Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “WHISKERS”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 19 records

Validation of the dynamic recrystallization (DRX) mechanism for whisker and hillock growth on thin films

Our study was performed to validate a first-principles model for whisker and hillock formation based on the cyclic dynamic recrystallization (DRX) mechanism in conjunction with long-range diffusion. The test specimens were evaporated Sn films on Si having thicknesses of 0.25 μm, 0.50 μm, 1.0 μm, 2.0 μm, and 4.9 μm. Air annealing was performed at 35°C, 60°C, 100°C, 120°C, or 150°C over a time duration of 9 days. The stresses, anelastic strains, and strain rates in the Sn films were predicted by a computational model based upon the constitutive properties of 95.5Sn-3.9Ag-0.6Cu (wt.%) as a surrogate for pure Sn. The cyclic DRX mechanism and, in particular, whether long whiskers or hillocks were formed, was validated by comparing the empirical data against the three hierarchal requirements: (1) DRX to occur at all: εc = A D o m Z n , (2) DRX to be cyclic: D o < 2D r, and (3) Grain boundary pinning (thin films): h versus d. Continuous DRX took place in the 2.0-μm and 4.9-μm films that resulted in short stubby whiskers. Depleted zones, which resulted solely from a tensile stress-driven diffusion mechanism, confirmed the pervasiveness of long-range diffusion so that it did not control whisker or hillock formation other than a small loss of activity by reduced thermal activation at lower temperatures. Furthermore, a first-principles DRX model paves the way to develop like mitigation strategies against long whisker growth.

36 MATERIALS SCIENCE↗

Platelet composite coatings for tin whisker mitigation

In this study, reliable methods for tin whisker mitigation are needed for applications that utilize tin-plated commercial components. Tin can grow whiskers that can lead to electrical shorting, possibly causing critical systems to fail catastrophically. The mechanisms of tin whisker growth are unclear and this makes prediction of the lifetimes of critical components uncertain. The development of robust methods for tin whisker mitigation is currently the best approach to eliminating the risk of shorting. Current mitigation methods are based on unfilled polymer coatings that are not impenetrable to tin whiskers. In this paper we report tin whisker mitigation results for several filled polymer coatings. The whisker-penetration resistance of the coatings was evaluated at elevated temperature and high humidity and under temperature cycling conditions. The composite coatings comprised Ni and MgF 2 -coated Al/Ni/Al platelets in epoxy resin or silicone rubber. In addition to improved whisker mitigation, these platelet composites have enhanced thermal conductivity and dielectric constant compared with unfilled polymers.

36 MATERIALS SCIENCE↗

Mullite Whiskers and Mullite-whisker Felt

The Naval Surface Warfare Center has developed processes for the preparation of mullite (3(Al2O3)(dot)2(SiO2)) whiskers and mullite-whisker felt. Three patents on the technology were issued in 1990. The processes are based on chemical reactions between AlF3, Al2O3, and SiO2. The felt is formed in-situ during the processing of shaped powdered precursors. It consists of randomly oriented whiskers which are mutually intergrown forming a rigid structure. The microstructure and properties of the felt and size of the whiskers can be modified by varying the amount of Al2O3 in the starting mixture. Loose mullite whiskers can be used as a reinforcement for polymer-, metal-, and ceramic-matrix composites. The felt can be used as preforms for fabricating composite materials as well as for thermal insulation and high temperature, chemically stable filters for liquids (melts) and gases.

Talmy, Inna G.↗

Local, submicron, strain gradients as the cause of Sn whisker growth.

It has been shown experimentally that local in-plane residual strain gradients occur around the root of spontaneously growing Sn whiskers on the surface of Sn coatings deposited on Cu. The strain distribution has been determined with synchrotron white beam micro Laue diffraction measurements. The observed in-plane residual strain gradients in combination with recently revealed out-of-plane residual strain-depth gradients [M. Sobiech et al., Appl. Phys. Lett. 93, 011906 (2008)] provide the driving forces for whisker growth.

43 PARTICLE ACCELERATORS↗

NASA Goddard Space Flight Center Tin Whisker (and Other Metal Whisker) Homepage

This website provides information about tin whiskers and related research. The independent research performed during the past 50+ years is so vast that it is impractical to cover all aspects of tin whiskers in this one resource. Therefore, the absence of information in this website about a particular aspect of tin whiskers should NOT be construed as evidence of absence.

