At least 19 records

Defect chemistry and characterization of Hg sub 1x Cd sub x Te

Single crystal samples of undoped and doped Hg sub 1-x Cd sub x Te were annealed at varying temperatures and partial pressures of Hg. Hall effect and mobility measurements were carried out on these samples after quenching to room temperature. Based on the variation of the carrier concentration and the carrier mobility as a function of the partial pressure of Hg temperature, and dopant concentration, defect models were established for the doped and the undoped crystals. These models indicate that the native acceptor defects in both Hg0.8Cd0.2Te and Hg0.6Cd0.4Te doubly ionized and the native donor defects are negligible in concentration, implying that p to n conversion in these alloys occurs due only to residual donors. Incorporation mechanism of copper, indium, iodine, and phosphorus were investigated. A large concentration of indium is found to be paired with the native acceptor defects. Results on crystals doped with phosphorus indicate that phosphorus behaves amphoterically, acting as a donor on Hg lattice sites and as an acceptor intersitially on Te lattice sites. A majority of the phosphorus is found to be present as neutral species formed from the pairing reaction between phosphorus on Hg lattice sites and phosphorus in interstitial sites. Equilibrium constants for the intrinsic excitation reaction, as well as for the incorporation of the different dopants and the native acceptor defects were established.

Vydyanath, H. R.

Defect chemistry and characterization of Hg(1-x)Cd(x)Te

Undoped mercury cadmium telluride crystals were subjected to high temperature equilibration at temperatures ranging from 400 C to 655 C in various Hg atmospheres. Hall effect and mobility measurements were carried out on the crystals quenched to room temperature subsequent to the high temperature equilibration. The variation of the hole concentration in the cooled crystals at 77 K as a function of the partial pressure of Hg at the equlibration temperatures, together with a comparison of the hole mobility in the undoped samples with that in the copper and phosphorous doped samples yielded a defect model for the undoped crystals, according to which, the undoped crystals are essentially intrinsic at the equilibration temperatures and the native acceptor defects are doubly ionized. Native donor defects appear to be negligible in concentration, implying that the p to n conversion in these alloys is mainly due to residual foreign donor impurities. The thermodynamic constants for the intrinsic excitation process as well as for the incorporation of the doubly ionized native acceptor defects in the undoped crystals were obtained.

Vydyanath, H. R.

Lattice defects in semiconducting Hg/1-x/Cd/x/Te alloys. III - Defect structure of undoped Hg0.6Cd0.4Te

Hall effect measurements were carried out on undoped Hg0.6Cd0.4Te crystals quenched to room temperature subsequent to equilibration at temperatures varying from 450 to 720 C under various partial pressures of Hg. The variation of the hole concentration as a function of the partial pressure of Hg indicates that the native acceptor defects are doubly ionized. Native donor defects are found to be negligible in concentration and the p-type to n-type conversion is shown to be due to residual donors and not due to native donor defects. Thermodynamic constant for the incorporation of the doubly ionized native acceptor defect has been established.

Vydyanath, H. R.

Lattice defects in semiconducting Hg/1-x/Cd/x/Te alloys. I - Defect structure of undoped and copper doped Hg/0.8/Cd/0.2/Te. II - Defect structure of indium-doped Hg/0.8/Cd/0.2/Te

Hall effect and mobility measurements were conducted on undoped Hg(0.8)Cd(0.2)Te crystals which were quenched to room temperature after being subjected to equilibration at temperatures ranging from 400 to 655 C in various Hg atmospheres. The variation of the hole concentration in the cooled crystals at 77 K as a function of Hg's partial pressure at the equilibration temperature, together with a comparison of the hole mobility in the undoped samples with that in copper-doped ones, yields a defect model for the undoped crystals according to which they are intrinsic at the equilibration temperatures and the native acceptor defects are doubly ionized. In the second part of this paper, the effects of indium doping are considered. The concentration of electrons obtained in the cooled crystals was found to be lower than the intrinsic carrier concentration at the equilibration temperatures. A defect model is proposed according to which most of the indium is incorporated as In2Te3(s) dissolved in the crystal, with only a small fraction of indium acting as single donors occupying Hg lattice sites.

