Engineering PapersSearch

SEARCH · Engineering Papers

Results for “Single fiber pull-out”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

Influence of sizing concentration on strength, stiffness, and porosity in textile grade carbon fiber (TCF)-Epoxy composites: Revealing inverse trends

The effect of fiber sizing (i.e., surface treatment) concentration (0 %, 1.36 %, 1.52 %, 1.94 %, and 2.13 %) on the mechanical properties (tensile, flexural, interlaminar shear strength (ILSS), and low velocity impact) of textile grade carbon fiber (TCF)-epoxy composite is examined. An inverse relationship between the strength and stiffness of the composite is observed with increased sizing concentration. The root mean square (RMS) roughness of the fiber surface increased from 17.8 nm (unsized) to 22.7 nm with 2.13 % sizing concentration. It was found that the tensile strength increased by 131 % from 221.4 ± 18.5 MPa (unsized) to 510.8 ± 28.05 MPa (for 1.36 % sizing) and further by 155 %–563.7 ± 14.95 MPa at 2.13 % sizing. On the contrary, the stiffness is initially increased by 126 % from 33.52 ± 7.80 GPa (unsized) to 75.9 ± 3.21 GPa (for 1.36 % sizing) but reduced with further increase in the sizing concentration. A single fiber pull-out test is simulated using the finite element method to validate the reverse trend in strength and stiffness. The varying sizing concentration is simulated by introducing an interface of varying thickness between fibers and matrix. Simulation results confirm that a thicker interface, corresponding to a higher sizing concentration, decreases interfacial shear stress, enhancing material strength while decreasing stiffness. The reverse trend in strength and stiffness with the sizing concentration aligns with experimental observations. In conclusion, the present study emphasizes the importance of sizing concentration for mechanical properties and provide a design criterion for customized high-strength and high-stiffness applications.

Porosity

A mild calcium carbonate treatment improves moisture resistance and mechanical/interfacial properties of jute and hemp fibers

Natural fibers are attractive, sustainable reinforcements, but often exhibit high moisture uptake and weak bonding with polymer matrices. In this study, jute and hemp were treated by immersion in aqueous calcium carbonate (CaCO3) suspensions (10–40?wt.%, 1.5?h, room temperature) and were characterized by scanning electron microscopy (SEM), X-ray diffraction (XRD), moisture sorption testing, single-fiber tensile testing, and bundle pull-out testing. SEM showed granular CaCO3 deposition on fiber surfaces, with particulates bridging surface voids and microcracks. At 40 wt.% CaCO3, equilibrium moisture uptake decreased to ~5% (hemp) and ~3% (jute), while tensile strength increased to ~904 MPa (hemp) and ~960 MPa (jute). Apparent interfacial shear strength from pull-out testing increased up to ~1.35 MPa (hemp) and ~0.56 MPa (jute). These results indicate that CaCO3 deposition is a mild, scalable surface treatment that improves moisture resistance, fiber tensile strength, and interfacial load transfer relevant to semi-structural composite applications, including interior and secondary automotive components.

Calcium carbonate treatment