Conductive two-dimensional titanium carbide ‘clay’ with high volumetric capacitance
Explore the source record for details and available documents.
SEARCH · Engineering Papers
Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.
Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.
Explore the source record for details and available documents.
The high intercalation capacitance of MXenes is attractive, but their performance as electrodes in supercapacitors is limited by mass transport when increasing the thickness and mass loading of the electrodes. Here, we report a combined experimental and computational study, through which we reveal the diffusion of hydrated ionic species at the interlayer spaces. We find that the cyclic voltammetry curves for the delaminated Ti 3 C 2 T x exhibit distinct features in acid (H 2 SO 4 ) and alkaline (KOH) electrolytes. The DFT-calculated migration profile of K + and H + , in the presence and absence of water, suggests that the intercalated water molecules stabilize the charged ions, facilitating their diffusion from two dimension to three dimension manifested by the reduced activation barriers and movement pathways. In addition, we show that the diffusion of low and high concentrations of protons is significantly different. That is, protons of high concentrations can adsorb at both sides of the interlayer spaces, and water drives frequent proton hopping between stable adsorption sites as shown in the ab initio molecular dynamics simulations. The calculations can thus explain the varied capacitance and distorted CV curves when the experiments are conducted in acid and alkaline electrolytes. Furthermore, these results can provide the guidance to improve the fast transport of ions and electrons in MXenes with high mass loading.
Titanium carbide (TiC) nanoparticles have been successfully synthesized by carbo-thermic reaction of titanium and acetone at 800 °C. This method is relatively low temperature synthesis route. It can be used for large scale production of TiC. The synthesized nanoparticles have been characterized by X-ray diffraction (XRD), scanning electron microscopy (SEM) and differential thermal analyzer (DTA) techniques. XRD analysis confirmed the formation of single phase TiC. XRD analysis confirmed that the particles are spherical in shape with an average particle size of 13 nm. DTA analysis shows that the phase is stable upto 900 °C and the material can be used for high temperature applications.
ABSTRACT Physical and chemical properties of graphene-metal interfaces have been largely examined with the objective of producing nanostructured carbon-based electronic devices. Although electronic properties are key to such devices, appropriate structural, thermal and mechanical properties are important for device performance as well. One of the most studied is the graphene-titanium (G-Ti) interface. Titanium is a low density, high strength versatile metal that can form alloys with desirable properties for applications ranging from aerospace to medicine. Small clusters and thin films of titanium deposited on graphene have also been examined. However, while some experiments show that thin films of titanium on graphene can be removed without damaging graphene hexagonal structure, others reported the formation of titanium-carbide (TiC) at G-Ti interfaces. In a previous work [ACS Appl. Mater. Interfaces, 2017, 9 (38), pp 33288-33297], we have shown that pristine G-Ti interfaces are resilient to large thermal fluctuations even when G-Ti structures lie on curved or kinked substrates. Here, using classical molecular dynamics with the third-generation Charge Optimized Many Body (COMB3) potential, we show that di-interstitial defective G-Ti structures on a copper substrate with a relatively large curvature kink, present signs of TiC formation. This result might help explain the different experimental results mentioned above.
Titanium carbide and its cation (TiC/TiC{sup +}) have been investigated by the two-color visible (VIS)-ultraviolet (UV) resonance-enhanced photoionization and pulsed field ionization-photoelectron (PFI-PE) methods. Two visible excitation bands for neutral TiC are observed at 16 446 and 16 930 cm{sup −1}. Based on rotational analyses, these bands are assigned as the respective TiC({sup 3}Π{sub 1}) ← TiC(X{sup 3}Σ{sup +}) and TiC({sup 3}Σ{sup +}) ← TiC(X{sup 3}Σ{sup +}) transition bands. This assignment supports that the electronic configuration and term symmetry for the neutral TiC ground state are …7σ{sup 2}8σ{sup 1}9σ{sup 1}3π{sup 4} (X{sup 3}Σ{sup +}). The rotational constant and the corresponding bond distance of TiC(X{sup 3}Σ{sup +}; v″ = 0) are determined to be B{sub 0}″ = 0.6112(10) cm{sup −1} and r{sub 0}″ = 1.695(2) Å, respectively. The rotational analyses of the VIS-UV-PFI-PE spectra for the TiC{sup +}(X; v{sup +} = 0 and 1) vibrational bands show that the electronic configuration and term symmetry for the ionic TiC{sup +} ground state are …7σ{sup 2}8σ{sup 1}3π{sup 4} (X{sup 2}Σ{sup +}) with the v{sup +} = 0 → 1 vibrational spacing of 870.0(8) cm{sup −1} and the rotational constants of B{sub e}{sup +} = 0.6322(28) cm{sup −1}, and α{sub e}{sup +} = 0.0085(28) cm{sup −1}. The latter rotational constants yield the equilibrium bond distance of r{sub e}{sup +} = 1.667(4) Å for TiC{sup +}(X{sup 2}Σ{sup +}). The cleanly rotationally resolved VIS-UV-PFI-PE spectra have also provided a highly precise value of 53 200.2(8) cm{sup −1} [6.5960(1) eV] for the adiabatic ionization energy (IE) of TiC. This IE(TiC) value along with the known IE(Ti) has made possible the determination of the difference between the 0 K bond dissociation energy (D{sub 0}) of TiC{sup +}(X{sup 2}Σ{sup +}) and that of TiC(X{sup 3}Σ{sup +}) to be D{sub 0}(Ti{sup +}−C) − D{sub 0}(Ti−C) = 0.2322(2) eV. Similar to previous experimental observations, the present state-to-state PFI-PE study of the photoionization transitions, TiC{sup +}(X{sup 2}Σ{sup +}; v{sup +} = 0 and 1, N{sup +}) ← TiC({sup 3}Π{sub 1}; v′, J′), reveals a strong decreasing trend for the photoionization cross section as |ΔN{sup +}| = |N{sup +} – J′| is increased. The maximum |ΔN{sup +}| change of 7 observed here is also consistent with the previous experimental results for the 3d transition-metal carbides, oxides, and nitrides. However, the VIS-UV-PFI-PE spectra for TiC{sup +}(X{sup 2}Σ{sup +}; v{sup +} = 0 and 1, N{sup +}) are found to display only the negative ΔN{sup +} (N{sup +}–J′≤ 0) transitions, indicating that the cross sections for the formation of positive ΔN{sup +} (N{sup +}–J′ > 0) transitions by both the channel coupling mechanism and direct photoionization are negligibly small.
