Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “Tensile testing”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 19 records

Testing Tensile and Shear Epoxy Strength at Cryogenic Temperatures

This paper covers cryogenic, tensile testing and research completed on a number of epoxies used in cryogenic applications. Epoxies are used in many different applications; however, this research focused on the use of epoxy used to bond MLI standoffs to cryogenic storage tanks and the loads imparted to the tank through the MLI. To conduct testing, samples were made from bare stainless steel, aluminum and primed aluminum. Testing involved slowly cooling test samples with liquid nitrogen then applying gradually increasing tensile loads to the epoxy. The testing evaluated the strength and durability of epoxies at cryogenic temperatures and serves as a base for future testing. The results of the tests showed that some epoxies withstood the harsh conditions while others failed. The two epoxies yielding the best results were Masterbond EP29LPSP and Scotch Weld 2216. For all metal surfaces tested, both epoxies had zero failures for up to 11.81 kg of mass.

multilayer insulation↗

Testing Tensile and Shear Epoxy Strength at Cryogenic Temperatures

This paper covers cryogenic, tensile testing and research completed on a number of epoxies used in cryogenic applications. Epoxies are used in many different applications; however, this research focused on the use of epoxy used to bond MLI standoffs to cryogenic storage tanks and the loads imparted to the tank through the MLI. To conduct testing, samples were made from bare stainless steel, aluminum and primed aluminum. Testing involved slowly cooling test samples with liquid nitrogen then applying gradually increasing tensile loads to the epoxy. The testing evaluated the strength and durability of epoxies at cryogenic temperatures and serves as a base for future testing. The results of the tests showed that some epoxies withstood the harsh conditions while others failed. The two epoxies yielding the best results were Masterbond EP29LPSP and Scotch Weld 2216. For all metal surfaces tested, both epoxies had zero failures for up to 11.81 kg of mass..

epoxy↗

A numerical and experimental approach to compare the effect of sample thickness in small in-situ SEM and large ex-situ tensile testing in Alloy 709

ASTM standards for tensile tests define specific sample size requirements regardless of grain size of the material. However, sample size requirements for testing should be considered in conjunction with the number of grains within its reduced cross-sectional area. This is particularly important for in-situ Scanning Electron Microscope (SEM) tensile tests, as they have to be conducted on smaller samples. In this study, a comprehensive experimental and numerical evaluation of the effect of specimen thickness (and the resulting number of grains within the cross-section) were conducted using in-situ SEM tensile test (on submillimeter thick samples) and ex-situ tensile tests (on samples of 0.68–5.9 mm thickness) and the results are compared with FEM simulations outcome. All tests were conducted at room temperature and the results are correlated to the number of grains within the thickness of specimens. The tensile test results indicated that even though the 0.2% proof stress and the tensile strength do not vary for the current range of thicknesses (with number of grains in the cross-section varying from 13 to 118), a difference in necking mechanism exists. Post tensile strength, thinner samples undergo more shear failure and diagonal localized necking whereas thicker samples experience more diffuse necking indicated by decreased area of shear failure at the edges and increased area of dimpled tensile failure at the center of the sample. Further, FEM results complement the experimental findings by showing the formation of conjugated localized shear bands on the upper and lower surface in the 0.68 mm thick sample and shear bands combining to form singular shear bands in thicker samples. These results also confirm the validity of the in-situ SEM tensile tests conducted on thinner samples as long as the required minimum number of grains exist within the cross-section.

36 MATERIALS SCIENCE↗

Swab Tensile Testing and Procedures

This tensile test is to mimic the worst-case scenario of the swab being caught on an obstruction when being pulled out of the nasopharyngeal space. It is to determine how much tensile force the swab can withstand without breaking. A variety of different swabs (different materials and different geometries) were tested using the protocol outlined in Section 2 (Tensile Testing Procedure). Not all of the swabs were pre-treated using the Autoclave. For those swabs that were pre-treated using the Autoclave, the tensile tests were performed within 6 hours of completion of the Autoclave pre-treatment, unless otherwise noted. The FormLabs-USF and FormLabs-Northwell were printed at LLNL using FormLabs Surgical Grade V1 Resin on a Form 3B Printer. Results Summary: All FormLabs design and treatment variations (e.g. autoclaving and “aging”) had higher tensile strength compared commercial swabs. Autoclaving degraded the tensile strength. “Aging” after autoclaving improved the tensile strength. “Aging” without autoclaving degraded the tensile strength. No differences were observed in tensile strength with different autoclaving protocols. No significant differences were observed in tensile strength for different batches.

59 BASIC BIOLOGICAL SCIENCES↗

Swab Tensile Testing Results and Procedures

This tensile test is to mimic the worst-case scenario of the swab being caught on an obstruction when being pulled out of the nasopharyngeal space. It is to determine how much tensile force the swab can withstand without breaking. A variety of different swabs (different materials and different geometries) were tested using the protocol outlined in Section 2 (Tensile Testing Procedure). Not all of the swabs were pre-treated using the Autoclave. For those swabs that were pre-treated using the Autoclave, the tensile tests were performed within 6 hours of completion of the Autoclave pre-treatment, with the exception of the “Aged” swabs. For the “Aged” swabs, the tensile tests were performed 7 days after the Autoclave pre -treatment. All swabs were provided by HP.

