Fabrication And Evaluation Of Sic/Sic Tubes With Various Fiber Architectures

SiC/SiC composites are excellent material candidates for high temperature applications where the performance requirements are high strength, high creep-rupture resistance, high environmental durability, and high thermal conductivity. In the past, the NASA UEET program has demonstrated fabrication of high-performance SiC/SiC flat panels reinforced by Sylramic-iBN SiC fibers. Currently NASA UEET is scaling up this SiC/SiC system by fabrication of more complex shaped components using the same fiber type. This paper reports the effects of various fiber architectures on the processing, mechanical, and durability behavior of small-diameter 0.5" ID SiC/SiC tubes, which are potential sub-elements for leading edges and cooling channels in turbine vanes and blades. Nine different fiber architectures were utilized for construction of seamless tube preforms, from simple 2D jelly-rolling to complex braiding, pin-weaving, filament-winding and 3D orthogonal weaving with approximately 5% fibers in the thru-thickness direction. Using the BN interphase and Sic matrix processing steps established for the flat panels, SiC/SiC tubes were fabricated with wall thicknesses of approximately 60 mils and total fiber fractions of approximately 35%. The "D" split ring tests for hoop tensile properties, micro-structural examinations for relationship between fiber architecture formation and matrix infiltration, and the low-pressure burner rig tests for the high temperature durability under thru-thickness thermal gradient were conducted. The better matrix infiltration and higher hoop strength were achieved using the tri-axial braided and the three-float pin woven SiC/SiC tubes. In general, it needs not only higher hoop direction fibers but also axial direction fibers for the higher hoop strength and the better infiltration, respectively. These results are analyzed to offer general guidelines for selecting fiber pre-form architectures and SiC/SiC processes that maximize tube hoop strength, thru-thickness thermal conductivity, and burner-rig durability under a high thermal gradient.

Yun, H. M.

Modeling Creep Effects within SiC/SiC Turbine Components

Anticipating the implementation of advanced SiC/SiC ceramic composites into the hot section components of future gas turbine engines, the primary objective of this on-going study is to develop physics-based analytical and finite-element modeling tools to predict the effects of constituent creep on SiC/SiC component service life. A second objective is to understand how to possibly select and manipulate constituent materials, processes, and geometries in order to minimize these effects. In initial studies aimed at SiC/SiC components experiencing through-thickness stress gradients, creep models were developed that allowed an understanding of detrimental residual stress effects that can develop globally within the component walls. It was assumed that the SiC/SiC composites behaved as isotropic visco-elastic materials with temperature-dependent creep behavior as experimentally measured in-plane in the fiber direction of advanced thin-walled 2D SiC/SiC panels. The creep models and their key results are discussed assuming state-of-the-art SiC/SiC materials within a simple cylindrical thin-walled tubular structure, which is currently being employed to model creep-related effects for turbine airfoil leading edges subjected to through-thickness thermal stress gradients. Improvements in the creep models are also presented which focus on constituent behavior with more realistic non-linear stress dependencies in order to predict such key creep-related SiC/SiC properties as time-dependent matrix stress, constituent creep and content effects on composite creep rates and rupture times, and stresses on fiber and matrix during and after creep.

DiCarlo, J. A.

High-Performance SiC/SiC Ceramic Composite Systems Developed for 1315 C (2400 F) Engine Components

As structural materials for hot-section components in advanced aerospace and land-based gas turbine engines, silicon carbide (SiC) ceramic matrix composites reinforced by high performance SiC fibers offer a variety of performance advantages over current bill-of-materials, such as nickel-based superalloys. These advantages are based on the SiC/SiC composites displaying higher temperature capability for a given structural load, lower density (approximately 30- to 50-percent metal density), and lower thermal expansion. These properties should, in turn, result in many important engine benefits, such as reduced component cooling air requirements, simpler component design, reduced support structure weight, improved fuel efficiency, reduced emissions, higher blade frequencies, reduced blade clearances, and higher thrust. Under the NASA Ultra-Efficient Engine Technology (UEET) Project, much progress has been made at the NASA Glenn Research Center in identifying and optimizing two highperformance SiC/SiC composite systems. The table compares typical properties of oxide/oxide panels and SiC/SiC panels formed by the random stacking of balanced 0 degrees/90 degrees fabric pieces reinforced by the indicated fiber types. The Glenn SiC/SiC systems A and B (shaded area of the table) were reinforced by the Sylramic-iBN SiC fiber, which was produced at Glenn by thermal treatment of the commercial Sylramic SiC fiber (Dow Corning, Midland, MI; ref. 2). The treatment process (1) removes boron from the Sylramic fiber, thereby improving fiber creep, rupture, and oxidation resistance and (2) allows the boron to react with nitrogen to form a thin in situ grown BN coating on the fiber surface, thereby providing an oxidation-resistant buffer layer between contacting fibers in the fabric and the final composite. The fabric stacks for all SiC/SiC panels were provided to GE Power Systems Composites for chemical vapor infiltration of Glenn designed BN fiber coatings and conventional SiC matrices. Composite panels with system B were heat treated at Glenn, and the pores that remained open were filled by silicon melt infiltration (MI). Panels with system A and the other SiC/SiC systems were not heat treated, and remaining open pores in these systems were filled with SiC slurry and silicon MI.

