticated theoretical models. Ionic conduction and thermoelectric power data suggest that the dispersed Al2O3 generates an excess of cation vacancies and thereby enhances the conductivity and suppresses the thermoelectric power of the matrix. The individual heats of transport of cation interstitials and vacancies have been estimated and compared to their respective migration energies.

Shahi, K.↗

Oxygen vacancy migration and impact on high voltage DC polarization in 0.8BaTiO 3 –0.2BiZn 0.5 Ti 0.5 O 3

Electrical polarization and defect transport are examined in 0.8BaTiO 3 –0.2BiZn 0.5 Ti 0.5 O 3 , an attractive capacitor material for high power electronics. Oxygen vacancies are suggested to be the majority charge carrier at or below 250°C with a grain conduction hopping activation energy of 0.97 eV and 0.92 eV for thermally stimulated depolarization current (TSDC) and impedance spectroscopy measurements, respectively. At higher temperature, thermally generated electronic conduction with an activation energy of 1.6 eV is dominant. Significant oxygen vacancy concentration is indicated (up to ~1%) due to cation vacancy formation (i.e., acceptor defects) from observed Bi (and likely Zn) volatility. Oxygen vacancy diffusivity is estimated to be 10 -12.8 cm 2 /s at 250°C. Low diffusivity and high activation energies are indicative of significant defect interactions. Dipolar oxygen vacancy defects are also indicated, with an activation energy of 0.59 eV from TSDC measurements. In conclusion, the large oxygen vacancy content leads to a short lifetime during high voltage (30 kV/cm), high temperature (250°C) direct current (DC) electrical measurements.

46 INSTRUMENTATION RELATED TO NUCLEAR SCIENCE AND ↗

The evolution and growth of Al2O3 scales on beta-NiAl

The formation and growth of Al2O3 scales on (beta)-NiAl were studied using electron microscopy and other analytical techniques to gain an understanding of the oxidation properties of (beta)-NiAl and of alumina-forming alloys, in general. The transient and mature stages of oxidation were studied as well as the transformation stage during which the oxide scale transforms from metastable Al2O3 phases to the thermodynamically stable alpha-Al2O3 phase. The transient oxidation stages were studied at 800 deg C and for short times at 1100C. At 800C, the scales consist predominantly of delta-Al2O3 which forms by cation vacancy ordering in the defective spinel lattice of gamma-Al2O3. At 1100C, a fast-growth morphology of theta-Al2O3 forms as a surface layer over delta-Al2O3. For both oxidation temperatures, the scales are often epitaxially oriented with respect to the metal. The transient scales grow by outward cation diffusion as evidenced by surface growth morphologies. The transformation to alpha-Al2O3 occurs within 1 hour at 1100C by a nucleation and radial growth process. The large volume decrease associated with the transformation results in a highly strained alpha-Al2O3 microstructure. A change in scale growth mechanism from outward cation to inward anion diffusion allows transient surface morphologies to be smoothed by surface diffusion. The mature stage of oxidation involves the growth of an alpha-Al2O3 scale having the lacey morphology formed as a result of the gamma yields alpha transformation. Growth of the scale occurs by counterdiffusion along grain boundaries resulting in ridges formed by impingement of alpha-Al2O3 nuclei during the transformation stage. Also scale growth occurs by inward oxygen diffusion through healed cracks; the cracks result from transformation stresses. The measured growth rates of scales having the lacey morphology are an order of magnitude less than fine-grained alpha-Al2O3 scales. Metal orientations were found to have a large effect on oxide morpholoies during all stages of oxidation.

Doychak, J. K.↗

Crystal Chemistry of Meteoritic Hibonites

The characteristics of cation vacancies and site occupancies of natural hibonites in meteors are discussed. Note is taken of the effect of the specific locations of the hibonites in the matrices on the crystal chemistry, electronic stabilities, and spectral features of the metal ions which replace the Al(3+). Hibonites form beta-alumina hexagonal cells with 26 cation sites. Fe cations are found in octahedral, tetrahedral, and five-fold coordinates. Fe(2+) is found in face-shared Al(3) octahedra, a siting explained in terms of ionic radius and crystal field stabilization energy criteria. Spectral colors are attributed to V(3+) and Ti(3+) field transitions at 400 and 700 nm, respectively, although the 700 nm line may arise from transitions of Ti(3+) to Ti(4+) or Fe(2+) to Fe(3+) during heating. Excesses of Mg-26 can be traced to decay of nebular Al-26.