Brusse, Jay↗

Refining whisker size of 2024Al/Al18B4O33w composite through extrusion and its effects on the material's micro-structures and mechanical properties

Highlights: • The nonuniform distributions of stress and velocity along whisker lead to whisker breakage. • The microcrack between broken whiskers can propagate into interface or matrix, related to the wedge angle of broken whisker. • The whisker breakage and staggered result in the decreasing distance between neighboring whiskers. • The smaller distance between neighboring whiskers reduces the resistance to the propagation of crack resulting in the lower ultimate tensile strength of extruded composite. - Abstract: Hot extrusion is used to improve the distribution of whiskers and refine the whisker sizes of 2024Al/Al{sub 18}B{sub 4}O{sub 33}w composite. The grain size and the ultimate tensile strength of the extruded 2024Al/Al{sub 18}B{sub 4}O{sub 33}w composite are analyzed. The results show that the average length of whiskers decreases due to the whisker breakage. The nonuniform distributions of stress and velocity along the whisker lead to whisker breakage. The microcrack between the broken whiskers can propagate into the interface or the matrix, related to the wedge angle of the broken whisker. The extrusion is beneficial to the whisker staggered and makes it easy for the microcracks filled with matrix. The whisker breakage and the whisker staggered result in the decreasing distance between the neighboring whiskers. Due to the dislocation motion constrained by matrix and the overlap of the deformation areas, the decreasing distance between the neighboring whiskers promoting the recrystallization results in the smaller grain size. During tensile tests, due to the smaller resistance with the smaller distance between the neighboring whiskers, the cracks between the progressive broken whiskers are easy to coalesce resulting in the lower ultimate tensile strength of the extruded composite.

36 MATERIALS SCIENCE↗

Understanding and Predicting Metallic Whisker Growth and its Effects on Reliability (LDRD Final Report)

Tin (Sn) whiskers are conductive Sn filaments that grow from Sn-plated surfaces, such as surface finishes on electronic packages. The phenomenon of Sn whiskering has become a concern in recent years due to requirements for lead (Pb)-free soldering and surface finishes in commercial electronics. Pure Sn finishes are more prone to whisker growth than their Sn-Pb counterparts and high profile failures due to whisker formation (causing short circuits) in space applications have been documented. At Sandia, Sn whiskers are of interest due to increased use of Pb-free commercial off-the-shelf (COTS) parts and possible future requirements for Pb-free solders and surface finishes in high-reliability microelectronics. Lead-free solders and surface finishes are currently being used or considered for several Sandia applications. Despite the long history of Sn whisker research and the recently renewed interest in this topic, a comprehensive understanding of whisker growth remains elusive. This report describes recent research on characterization of Sn whiskers with the aim of understanding the underlying whisker growth mechanism(s). The report is divided into four sections and an Appendix. In Section 1, the Sn plating process is summarized. Specifically, the Sn plating parameters that were successful in producing samples with whiskers will be reviewed. In Section 2, the scanning electron microscopy (SEM) of Sn whiskers and time-lapse SEM studies of whisker growth will be discussed. This discussion includes the characterization of straight as well as kinked whiskers. In Section 3, a detailed discussion is given of SEM/EBSD (electron backscatter diffraction) techniques developed to determine the crystallography of Sn whiskers. In Section 4, these SEM/EBSD methods are employed to determine the crystallography of Sn whiskers, with a statistically significant number of whiskers analyzed. This is the largest study of Sn whisker crystallography ever reported. This section includes a review of previous literature on Sn whisker crystallography. The overall texture of the Sn films was also analyzed by EBSD. Finally, a short Appendix is included at the end of this report, in which the X-Ray diffraction (XRD) results are discussed and compared to the EBSD analyses of the overall textures of the Sn films. Sections 2, 3, and 4 have been or will be submitted as stand-alone papers in peer-reviewed technical journals. A bibliography of recent Sandia Sn whisker publications and presentations is included at the end of the report.

36 MATERIALS SCIENCE↗

A mechanistic study on the synthesis of β-Sialon whiskers from coal fly ash

Graphical abstract: The appearance of bead-like whiskers indicated that the growth mechanism of the β-Sialon whiskers was different from the conventional one, in which a chain of droplets were formed and then consumed to participate in the formation of the whiskers. - Highlights: • β-Sialon whiskers were synthesized using waste fly ash by carbothemal reduction reaction under nitrogen atmosphere. • Rod-like β-Sialon whiskers with a diameter of 100–500 nm were formed. • Bead-like whiskers as intermediate morphology of the growing β-Sialon whiskers were found with increasing sintering time. • The growth mechanism of β-Sialon whiskers was different from the conventional VLS mechanism. • A chain of droplets were formed and participated in the formation of the whiskers. - Abstract: β-Sialon whiskers were produced at 1420 °C through carbothemal reduction reaction under nitrogen atmosphere using fly ash from coal-fired power plants. The effects of sintering time on the phase formation and morphology of the products were investigated by X-ray diffraction (XRD), scanning electron microscope (SEM) and energy dispersive spectrometer (EDS) techniques. Rod-like β-Sialon whiskers with the diameter of 100–500 nm were successfully formed. With increasing sintering time, bead-like morphology during the growth process of the whiskers was found, and growth mechanism of β-Sialon whiskers was also discussed in detail. The growth mechanism proposed in this study was different from the conventional vapor–liquid–solid (VLS) mechanism.

