At least 19 records

A trid(alkyl)yttrium compound cotaining six beta-agostic Si-H interactions

The new homoleptic rare earth compound [Y(C(SiHMe{sub 2}){sub 3}){sub 3}] ( 2) is prepared in 82% yield by salt metathesis of YCl{sub 3} and 3 equivalents of [KC(SiHMe{sub 2}){sub 3}] (1); two {beta}-agostic Y...(H-Si) interactions are observed for each C(SiHMe{sub 2}){sub 3} ligand in 2, giving six agostic interactions per yttrium(III) center.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Comparative study of three yttrium organometallic compounds for the stabilization of the cubic phase in YSZ deposited by PE-CVD

In this work, the efficiencies of three organometallic yttrium precursors used to produce YSZ coatings by plasma-enhanced chemical vapor deposition were studied. Yttrium (III) acetylacetonate, Y (acac) 3 , yttrium (III) hexafluoroacetylacetonate, Y (acacF 6 ) 3 , and yttrium (III) tris(2,2,6,6-tetramethyl-3,5-heptanedionate), Y (tmhd) 3 , were used to stabilize the cubic phase in zirconia deposited at temperatures from 500 to 800 °C. Our results showed that at temperatures between 500 and 600 °C, Y (tmhd) 3 appeared to be the most efficient dopant as it introduced the highest concentration of yttria (1–2.7 mol%) with only 6.4–5.6 at.% carbon. However, at 700 and 800 °C, Y (acac) 3 introduced twice as much yttria (8–15 mol%) as Y (tmhd) 3 with almost the same amount of carbon (5.4–3 at.%). Conversely, Y (acacF6)3 was the least efficient as it maintained a low concentration of yttria of around 0.7–1.8 mol% with 3.6–8.2 at.% carbon for all the deposition temperatures. Among these precursors, only Y (acac) 3 surpassed 8 mol% yttria and achieved a fully stabilized cubic phase at 800 °C, with the remaining samples stabilizing only the tetragonal phase. The tetragonal phase was stabilized due to the formation of crystallites of around 10 nm. The observed difference in the efficiency of the three precursors was correlated to important differences in their decomposition behavior as observed by mass spectrometry and thermogravimetry/differential scanning calorimetry.

36 MATERIALS SCIENCE↗

Condensed rare-earth metal-rich tellurides. Extension of layered Sc{sub 6}PdTe{sub 2}-type compounds to yttrium and lutetium analogues and to Y{sub 7}Te{sub 2}, the limiting binary member

Six isotypic R{sub 6}ZTe{sub 2} phases have been synthesized in Ta at elevated temperatures and characterized by single crystal X-ray refinements for R=Y, Z=Rh, Pd, Ag, Y and for R=Lu, Z=Cu, Ag. All crystallize in the Sc{sub 6}PdTe{sub 2}-type structure, Pnma, Z=4, a{approx}21.5 A, b{approx}4.1 A, c{approx}11.4 A. The results can be viewed as the replacement of Te3 atoms in the parent isotypic Sc{sub 2}Te (or in the hypothetical Y{sub 2}Te or Lu{sub 2}Te analogues) by the above the Z, the Y example giving the new binary phase Y{sub 7}Te{sub 2}. The shorter (and stronger) metal-metal bonds concentrate in the region of metal (Z, Y) substitution, as revealed by larger integrated crystal orbital Hamilton population (ICOHP) values derived from linear muffin-tin-orbital (LMTO) calculations. Partial densities-of-states data for Y{sub 7}Te{sub 2} reflect a similar behavior. Individual R-R bond distances are seen to deviate appreciably from the more fundamental overlap population measures for each. - Graphical abstract: Substitutions at the same site in a common orthorhombic host structure convert the hypothetical Y{sub 2}Te (above) to eitherY{sub 6}ZTe{sub 2} or the new binary Y{sub 7}Te{sub 2}.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Treatment of exhaust fluorescent lamps to recover yttrium: Experimental and process analyses