DiCarlo, James A.

Modeling Creep-Induced Stress Relaxation at the Leading Edge of SiC/SiC Airfoils

Anticipating the implementation of advanced SiC/SiC composites into internally cooled airfoil components within the turbine section of future aero-propulsion engines, the primary objective of this study was to develop physics-based analytical and finite-element modeling tools to predict the effects of composite creep and stress relaxation at the airfoil leading edges, which will generally experience large thermal gradients at high temperatures. A second objective was to examine how some advanced NASA-developed SiC/SiC systems coated with typical EBC materials would behave as leading edge materials in terms of long-term steady-state operating temperatures. Because of the complexities introduced by mechanical stresses inherent in internally cooled airfoils, a simple cylindrical thin-walled tube model subjected to thermal stresses only is employed for the leading edge, thereby obtaining a best-case scenario for the material behavior. In addition, the SiC/SiC composite materials are assumed to behave as isotropic materials with temperature-dependent viscoelastic creep behavior as measured in-plane on thin-walled panels. Key findings include: (1) without mechanical stresses and for typical airfoil geometries, as heat flux is increased through the leading edge, life-limiting tensile crack formation will occur first in the hoop direction on the inside wall of the leading edge; (2) thermal gradients through all current SiC/SiC systems should be kept below approx.300 F at high temperatures to avoid this cracking; (3) at temperatures near the maximum operating temperatures of advanced SiC/SiC systems, thermal stresses induced by the thermal gradients will beneficially relax with time due to creep; (4) although stress relaxation occurs, the maximum gradient should still not exceed 300oF because of residual tensile stress buildup on the airfoil outer wall during cool-down; and (5) without film cooling and mechanical stresses, the NASA-developed N26 SiC/SiC system with thru-thickness Sylramic-iBN fiber reinforcement and a typical EBC coating has the potential of offering a maximum long-term steady-state operating temperature of approx.3100 F at the surface of the EBC.

Lang, Jerry

Further Developments in Modeling Creep Effects Within Structural SiC/SiC Components

Anticipating the implementation of advanced SiC/SiC composites into turbine section components of future aero-propulsion engines, the primary objective of this on-going study is to develop physics-based analytical and finite-element modeling tools to predict the effects of constituent creep on SiC/SiC component service life. A second objective is to understand how to possibly manipulate constituent materials and processes in order to minimize these effects. Focusing on SiC/SiC components experiencing through-thickness stress gradients (e.g., airfoil leading edge), prior NASA creep modeling studies showed that detrimental residual stress effects can develop globally within the component walls which can increase the risk of matrix cracking. These studies assumed that the SiC/SiC composites behaved as isotropic viscoelastic continuum materials with creep behavior that was linear and symmetric with stress and that the creep parameters could be obtained from creep data as experimentally measured in-plane in the fiber direction of advanced thin-walled 2D SiC/SiC panels. The present study expands on those prior efforts by including constituent behavior with non-linear stress dependencies in order to predict such key creep-related SiC/SiC properties as time-dependent matrix stress, constituent creep and content effects on composite creep rates and rupture times, and stresses on fiber and matrix during and after creep.

