Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “Ti3Al”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 19 records

Substitutional and Interstitial Diffusion in alpha2-Ti3Al(O)

The reaction between Al2O3 and alpha2-Ti3Al was studied with a series of Al2O3/alpha2-Ti3Al multiphase diffusion couples annealed at 900, 1000 and 1100 C. The diffusion-paths were found to strongly depend on alpha2- Ti3Al(O) composition. For alloys with low oxygen concentrations the reaction involved the reduction of Al2O3, the formation of a gamma-TiAl reaction-layer and diffusion of Al and O into the alpha2-Ti3Al substrate. Measured concentration profiles across the interaction-zone showed "up-hill" diffusion of O in alpha2-Ti3Al(O) indicating a significant thermodynamic interaction between O and Al, Ti or both. Diffusion coefficients for the interstitial O in alpha2-Ti3Al(O) were determined independently from the interdiffusion of Ti and Al on the substitutional lattice. Diffusion coefficients are reported for alpha2-Ti3Al(O) as well as gamma-TiAl. Interpretation of the results were aided with the subsequent measurement of the activities of Al, Ti and O in alpha 2-Ti3Al(O) by Knudsen effusion-cell mass spectrometry.

Copland, Evan↗

A new ordered tetragonal phase in the Ti3Al+Nb system

Results are reported from an experimental study of phase stability in a plasma-sprayed Ti3Al+Nb alloy using TEM and electron diffraction techniques. The alloys was produced from Ti3Al+Nb powder via an inductively coupled plasma deposition process. Evidence was found for the ordering of the B2 phase to a structure similar to the DO3-type phase, but with a tetragonal distortion. An ordered tetragonal phase (T) is proposed to account for these observations, and the existence of the B2 - T ordering transformation in the Ti3Al+Nb system is suggested. The T phase can be regarded as a DO3-like phase with a tetragonal distortion. The tegragonality c0/a0 is approximately equal to 1.02, and a0 equals 0.65 +/-0.01 nm.

Hsiung, L. M.↗

Cyclic oxidation of aluminide coatings on Ti3Al+Nb

A number of pack aluminide coatings were produced on fiber-reinforced Ti3Al+Nb composites and were compared for their protection effect in cyclic oxidation at 982 C. It was found that pack aluminizing of Ti3Al+Nb can successfully produce an oxidation resistant TiAl3 coating which forms alpha-Al2O3 scales. These coatings offer a substantial improvement over the uncoated matrix material in 982 C cyclic oxidation. Coating cracks were found to contribute to degradation of thick coatings.

Smialek, James L.↗

A novel hydride phase in hydrogen charged Ti3Al

The effect of internal hydrogen on the microstructural modification of Ti3Al (alpha-2) compound was studied by large-angle neutron scattering and TEM. Ti-25 at. pct Al (Ti3Al) specimens were exposed to gaseous hydrogen atmosphere at 600 C that resulted in internal hydrogen concentration of 2000 ppm. The hydrogen-charged alloy consisted of a mixture of alpha-2 phase and a novel Ti3AlH phase with the E2(1), (Pm3m) crystal structure. The lattice parameters and atomic arrangement of the Ti3AlH phase were determined.

Schwartz, D. S.↗

Tribological properties of ceramic-(Ti3Al-Nb) sliding couples for use as candidate seal materials to 700 C

Tribological properties of Ti3Al-Nb intermetallic disks sliding against alumina-boria-silicate fabric were ascertained in air at temperatures from 25 to 700 C. These materials are candidates for sliding seal applications for the National AeroSpace Plane. The tests were done using a pin on disk tribometer. Sliding was unidirectional at 0.27 m/sec under a nominal contact stress of 340 kPa. Gold sputter or ion plating deposited films were used to reduce friction and wear. Rhodium and palladium films were used beneath the gold lubricating films to prevent diffusion of the substrate into the gold at high temperature. The friction and wear of the unlubricated specimens was unacceptable. Friction coefficients were generally greater than 1.0. The ion plated gold films, when used with a rhodium diffusion barrier reduced friction by almost a factor of 2. Wear was also substantially reduced. The sputter deposited films were not adherent unless the substrate was sputter cleaned immediately prior to film deposition. Palladium did not function as a diffusion barrier.