Highlights: > Recovery of yttrium from spent fluorescent lamps by sulphuric acid leaching. > The use of sulphuric acid allows to reduce calcium dissolutions. > Main contaminant of fluorescent powder are Si, Pb, Ca and Ba. > Hydrated yttrium oxalate, recovered by selective precipitation, is quite pure (>90%). > We have studied the whole process for the treatment of dangerous waste (plant capability). - Abstract: The paper deals with recovery of yttrium from fluorescent powder coming from dismantling of spent fluorescent tubes. Metals are leached by using different acids (nitric, hydrochloric and sulphuric) and ammonia in different leaching tests. These tests show that ammonia is not suitable to recover yttrium, whereas HNO{sub 3} produces toxic vapours. A full factorial design is carried out with HCl and H{sub 2}SO{sub 4} to evaluate the influence of operating factors. HCl and H{sub 2}SO{sub 4} leaching systems give similar results in terms of yttrium extraction yield, but the last one allows to reduce calcium extraction with subsequent advantage during recovery of yttrium compounds in the downstream. The greatest extraction of yttrium is obtained by 20% w/v S/L ratio, 4 N H{sub 2}SO{sub 4} concentration and 90 deg. C. Yttrium and calcium yields are nearly 85% and 5%, respectively. The analysis of variance shows that acid concentration alone and interaction between acid and pulp density have a significant positive effect on yttrium solubilization for both HCl and H{sub 2}SO{sub 4} medium. Two models are empirically developed to estimate yttrium and calcium concentration during leaching. Precipitation tests demonstrate that at least the stoichiometric amount of oxalic acid is necessary to recover yttrium efficiently and a pure yttrium oxalate n-hydrate can be produced (99% grade). The process is economically feasible if other components of the fluorescent lamps (glass, ferrous and non-ferrous scraps) are recovered after the equipment dismantling and valorized, besides the cost that is usually paid to recycling companies for collection, treatment or final disposal of such fluorescent powders.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

A simple and general route for the preparation of pure and high crystalline nanosized lanthanide silicates with the structure of apatite at low temperature

Rare earth silicates with the structure of apatite are attracting considerable interest since they show oxygen ion conductivities higher than that of yttria-stabilized zirconia (YSZ) at moderate temperature. Based on the hydrothermal synthesis we presented a simple one step process for the direct preparation of the pure and the high crystalline nanosized rare earth silicates with the structure of apatite under a mild condition (230 {sup o}C). Since the preparation of the high crystalline silicon based rare earth apatites is performed at high temperature previously and accompanied by subsequent process of grinding, results of this work provide a promising alternative of the existing methodology. Furthermore, due to the relatively low temperature of the preparation of these materials, high doping of monovalent cation can be done, which was not achieved before. -- Graphical abstract: A simple one step process for the preparation of the rare earth silicates with the structure of apatite under a mild condition (230 {sup o}C) is presented. The process is based on the hydrothermal synthesis and the obtained powder materials are pure, high crystalline and with nanosize. Display Omitted

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Mixed conductivity, structural and microstructural characterization of titania-doped yttria tetragonal zirconia polycrystalline/titania-doped yttria stabilized zirconia composite anode matrices

Taking advantage of the fact that TiO{sub 2} additions to 8YSZ cause not only the formation of a titania-doped YSZ solid solution but also a titania-doped YTZP solid solution, composite materials based on both solutions were prepared by solid state reaction. In particular, additions of 15 mol% of TiO{sub 2} give rise to composite materials constituted by 0.51 mol fraction titania-doped yttria tetragonal zirconia polycrystalline and 0.49 mol fraction titania-doped yttria stabilized zirconia (0.51TiYTZP/0.49TiYSZ). Furthermore, Y{sub 2}(Ti{sub 1-y}Zr{sub y}){sub 2}O{sub 7} pyrochlore is present as an impurity phase with y close to 1, according to FT-Raman results. Lower and higher additions of titania than that of 15 mol%, i.e., x=0, 5, 10, 20, 25 and 30 mol% were considered to study the evolution of 8YSZ phase as a function of the TiO{sub 2} content. Furthermore, zirconium titanate phase (ZrTiO{sub 4}) is detected when the titania content is equal or higher than 20 mol% and this phase admits Y{sub 2}O{sub 3} in solid solution according to FE-SEM-EDX. The 0.51TiYTZP/0.49TiYSZ duplex material was selected in this study to establish the mechanism of its electronic conduction under low oxygen partial pressures. In the pO{sub 2} range from 0.21 to 10{sup -7.5} atm. the conductivity is predominantly ionic and constant over the range and its value is 0.01 S/cm. The ionic plus electronic conductivity is 0.02 S/cm at 1000 {sup o}C and 10{sup -12.3} atm. Furthermore, the onset of electronic conductivity under reducing conditions exhibits a -1/4 pO{sub 2} dependence. Therefore, it is concluded that the n-type electronic conduction in the duplex material can be due to a small polaron-hopping between Ti{sup 3+} and Ti{sup 4+}. -- Graphical abstract: FE-SEM micrograph of a polished and thermal etched surface of a Ti-doped YTZP/Ti-doped YSZ composite material. Display Omitted Research highlights: {yields} Ti-doped YTZP/Ti-doped YSZ composite materials are mixed conductors under low partial pressures. {yields} From 5 mol% of TiO{sub 2}, Y{sub 2}(Ti{sub 1-y},Zr{sub y}){sub 2}O{sub 7} pyrochlore is present as a minor phase, being y close to 1 according to FT-Raman studies. {yields} The onset of the electronic conductivity under reducing conditions exhibit a -1/4 pO{sub 2} dependence. The n-type electronic conduction is due to a small polaron-hopping between Ti{sup 3+} and Ti{sup 4+}.

