At least 19 records

Hermeticity of SiC/SiC composite and monolithic SiC tubes irradiated under radial high-heat flux

Demonstration of hermetic SiC fiber–reinforced SiC matrix composite cladding under normal operating environments has been identified as one of the most critical feasibility issues for accident-tolerant fuel cladding in light-water reactors. This study provides critical experimental data needed for understanding the effects of irradiation on hermeticity. SiC composite and monolithic tubes were neutron-irradiated to 2 displacements per atom with and without a nominal radial heat flux of 0.6 MW/m2 to produce a simulated in-pile stress state for the normal operation of a light-water reactor. The through-thickness temperature gradient under irradiation results in a gradient in swelling, which causes a significant stress buildup. Such irradiation-induced stress was modeled using a commercial finite element analysis code. The radial heat flux–irradiation synergism was experimentally investigated by constructing a special irradiation capsule and evaluating the helium hermeticity of the specimens. The simulated stress state exhibited a near equi-biaxial tensile axial and hoop stress of ~150 MPa at the inner surface of the SiC composite tube. This stress level is potentially beyond the matrix cracking stress. Degradation of hermeticity of the SiC composite tubes was observed after irradiation, indicating irradiation-induced cracking, whereas the irradiated monolithic SiC tubes remained hermetic. In conclusion, the results indicate that loss of hermeticity caused by radiation-induced microcracking is a potential issue for SiC composite cladding, depending on the magnitude of the temperature gradients. Coating the outer surface of the cladding was identified as a mitigation strategy that might overcome the cracking issue.

36 MATERIALS SCIENCE↗

In situ high-temperature 3D imaging of the damage evolution in a SiC nuclear fuel cladding material

Silicon carbide (SiC)-based nuclear fission fuel rod cladding has been considered as one of the possible designs for accident tolerant fuels. It is in the form of a SiC fibre reinforced SiC matrix composite tube (SiC f -SiC m ) with monolithic SiC outer and/or inner coating layers. This study focuses on the deformation and fracture processes in this material using in situ X-ray micro-computed tomography (XCT) at room temperature (RT) and 1200 °C in an inert gas environment in a C-ring compression loading configuration. Prior to testing, local properties and residual stresses were characterised using nanoindentation and Raman spectroscopy since they can impact the mechanical behaviour of the material. The 3D strain distribution, crack formation and propagation processes including the toughening mechanisms (e.g., crack deflection, micro-cracking, crack bridging and bifurcation) are investigated in the coating and underlying composites at RT and 1200 °C. There is no particular sequence which toughening mechanism occurs first – this is very different from the conventional toughening theory in ceramic-matrix composites under uniaxial tension loading. Indeed, no evidence of fibre pull-out or fibre fracture was observed in this SiC f -SiC m nuclear cladding material in the current C-ring compression configuration. The correlation between local measurements and bulk mechanical behaviour are discussed.

3D imaging↗

Solar optical performance of SiC receiver tubes

As part of a DOE Small Business Innovative Research (SBIR) project, CTP explored options to enhance the solar optical properties of its solar receiver tube. Sandia National Laboratories (Sandia) working with CTP, performed high-flux solar simulator tests on several receiver-tube specimens. Furthermore, the results demonstrated the excellent durability and optical performance of SiOC composite receiver tubes at 800°C surface temperatures.

14 SOLAR ENERGY↗

Phase separation during the direct powder bed fusion of SiC

Powder bed fusion (PBF) is an attractive additive manufacturing option for fabrication of SiC object with complex geometries. However, the density and microstructure controls remain a challenge. This study is aimed at understanding laser–SiC interactions, with emphasis on microstructure-processing relationships, to identify potential solutions for the process improvement. SiC tubes were fabricated by PBF of pure SiC powders without sintering additives. Further, comprehensive analysis by X-ray diffraction, Raman spectroscopy, and electron microscopy indicated that binding of SiC particles was achieved by incongruent melting of SiC to a Si/C mixture containing SiC micro- and nanocrystallites. The phase evolution under laser irradiation of SiC was explained by phase diagrams. This study uncovered the PBF SiC microstructure at different length scales and the relationship between the microstructure and the processing parameters.