Dellacorte, Christhopher↗

Evaluation of the Transient Liquid Phase (TLP) Bonding Process for Ti3Al-Based Honeycomb Core Sandwich Structure

The suitability of using transient liquid phase (TLP) bonding to fabricate honeycomb core sandwich panels with Ti-14Al-21Nb (wt%) titanium aluminide (T3Al) face sheets for high-temperature hypersonic vehicle applications was evaluated. Three titanium alloy honeycomb cores and one Ti3Al alloy honeycomb core were investigated. Edgewise compression (EWC) and flatwise tension (FWT) tests on honeycomb core sandwich specimens and tensile tests of the face sheet material were conducted at temperatures ranging from room temperature to 1500 F. EWC tests indicated that the honeycomb cores and diffusion bonded joints were able to stabilize the face sheets up to and beyond the face sheet compressive yield strength for all temperatures investigated. The specimens with the T3Al honeycomb core produced the highest FWT strengths at temperatures above 1000 F. Tensile tests indicated that TLP processing conditions resulted in decreases in ductility of the Ti-14Al-21Nb face sheets. Microstructural examination showed that the side of the face sheets to which the filler metals had been applied was transformed from equiaxed alpha2 grains to coarse plates of alpha2 with intergranular Beta. Fractographic examination of the tensile specimens showed that this transformed region was dominated by brittle fracture.

Bird, R. Keith↗

Neutron Diffraction Study Oxygen Dissolution Alpha(sub 2)-Ti3Al

Rietveld refinements of neutron powder diffraction data on alpha(sub 2)-Ti3Al have been performed to determine the crystal structure as a function of interstitial oxygen (O) concentration for three alloys with a Ti/Al ratio of approximately equal to 2.34 and O concentrations of 0.25%, 3.99% and 7.71%. The structures of the allows are hexagonal in space group P6(sub 3)/mmc where Ti and Al atoms populate unique sites with excess Al at the Ti site and O atoms occupy octahedral interstitial sites surrounded by six Ti sites. The length of the c-axis was found to increase linearly as the O occupancy of the interstitial sites increased; this lattice lengthening effect was much less pronounced along the alpha axis. Correspondingly, the increases in the lengths of Ti-Al and Ti-Ti bonds with a major component of their direction parallel to the c-axis were roughly an order of magnitude greater than the increases in the lengths of Ti-al and Ti-Ti bonds more closely aligned with the alpha-axis. Densities calculated form the lattice parameters and occupancy factors fall in the range (4.118 plus or minus 0.004) grams per cubic centimeter to (4.194 plus or minus 0.004) grams per cubic centimeter, and exhibit a nearly linear increase with oxygen concentration. Measured densities of (4.113 plus or minus 0.001) grams per cubic centimeter, (4.146 plus or minus 0.009) grams per cubic centimeter, and (4.191 plus or minus 0.002) grams per cubic centimeter for these alloys agree with the results of the refinements.

Jones, Camille Y.↗

Reaction zone microstructure in a Ti3Al + Nb/SiC composite

A composite of Ti-25Al-13Nb (atomic percent) matrix with a continuous SiC fiber (SCS-6) reinforcement was fabricated by hot pressing powder cloths and mats of fiber. The fiber/matrix reaction zone was studied using scanning electron microscopy (SEM) and transmission electron microscopy/analytical electron microscopy (TEM/AEM) techniques. The extent of reaction was determined, phases were identified, and solute partitioning among the phases was determined. It was found that the matrix had reacted only with a portion of the carbon-rich outer layer of the SCS-6 fiber. The reaction zone contained two concentric zones which are distinguished by the presence of different carbide phases. Both zones contained a hexagonal Si-bearing phase, and one of the zones also contained some fine scattered porosity. The results are discussed with reference to available phase equilibria data.