36 MATERIALS SCIENCE↗

Thermal properties of the optically transparent pore-free nanostructured yttria-stabilized zirconia

The authors report results of investigation of thermal conductivity of nanocrystalline yttria-stabilized zirconia. The optically transparent pore-free bulk samples were prepared via the spark plasma sintering process to ensure homogeneity. Thermal conductivity K was measured by two different techniques. It was found that the pore-free nanostructured bulk zirconia is an excellent thermal insulator with the room-temperature Kapprox1.7-2.0 W/m K. It was also shown that the 'phonon-hopping' model can accurately describe specifics of K dependence on temperature and the grain size. The obtained results are important for optimization of zirconia properties for specific applications in advanced electronics and coatings.

36 MATERIALS SCIENCE↗

Compositional effects on the growth of Mg(M)O films

The influence of the composition on the crystallographic properties of deposited Mg(M)O (with M=Al, Cr, Ti, Y, and Zr) films is studied. For a flexible control of the composition, dual reactive magnetron sputtering was used as deposition technique. Two different approaches to predict the composition are discussed. The first is an experimental way based on the simple relationship between the deposition rate and the target-substrate distance. The second is a route using a Monte Carlo based particle trajectory code. Both methods require a minimal experimental input and enable the user to quickly predict the composition of complex thin films. Good control and flexibility allow us to study the compositional effects on the growth of Mg(M)O films. Pure MgO thin films were grown with a (111) preferential out-of-plane orientation. When adding M to MgO, two trends were noticed. The first trend is a change in the MgO lattice parameters compared to pure MgO. The second tendency is a decrease in the crystallinity of the MgO phase. The experimentally determined crystallographic properties are shown to be in correspondence with the predicted properties from molecular dynamics simulations.

36 MATERIALS SCIENCE↗

Hydrostatic pressure decreases the proton mobility in the hydrated BaZr{sub 0.9}Y{sub 0.1}O{sub 3} proton conductor

Impedance spectroscopy on the hydrated proton conductor BaZr{sub 0.9}Y{sub 0.1}O{sub 3} at high temperatures shows that the bulk proton conductivity activation energy E{sub b} scales with the strain parameter epsilon, as achieved by hydrostatic pressures up to 2 GPa, suggesting that large lattices favor proton diffusivity. At high temperature, E{sub b} increases upon pressure by 40%. The grain boundary activation energy Eg is around twice as E{sub b}, indicating higher proton mobility in grain boundaries as a result of pressure induced sintering. An expanded lattice with strain parameter epsilon>1 should have lower E{sub b}, suggesting that thin films expansive tensile strain could have larger proton conductivity.

36 MATERIALS SCIENCE↗

Laser ablation plume dynamics in nanoparticle synthesis

The dynamics of the plume ejected from the surface of solid targets (YSZ, Nd:YAG and graphite) by a CO{sub 2} laser pulse with a duration of {approx}500 {mu}s (at the 0.03 level), energy of 1.0-1.3 J and peak power of 6-7 kW have been studied using high-speed photography of the plume luminescence and shadow. The targets were used to produce nanopowders by laser evaporation. About 200 {mu}s after termination of the pulse, shadowgraph images of the plumes above the YSZ and Nd:YAG targets showed dark straight tracks produced by large particles. The formation of large ({approx}10 {mu}m) particles is tentatively attributed to cracking of the solidified melt at the bottom of the ablation crater. This is supported by the fact that no large particles are ejected from graphite, which sublimes without melting. Further support to this hypothesis is provided by numerical 3D modelling of melt cooling in craters produced by laser pulses of different shapes. (interaction of laser radiation with matter. laser plasma)

