C2 Swan bands in comets
Relative population calculation of vibration levels of electronic levels assuming fluorescence mechanism for carbon-carbon bond Swan bands in comets
SEARCH · Engineering Papers
Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.
Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.
Relative population calculation of vibration levels of electronic levels assuming fluorescence mechanism for carbon-carbon bond Swan bands in comets
Mass spectral fragmentation of substituted aliphatic glycols and hydroxylated carbon-carbon bond
Development of reusable oxidation resistant carbon-carbon laminates and surface insulation materials for thermal protection systems
Lightweight oxidation resistant carbon-carbon composites for space shuttle leading edge components thermal protection
Thermophysical property measurements were made under transient heating conditions on several materials being considered for use in SCOUT rocket motors. The materials included were ATJ graphite, MX 2600 silica phenolic, FM 5272 cellulose phenolic, and two carbon-carbon composites: CARBITEX 700 and RPP-4. The ATJ was included as a reference or base line material to check performance of the transient tests as it was not expected to be sensitive to heating rate. Measurements included in the program were thermal conductivity, strength, compressive stress-strain (carbon-carbon only), thermal expansion and the effective thermal expansion under partially restrained conditions. Development of this latter measurement was a major part of the program. It consisted of partially restraining the expansion of a specimen as it was heated, measuring the load and strain which occurred (together with a simultaneous modulus determination by superimposing a small cyclic load) and using these quantities to calculate what the effective thermal expansion would have to be to produce the observed stress and deformation. For materials which are sensitive to heating rate, such as reinforced phenolics, it was believed that this would provide a more realistic determination of the thermal expansion as it more nearly simulates the conditions experienced in end use.
Analytical trade studies are presented that consider passive TPS configurations using the following material categories: (1) reuseable surface insulation - surface-coated rigidized ceramic fiber; (2) low density charring ablators; and (3) carbon-carbon and high density ablators for leading edge areas. Emphasized are effects on TPS weight by variations in entry trajectories and material thermal characteristics.
Pyrolized carbon-carbon has one unique advantage over other materials that makes its application to the space shuttle thermal protection system very attractive. This unique characteristic is the increase in material strength and modulus with increase in temperature up to about 2500 K (4040 F). Offsetting this unique advantage are disadvantages which include brittleness, high cost, and the tendency of the material to react with oxygen, particularly at high temperatures. The development of an oxidation inhibitor for the material and the definition of fabrication processes for selected full-scale components are considered.
A large variety of graphitic materials have been tested in an arc heated air stream at a surface pressure of 4.3 atm and a nominal surface temperature of 3925 K. Included were commercial and developmental grades of artificial graphites, both two and three dimensional carbon-carbon composites, composites seeded with refractory compounds, and several special materials such as pyrolytic graphite, mesophase graphite, glassy carbon, and natural graphite. ATJ graphite was used as a control material. Except for the seeded materials which had poor performance, the mass loss rate for all the man-made graphitic materials fell within the range of 17 per cent less to 30 per cent more than the rate for ATJ. Thus it is concluded that wide variations in constituents, processing, fabrication and structure have relatively little effect on the ablation performance of graphitic materials, at least under the conditions of the present tests. Particulate mass loss was observed for all the materials tested and is the dominant mechanism for mass removal at the present test conditions. It is suggested that this mechanism results from physical failure, primarily by compressive thermal stress.
Explore the source record for details and available documents.
A study performed to continue development of computational techniques for the Space Shuttle Thermal Protection System is reported. The resulting computer code was used to perform some additional optimization studies on several TPS configurations. The program was developed in Fortran 4 for the CDC 6400, and it was converted to Fortran 5 to be used for the Univac 1108. The computational methodology is developed in modular fashion to facilitate changes and updating of the techniques and to allow overlaying the computer code to fit into approximately 131,000 octal words of core storage. The program logic involves subroutines which handle input and output of information between computer and user, thermodynamic stress, dynamic, and weight/estimate analyses of a variety of panel configurations. These include metallic, ablative, RSI (with and without an underlying phase change material), and a thermodynamic analysis only of carbon-carbon systems applied to the leading edge and flat cover panels. Two different thermodynamic analyses are used. The first is a two-dimensional, explicit precedure with variable time steps which is used to describe the behavior of metallic and carbon-carbon leading edges. The second is a one-dimensional implicity technique used to predict temperature in the charring ablator and the noncharring RSI. The latter analysis is performed simply by suppressing the chemical reactions and pyrolysis of the TPS material.
