Enhancing mobility and interface state engineering via UV-ozone treatment in BEOL-compatible ultrathin TiO 2 transistors
It has emerged as a potential candidate to improve the performance of monolithic-three-dimensional (M3D) integration of fused logic and memories through low-temperature in situ synthesis of high-performance metal–oxide–semiconductor (MOS) transistors. Here, we report the demonstration of the BEOL-compatible low thermal budget (350 °C) fabrication process of ultrathin-TiO2 transistors by the combination of RTA and UV-ozone treatment (RTA-UVOz). UV–ozone (UVOz) treatment of TiO2 anatase films significantly enhances stability, boosting ION current and field effect mobility (μ FE ) by two times of magnitude in TiO2 TFTs. UV ozone treatment helps to eliminate pre-existing oxygen vacancies and carbon contamination on TiO2 channels even at low temperature (100 °C), resulting in high-quality channel/dielectric interfaces with low interface states (D it ). During UVOz treatment, oxygen species (O x ) passivate the oxygen vacancies ($V$$^{2+}_{o}$), and hence low concentration of $V$$^{2+}_{o}$ would be left for ionization/de-ionization under PBS/NBS, leading to improved bias stress stability. Furthermore, the TiO 2 TFTs with thin ZrO 2 gate dielectric exhibited excellent performance including a lower subthreshold swing (SS) of 98 mV/dec with high drive I ON current ∼ 4.5 μA/μm, a high I ON /I OFF > 10 9 , and mobility μFE of 7 cm 2 /V-s under a battery powered voltage of 1 V. UV–ozone treatment enables high-performance, CMOS-compatible TiO 2 transistors with a low thermal budget, ideal for next-generation flexible, energy-efficient electronics.