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Mechanosynthesis of nanopowders of the proton-conducting electrolyte material Ba(Zr, Y)O{sub 3-{delta}}

The formation of perovskite nanopowders of the common proton-conducting, electrolyte material Ba(Zr{sub 1-x}Y{sub x})O{sub 3-{delta}} is demonstrated by room temperature mechanosynthesis for the compositional range x=0, 0.058 and 0.148. This is achieved with a planetary ball mill at 650 rpm in zirconia vials, starting from BaO{sub 2} with ZrO{sub 2}, (ZrO{sub 2}){sub 0.97}(Y{sub 2}O{sub 3}){sub 0.03} or (ZrO{sub 2}){sub 0.92}(Y{sub 2}O{sub 3}){sub 0.08} precursors, respectively. Powder X-ray diffraction (XRD) reveals the formation of the perovskite phase in the early stages of milling with phase purity being achieved after milling times of 240 min for composition x=0.058 whereas 420 min is necessary for composition x=0.148. In contrast, traces of ZrO{sub 2} are apparent in composition x=0 even after milling times of 420 min. The use of BaCO{sub 3} as precursor does not allow the formation of the perovskite phase for any composition. The perovskite crystallites are spherical in shape with an average size determined from XRD of ca. 30 nm in agreement with transmission electron microscopy observations. FTIR spectra demonstrate that contamination levels of BaCO{sub 3} in the mechanosynthesized powders are very low. The spherical shape and nanoscale of the crystallites allow densification levels that are highly competitive when compared to BaZrO{sub 3}-based materials formed by alternative synthesis techniques documented in the literature. - Graphical abstract: The formation of perovskite nanopowders of the common proton-conducting, electrolyte, material Ba(Zr{sub 1-x}Y{sub x})O{sub 3-{delta}} is demonstrated by room temperature mechanosynthesis, starting from BaO{sub 2} with ZrO{sub 2}, (ZrO{sub 2}){sub 0.97}(Y{sub 2}O{sub 3}){sub 0.03} or (ZrO{sub 2}){sub 0.92}(Y{sub 2}O{sub 3}){sub 0.08} precursors.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

The electronic structures of vanadate salts: Cation substitution as a tool for band gap manipulation

The electronic structures of six ternary metal oxides containing isolated vanadate ions, Ba{sub 3}(VO{sub 4}){sub 2}, Pb{sub 3}(VO{sub 4}){sub 2}, YVO{sub 4}, BiVO{sub 4}, CeVO{sub 4} and Ag{sub 3}VO{sub 4} were studied using diffuse reflectance spectroscopy and electronic structure calculations. While the electronic structure near the Fermi level originates largely from the molecular orbitals of the vanadate ion, both experiment and theory show that the cation can strongly influence these electronic states. The observation that Ba{sub 3}(VO{sub 4}){sub 2} and YVO{sub 4} have similar band gaps, both 3.8 eV, shows that cations with a noble gas configuration have little impact on the electronic structure. Band structure calculations support this hypothesis. In Pb{sub 3}(VO{sub 4}){sub 2} and BiVO{sub 4} the band gap is reduced by 0.9-1.0 eV through interactions of (a) the filled cation 6s orbitals with nonbonding O 2p states at the top of the valence band, and (b) overlap of empty 6p orbitals with antibonding V 3d-O 2p states at the bottom of the conduction band. In Ag{sub 3}VO{sub 4} mixing between filled Ag 4d and O 2p states destabilizes states at the top of the valence band leading to a large decrease in the band gap (E{sub g}=2.2 eV). In CeVO{sub 4} excitations from partially filled 4f orbitals into the conduction band lower the effective band gap to 1.8 eV. In the Ce{sub 1-x}Bi{sub x}VO{sub 4} (0<=x<=0.5) and Ce{sub 1-x}Y{sub x}VO{sub 4} (x=0.1, 0.2) solid solutions the band gap narrows slightly when Bi{sup 3+} or Y{sup 3+} are introduced. The nonlinear response of the band gap to changes in composition is a result of the localized nature of the Ce 4f orbitals. - Graphical abstract: The electronic structures of six vanadate salts, Ba{sub 3}(VO{sub 4}){sub 2}, Pb{sub 3}(VO{sub 4}){sub 2}, YVO{sub 4}, BiVO{sub 4}, Ag{sub 3}VO{sub 4} and CeVO{sub 4}, are studied. The results show that the oxygen to vanadium charge transfer, which is largely responsible for the electronic structure near the Fermi level, can be altered significantly through interactions with the surrounding cations.