36 MATERIALS SCIENCE↗

Swab Tensile Testing Results and Procedures

This tensile test is to mimic the worst-case scenario of the swab being caught on an obstruction when being pulled out of the nasopharyngeal space. It is to determine how much tensile force the swab can withstand without breaking. A variety of different swabs (different materials and different geometries) were tested using the protocol outlined in Section 2 (Tensile Testing Procedure). Not all of the swabs were pre-treated using the Autoclave. For those swabs that were pre-treated using the Autoclave, the tensile tests were performed within 6 hours of completion of the Autoclave pre-treatment, with the exception of the Injection Molded samples. For the Injection Molded samples, the tensile tests were performed within 24 hours of the completion of the Autoclave pre-treatment. The FormLabs-USF and FormLabs-Northwell were printed at LLNL using FormLabs Surgical Grade V1 Resin on a Form 3B Printer. All other samples were provided by HP.

36 MATERIALS SCIENCE↗

Nanomechanical testing of freestanding polymer films: in situ tensile testing and Tg measurement

Abstract A method for small-scale testing and imaging of freestanding, microtomed polymer films using a push-to-pull device is presented. Central to this method was the development of a sample preparation technique which utilized solvents at cryogenic temperatures to transfer and deposit delicate thin films onto the microfabricated push-to-pull devices. The preparation of focused ion beam (FIB)-milled tensile specimens enabled quantitative in situ TEM tensile testing, but artifacts associated with ion and electron beam irradiation motivated the development of a FIB-free specimen preparation method. The FIB-free method was enabled by the design and fabrication of oversized strain-locking push-to-pull devices. An adaptation for push-to-pull devices to be compatible with an instrumented nanoindenter expanded the testing capabilities to include in situ heating. These innovations provided quantitative mechanical testing, postmortem TEM imaging, and the ability to measure the glass transition temperature, via dynamic mechanical analysis, of freestanding polymer films. Results for each of these mentioned characterization methods are presented and discussed in terms of polymer nanomechanics. Graphic Abstract

36 MATERIALS SCIENCE↗

Facile Tensile Testing Platform for In Situ Transmission Electron Microscopy of Nanomaterials

In situ tensile testing using transmission electron microscopy (TEM) is a powerful technique to probe structure-property relationships of materials at the atomic scale. In this work, a facile tensile testing platform for in situ characterization of materials inside a transmission electron microscope is demonstrated. The platform consists of: 1) a commercially available, flexible, electron-transparent substrate (e.g., TEM grid) integrated with a conventional tensile testing holder, and 2) a finite element simulation providing quantification of specimen-applied strain. The flexible substrate (carbon support film of the TEM grid) mitigates strain concentrations usually found in free-standing films and enables in situ straining experiments to be performed on materials that cannot undergo localized thinning or focused ion beam lift-out. The finite element simulation enables direct correlation of holder displacement with sample strain, providing upper and lower bounds of expected strain across the substrate. The tensile testing platform is validated for three disparate material systems: sputtered gold-palladium, few-layer transferred tungsten disulfide, and electrodeposited lithium, by measuring lattice strain from experimentally recorded electron diffraction data. The results show good agreement between experiment and simulation, providing confidence in the ability to transfer strain from holder to sample and relate TEM crystal structural observations with material mechanical properties.

2D materials↗

Improved Tensile Test for Ceramics

For almost-nondestructive tensile testing of ceramics, steel rod is bonded to sample of ceramic. Assembly is then pulled apart in conventional tensile-test machine. Test destroys only shallow surface layer which can be machined away making specimen ready for other uses. Method should be useful as manufacturing inspection procedure for low-strength brittle materials.

Osiecki, R. A.↗

Swab Tensile Testing Results and Procedures - PA11 Rev. 10 Swabs

This tensile test is to mimic the worst-case scenario of the swab being caught on an obstruction when being pulled out of the nasopharyngeal space. It is to determine how much tensile force the swab can withstand without breaking. All swabs were provided by HP and were the PA11 material and Rev 10 design. All of the swabs were tested using the protocol outlined in Section 2 (Tensile Testing Procedure). Not all of the swabs were pre-treated using the Autoclave. For those swabs that were pre-treated using the Autoclave, the tensile tests were performed within 6 hours of completion of the Autoclave pre-treatment, with the exception of the “Aged” swabs. For the “Aged” swabs, the tensile tests were performed 7 days after the Autoclave pre -treatment. The “Aged” swabs that were not pre-treated using the Autoclave, were tested 7 days after those that were not “Aged.”