36 MATERIALS SCIENCE↗

Effects of Conformal Coat on Tin Whisker Growth

A whisker from a tin plated part was blamed for the loss of a commercial spacecraft in 1998. Although pure tin finishes are prohibited by NASA, tin plated parts, such as hybrids, relays and commercial off the shelf (COTS) parts, are something discovered to have been installed in NASA spacecraft. Invariably, the assumption is that a conformal coat will prevent the growth of, or short circuits caused by, tin whiskers. This study measures the effect a Uralane coating has on the initiation and growth of tin whiskers, on the ability of this coating to prevent a tin whisker from emerging from the coating, and on the ability to prevent shorting. A sample of fourteen brass substrates (1 inch by 4 inches by 1/16 inch) were plated by two separate processes: half of the specimens were 'bright' tin plated directly over the brass substrate and half received a copper flash over the brass substrate prior to 'bright' tin plating. Each specimen was coated on one half of the substrate with three bi-directional sprays of Uralane 5750 to a nominal thickness of 25 to 75 micrometers (1 to 3 mils). Several specimens of both types, Cu and non-Cu flashed, were placed in an oven maintained at 50 C as others' work suggests that this is the optimal temperature for whisker formation. The remaining specimens were maintained at room ambient conditions. The surfaces of each specimen have been regularly inspected using both optical (15 to 400x power) and Scanning Electronic Microscopy (SEM). Many types of growths, including needle-like whiskers, first appeared approximately three months after plating on the non-conformally coated sides of all specimens. At four months, 4 to 5 times more growth sites were observed on the coated side; however, the density of growth sites on the non-conformally coated side has since increased rapidly, and now, at one year, is about the same for both sides. The density of growth sites is estimated at 90/sq mm with 30 percent of the sites growing whiskers (needle-like forms) with the potential to cause short circuit bridging. The average growth rate of the needle-like whiskers on the non-conformally coated areas is about 130 micrometers per year with some outliers reaching 800 micrometers after one year. It is more difficult to make growth measurements under the conformal coat. As yet no whiskers have been observed to penetrate through the coating surface, however, a number of tin nodules appear on the verge of breaking through the thinner regions of the coating surface. These domes are developing sharper and sharper tips, as if a growing whisker is about to push its way through a tough skin. Our observations are that the specimens with copper flash show a much lower density of nucleation sites and significantly slower whisker growth compared to the specimens that have only bright tin plating over brass. The specimens kept at room temperature have a higher whisker density than those stored at 50 C. This is an unexpected result and does not agree with the published findings of others. All of the whiskers originate from small surface defects (thin, tiny scratches) that appear over the entire surface of each specimen.

Kadesch, Jong S.↗

A study on in situ growth of TaC whiskers in Al{sub 2}O{sub 3} matrix powder for ceramic cutting tools

Graphical abstract: In situ growth of TaC whiskers (TaC{sub w}) was synthesized in an α-Al{sub 2}O{sub 3} matrix powder via a carbothermal reduction technique. The whiskers were 0.2–0.5 μm in diameter and 5–15 μm in length; they were straight and had smooth surfaces. Highlights: ► In situ growth of TaC whiskers was synthesized in an α-Al{sub 2}O{sub 3} matrix powder. ► The wet mixing method and 1450 °C were suitable for whiskers growth. ► The growth of TaC whiskers is not influenced by the Al{sub 2}O{sub 3} powder. ► The major impurities were TaC particles, nickel and unreacted carbon. -- Abstract: In situ growth of tantalum carbide (TaC) whiskers was synthesized in an α-Al{sub 2}O{sub 3} matrix powder via a carbothermal reduction technique within a temperature range of 1350–1500 °C in an argon atmosphere. The starting materials consisted of Ta{sub 2}O{sub 5}, C, Ni and NaCl powders. Different mixing methods and various reaction temperatures were employed. Most of the prepared whiskers were 0.2–0.5 μm in diameter and 5–15 μm in length. The reaction temperature of 1400–1450 °C was suitable for the growth of TaC whiskers and a wet mixing method was beneficial to increase the whisker yield. Some of the whiskers exhibited the needle shape while others exhibited the screw shape. The growth mechanism of the whiskers was a complex mechanism involving a helical screw dislocation mechanism and a vapor–liquid–solid process. No obvious influences of the Al{sub 2}O{sub 3} matrix powder on the growth of TaC whiskers were found and the major impurities in the obtained powder were TaC particles, nickel and unreacted carbon.