36 MATERIALS SCIENCE↗

Structural and conductivity studies of Y{sub 10-x}La{sub x}W{sub 2}O{sub 21}

The aim of this work was to determine structural parameters of the Y{sub 10-x}La{sub x}W{sub 2}O{sub 21} (x=0-10) solid solution series and investigate their electric properties. Crystallographic data shows a gradual increase in symmetry with increasing La content, as the structure evolves from orthorhombic, Y{sub 10}W{sub 2}O{sub 21}, towards the pseudo-cubic structure of Y{sub 5}La{sub 5}W{sub 2}O{sub 21}. The solubility limit of La{sub 2}O{sub 3} was found to be 50% (x=5). Above this level two phases were observed, La{sub 6}W{sub 2}O{sub 15} and (La,Y){sub 10+x}W{sub 2-x}O{sub 21-{delta}}. The conductivity of Y rich samples was very low, with sigma of the order 2x10{sup -5}-5x10{sup -5} S cm{sup -1} at 1000 deg. C, whilst ionic conductivity was observed for most La rich doped samples. The highest conductivity was observed for La{sub 10}W{sub 2}O{sub 21} and its doped analogues, at 1x10{sup -3}-5x10{sup -3} S cm{sup -1} at 1000 deg. C. Unit cell parameters were determined as a function of temperature from 0 to 1000deg. C, and thermal expansion of these materials was determined from temperature studies carried out at the Australian Synchrotron facility in Melbourne, Victoria, Australia. - Graphical abstract: The solubility limit of La{sub 2}O{sub 3} in Y{sub 10}W{sub 2}O{sub 21} was found to be >50% after which the structure was found to change to Weberite type structure, A' A''B' B''O{sub 7} that is closely related to the pyrochlore.

36 MATERIALS SCIENCE↗

Synthesis and photoluminescence properties of the high-brightness Eu{sup 3+}-doped M{sub 2}Gd{sub 4}(MoO{sub 4}){sub 7} (M=Li, Na) red phosphors

A series of red-emitting phosphors Eu{sup 3+}-doped M{sub 2}Gd{sub 4}(MoO{sub 4}){sub 7} (M=Li, Na) have been successfully synthesized at 850 Degree-Sign C by solid state reaction. The excitation spectra of the two phosphors reveal two strong excitation bands at 396 nm and 466 nm, respectively, which match well with the two popular emissions from near-UV and blue light-emitting diode chips. The intensity of the emission from {sup 5}D{sub 0} to {sup 7}F{sub 2} of M{sub 2}(Gd{sub 1-x}Eu{sub x}){sub 4}(MoO{sub 4}){sub 7} phosphors with the optimal compositions of x=0.85 for Li or x=0.70 for Na is about five times higher than that of Y{sub 2}O{sub 3}:Eu{sup 3+}. The quantum efficiencies of the entitled phosphors excited under 396 nm and 466 nm are also investigated and compared with commercial phosphors Sr{sub 2}Si{sub 5}N{sub 8}:Eu{sup 2+} and Y{sub 3}A{sub 5}O{sub 12}:Ce{sup 3+}. The experimental results indicate that the Eu{sup 3+}-doped M{sub 2}Gd{sub 4}(MoO{sub 4}){sub 7} (M=Li, Na) phosphors are promising red-emitting phosphors pumped by near-UV and blue light. - Graphical Abstract: The intensity of the red emission of M{sub 2}(Gd{sub 1-x}Eu{sub x}){sub 4}(MoO{sub 4}){sub 7} (M=Li, Na) phosphors with the optimal compositions is about five times higher than that of Y{sub 2}O{sub 3}:Eu{sup 3+}. Highlights: Black-Right-Pointing-Pointer Two novel Eu{sup 3+}-doped red phosphors (Na{sub 2}Gd{sub 4}(MoO{sub 4}){sub 2}, Li{sub 2}Gd{sub 4}(MoO{sub 4}){sub 7}) were synthesized. Black-Right-Pointing-Pointer Their emission intensities are about five times higher than that of Y{sub 2}O{sub 3}:Eu{sup 3+}. Black-Right-Pointing-Pointer Their quantum efficiencies are higher than that of commercial red phosphor Sr{sub 2}Si{sub 5}N{sub 8}:Eu{sup 2+}.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Effects of grain modification on the dielectric properties of A{sub 0.03}Ti{sub 0.10}Ni{sub 0.87}O (A:K{sup +},Mg{sup 2+},Y{sup 3+}) ceramics