36 MATERIALS SCIENCE↗

Mechanical degradation of duplex SiC-fiber reinforced SiC matrix composite tubes under a controlled high-temperature steam environment

This paper describes results from the mechanical evaluation of unirradiated SiC fiber–reinforced SiC matrix composite tubes under a controlled high-temperature steam environment. The experiments were aimed at identifying key material degradation behavior under environments relevant to loss-of-coolant accidents of light water reactors. Mechanical tests of the SiC composite tubes at 1000 °C under steam and inert environments were conducted using a unique test capability. Further, the material tested was a duplex tube with a thick monolithic SiC layer on the outer surface. The tubes were subjected to preloading at ~100 MPa in tension before exposure to high-temperature steam with up to 75% of the preload at a constant displacement. In the presence of matrix cracks, the steam exposure caused embrittlement of the SiC composite tubes and failure at a stress level below the pretest stress. The material degradation was explained by a fiber oxidation model, which can be applied to various SiC cladding concepts. The embrittlement could be a limiting factor for using SiC cladding subjected to loss-of-coolant accident conditions.

36 MATERIALS SCIENCE↗

Silicon Carbide Multilayer Piping for High Temperature sCO 2 Brayton Cycle

Efficiencies of greater than 50% in supercritical carbon dioxide (sCO 2 ) Brayton power cycle systems can be achieved only at turbine inlet temperatures of above 700°C. In support of the push to higher temperatures, a finite element model was developed by Materials Research & Design, Inc. (MR&D) with support from Ceramic Tubular Products, LLC. (CTP) to guide the refinement of CTP’s high temperature ceramic multilayer piping. The multilayer technology combines the advantages of a monolithic silicon carbide (SiC) tube and a SiOC f /SiOC ceramic matrix composite (CMC), the result of which is a material with high-temperature strength and stability, high mechanical and thermal shock resistance, and high corrosion resistance. In addition to fabricating test specimens to refine the finite element model, long-duration, high temperature CO 2 exposure tests were performed by Sandia National Laboratories (SNL) on two varieties of inner monolithic SiC.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Flash Heating of a Hollow Rod to Determine Thermal Properties

In a nuclear reactor, prolonged exposure to high neutron flux levels can change material properties of reactor components. Due to the danger posed to personnel by highly radioactive components such as spent fuel, noncontact methods must be used to determine these properties. The objective of the current research is to test the viability of using a flash-heating method to determine the thermal diffusivity of a silicon carbide (SiC) tube, which could be used as cladding for a nuclear fuel rod. The flash-heating experiment was conducted at Oak Ridge National Laboratory and temperature results were analyzed as a two-Dimensional cross section which assumed axial symmetry. The model was fitted iteratively to the temperature measurements using nonlinear regression which required values for thermal diffusivity, Biot number and a term to determine the magnitude of the heat absorbed by the flash. The method could be expanded in the future to estimate the thermal diffusivity of spent nuclear fuel rods in an effort to increase the certainty of new reactor designs using precise thermal properties throughout the core life. A statistical analysis of the results of this work is provided as part of the analysis.

