A robust protonic ceramic fuel cell with a triple conducting oxygen electrode under accelerated stress tests
Accelerated stress test of protonic ceramic fuel cells for evaluating the durability of materials and interfaces.
SEARCH · Engineering Papers
Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.
Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.
Accelerated stress test of protonic ceramic fuel cells for evaluating the durability of materials and interfaces.
Cerium is a radical scavenger which improves polymer electrolyte membrane (PEM) fuel cell durability. During operation, however, cerium rapidly migrates in the PEM and into the catalyst layers (CLs). In this work, membrane electrode assemblies (MEAs) were subjected to accelerated stress tests (ASTs) under different humidity conditions. Cerium migration was characterized in the MEAs after ASTs using X-ray fluorescence. During fully humidified operation, water flux from cell inlet to outlet generated in-plane cerium gradients. Conversely, cerium profiles were flat during low humidity operation, where in-plane water flux was negligible, however, migration from the PEM into the CLs was enhanced. Humidity cycling resulted in both in-plane cerium gradients due to water flux during the hydration component of the cycle, and significant migration into the CLs. Fluoride and cerium emissions into effluent cell waters were measured during ASTs and correlated, which signifies that ionomer degradation products serve as possible counter-ions for cerium emissions. Fluoride emission rates were also correlated to final PEM cerium contents, which indicates that PEM degradation and cerium migration are coupled. Lastly, it is proposed that cerium migrates from the PEM due to humidification conditions and degradation, and is subsequently stabilized in the CLs by carbon catalyst supports.
Abstract not provided.
Not Available
This paper presents the indoor extended accelerated stress testing (EAST) results of glass/glass (GG), glass/backsheet (GB) and glass/transparent backsheet (GT) modules having identical cells and two different encapsulant types, ethyl-vinyl-acetate (EVA) and polyolefin-elastomer (POE). Six 4-cell modules having the above-mentioned construction combinations were subjected to extended ultraviolet (UV; 600 kWh/m2), damp-heat (DH; 2000 hours) and thermal-cycling (TC; 600 cycles) tests. The post-stress UV fluorescent imaging, electroluminescent imaging, reflectance spectrophotometry and colorimetry results indicated that the grid finger degradation and encapsulant browning are slightly higher in the GG modules compared to the GB modules. The post-stress IV test results indicated, in general, that the GG/EVA modules tend to perform inferior to the GG/POE modules with the EAST evaluation.
The primary goal of this study was to ascertain the presence and types of mechanisms affecting CdS/CdTe device stability in the temperature range of 60 to 120 ..deg..C. It should be noted that the results presented were specific to cells made using the specific growth conditions described.
Concentrating photovoltaic (CPV) systems have great potential to reduce photovoltaic (PV) electricity costs because of the relatively low cost of optical components as compared to PV cells. A transparent polymeric material is used to optically couple the PV cell to optical components and is thus exposed to the concentrated light source at elevated temperatures. In this work polymeric encapsulant materials are positioned close to a Xenon arc lamp to expose them to ultraviolet radiation (UV) that is about 42 times as intense as sunlight. Furthermore, different glass types are used as filters to modify the spectral distribution of light in the UV range. A strong sensitivity of non-silicone-based encapsulants to light below ~350 nm is demonstrated. Of all the materials examined in this study, the polydimethyl silicone samples performed the best. The next best material was an ionomer which maintained optical transmission but became photo-oxidized where exposed to the atmosphere.
By applying multiple environmental stresses in fieldrepresentative combinations and sequences, combined-accelerated stress testing (CAST) identifies degradation modes and failure mechanisms of photovoltaic (PV) modules and components that are missed by single stress factor accelerated testing.
Combined‐accelerated stress testing (C‐AST) is developed to establish the durability of photovoltaic (PV) products, including for degradation modes that are not a priori known or examined in standardized tests. C‐AST aims to comprehensively represent the sample, stress factors, and their combinations using levels at the statistical tails of the natural environment. Acceleration factors for relevant climate sequences within the C‐AST cycle with respect to the Florida USA climate are estimated for selected degradation mechanisms. It is found that for degradation of the outer backsheet polymer layer, the acceleration factor of the tropical climate sequence (the longest of the climate sequences) is f ( T , G ) = 17.3 with ultraviolet photodegradation; for polyethylene terephthalate hydrolysis (backsheets), f ( T , RH ) = 426; for electrochemical corrosion (PV cell), f ( I ) = 14.1; and for PbSn solder fatigue f (Δ T , r ( T )) = 17.3. Here, T is the module temperature, G is the broadband spectrum irradiance on the plane of array of the module, RH is the relative humidity on the module surface, I is the leakage current through the module packaging, and r ( T ), the number of temperature reversals. The methods discussed herein are generally applicable for evaluating acceleration factors in other accelerated test methods.