Vydyanath, H. R.

Defect chemistry and characterization Hg(1-x)Cd(x)Te

Iodine doped single crystal samples of mercury cadmium telluride were annealed at temperatures varying from 450 C to 600 C in Hg vapor and quenched to room temperature. Hall effect measurements at 77 K on the crystals cooled to room temperature indicate the samples to be n-type after anneals at high Hg pressures whereas they turn p-type after anneals at low Hg pressures; the electron concentration increases with increase in Hg pressure. The results are explained on the basis that the crystals are saturated with (Hg,Cd)I2, with a fraction of the iodine being present as donor occupying tellurium lattice sites and a fraction being present as acceptors resulting from the iodine on tellurium lattice sites pairing with the doubly ionized native acceptor defects. The solubility of the donor species increases with increase in Hg pressure, whereas that of the acceptor species increases with decrease in Hg pressure. Equilibrium constants for the incorporation of the iodine species as well as the pairing reaction were established.

Vydyanath, H. R.

Doping behavior of iodine in Hg/0.8/Cd/0.2/Te

The defect state prevailing in iodine doped single-crystal samples of Hg0.8Cd0.2Te, annealed at 450-600 C in Hg vapor, has been deduced from Hall effect measurements on samples cooled to 77 K from the annealing temperature. Results are found to be similar to those previously obtained for iodine doped CdS, i.e. iodine acts as a single donor occupying Te lattice sites with a fraction paired with the native acceptor defects. The concentration of iodine on tellurium lattice sites increases with the partial pressure of Hg, whereas that of the pair species increases as the partial pressure of Hg decreases.

Vydyanath, H. R.

Molecules with enhanced electronic polarizabilities based on defect-like states in conjugated polymers

Highly conjugated organic polymers typically have large non-resonant electronic susceptibilities, which give the molecules unusual optical properties. To enhance these properties, defects are introduced into the polymer chain. Examples include light doping of the conjugated polymer and synthesis, conjugated polymers which incorporate either electron donating or accepting groups, and conjugated polymers which contain a photoexcitable species capable of reversibly transferring its electron to an acceptor. Such defects in the chain permit enhancement of the second hyperpolarizability by at least an order of magnitude.

Beratan, David N.

Residual double acceptors in bulk GaAs

By using infrared absorption, photoluminescence, and Hall measurements we have observed an additional level associated with a residual acceptor in liquid encapsulated Czochralski GaAs. These results indicate that the defect is a double acceptor with levels 78 and 200 meV above the valence band.

Elliott, K. R.

Advanced methods for preparation and characterization of infrared detector materials

Mercury cadmium telluride crystals were prepared by the Bridgman method with a wide range of crystal growth rates and temperature gradients adequate to prevent constitutional supercooling under diffusion-limited, steady state, growth conditions. The longitudinal compositional gradients for different growth conditions and alloy compositions were calculated and compared with experimental data to develop a quantitative model of the crystal growth kinetics for the Hg(i-x)CdxTe alloys, and measurements were performed to ascertain the effect of growth conditions on radial compositional gradients. The pseudobinary HgTe-CdTe constitutional phase diagram was determined by precision differential thermal analysis measurements and used to calculate the segregation coefficient of Cd as a function of x and interface temperature. Computer algorithms specific to Hg(1-x)CdxTe were developed for calculations of the charge carrier concentrations, charge carrier mobilities, Hall coefficient, optical absorptance, and Fermi energy as functions of x, temperature, ionized donor and acceptor concentrations, and neutral defect concentrations.

Lehoczky, S. L.