Baumann, S. F.↗

Investigation of reaction kinetics and interfacial phase formation in Ti3Al + Nb composites

Titanium aluminide metal matrix composites are prominent materials systems being considered for high temperature aerospace applications. One of the major problems with this material is the reactivity between existing reinforcements and the matrix after prolonged thermal exposure. This paper presents results from an investigation of reaction kinetics between Ti-14Al-21Nb (wt pct) and SCS-6 fibers and SiC fibers with surface coatings of TiB2, TiC, TiN, W, and Si. Microstructural evaluation of the reaction layers as well as matrix regions around the fibers is presented.

Wawner, F. E.↗

Hydrogen tolerance of a Ti3Al-based alloy

The Ti-24Al-11Nb (Ti-24-11) alloy heat-treated to the fine basketweave microstructure was shown previously to be hydrogen-tolerant. In order to assess its limit of hydrogen tolerance, the tensile, creep, fracture toughness, and sustained-load crack growth behaviors of this alloy were studied as a function of hydrogen content. The mechanical test results indicated that the fine basketweave microstructure was tolerant to hydride embrittlement for hydrogen contents up to about 1500 wppm. On the other hand, hydrogen charging experiments indicated that the Ti-24-11 alloy was severely cracked and pulverized under zero load when the hydrogen content exceeded 3000 wppm. X-ray diffraction results revealed that the dichotomous behaviors might be due to the formation of face-centered cubic (fcc) delta-type hydrides at higher hydrogen contents but face-centered tetragonal (fct) gamma-type hydrides at lower hydrogen contents.

Chan, Kwai S.↗

The effect of alloy composition on the mechanism of stress-corrosion cracking of titanium alloys in aqueous environments

A detailed study was made of the relation between the size distribution of Ti3Al particles in a Ti-8Al alloy and the tensile properties measured in air and in saltwater. The size distribution of Ti3Al was varied by isothermal aging for various times at temperatures in the range 770 to 970 K (930 to 1290 F). The aging kinetics were found to be relatively slow. Quantitative measurements of the particle coarsening rate at 920 K (1200 F) showed good agreement with the predicted behavior for coarsening controlled by matrix diffusion, and suggested that the specific free energy of the Ti3Al alpha interface in negligible small. In all cases, the Ti3Al particles were sheared by the glide dislocations. It was concluded that there is a definite correlation between the presence of deformable Ti3Al particles and an alloy's susceptibility to aqueous stress corrosion cracking. Furthermore, the appearance of the surface slip lines and the dislocation substructure in deformed specimens suggest that the specific effect of the Ti3Al particles is to cause a nonhomogeneous planar slip character and an enhanced chemical potential of the slip bands.

Wood, R. A.↗

Chemical compatibility issues related to use of copper as an interfacial layer for SiC fiber reinforced Ti3Ai+Nb composite

The reaction of Cu, a potential interfacial compliant layer for the Ti3Al plus Nb/SiC composite, with SiC, SCS-6 fiber, and the Ti3Al plus Nb matrix was examined at two temperatures: 1223 and 1273 K. Reaction of Cu with SiC resulted in the formation of a CuSi solution and free carbon, the reaction product being molten at 1273 K. Hot pressing the SCS-6 fiber in a Cu matrix at 1273 K resulted in cracking and delamination of the outer carbon-rich coating, thus allowing the Cu to penetrate to the SiC-carbon coating interface and react with SiC. In contrast, no such damage to the outer coating was observed at 1223 K. There was excessive reaction between Cu and the Ti3Al plus Nb matrix, the reaction product being molten both at 1223 and 1273 K. An interlayer of Nb between Cu and Ti3Al plus Nb matrix prevented the reaction between the two.

Misra, Ajay K.↗

Relation between surface slip topography and stress corrosion cracking in Ti-8 wt % Al

The deformation behavior of Ti-8 wt % Al has been investigated in an inert environment (air), and an aggressive environment (salt water). Details of surface slip geometry were examined by high resolution surface replicas at various stages of deformation in both environments. Specimens aged to contain a fine dispersion of Ti3Al precipitates failed by subcritical crack growth in salt water, whereas specimens in the single phase condition showed no effects of environment on the yield or fracture characteristics. The Ti3Al precipitates produce little change in strength level or slip character compared to the single phase alloy, and there is no evidence of any effects of environment on the character of surface slip. Rather, the presence of trenches along slip bands on the surface of aged specimens suggest that the specific effect of the Ti3Al precipitates is to render the surface slip steps chemically active relative to the surrounding matrix by slip induced dissolution of the particles.