A combined chemical/mechanical accelerated stress test (AST) was developed for proton exchange membrane (PEM) fuel cells based on relative humidity cycling (RHC) between dry and saturated gases at open circuit voltage (OCV). Membrane degradation and failure were investigated using scanning electron microscopy and small- and wide-angle X-ray scattering. Changes to membrane thickness, hydrophilic domain spacing, and crystallinity were observed to be most similar between field-operated cells and OCV RHC ASTs, where local thinning and divot-type defects are the primary failure modes. While RHC in air also reproduces these failure modes, it is not aggressive enough to differentiate between different membrane types in >1,333 hours (55 days) of testing. Conversely, steady-state OCV tests result in significant ionomer morphology changes and global thinning, which do not replicate field degradation and failure modes. It is inferred that during the OCV RHC AST, the decay of the membrane's mechanical properties is accelerated such that materials can be evaluated in hundreds, instead of thousands, of hours, while replicating the degradation and failure modes of field operation; associated AST protocols are recommended as OCV RHC at 90°C for 500 hours with wet/dry cycle durations of 30s/45s and 2m/2m for automotive and bus operation, respectively.
Extrapolation of accelerated testing to the long-term results expected in the field has uncertainty associated with the acceleration factors and the range of possible stresses in the field. When multiple stresses (such as temperature and humidity) can be used to increase the acceleration, the uncertainty may be reduced according to which stress factors are used to accelerate the degradation.
This talk reviews sequential and combined accelerated stress tests of the past decade that have been shown to better replicate degradation mechanisms seen in the field, that single-factor steady-state tests have failed to reproduce. When designing stress tests for PV modules, it is shown, with examples, how it is beneficial to consider representation of the shipping module, the stress factors applied, and how the stress factors are sequenced or combined in the natural environment. Finally, current and future efforts to realize accelerated stress tests based on these concepts are discussed.
Previously undiscovered failure modes in photovoltaic (PV) modules continue to emerge in field installations despite passing protocols for design qualification and quality assurance. Failure to detect these modes prior to widespread use could be attributed to the limitations of present-day standard accelerated stress tests (ASTs), which are primarily designed to identify known degradation or failure modes at the time of development by applying simultaneous or sequential stress factors (usually two at most). Here, we introduce an accelerated testing method known as the combined-accelerated stress test (C-AST), which simultaneously combines multiple stress factors of the natural environment. Simultaneous combination of multiple stress factors allows for improved identification of failure modes with better ability to detect modes not known a priori. A demonstration experiment was conducted that reproduced the field-observed cracking of polyamide- (PA-) and polyvinylidene fluoride (PVDF)–based backsheet films, a failure mode that was not detected by current design qualification and quality assurance testing requirements. In this work, a two-phase testing protocol was implemented. The first cycle (“Tropical”) is a predominantly high-humidity and high-temperature test designed to replicate harsh tropical climates. The second cycle (“Multi-season”) was designed to replicate drier and more temperate conditions found in continental or desert climates. Testing was conducted on 2 × 2-cell crystalline-silicon cell miniature modules constructed with both ultraviolet (UV)–transmitting and UV-blocking encapsulants. Cracking failures were observed within a cumulative 120 days of the Tropical condition for one of the PA-based backsheets and after 84 days of Tropical cycle followed by 42 days of the Multi-season cycle for the PVDF-based backsheet, which are both consistent with failures seen in fielded modules. In addition to backsheet cracking, degradation modes were observed including solder/interconnect fatigue, various light-induced degradation modes, backsheet delamination, discoloration, corrosion, and cell cracking. The ability to simultaneously apply multiple stress factors may allow many of the test sequences within the standardized design qualification procedure to be performed using a single test setup.