Advanced methods for preparation and characterization of infrared detector materials

Crystals were prepared by the Bridgman-Stockbarger method with a wide range of crystal growth rates and temperature gradients adequate to prevent constitutional supercooling under diffusion-limited, steady-state, growth conditions. The longitudinal compositional gradients for different growth conditions and alloy compositions were calculated and compared with experimental data to develop a quantitative model of solute redistribution during the crystal growth of the alloys. Measurements were performed to ascertain the effect of growth conditions on radial compositional gradients. The pseudobinary HgTe-CdTe constitutional phase diagram was determined by precision differential-thermal-analysis measurements and used to calculate the segregation coefficient of Cd as a function of x and interface temperature. Experiments were conducted to determine the ternary phase equilibria in selected regions of the Hg-Cd-Te constitutional phase diagram. Electron and hole mobilities as functions of temperature were analyzed to establish charge-carrier scattering probabilities. Computer algorithms specific to Hg(1-x)CdxTe were developed for calculations of the charge-carrier concentration, charge-carrier mobilities, Hall coefficient, and Dermi Fermi energy as functions of x, temperature, ionized donor and acceptor concentrations, and neutral defect concentrations.

Broerman, J. G.

Metastable defects in Be-doped Al(x)Ga(1-x)As

Deep-level transient spectroscopy has been used to study metastable defects in Be-doped Al(x)Ga(1-x)As grown by molecular-beam epitaxy. The metastability manifests itself by the appearance of different spectra depending upon whether the sample is cooled from a high temperature with zero bias or a reverse bias applied to it. The defects are found in concentrations of 10 to the 15th/cu cm in a sample doped with 10 to the 18th Be/cu cm and in much lower concentrations in a 10 to the 17th Be/cu cm sample. Isochronal annealing experiments indicate that the defect is multistable and that it is best modeled as a mobile interstitial which can reside at several sites near acceptor. The activation energies for these defects are between 0.2 and 0.5 eV above the valence band.

Magno, R.

Defect chemistry and characterization of (Hg, Cd)Te

Single crystal samples of phosphorus doped Hg sub 0.8 Cd sub 0.2 Te were anneald at temperatures varying from 450 C to 600 C in various Hg atmospheres. The samples were quenched to room temperature from the annealing temperatures. Hall effect and mobility measurements were performed at 77 K on all these samples. The results indicate the crystals to be p type for a total phosphorus concentration of 10 to the 19th power/cu cm in all the samples. The hole concentration at 77 K increases with increasing Hg pressures at 450 C and 500 C contrary to the observation in undoped crystals. Also, at low Hg pressures the concentration of holes in the phosphorus doped crystals is lower than in the undoped crystals. The hole concentration in all the samples is lower than the intrinsic carrier concentration at the annealing temperatures. The hole mobility in the doped crystals is similar to that in the undoped crystals. A defect model according to which phosphorus behaves as a single acceptor interstitially, occupying Te lattice sites while it acts as a single donor occupying Hg lattice sites was established. Equilibrum constants established for the incorporation of all the phosphorus species explain the experimental results

Vydyanath, H. R.

Characterization of PVT Grown ZnSe by Low Temperature Photoluminescence

ZnSe, a II-VI semiconductor with a large direct band gap of 2.7 eV at room temperature and 2.82 eV at 10 K, is considered a promising material for optoelectric applications in the blue-green region of the spectrum. Photoemitting devices and diode laser action has been demonstrated as a result of decades of research. A key issue in the development of II-VI semiconductors is the control of the concentration of the various impurities. The II-VI semiconductors seem to defy the effort of high level doping due to the well known self compensation of the donors and the acceptors. A good understanding of roles of the impurities and the behavior of the various intrinsic defects such as vacancies, interstitials and their complexes with impurities is necessary in the development and application of these materials. Persistent impurities such as Li and Cu have long played a central role in the photoelectronic properties of many II-VI compounds, particularly ZnSe. The shallow centers which may promote useful electrical conductivity are of particular interest. They contribute the richly structured near gap edge luminescence, containing weak to moderate phonon coupling and therefore very accessible information about the energy states of the different centers. Significance of those residual impurities which may contribute such centers in II-VI semiconductors must be fully appreciated before improved control of their electrical properties may be possible. Low temperature photoluminescence spectroscopy is an important source of information and a useful tool of characterization of II-VI semiconductors such as ZnSe. The low temperature photoluminescence spectrum of a ZnSe single crystal typically consists of a broad band emission peaking at 2.34 eV, known as the Cu-green band, and some very sharp lines near the band gap. These bands and lines are used to identify the impurity ingredients and the defects. The assessment of the quality of the crystal based on the photoluminescence analysis is then possible. In this report we present the characterization of a ZnSe single crystal as grown by the physical vapor transport method, with special intention paid to the possible effects of the gravitational field to the growth of the crystal.

