Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “TIN 125”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

Thermal Cycle Reliability of PBGA/CCGA 717 I/Os

Status of thermal cycle test results for a nonfunctional daisy-chained peripheral ceramic column grid array (CCGA) and its plastic ball grid array (PBGA) version. both having 560 I/Os. were presented in last year's conference. Test results included environmental data for three different thermal cycle regimes (-55 C/125 C, -55 C/100 C, and -50 C /75 C). Update information on these - especially failure type for assemblies with high and low solder volumes-were presented. The thermal cycle test procedure followed those recommended IPC-9701 for tin-lead solder joint assemblies. Revision A of this specification covers guideline thermal cycle requirements for Pb-free solder joints. Some background information discussed during release of this specification with its current guideline recommendations were also presented. In a recent reliability investigation a fully populated CCGA with 717 I/Os was also considered for assembly reliability. evaluation. The functional package is a field-programmable gate array that has much higher processing power than its previous version. This new package is smaller in dimension, has no interposer, and has a thinner column wrapped with copper for reliability improvement. This paper will also present thermal cycle test results for this package assembly and its plastic version with 728 I/Os. both of which were exposed to three different cycle regimes. Two cycle profiles were those specified by IPC- 9701A for tin-lead, i.e. -55 to 100 C and -55 to 125 C and one was a cycle profile specified by Mil-Std-883, i.e.. -65 C/150 C which is generally used for ceramic hybrid packages. Per IPC-9701 A, test vehicles were built using daisy chain packages and were continuously monitored. The effects of many process and assembly variables-including corner staking commonly used for improving resistance to mechanical loading such as drop and vibration loads--were also considered as part of the test matrix. Optical photomicrographs were taken at various thermal cycle intervals to document damage progress and behavior. Representative samples of these along with cross-sectional photomicrographs at higher magnification taken by scanning electron microscopy (SEM) to determine crack propagation and failure analyses for packages are also presented.

staking↗

Ecology and thermal inactivation of microbes in and on interplanetary space vehicle components

Dry heat inactivation characteristics were compared for 4-6 (B. brevis) spores and microbes from the Cincinnati soil samples at 105, 112, and 125. Characterized were the survival curves of 4-6 (B. brevis) spores at 112, 115, 118, 120, and 125 C, and 1.2 microgram of water per ml of headspace air (closed tin-can system), and the morphological characteristics of 4-6 (B. brevis), 6-12 (B. lentus), 7-11 (B. coagulans), and B. subtilis var. niger spores by scanning electron microscopy.

Reyes, A. L.↗

Platinized tin oxide catalysts for CO2 lasers: Effects of pretreatment

Platinized tin oxide surfaces used for low-temperature CO oxidation in CO2 lasers have been characterized before and after reduction in CO at 125 and 250 C using ion scattering spectroscopy (ISS) and X ray photoelectron spectroscopy (XPS). XPS indicates that the Pt is present initially as PtO2. Reduction at 125 C converts the PtO2 to Pt(OH)2 while reduction at 250 C converts the PtO2 to metallic Pt. ISS shows that the Pt in the outermost atomic layer of the catalyst is mostly covered by substrate species during the 250 C reduction. Both the ISS and XPS results are consistent with Pt/Sn alloy formation. The surface dehydration and migration of substrate species over surface Pt and Sn appear to explain why a CO pretreatment at 250 C produces inferior CO oxidation activities compared to a 125 C pretreatment.

Gardner, Steven D.↗

Platinized tin oxide catalysts for CO2 lasers - Effects of pretreatment

Platinized tin oxide surfaces used for low-temperature CO oxidation in CO2 lasers have been characterized before and after reduction in CO at 125 and 250 C using ion scattering spectroscopy (ISS) and X-ray photoelectron spectroscopy (XPS). XPS indicates that the Pt is present initially as Pto2. Reduction at 125 C converts the PtO2 to Pt(OH)2 while reduction at 250 C converts the PtO2 to metallic Pt. ISS shows that the Pt in the outermost atomic layer of the catalyst is mostly covered by substrate species during the 250 C reduction. Both the ISS and XPS results are consistent with Pt/Sn alloy formation. The surface dehydration and migration of substrate species over surface Pt and Sn appear to explain why a CO pretreatment at 250 C produces inferior CO oxidation activities compared to a 125 C pretreatment.

Gardner, Steven D.↗

Fabrication and Testing of Polyvinylidene Fluoride Capacitors

High energy density capacitors made from metallized polyvinylidene fluoride film were built and tested. Terminations of aluminum-babbitt, tin-babbitt, and all-babbitt were evaluated. All-babbit terminations appeared to be better. The 0.1 microfarad and 2 microfarad capacitors were made of 6 micrometer material. Capacitance, dissipation factor, and insulation resistance measurements were made over the ranges -55 C to 125 C and 10 Hz to 100 kHz. Twelve of forty-one 0.1 microfarad capacitors survived a 5000 hour dc plus ac life test. Under the same conditions, the 2 microfarad capacitors exhibited overheating because of excessive power loss. Some failures occurred after low temperature exposures for 48 hours. No failures were caused by vibration or temperature cycling.

Buritz, R. S.↗