Large diameter, carbon-carbon composite, monofilaments were produced from the pyrolysis of organic precursor resins reinforced with high-strenght carbon fibers. The mechanical properties were measured before and after pyrolysis and the results were correlated with the properties of the constituents. The composite resulting from the combination of Thornel 75 and GW-173 resin precursor produced the highest tensile strength. The importance of matching strain-to-failure of fibers and matrix to obtain all the potential reinforcement of fibers is discussed. Methods are described to reduce, within the carbonaceous matrix, pyrolysis flaws which tend to reduce the composite strength. Preliminary studies are described which demonstrated the feasibility of fiber-matrix copyrolysis to alleviate matrix cracking and provide an improved matrix-fiber interfacial bonding.
Refractory composites of carbon-carbon material are considered for application in: (a) rocket motor nozzles and skirts, (b) a unique integrated propulsion structure, and (c) planetary atmospheric entry shells. Technical developments and plans in each of these areas are described.
An oxidation resistant carbon-carbon composite has been developed for use on the NASA Space Shuttle Orbiter Vehicle which can function on the high temperature surfaces to satisfy the 100 mission reuse capability requirement. This paper describes the design requirements, materials and processes developed, and the successful testing of simulated full-scale prototype hardware. Materials considerations are illustrated, including strength and oxidation testing, along with physical property determinations, characterizing the material over the predicted temperature range of use.
A heat-pipe-cooled Space Shuttle orbiter wing leading edge was compared and evaluated against three alternate leading edge candidates: a refurbishable ablative design, and two other reusable versions employing coated columbium and carbon-carbon high-temperature segments. Each candidate concept was shown feasible in the Phase B environment. The reusable versions were all found to cost nearly the same and substantially less than the nonreusable ablative version. However, since current Shuttle trajectories produce higher heating rates than those used in this study, the carbon-carbon and heat pipe concepts are now the prime candidates for Shuttle leading edge thermal protection.
The construction of two test modules is presented for a feasibility demonstration of a concept for reusable space shuttle wing leading edge surfaces. In this leading edge concept high temperature heat pipes were incorporated into the structure to cool the stagnation region, allowing the use of super-alloys in place of refractory metal, ablator protected, or carbon-carbon structures. The program included the analysis and design of the heat pipes, their integration into the test module structure, heat pipe development testing, construction of the test modules and a facility adapter, and formulation of recommended testing conditions. The results of the heat pipe and leading edge module thermal analyses indicate the test modules will meet the design goal; reducing the leading edge temperature at the stagnation line from 1315 C (2400 F) to less than 1010 C (1850 F). The development tests demonstrated that the module assembly could be brazed with active heat pipes, as was borne out by the subsequent successful brazing of both modules with active heat pipes loaded with sodium.
A method was developed for predicting oxidation performance, in an earth atmospheric entry environment, of reinforced carbon-carbon material, coated for oxidation resistance. A model was developed which describes oxidation control mechanisms, and the equations defining these mechanisms were derived. These relations were used to correlate oxidation test data, and to infer pertinent rate constants. Predictions were made of material oxidation performance in a representative entry environment, and the predictions were compared with ground test data. Results indicate that the method can be successfully used for predicting material oxidation performance.
To improve the oxidation resistance of a carbon-carbon composite, impregnations were performed using pitches, polyfurfuryl alcohols, and phenolic resins, including a silicon-doped phenolic resin. Oxidation resistance and strength increased for all of the composites as the impregnant-carbon residue increased. The properties of the composites impregnated with the nonsilicon-bearing resins were nearly identical and depended only on the amount of impregnant residue present. However, for equivalent residue concentrations, composites produced with the silicon-bearing resin gave higher strengths and at least 100% better oxidation resistance than was observed for the other composites or for a prototype control material.
The effect of weave geometry on the onset of transition from laminar to turbulent flow around a sample of an orthogonally woven fine weave carbon-carbon material tested in an arc-jet is investigated. Seventeen post-test models which had undergone only partial transition around the circumference were examined as to location of turbulent regions relative to the weave axes. It was statistically shown that the weave axes had the lowest probability of being a position of initial transition onset. The probability generally increased with distance from a major axis, with some rays, notably the 45 deg rays, showing better transition resistance than the adjacent rays. The incidence of initial transition onset correlated well with the number of X or Y fibers that the flow passes over from stagnation point to the shoulder.