We prepared K{sup +}-, Mg{sup 2+}-, and Y{sup 3+}-doped Ni-Ti-O polycrystalline ceramics by chemical synthesis combined with a traditional ceramic processing. Analysis of the microstructure and phase composition reveals that a core/shell structure can be observed and NiTiO{sub 3} phase exists as the grain boundary. Our results indicate that K{sup +}, Mg{sup 2+}, and Y{sup 3+} doping have remarkable influence on the dielectric properties of these NiO-based ceramics, which should be mainly attributed to the large variation of the activation energies of the conductivity in the grain interiors. The special core/shell structure and related interfacial polarization are responsible for the observed high dielectric behavior.

36 MATERIALS SCIENCE↗

Low dielectric loss and non-Debye relaxation of gamma-Y{sub 2}Si{sub 2}O{sub 7} ceramic at elevated temperature in X-band

Bulk single-phase gamma-Y{sub 2}Si{sub 2}O{sub 7} ceramic has been synthesized from a mixture of Y{sub 2}O{sub 3} powder and SiO{sub 2} nanopowder at 1400 deg. C. The dielectric properties are reported at the temperature ranging from room temperature to 1400 deg. C in X-band. The results show that gamma-Y{sub 2}Si{sub 2}O{sub 7} exhibits low dielectric loss and non-Debye relaxation behavior different from that of SiO{sub 2}. The peculiar relaxation peak is attributed to the structural relaxation polarization caused by thermal-excitation structural defects, which implies that no ionic conductance exists in this material. Such low dielectric loss will draw much attention for potential dielectric applications at high temperature.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Concentration dependence of the Er{sup 3+} visible and infrared luminescence in Y{sub 2-x}Er{sub x}O{sub 3} thin films on Si

Y{sub 2-x}Er{sub x}O{sub 3} thin films, with x varying between 0 and 0.72, have been successfully grown on crystalline silicon (c-Si) substrates by radio-frequency magnetron cosputtering of Y{sub 2}O{sub 3} and Er{sub 2}O{sub 3} targets. As-deposited films are polycrystalline, showing the body-centered cubic structure of Y{sub 2}O{sub 3}, and show only a slight lattice parameter contraction when x is increased, owing to the insertion of Er ions. All the films exhibit intense Er-related optical emission at room temperature both in the visible and infrared regions. By studying the optical properties for different excitation conditions and for different Er contents, all the mechanisms (i.e., cross relaxations, up-conversions, and energy transfers to impurities) responsible for the photoluminescence (PL) emission have been identified, and the existence of two different well-defined Er concentration regimes has been demonstrated. In the low concentration regime (x up to 0.05, Er-doped regime), the visible PL emission reaches its highest intensity, owing to the influence of up-conversions, thus giving the possibility of using Y{sub 2-x}Er{sub x}O{sub 3} films as an up-converting layer in the rear of silicon solar cells. However, most of the excited Er ions populate the first two excited levels {sup 4}I{sub 11/2} and {sup 4}I{sub 13/2}, and above a certain excitation flux a population inversion condition between the former and the latter is achieved, opening the route for the realization of amplifiers at 2.75 mum. Instead, in the high concentration regime (Er-compound regime), an increase in the nonradiative decay rates is observed, owing to the occurrence of cross relaxations or energy transfers to impurities. As a consequence, the PL emission at 1.54 mum becomes the most intense, thus determining possible applications for Y{sub 2-x}Er{sub x}O{sub 3} as an infrared emitting material.

36 MATERIALS SCIENCE↗

Growth and properties of epitaxial GdN

Epitaxial gadolinium nitride films with well-oriented crystallites of up to 30 nm have been grown on yttria-stabilized zirconia substrates using a plasma-assisted pulsed laser deposition technique. We observe that the epitaxial GdN growth proceeds on top of a gadolinium oxide buffer layer that forms via reaction between deposited Gd and mobile oxygen from the substrate. Hall effect measurements show the films are electron doped to degeneracy, with carrier concentrations of 4x10{sup 20} cm{sup -3}. Magnetic measurements establish a T{sub C} of 70 K with a coercive field that can be tuned from 200 Oe to as low as 10 Oe.

36 MATERIALS SCIENCE↗