Herein, electroluminescence (EL) and thermal imaging are used to examine p–i–n metal halide perovskite (MHP) photovoltaic (PV) mini-modules (MA0.6FA0.4PbI3, 20 cells, 78 cm2) before and after indoor-accelerated stress testing or outdoor deployment. Distinct spatial patterns in the EL images emerge, which depend on the external stress conditions experienced by the mini-module. Imaging results highlight a distribution of dark speckle features that dominate after UV stress, attributed to widespread interfacial contact degradation. Lateral intensity gradients across cells dominate after thermal cycling (TC) stress, attributed to current crowding near scribe defects. While current–voltage analysis alone does not give full insight on the degradation process, this study shows that distinct degradation modes can be further defined by multimodal electro-optical imaging (i.e., EL combined with photoluminescence and dark lock-in thermography). Neither UV exposure nor TC-accelerated stress testing alone replicates the same degradation signatures observed after outdoor deployment, suggesting that multiple degradation modes occur under concurrent stressors outdoors. Finally, spatial characterization of degradation modes in MHP PV mini-modules before and after accelerated stress testing lays the groundwork for developing targeted accelerated stress testing procedures through comparison with outdoor aging.
The viability of novel coextruded, fluoropolymer-free backsheets for photovoltaic (PV) modules has been questioned as a result of a large number of early-life backsheet failures in PV installations containing one of the earliest co-extruded polyamide (PA)-based backsheet to reach the market, “AAA.” New PV reliability testing protocols have been recently developed and applied to backsheets to reproduce failures observed in the field and evaluate the durability of novel backsheet materials and designs prior to commercialization. A new co-extruded PA-based backsheet was tested using combined-accelerated stress testing (C-AST) and demonstrated a greater lifetime than AAA, and some other fluoropolymer-based backsheets such as polyvinylidene fluoride. The improved PA-based backsheet also eventually failed by through-thickness cracking. Using surface and bulk material characterization techniques, we performed a comprehensive study of material properties before and after the stress testing. Aging of the backsheet resulted in an increase of surface roughness by erosion of the outer PA layer. However the failure is more likely related to an increase in crystallinity of the polyolefin core layer reducing the backsheet tearing energy. The analysis can ultimately inform on the specific weaknesses of the materials so that the manufacturer can improve the backsheet design to extend its lifetime.
Cracking of polyamide (PA)-based photovoltaic (PV) backsheet materials has been widely reported for field-aged modules. Failure was not detected by conventional accelerated stress tests (ASTs), which lacked the necessary combination of stress factors and/or factor sequences. PA-based AAA backsheet cracking has since been reproduced through combined and sequential stress testing. Planar- and cross-sectional-optical microscopy as well as Fourier-transform Infrared Spectroscopy (FTIR), have been used to elucidate the mechanical and chemical changes which lead to failure of the backsheet. Field-aged backsheet samples demonstrating failure in various climates (including locations in China and Italy) are also analyzed. Through the analysis, a comparison is made between the different stress testing protocols and the field-aged samples to validate relevance of the advanced stress tests. It is shown that the changes induced through combined-accelerated stress testing (C-AST) were most representative of changes induced by the field, supporting the relevance of C-AST and providing validity for the test protocol.
The electrochemical behavior for Pt catalysts supported on multiwalled carbon nanotubes and Vulcan XC-72 in proton exchange membrane fuel cells under accelerated stress test was examined by cyclic voltammetry, electrochemical impedance spectroscopy, and polarization technique. Pt catalyst supported on multiwalled carbon nanotubes exhibited highly stable electrochemical surface area, oxygen reduction kinetics, and fuel cell performance at a highly oxidizing condition, indicating multiwalled carbon nanotubes show high corrosion resistance and strong interaction with Pt nanoparticles. The Tafel slope, ohmic resistances, and limiting current density determined were used to differentiate kinetic, ohmic, mass-transfer polarization losses from the actual polarization curve. Kinetic contribution to the total overpotential was larger throughout the stress test. However, the fraction of kinetic overpotential decreased and mass-transfer overpotential portion remained quite constant during accelerated stress test, whereas the fraction of ohmic overpotential primarily originating from severe proton transport limitation in the catalyst layer increased under the anodic potential hold.
These are a set of slides that deal with membrane degradation accelerated stress test. Specifically, the following topics are covered: membrane degradation FCTT drive cycle; membrane ASTs; current membrane ASTs damage mechanisms; proposed membrane AST, RH cycling in H 2 /Air; current proposed AST; 2min/2min AST damage mechanism; 30sec/45sec RH cycling at OCV.