McMasters, Robert L [Virginia Military Institute, ↗

Screening and qualification methodology for SiC end plug processing methods

Deployment of SiC-ceramic-based fuel cladding for light water reactors requires a hermetic end plug–to–cladding joint that can withstand neutron irradiation during normal operation and maintain integrity during design-basis accidents. Reactor experiments have shown that some SiC composite tubes with SiC end plugs can retain hermeticity after irradiation. However, achieving consistent joint performance under irradiation remains a key challenge. Resolving this issue is essential to enable integral irradiation testing and to demonstrate fuel integrity under commercial-reactor irradiation conditions. This report aims to: (1) provide guidance for designing radiation-tolerant end plug joints for SiC cladding; (2) demonstrate experimental methods to detect processing defects that are unstable under neutron irradiation at light-water-reactor-relevant temperatures and doses; and (3) outline a step-by-step approach for designing and conducting reactor experiments to screen joining methods. The resulting data will be used to improve joint processing and to define critical defect types and sizes that must be detected and eliminated through non-destructive evaluation for quality assurance. Based on prior irradiation experiments at the High Flux Isotope Reactor, differential swelling among the cladding, bonding layer, and end plug was identified as an underlying mechanism for irradiation-induced joint degradation. Accordingly, this effect must be considered in the design of radiation-tolerant joining techniques. In this work, miniature SiC end plug joint specimens irradiated during the previous project were analyzed using X-ray computed tomography to characterize the joint microstructure. Digital volume correlation of the tomography data quantified radiation-induced microstructural changes and enabled evaluation of defect-related risks. Finally, ongoing neutron irradiation efforts using larger specimen volumes are presented. These efforts aim to statistically assess joint performance and to build a microstructure–performance (e.g., leak-tightness) dataset to inform processing improvements and quality control.

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

High-Temperature SiC Cladding End Plug Irradiation Design and HFIR Readiness

This report documents the design of a High Flux Isotope Reactor (HFIR) irradiation experiment intended to evaluate irradiation effects on the hermeticity of silicon carbide (SiC) end plug specimens under a radial fast neutron flux gradient at representative light-water reactor (LWR) temperatures of approximately 300 °C. The overarching goal of this work is to statistically evaluate SiC end plug hermeticity and mechanical properties following irradiation using the high-throughput irradiation capability discussed here. Each specimen consists of a short section of SiC fiber–reinforced SiC (SiC/SiC) tube with a single monolithic SiC end plug joined to one end. The experiment allows up to 66 specimens to be irradiated in six different stacks within a dry, sealed irradiation capsule derived from the previously developed high-temperature SiC/SiC cladding bowing experiment. The neutronics basis, thermal analysis, and HFIR readiness of the experiment are discussed in this report for two possible design cases. The first design case is based on existing approval documentation and components that are on hand and approved for use, so the experiment insertion would require only specimen receipt, specimen pre-irradiation characterization, experiment assembly, and final fabrication package approval. The second design case provides improved thermal robustness and the preferred end plug geometry but requires fabrication of a modified holder and revisions to the HFIR approval documentation, in addition to the other activities required for the first design case, before insertion.

Hott, Daniel [Oak Ridge National Laboratory (ORNL)↗

Damage progression and failure of SiC/SiC composite tubes under hard-contact radial expansion

The response of silicon carbide (SiC) fiber-reinforced SiC matrix (SiC/SiC) composite cladding to mechanical interaction with fissile fuel is a knowledge gap that must be overcome to design and assess SiC-based cladding systems for advanced nuclear applications. This study developed the relevant mechanical testing capability and identified the failure behavior and the critical microstructural features and processing defects. Sections of SiC composite tube were subjected to a modified expansion-due-to-compression (EDC) test in an X-ray computed tomography microscope: a polyurethane plug pressed surrogate Al 2 O 3 into the inner walls of the SiC/SiC composite tubes to achieve hard contact. A pure EDC test with just a polyurethane plug was also performed as a reference. Through the use of displacement fields, digital volume correlation revealed inhomogeneous deformation fields in the tubes, even for pure EDC, which was related to the inherent defects in the structure. Deep learning–aided segmentation and systematic data analysis revealed that the presence of inhomogeneous deformation applied by the hard contact was exaggerated by the presence of inner surface imperfections left behind from the matrix densification process. In conclusion, the findings provide insights into the applications, highlighting the necessity for improvements in inner surface roughness and the incorporation of localized contacts in pellet–cladding mechanical interaction computational models.