Lang, Jerry

Brazing SiC/SiC Composites to Metals

Experiments have shown that active brazing alloys (ABAs) can be used to join SiC/SiC composite materials to metals, with bond strengths sufficient for some structural applications. The SiC/SiC composite coupons used in the experiments were made from polymerbased SiC fiber preforms that were chemical-vapor-infiltrated with SiC to form SiC matrices. Some of the metal coupons used in the experiments were made from 304 stainless steel; others were made from oxygen-free, high-conductivity copper. Three ABAs were chosen for the experiments: two were chosen randomly from among a number of ABAs that were on hand at the time; the third ABA was chosen because its titanium content (1.25 percent) is less than those of the other two ABAs (1.75 and 4.5 percent, respectively) and it was desired to evaluate the effect of reducing the titanium content, as described below. The characteristics of ABAs that are considered to be beneficial for the purpose of joining SiC/SiC to metal include wettability, reactivity, and adhesion to SiC-based ceramics. Prior to further development, it was verified that the three chosen ABAs have these characteristics. For each ABA, suitable vacuum brazing process conditions were established empirically by producing a series of (SiC/SiC)/ABA wetting samples. These samples were then sectioned and subjected to scanning electron microscopy (SEM) and energy-dispersive x-ray spectrometry (EDS) for analysis of their microstructures and compositions. Specimens for destructive mechanical tests were fabricated by brazing of lap joints between SiC/SiC coupons 1/8-in. (.3.2- mm) thick and, variously, stainless steel or copper tabs. The results of destructive mechanical tests and the SEM/EDS analysis were used to guide the development of a viable method of brazing the affected materials.

Steffier, Wayne S.

Advances in SiC/SiC Composites for Aero-Propulsion

In the last decade, considerable progress has been made in the development and application of ceramic matrix composites consisting of silicon carbide (SiC) based matrices reinforced by small-diameter continuous-length SiC-based fibers. For example, these SiC/SiC composites are now in the early stages of implementation into hot-section components of civil aero-propulsion gas turbine engines, where in comparison to current metallic components they offer multiple advantages due to their lighter weight and higher temperature structural capability. For current production-ready SiC/SiC, this temperature capability for long time structural applications is ~1250 degC, which is better than ~1100 degC for the best metallic superalloys. Foreseeing that even higher structural reliability and temperature capability would continue to increase the advantages of SiC/SiC composites, progress in recent years has also been made at NASA toward improving the properties of SiC/SiC composites by optimizing the various constituent materials and geometries within composite microstructures. The primary objective of this chapter is to detail this latter progress, both fundamentally and practically, with particular emphasis on recent advancements in the materials and processes for the fiber, fiber coating, fiber architecture, and matrix, and in the design methods for incorporating these constituents into SiC/SiC microstructures with improved thermo-structural performance.

DiCarlo, James A.

Creep/Stress Rupture Behavior and Failure Mechanisms of Full CVI and Full PIP SiC/SiC Composites at Elevated Temperatures in Air

SiC/SiC composites fabricated by melt infiltration are being considered as potential candidate materials for next generation turbine components. However these materials are limited to 2400 F application because of the presence of residual silicon in the SiC matrix. Currently there is an increasing interest in developing and using silicon free SiC/SiC composites for structural aerospace applications above 2400 F. Full PIP or full CVI or CVI + PIP hybrid SiC/SiC composites can be fabricated without excess silicon, but the upper temperature stress capabilities of these materials are not fully known. In this study, the on-axis creep and rupture properties of the state-of-the-art full CVI and full PIP SiC/SiC composites with Sylramic-iBN fibers were measured at temperatures to 2700 F in air and their failure modes examined. In this presentation creep rupture properties, failure mechanisms and upper temperature capabilities of these two systems will be discussed and compared with the literature data.

Creep Durability

Thermographic Characterization of Impact Damage in SiC/SiC Composite Materials

SiC/SiC composite materials targeted as turbine components for next-generation aero-engines are being investigated at NASA Glenn Research Center. In order to examine damage mechanisms in these materials, SiC/SiC coupons were impacted with 1.59 mm diameter steel spheres at increasing velocities from 115 m/s to 400 m/s. Pulsed thermography, a nondestructive evaluation technique that monitors the thermal response of a sample over time, was utilized to characterize the impact damage. A thermal standard of similar material was fabricated to aid in the interpretation of the thermographic data and to provide information regarding thermography system detection capabilities in 2.4 mm thick SiC/SiC composite materials. Flat bottom holes at various depths with aspect ratios greater than 2.5 were detectable in the thermal images. In addition, the edges of holes at depths of 1.93 mm into the sample were not as resolvable as flat bottom holes closer to the surface. Finally, cooling behavior was characterized in SiC/SiC materials and used to determine impact damage depth within an 8.5% error of a known depth.

Fox, Dennis S.