36 MATERIALS SCIENCE↗

Understanding the limitations and potential of micro tensile testing of tungsten and needs for crystal plasticity modelling

Tungsten is the leading plasma facing material candidate due to its exceptional properties. Understanding the response to neutron irradiation is crucial for the lifetime evaluation of tungsten. The limited space in nuclear reactors and the high levels of radioactivity of the specimens after irradiation are significant barriers to accurately measuring the mechanical properties after neutron irradiation. Testing of micro tensile specimens is one approach to reduce the total amount of irradiated material needed for a set of mechanical testing experiments. However, micro samples are not necessarily measuring the bulk material properties, as size effects produce higher measured mechanical properties than is observed in engineering size counterparts. Determining the minimal sample size for reliable bulk property measurement, combined with modeling efforts, is essential. We conducted room temperature tensile tests on tungsten micro tensile specimens fabricated with focused ion beam, plasma focused ion beam and femto-second laser ablation system to dimension of 2×2×7?µm³, 7×7×18?µm³, and 80×100×233?µm³ (width×thickness×gauge-length), respectively. Elevated tensile testing was performed up to 475°C on 5×5×18?µm³ specimens fabricated with focused ion beam. The smallest specimens exhibited a high degree of ductility and strength, whereas the largest specimens demonstrated behavior akin to bulk tungsten. To investigate the effects introduced by the micro specimen fabrication processes and to obtain the necessary bulk dislocation density for the crystal plasticity model, we employed X-ray diffraction depth profiling. This measurement was performed using different X-ray sources with varying penetration depths. Finally, the potential and limitations of micro mechanical tests for tungsten will be discussed.

36 - MATERIALS SCIENCE↗

Analyzing the effect of misalignment on single-filament carbon fiber tensile testing via stereoscopic computer vision imaging

An understanding of the constitutive properties of carbon fibers (CF) is critical to the accuracy of high-resolution composite simulations and to the development of CF derived from low-cost alternative precursor materials. Single-fiber tensile testing is a capable tool to measure CF properties and is well suited to research efforts where only a small number of fibers may be available. However, single-fiber tensile tests are challenging to conduct due to the difficulty in handling small diameter fibers (5-15 μm), the brittleness of single fibers, and the required nanoscale/microscale resolution of testing equipment. The accuracy of the measured properties depends on several factors, but a critical factor is fiber misalignment, especially at short gauge lengths. Current standards do not address the effect of tensile specimen misalignment on measured properties. Furthermore, this work presents a robust method of fiber alignment using stereoscopic computer vision that enables users to align fibers vertically for tensile testing to improve the accuracy of resulting mechanical properties. Additionally, an analytical relationship between fiber misalignment angle and measured properties is developed and validated against the experimental results. As a result, new best practices for single-fiber tensile testing of CF are recommended.

47 OTHER INSTRUMENTATION↗

Investigating the failure behavior of cast Al-11Ce-0.4Mg alloys using in-situ scanning electron microscopy tensile testing

Within the last decade, research on Al-Ce-Mg alloys has reported promising results for use in cast part applications. In this paper, the failure behavior of cast Al-11Ce-0.4Mg (wt%) was investigated experimentally with focus on the effect the matrix and intermetallic phases have on the fracture propagation behavior at failure. For the first time, in-situ SEM tensile testing was used to study the failure behavior of cast Al-Ce alloys, reporting results for uniaxial, DIC, and single edge notch tensile tests. The results of the in-situ SEM tensile testing were compared with the materials characterization experiments, which included serial sectioning, EBSD, EDS, and fractography. Analysis of EBSD and EDS mapping of cast Al-11Ce-0.4Mg showed that the cast microstructure was a hypereutectic two phase Al-Ce alloy with grains encompassing large complex colonies of laminar eutectic Al 11 Ce 3 intermetallic. The uniaxial tensile results reported the effect casting defects have on the strength and ductility of the alloy, and DIC in-situ testing showed that the eutectic colonies plastically deform less than the matrix phase. In-situ SEM single edge notch tensile testing displayed how the strength of an individual phase affected the crack propagation direction in the alloy. The results of both the materials characterization and in-situ tensile testing experiments on the failure of this alloy revealed further directions for future alloy development that can improve both the strength and fracture toughness of Al-Ce-Mg alloys.

36 MATERIALS SCIENCE↗

High temperature tensile testing of ceramic composites

The various components of a high temperature tensile testing system are evaluated. The objective is the high temperature tensile testing of SiC fiber reinforced reaction bonded Si3N4 specimens at test temperatures up to 1650 C (3000 F). Testing is to be conducted in inert gases and air. Gripping fixtures, specimen configurations, furnaces, optical strain measuring systems, and temperature measurement techniques are reviewed. Advantages and disadvantages of the various techniques are also noted.

Gyekenyesi, John Z.↗

Method and apparatus for tensile testing of metal foil

A method for obtaining accurate and reproducible results in the tensile testing of metal foils in tensile testing machines is described. Before the test specimen are placed in the machine, foil side edges are worked until they are parallel and flaw free. The specimen are also aligned between and secured to grip end members. An aligning apparatus employed in the method is comprised of an alignment box with a longitudinal bottom wall and two upright side walls, first and second removable grip end members at each end of the box, and a means for securing the grip end members within the box.

Wade, O. W.↗