Composites↗

Evaluating steam oxidation kinetics of environmental barrier coatings

Environmental barrier coatings (EBCs) are a commercially proven means of protecting SiC-based materials in gas turbine environments. However, there are little specific data in the literature on the impact of coatings like Yb 2 Si 2 O 7 on preventing accelerated SiO 2 growth in the presence of H 2 O. Quantification of reduced rates are necessary for evaluating and comparing EBC effectiveness and incorporation of silica growth rates into future EBC lifetime models. In this study, baseline kinetics of silica formation on bare Si and chemically vapor deposited (CVD) SiC in the 1250–1425 °C range were obtained via 100 h isothermal exposures in dry air and steam environments utilizing a SiC reaction tube to mitigate specimen volatility. An Arrhenius plot of the resulting rates was constructed, representing baseline minimum and maximum rates for Si and SiC oxidation at ambient pressure. Various EBC systems on CVD SiC substrates including air plasma sprayed (APS) EBCs with and without a Si bond coating and with surface roughening to enhance Yb 2 Si 2 O 7 adhesion were subjected to 1-h furnace cycle testing in air with 90vol%H 2 O at 1250–1350°C for up to 500 cycles. After exposure, silica formation rates were measured and compared to the baseline rates to assess EBC effectiveness, where EBC effectiveness is gauged as the propensity to reduce underlying rates of silica formation. With a Si bond coating, a ~180 µm Yb 2 Si 2 O 7 (YbDS) top coating reduced rates over the entire 1250°-1350°C range. Without a Si bond coating, ~60 µm (YbDS) coatings deposited directly onto CVD SiC exhibited poor adhesion, and had to be deposited onto substrates with enhanced roughness at 1350°C. Finally, while exhibiting good adhesion at 1350°C, overall the single layer YbDS coating exhibited a decreasing effectiveness from 1250° to 1350°C.

36 MATERIALS SCIENCE↗

SolarPACES 2022

Performance of Silicon Carbide Fiber Composite Receiver Tubes for Concentrating Solar Power

14 SOLAR ENERGY↗

Advancing SiC clad fuel performance model: bridging micro- and macro-scale models and experimental validation

This report presents a workflow for advancing fuel performance modeling of SiC composite cladding for light-water reactors by linking microscale, experimental data-informed finite element analysis with rod-scale fuel performance codes such as BISON. The workflow uses X-ray computed tomography (XCT) to capture the actual geometry and processing-induced defects of as-fabricated SiC composite tube specimens, particularly porosity and wall-thickness variations, and converts the segmented XCT volumes into image-based finite element meshes for high fidelity structural analysis.

Koyanagi, Takaaki [Oak Ridge National Laboratory (↗

Formation of Composite SiC/SiC Joints by Embedded Wire Chemical Vapor Deposition

The joining of ceramic monoliths or composites to date has primarily been limited to the formation of brittle monolithic joints using heterogeneous (dissimilar) materials, similar to brazing in metals. The development of a damage-tolerant joint layer by SiC fiber reinforcements is demonstrated here. Tube workpieces made of SiC fiber-SiC matrix composite are joined using a nonwoven SiC fiber mat densified by embedded wire chemical vapor deposition (EWCVD), creating a fiber-reinforced weld-like joint by homogeneous joining. EWCVD uses a localized heating method to target deposition and growth to the joint region specifically, while minimizing thermal damage to the surrounding composite tube material. X-ray computed tomography (XCT) is used to nondestructively characterize as-made joints for relative density, adhesion, and composition. In situ XCT analysis during mechanical testing revealed crack deflections in the bonding layer, which indicates a toughening mechanism typical of ceramic matrix composite phase. Gas permeation testing of these proof-of-concept composite joints identified relatively high leak rates in comparison to fully coated SiC/SiC composite tube workpieces. In conclusion, the novelty of the composite joining method and current technology challenges, including gas permeability, are discussed in comparison with traditional ceramic joints and materials.