Constituent-Based Life Models Being Developed for SiC/SiC Composites

For the successful utilization of ceramic matrix composites (CMC) as hot-section components in advanced aeropropulsion engines, the CMC constituents will need to be tailored and optimized to meet all the critical property demands of each component. Under the High-Speed Research (HSR) and Advanced High-Temperature Engine Materials Technology (HITEMP) Programs, the NASA Glenn Research Center at Lewis Field initiated research to develop mechanistic models for key CMC thermostructural properties. These models would describe the effects of different constituent factors (composition, geometry, and volume fraction) and of potential application conditions (stress, time, temperature, and environment) on these properties. Particular focus was placed on both analytical and numerical modeling of state-of-the-art SiC/SiC composites where the primary load-bearing constituents are stoichiometric SiC fibers in a complex multiphase SiC matrix produced by chemical vapor infiltration and melt infiltration. Recent studies have resulted in computer-based numerical models for the elastic modulus, thermal expansion, and thermal conductivity properties of the SiC/SiC system. Additional studies have generated analytical and empirical models for the time dependence of composite rupture strength at temperatures above 2200 F (1200 C), where CMC's have an important thermostructural advantage over current nickel-based superalloys. These life models utilize thermal activation theory and fiber stress-rupture results measured at Glenn to generate Larson-Miller (L M) plots of fiber rupture strength versus q, a single time- and temperature-dependent parameter. Assuming a worse case in which the SiC matrix is cracked, rupture is then controlled by the time-dependent fracture characteristics of the fiber bundles bridging the matrix cracks. With this as the controlling mechanism, one can then use simple composite theory and the fiber L M plots to predict CMC rupture strength versus the q parameter. The dashed line shows the predicted rupture strength of a SiC/SiC composite that is reinforced by a state-of-the-art stoichiometric SiC fiber. For the q parameter, time is in hours and temperature in degrees kelvin. To generate these predictions, a two-dimensional 0 /90 composite with approximately 16 percent fiber in the applied stress direction and an air test environment were assumed. As such, it is possible to compare the model predictions against limited stress-rupture data for this CMC as shown by the data points. The good agreement confirms the rupture model at least for the selected CMC and test conditions. Thus for this particular SiC/SiC composite, one can estimate a 1000-hr rupture strength of approximately 12 ksi at 2400 F (T = 1588 K and q = 39 700 K). At lower CMC application stresses, the SiC matrix is typically uncracked, so both the fiber and matrix constituents share the composite load. In this case, CMC rupture is controlled by the constituent with the longest rupture time based on the creep rate of the composite. Measured Monkman-Grant plots of rupture time versus creep rate for the two SiC constituents have been used to develop CMC life models for this important application condition. NASA and DOD are currently using this information to establish application and material goals for more advanced CMC's that can be used at even higher temperatures.

DiCarlo, James A.

Thermostructural Properties Of Sic/Sic Panels With 2.5d And 3d Fiber Architectures

CMC hot-section components in advanced engines for power and propulsion will typically require high cracking strength, high ultimate strength and strain, high creep- rupture resistance, and high thermal conductivity in all directions. In the past, NASA has demonstrated fabrication of a variety of SiC/SiC flat panels and round tubes with various 2D fiber architectures using the high-modulus high-performance Sylramic-iBN Sic fiber and Sic-based matrices derived by CVI, MI, and/or PIP processes. The thermo- mechanical properties of these CMC have shown state-of-the-art performance, but primarily in the in-plane directions. Currently NASA is extending the thermostructural capability of these SiC/SiC systems in the thru-thickness direction by using various 2.5D and 3D fiber architectures. NASA is also using specially designed fabrication steps to optimize the properties of the BN-based interphase and Sic-based matrices. In this study, Sylramic-iBN/SiC panels with 2D plain weave, 2.5D satin weave, 2.5D ply-to-ply interlock weave, and 3D angle interlock fiber architectures, all woven at AITI, were fabricated using matrix densification routes previously established between NASA and GEPSC for CVI-MI processes and between NASA and Starfire-Systems for PIP processes. Introduction of the 2.5 D fiber architecture along with an improved matrix process was found to increase inter-laminar tensile strength from 1.5 -2 to 3 - 4 ksi and thru-thickness thermal conductivity from 15-20 to 30-35 BTU/ft.hr.F with minimal reduction in in-plane strength and creep-rupture properties. Such improvements should reduce thermal stresses and increase the thermostructural operating envelope for SiC/SiC engine components. These results are analyzed to offer general guidelines for selecting fiber architectures and constituent processes for high-performance SiC/SiC engine components.

Yun, H. M.