Boyd, J. D.↗

Thermodynamics of Titanium-Aluminum-Oxygen Alloys Studied

Titanium-aluminum alloys are promising intermediate-temperature alloys for possible compressor applications in gas-turbine engines. These materials are based on the a2-Ti3Al + g-TiAl phases. The major issue with these materials is high oxygen solubility in a2-Ti3Al, and oxidation of unsaturated alloys generally leads to mixed non-protective TiO2+Al2O3 scales. From phase diagram studies, oxygen saturated a2-Ti3Al(O) is in equilibrium with Al2O3; however, oxygen dissolution has a detrimental effect on mechanical properties and cannot be accepted. To better understand the effect of oxygen dissolution, we examined the thermodynamics of titanium-aluminum-oxygen alloys.

Copland, Evan H.↗

Control of interface reactions in SIC/TI composites

The reaction between a 0.5 to 1.0 Al film and a thick Ti substrate to form TiAl3 occurs very rapidly on heating to 635 C and causes the Al to be confined to the surface region. After heating to 900 C Ti3Al is formed with little release of Al into alpha Ti. Further annealing at 900 C eventually causes the Ti3Al phase to decompose and a substantial amount of Al is released into alpha Ti. The interdiffusion coefficient for Al in alpha Ti at 900 C increases by less than one order of magnitude as Al is varied from 0 to 20 at %. These data were obtained from the (101) X-ray diffraction intensity band using polycrystalline samples. Improvements in the analysis of X-ray diffraction data for the determination of composition profiles are discussed.

Houska, C. R.↗

Reactions and diffusion between an Al film and a Ti substrate

The reaction between a 0.5 to 1.0 micron Al film and a thick Ti substrate to form TiAl3 occurs very rapidly on heating to 635 C and causes the Al to be confined to the surface region. After heating to 900 C, Ti3Al is formed with little release of Al into alpha-Ti. Further annealing at 900 C eventually causes the Ti3Al phase to decompose and a substantial amount of Al is released into alpha-Ti. The interdiffusion coefficient for Al in alpha-Ti at 900 C was found to increase by less than one order of magnitude as Al is varied from 0 to 20 at. pct. These data were obtained from the (101) X-ray diffraction intensity band using polycrystalline samples. Improvements in the analysis of X-ray diffraction data for the determination of composition profiles are discussed.

Rao, V. B.↗

Parametric studies to determine the effect of compliant layers on metal matrix composite systems

Computational simulation studies are conducted to identify compliant layers to reduce matrix stresses which result from the coefficient of thermal expansion mismatch and the large temperature range over which the current metal matrix composites will be used. The present study includes variations of compliant layers and their properties to determine their influence on unidirectional composite and constituent response. Two simulation methods are used for these studies. The first approach is based on a three-dimensional linear finite element analysis of a 9 fiber unidirectional composite system. The second approach is a micromechanics based nonlinear computer code developed to determine the behavior of metal matrix composite system for thermal and mechanical loads. The results show that an effective compliant layer for the SCS 6 (SiC)/Ti-24Al-11Nb (Ti3Al + Nb) and SCS 6 (SiC)/Ti-15V-3Cr-3Sn-3Al (Ti-15-3) composite systems should have modulus 15 percent that of the matrix and a coefficient of thermal expansion of the compliant layer roughly equal to that of the composite system without the CL. The matrix stress in the longitudinal and the transverse tangent (loop) direction are tensile for the Ti3Al + Nb and Ti-15-3 composite systems upon cool down from fabrication. The fiber longitudinal stress is compressive from fabrication cool down. Addition of a recommended compliant layer will result in a reduction in the composite modulus.

Caruso, J. J.↗