Foam titanium carbide (TiC) ceramics with a three-dimensional network structure were fabricated by the reaction sintering process, in which polyurethane foam was taken as the template, and TiO{sub 2} and phenolic resin were used as the reactants. Phase, microstructures and fracture morphologies of foam TiC ceramics were characterized by x-ray diffraction (XRD) and scanning electron microscopy (SEM), respectively. The results show that when the mass ratios of phenolic resin and TiO{sub 2} (F/T) are (0.8-1.2): 1, foam TiC ceramics with pure TiC phase can be formed. As the F/T ratios increase, crystal lattice parameters of fabricated foam TiC ceramics become bigger. When the value of F/T decreases from 1.2 to 0.8, grain size of TiC grows larger and microstructures get denser; meanwhile, the compressive strength increases from 0.10 to 1.05 MPa. Additionally, either raising the sintering temperatures or extending holding time can facilitate the completion of the reaction process and increase the compressive strength.
Deposition of Titanium Carbide coatings on Ti6Al4V substrate, through the reactive magnetron sputtering technique is here presented. The mechanical characterization of the coatings has been carried out through a set of indentation tests at different maximum applied loads. The elastic stiffness as well as the hardness of the coating-substrate system indicate that these coatings are suitable candidates for wear resistance applications in the orthopaedic field. Numerical simulation of the indentation tests allowed the identification of the constitutive parameters of the titanium carbide. Good agreement was achieved between experimental and numerical results.
The amplitude of thermal (dynamic) atomic vibrations and meansquare static atomic displacements in titanium carbide TiC{sub x} (x = 0.97, 0.88, 0.70) have been separately determined by measuring neutron diffraction patterns at two temperatures (T{sub 1} = 300 K and T{sub 2} = 80 K). The static lattice distortions in stoichiometric titanium carbide are experimentally found to be negligible. In the TiC{sub x} homogeneity range, the amplitude {radical}u{sup 2}{sub dyn} of thermal atomic vibrations significantly increases with a decrease in the carbon concentration. The Debye temperature has been determined for the first time in the TiC{sub x} homogeneity range at both room and liquid-nitrogen temperatures.
During the deposition of diamond films on Ti alloy substrates, titanium carbide is a common precipitated phase, preferentially formed at the interfacial region. However, in this case, the precipitation of an ordered structure of titanium carbide has not been reported. In our work, a long periodic ordered structure of TiC has been observed at the deposited diamond film/Ti alloy interface by high resolution transmission electron microscopy (HRTEM). The long periodic ordered structure is identified as 6H-type. The formation mechanism is revealed by comparative studies on the different structures of TiC precipitated under different diamond deposition conditions in terms of deposition time, atmosphere and temperature. A large number of carbon vacancies in the interfacial precipitated TiC phase are verified through electron energy loss spectroscopy (EELS) quantification analysis. However, an ordered arrangement of these carbon vacancies occurs only when the interfacial stress is large enough to induce the precipitation of 6H-type TiC. The supplementary analysis by X-ray diffraction (XRD) further confirms that additional diffraction peaks presented in the XRD patterns are corresponding to the precipitation of 6H-type TiC. - Highlights: •Different structures of TiC are observed during deposited diamond on Ti alloy. •One is common NaCl structure, the other is periodic structure. •The periodic structure is identified as 6H-type by HRTEM. •Carbon vacancies are verified to always exist in the TiC phase. •The precipitation of 6H-type TiC is mainly affected by interfacial stress.