36 MATERIALS SCIENCE↗

An analysis of the wear behavior of SiC whisker reinforced alumina from 25 to 1200 C

A model is described for predicting the wear behavior of whisker reinforced ceramics. The model was successfully applied to a silicon carbide whisker reinforced alumina ceramic composite subjected to sliding contact. The model compares the friction forces on the whiskers due to sliding, which act to pull or push them out of the matrix, to the clamping or compressive forces on the whiskers due to the matrix, which act to hold the whiskers in the composite. At low temperatures, the whiskers are held strongly in the matrix and are fractured into pieces during the wear process along with the matrix. At elevated temperatures differential thermal expansion between the whiskers and matrix can cause loosening of the whiskers and lead to pullout during the wear process and to higher wear. The model, which represents the combination of elastic stress analysis and a friction heating analysis, predicts a transition temperature at which the strength of the whiskers equals the clamping force holding them in the matrix. Above the transition the whiskers are pulled out of the matrix during sliding, and below the transition the whiskers are simply fractured. The existence of the transition gives rise to a dual wear mode or mechanism behavior for this material which was observed in laboratory experiments. The results from this model correlate well with experimentally observed behavior indicating that the model may be useful in obtaining a better understanding of material behavior and in making material improvements.

Dellacorte, Christopher↗

An analysis of the wear behavior of SiC whisker-reinforced alumina from 25 to 1200 C

A model is described for predicting the wear behavior of whisker reinforced ceramics. The model was successfully applied to a silicon carbide whisker reinforced alumina ceramic composite subjected to sliding contact. The model compares the friction forces on the whiskers due to sliding, which act to pull or push them out of the matrix, to the clamping or compressive forces on the whiskers due to the matrix, which act to hold the whiskers in the composite. At low temperatures, the whiskers are held strongly in the matrix and are fractured into pieces during the wear process along with the matrix. At elevated temperatures differential thermal expansion between the whiskers and matrix can cause loosening of the whiskers and lead to pullout during the wear process and to higher wear. The model, which represents the combination of elastic stress analysis and a friction heating analysis, predicts a transition temperature at which the strength of the whiskers equals the clamping force holding them in the matrix. Above the transition the whiskers are pulled out of the matrix during sliding, and below the transition the whiskers are simply fractured. The existence of the transition gives rise to a dual wear mode or mechanism behavior for this material which was observed in laboratory experiments. The results from this model correlate well with experimentally observed behavior indicating that the model may be useful in obtaining a better understanding of material behavior and in making material improvements.

Dellacorte, Christopher↗

Temperature-dependent transformation from whisker- to nanoparticle-strengthened composite interface in the Al{sub 2}O{sub 3}/Ag-based alloy system and mechanical properties of the joints

Al{sub 4}B{sub 2}O{sub 9}-whisker-coated Al{sub 2}O{sub 3} ceramics were bonded by AgCu–4.5 wt.%Ti alloy in vacuum. The microstructure of the whisker-coated Al{sub 2}O{sub 3} joints was investigated by scanning electron microscopy, transmission electron microscopy and X-ray diffraction. A continuous (Cu,Al){sub 3}Ti{sub 3}O layer formed against the alloy at lower bonding temperatures, and a complex transition zone bordering the whiskers was observed, which consisted of Ag nanoparticles, titanium oxides, TiB{sub 2}, (Cu,Al){sub 3}Ti{sub 3}O nanoparticles and possible Ag{sub 3}Al. As the bonding temperature increased, the Al{sub 2}O{sub 3}/AgCuTi interface was found to transform from whisker- to nanoparticle-strengthened composite region. Bend test results revealed that both the whiskers grown on Al{sub 2}O{sub 3} and the dispersive nanoscale products in the alloy played positive roles in improving the joint properties. The maximum bend strength of the whisker-coated Al{sub 2}O{sub 3} joints was 313 MPa at the bonding temperature of 820 °C. - Highlights: • Al{sub 4}B{sub 2}O{sub 9}-whisker-coated Al{sub 2}O{sub 3} ceramics were bonded by AgCu–4.5 wt.%Ti alloy in vacuum. • Microstructures of whisker-coated Al{sub 2}O{sub 3} joints were investigated in detail. • Both whiskers and the dispersive nanoscale products can improve the joint properties. • The maximum bend strength of the whisker-coated Al{sub 2}O{sub 3} joints was 313 MPa.

36 MATERIALS SCIENCE↗