SiC↗

Uncertainty quantification in elastic constants of SiC f /SiC m tubular composites using global sensitivity analysis

Silicon carbide fiber and silicon carbide matrix (SiC f /SiC m ) tubes produced through the chemical vapor infiltration process have become a candidate cladding material in nuclear applications. The performance of this composite is influenced by many variables such as braiding angle, porosity, material properties, etc., which vary over a range of values due to the inherent fluctuations in the manufacturing process. In this study, the variability in elastic constants of SiC f /SiC m composite has been quantified through multiscale finite element (FE) simulations, variable screening, and high-fidelity surrogate modeling. The key variables dominantly affecting the elastic constants of SiC f /SiC m tubes were identified using global sensitivity analysis. A surrogate to the high-fidelity FE-based model was used in Monte Carlo simulations to generate a hundred thousand samples from which the uncertainty in elastic constants was assessed. It turned out that the coefficient of variation was less than 10%.

Materials Science↗

Experimental investigation of probabilistic failure of SiC/SiC composite tubes under multiaxial loading

This paper presents an experimental investigation of the failure behavior of SiC fiber-reinforced SiC matrix (SiC/SiC) composite tubes under multiaxial loading. A new testing apparatus is designed to independently apply axial stress and internal pressure to SiC/SiC tubes. Acoustic emission (AE) is used to monitor the damage growth in the specimen. Based on the measured stress–strain response, a strain-based criterion is proposed to determine the proportional limit stress (PLS). The proposed strain-based criterion is compared with the PLS determined by the AE measurement. The PLS is determined for different loading ratios to form a multiaxial failure surface. By testing multiple replicates, the statistical variations of the PLS are determined. In conclusion, based on the experimental results, a mathematical model is developed to characterize the probability distribution of the PLS of SiC/SiC composites under multiaxial loading.

36 MATERIALS SCIENCE↗

Influence of weave architecture on mechanical response of SiC f -SiC m tubular composites

Due to their high resistance to radiation damage and elevated temperature, silicon carbide fiber-reinforced, silicon carbide matrix composites (SiC f -SiC m ) are identified as potential cladding structures for use in nuclear reactors. In this study, four composite architectures with varying ply numbers along the thickness direction and different biaxial or triaxial plain weave orientations at either 45° or 60°, were systematically evaluated under various stress states to assess the influence of weave architecture on mechanical performance. Experiments were conducted on SiC f -SiC m composite tubes under tensile hoop, axial compression, and rotating flexural loading to evaluate the mechanical response and investigate the failure modes using high-speed imaging and digital image correlation (DIC) techniques. It was found that for tensile hoop burst and flexural loading, the braiding angle had the most significant influence on the strength of the composite, whereas the effect of fiber angle was more limited for compression testing. Under axial compression a unique failure mode where a microcrack nucleates and grows only to a length equal to the thickness of a single yarn was identified. This crack growth behavior is reflected as periodic oscillations in the load-displacement response. For both axial and hoop loading, regardless of weave angle and number of plies, failure always initiated parallel to the tube axis in a single yarn and the cumulative interaction of these microcracks lead to either axial burst or fracture at an angle to the tube axis along a yarn. Furthermore, these results point to the importance of customizing the design of tube architecture for enhanced performance in specified nuclear applications.

36 MATERIALS SCIENCE↗

Stress rupture of SiC/SiC composite tubes under high-temperature steam

SiC-fiber–reinforced SiC matrix composite cladding for light water reactor fuel elements must withstand high-temperature steam oxidation in a loss-of-coolant accident scenario (LOCA). Current composite designs include an outer monolithic SiC layer, in part, to increase steam oxidation resistance. However, it is not clear how such a structure would behave under high-temperature steam in the case when the monolithic layer cracks and carbon interphases and SiC fibers are exposed to the environment. To fill this knowledge gap, stress-rupture tests of prototypic SiC composite cladding at 1000°C under steam and inert environments were conducted. The applied stress was ~120 MPa, which was beyond the initial cracking stress. The failure lifetime under steam was 400–1300 s, while 75% of the composite specimens did not fail after 3 h of total exposure under inert gases. Microstructural observations suggest that steam oxidation activated slow crack growth in the fibers, which led to failure of the composite. The results from this study suggest that stress rupture in steam environments could be a limiting factor of the cladding under reactor LOCA conditions.