The results of a study on the production of cubic titanium carbide in direct-current arc discharge plasma initiated in open air are presented. A feature of the method is its implementation without the use of gas or liquid protective media preventing the oxidation of products and initial reagents with air oxygen. According to the X-ray diffraction data, graphite gC, hexagonal titanium α-Ti, and cubic titanium carbide TiC are identified in the composition of the powder product. The TiC particles are represented by objects with a regular characteristic cut and sizes from units to tens of micrometers.
The Rotating Impeller In-Situ Gas–Liquid Reaction Method is employed for the production of Al-TiC composites. The method relies on injecting a carbon-bearing gas by means of a rotating impeller into a specially formulated molten aluminum-titanium alloy. Under the optimal conditions of temperature and composition, the gas reacts preferentially with titanium to form titanium carbide particles. The design of the apparatus, the process operation window, and the routes for forming titanium carbide particles with different sizes are elucidated.
Highlights: {yields} The synthesized temperature is lower than some conventional methods. {yields} These raw materials are safe; all manipulations are rather safe and convenient. {yields} The product exhibits photocatalytic activity in degradation of Rhodamine-B. -- Abstract: Titanium carbide (TiC) was prepared via one simple route by the reaction of metallic magnesium powders with titanium dioxide (TiO{sub 2}) and potassium acetate (CH{sub 3}COOK) in an autoclave at 600 {sup o}C and 8 h. Phase structure and morphology were characterized by X-ray powder diffraction (XRD) and Scanning electron microscopy (SEM). The results indicated that the product was cubic TiC, which consisted of particles with an average size of about 100 nm in diameter. The product was also studied by the thermogravimetric analysis (TGA) and its photocatalysis. It had good thermal stability and oxidation resistance below 350 {sup o}C in air. In addition, we discovered that the cubic TiC powders exhibited photocatalytic activity in degradation of Rhodamine-B (RhB) under 500 W mercury lamp light irradiation.
A method of synthesizing mechanically resilient titanium carbide (TiC) nanofibrous felts comprising continuous nanofibers or nano-ribbons with TiC crystallites embedded in carbon matrix, comprising: (a) electrospinning a spin dope for making precursor nanofibers with diameters less than 0.5 J.Lm; (b) overlaying the nanofibers to produce a nanofibrous mat (felt); and then (c) heating the nano-felts first at a low temperature, and then at a high temperature for making electrospun continuous nanofibers or nano-ribbons with TiC crystallites embedded in carbon matrix; and (d) chlorinating the above electrospun nano-felts at an elevated temperature to remove titanium for producing carbide derived carbon (CDC) nano-fibrous felt with high specific surface areas.
Herein we show that hydrazine intercalation into 2D titanium carbide (Ti 3 C 2 -based MXene) results in changes in its surface chemistry by decreasing the amounts of fluorine, OH surface groups and intercalated water. It also creates a pillaring effect between Ti 3 C 2 T x layers pre-opening the structure and improving the accessability to active sites. Furthermore, the hydrazine treated material has demonstrated a greatly improved capacitance of 250 F g –1 in acidic electrolytes with an excellent cycling ability for electrodes as thick as 75 μm.
We used the DV-X alpha method to analyze the high-resolution soft X-ray emission and absorption spectra in the CK region of titanium carbide (TiC). The spectral profiles of the X-ray emission and absorption can be ssuscfucelly reproduced by the occupied and unoccupied density of states (DOS ), respectively, in the C2p orbitals of the center carbon atoms in a Ti62C63 cluster model, suggesting that the center carbon atom in a large cluster model expanded to the cubic-structured 53 (= 125) atoms provides sufficient DOS for the X-ray spectral analysis of rock-salt structured metal carbides.
Here, noble metal (gold or silver) nanoparticles or patterned films are typically used as substrates for surface-enhanced Raman spectroscopy (SERS). Two-dimensional (2D) carbides and nitrides (MXenes) exhibit unique electronic and optical properties, including metallic conductivity and plasmon resonance in the visible or near-infrared range, making them promising candidates for a wide variety of applications. Herein, we show that 2D titanium carbide, Ti 3 C 2 T x , enhances Raman signal from organic dyes on a substrate and in solution. As a proof of concept, MXene SERS substrates were manufactured by spray-coating and used to detect several common dyes, with calculated enhancement factors reaching ~10 6 . Titanium carbide MXene demonstrates SERS effect in aqueous colloidal solutions, suggesting the potential for biomedical or environmental applications, where MXene can selectively enhance positively charged molecules.
A series of superstructural reflections (described within the sp. gr. Fd3m) are found to be split into three symmetric parts in the neutron powder diffraction pattern of titanium carbide TiC{sub 0.60} annealed at a temperature of 600 Degree-Sign C. No splitting of superstructural reflections is observed in the neutron diffraction pattern of TiC{sub 0.60} annealed at relatively high temperatures (780 Degree-Sign C). This phenomenon can be explained by that fact that the ordering of carbon atoms at relatively high temperatures (780 Degree-Sign C) is accompanied by the formation of randomly oriented rather large antiphase domains (APDs) (450 A). At relatively low temperatures (600 Degree-Sign C), stacking faults arise in the arrangement of partially ordered carbon atoms. In this case, relatively small ordered APDs (290 A) are formed, along with disordered ones.