Wang, Ling Jun

Composition stability limits for the rocksalt-structure phase /Pb1-y Sny/1-xTex from lattice parameter measurements.

The parameter values measured are in agreement with those reported by Mazelsky and Lubell (1963) and data of Bis and Dixon (1969). The measurements for SnTe introduce a large amount of data into a defect model analysis that shows that the ratio of the number of holes per tin-vacancy acceptor to the 77 K Hall factor is independent of the apparent hole concentration. The measurements reveal some interesting problems in handling the Sn-rich alloys in fine powder form due to the uptake of oxygen.

Brebrick, R. F.

Effects of macroscopic inhomogeneities on electron mobility in semi-insulating GaAs

It is shown that defect inhomogeneities of sizes larger than the electron mean free path are responsible for the low values and anomalous temperature dependence of the electron mobility in semi-insulating (SI) GaAs. The room-temperature electron mobility values below about 6000 sq cm/V s cannot be uniquely used for the determination of the concentration of ionized defects, since the contribution from inhomogeneities usually exceeds that from scattering by ionized impurities. The effects of the macroscopically inhomogeneous distribution of residual acceptors and the major deep donor EL2 diminish at elevated temperatures between 600 and 900 K, which offers a means for identification of inhomogeneities, and furthermore explains recently reported steplike mobility versus temperature behavior in SI-GaAs.

Walukiewicz, W.

Interaction between boron and intrinsic defects in GaAs

A model has been developed to describe the interaction between boron and antisite defects in bulk grown undoped liquid uncapsulated Czochralski GaAs. This model helps explain the observed experimental behavior. The model indicates that the residual double acceptor can most likely be associated with either Ga(As) or B(As).

Elliott, K. R.

Infrared absorption study of neutron-transmutation-doped germanium

Using high-resolution far-infrared Fourier transform absorption spectroscopy and Hall effect measurements, the evolution of the shallow acceptor and donor impurity levels in germanium during and after the neutron transmutation doping process was studied. The results show unambiguously that the gallium acceptor level concentration equals the concentration of transmutated Ge-70 atoms during the whole process indicating that neither recoil during transmutation nor gallium-defect complex formation play significant roles. The arsenic donor levels appear at full concentration only after annealing for 1 h at 450 C. It is shown that this is due to donor-radiation-defect complex formation. Again, recoil does not play a significant role.

Park, I. S.

Electrical characterization of Hg(1-x)Cd(x)Te alloys

Theoretical models are described for calculations of charge-carrier concentrations, Fermi energy, and conduction electron mobility as functions of x, temperature, and ionized and neutral defect concentrations of Hg(1-x)Cd(x)Te alloys. Measurements are reported of electron concentration and electron mobility from 5-300 K for alloys with x values of between 0.17 and 0.30. The electrical data are in reasonable agreement with theory, and were analyzed to obtain estimates of donor and acceptor state concentrations. The electron mobilities are calculated in terms of a microscopic theory of electrical conduction derived from the solution of the Boltzmann equation for the perturbed steady-state electron distribution function, and they show that longitudinal optical-phonon and charged and neutral defect scattering are the dominant mobility-limiting mechanisms.

Lehoczky, S. L.