Burns, R. G.↗

Crystal chemistry of meteoritic hibonites

The characteristics of cation vacancies and site occupancies of natural hibonites in meteors are discussed. Note is taken of the effect of the specific locations of the hibonites in the matrices on the crystal chemistry, electronic stabilities, and spectral features of the metal ions which replace the Al(3+). Hibonites form beta-alumina hexagonal cells with 26 cation sites. Fe cations are found in octahedral, tetrahedral, and five-fold coordinations. Fe(2+) is found in face-shared Al(3) octahedra, a siting explained in terms of ionic radius and crystal field stabilization energy criteria. Spectral colors are attributed to V(3+) and Ti(3+) field transitions at 400 and 700 nm, respectively, although the 700 nm line may arise from transitions of Ti(3+) to Ti(4+) or Fe(2+) to Fe(3+) during heating. Excesses of Mg-26 can be traced to decay of nebular Al-26.

Burns, R. G.↗

Complex defect chemistry of hydrothermally-synthesized Nb-substituted β$'$-LiVOPO 4

Lithium vanadyl phosphate (LiVOPO 4 ) is a next-generation multielectron battery cathode that can intercalate up to two Li-ions per V-ion through the redox couples of V 4+ /V 3+ and V 5+ /V 4+ . However, its rate capacity is undermined by the sluggish Li-ion diffusion in the high-voltage region (4 V for V 5+ /V 4+ redox). Nb substitution was used to expand the crystal lattice to facilitate Li-ion diffusion. Here, in this work, Nb substitution was achieved via hydrothermal synthesis, which resulted in a new, lower symmetry β'-LiVOPO 4 phase with preferential Nb occupation of one of the two V sites. This phase presents complex defect chemistries, including cation vacancies and hydrogen interstitials, characterized by a combination of X-ray and neutron diffraction, elemental and thermogravimetric analyses, X-ray absorption spectroscopy, and magnetic susceptibility measurements. The Nb-substituted samples demonstrated improved capacity retention and rate capabilities in the high-voltage region, albeit an enlarged voltage hysteresis related to a partial V 4+ /V 3+ redox reaction, as evidenced by ex situ X-ray absorption spectroscopy and pair distribution function analysis. This work highlights the importance of understanding the complex defect chemistry and its consequence on electrochemistry in polyanionic intercalation compounds.

36 MATERIALS SCIENCE↗

Ultrawide bandgap semiconductor heterojunction p–n diodes with distributed polarization-doped p-type AlGaN layers on bulk AlN substrates

Ultrawide bandgap heterojunction p–n diodes with polarization-induced AlGaN p-type layers are demonstrated using plasma-assisted molecular beam epitaxy on bulk AlN substrates. Current–voltage characteristics show a turn-on voltage of Vbi≈5.5 V, a minimum room temperature ideality factor of η≈1.63, and more than 12 orders of current modulation at room temperature. A stable current operation of the ultrawide bandgap semiconductor diode is measured up to a temperature of 300 °C. The one-sided n+–p heterojunction diode design enables a direct measurement of the spatial distribution of polarization-induced mobile hole density in the graded AlGaN layer from the capacitance–voltage profile. The measured average mobile hole density is p∼5.7×1017 cm−3, in close agreement with what is theoretically expected from distributed polarization doping. Light emission peaked at 260 nm (4.78 eV) observed in electroluminescence corresponds to interband radiative recombination in the n+ AlGaN layer. A much weaker deep-level emission band observed at 3.4 eV is attributed to cation-vacancy and silicon complexes in the heavily Si-doped AlGaN layer. These results demonstrate that distributed polarization doping enables ultrawide bandgap semiconductor heterojunction p–n diodes that have wide applications ranging from power electronics to deep-ultraviolet photonics. These devices can operate at high temperatures and in harsh environments.

Physics↗

Reducing Dark Conductivity of Cesium Tin Halide Perovskites with Donor Doping

The inorganic tin halide perovskites (such as Cs Sn Br 3 and Cs Sn I 3 ) exhibit high hole concentrations, which have been attributed to the presence of intrinsic defects such as cation vacancies. Despite their promise as photovoltaic materials, this high intrinsic conductivity limits deployment. Using hybrid density functional theory, we examine the impact of these intrinsic defects on the electronic properties of Cs Sn Br 3 and Cs Sn I 3 . We find that tin and cesium vacancies have low formation energies, especially under Sn -poor conditions, in agreement with prior work, and that the presence of these native acceptor defects can lead to high hole concentrations. However, effective donor doping of these systems can be obtained via Sc or Y incorporation. These impurities substitute on the Sn site, where they act as single donors. By examining the formation energy of these dopants versus the native defects, we show that Sc or Y doping should lead to a strong compensation, reducing hole concentrations under Sn -rich conditions. Published by the American Physical Society 2025

Lyons, John L. (ORCID:0000000180233055)↗