Foreign Object Damage Resistance of Uncoated and EBC Coated SiC/SiC Composites

SiC/SiC composites fabricated by the melt infiltration method are candidate materials for the turbine components such as combustor liners, nozzle vanes and blades because of their high temperature strength, and thermal conductivity. To avoid surface recession in a combustion environment containing moisture, these materials also require an environmental barrier coating (EBC). Under thermal loading condition alone, the EBC coated SiC/SiC components show microstructural and strength stability after -1 5000 hr exposure to 12OO0C in combustion environment. However, the stability of SiC/SiC composites under impact conditions is not fully understood. In this study, both uncoated and EBC coated SiC/SiC composite specimens were impact tested by steel-ball projectiles at room temperature and at 1300 C in air. After impact, the specimens were analyzed under a scanning electron microscope to assess coating damage, and then tensile and bend tested at room temperature to determine their residual strength. The extent of coating and substrate damage with increasing projectile velocity was imaged and analyzed using nondestructive evaluation (NDE) methods such as micro focus x-ray radiography, tomography, and thermal wave imaging. The mechanical property results of impacted specimens are correlated with the NDE results and the scanning electron microscopy (SEM) observations. Influence of projectile velocity on impact damage of the coating/substrate, and the implication coating damage on durability of the composite will be discussed.

Bhatt, R. T.

Environmental Barrier Coating Development for SiC/SiC Ceramic Matrix Composites: Recent Advances and Future Directions

This presentation briefly reviews the SiC/SiC major environmental and environment-fatigue degradations encountered in simulated turbine combustion environments, and thus NASA environmental barrier coating system evolution for protecting the SiC/SiC Ceramic Matrix Composites for meeting the engine performance requirements. The presentation will review several generations of NASA EBC materials systems, EBC-CMC component system technologies for SiC/SiC ceramic matrix composite combustors and turbine airfoils, highlighting the temperature capability and durability improvements in simulated engine high heat flux, high pressure, high velocity, and with mechanical creep and fatigue loading conditions. This paper will also focus on the performance requirements and design considerations of environmental barrier coatings for next generation turbine engine applications. The current development emphasis is placed on advanced NASA candidate environmental barrier coating systems for SiC/SiC CMCs, their performance benefits and design limitations in long-term operation and combustion environments. The efforts have been also directed to developing prime-reliant, self-healing 2700F EBC bond coat; and high stability, lower thermal conductivity, and durable EBC top coats. Major technical barriers in developing environmental barrier coating systems, the coating integrations with next generation CMCs having the improved environmental stability, erosion-impact resistance, and long-term fatigue-environment system durability performance will be described. The research and development opportunities for turbine engine environmental barrier coating systems by utilizing improved compositions, state-of-the-art processing methods, and simulated environment testing and durability modeling will be briefly discussed.

Environmental Barrier Coatings

Durability Evaluation of a Thin Film Sensor System With Enhanced Lead Wire Attachments on SiC/SiC Ceramic Matrix Composites

An advanced thin film sensor system instrumented on silicon carbide (SiC) fiber reinforced SiC matrix ceramic matrix composites (SiC/SiC CMCs), was evaluated in a Mach 0.3 burner rig in order to determine its durability to monitor material/component surface temperature in harsh environments. The sensor system included thermocouples in a thin film form (5 microns thick), fine lead wires (75 microns diameter), and the bonds between these wires and the thin films. Other critical components of the overall system were the heavy, swaged lead wire cable (500 microns diameter) that contained the fine lead wires and was connected to the temperature readout, and ceramic attachments which were bonded onto the CMCs for the purpose of securing the lead wire cables, The newly developed ceramic attachment features a combination of hoops made of monolithic SiC or SiC/SiC CMC (which are joined to the test article) and high temperature ceramic cement. Two instrumented CMC panels were tested in a burner rig for a total of 40 cycles to 1150 C (2100 F). A cycle consisted of rapid heating to 1150 C (2100 F), a 5 minute hold at 1150 C (2100 F), and then cooling down to room temperature in 2 minutes. The thin film sensor systems provided repeatable temperature measurements for a maximum of 25 thermal cycles. Two of the monolithic SiC hoops debonded during the sensor fabrication process and two of the SiC/SiC CMC hoops failed during testing. The hoops filled with ceramic cement, however, showed no sign of detachment after 40 thermal cycle test. The primary failure mechanism of this sensor system was the loss of the fine lead wire-to-thin film connection, which either due to detachment of the fine lead wires from the thin film thermocouples or breakage of the fine wire.

Lei, Jih-Fen

Progress in SiC/SiC Ceramic Composite Development for Gas Turbine Hot-Section Components under NASA EPM and UEET Programs

The successful application of ceramic matrix composites as hot-section components in advanced gas turbine engines will require the development of constituent materials and processes that can provide the material systems with the key thermostructural properties required for long-term component service. Much initial progress in identifying these materials and processes was made under the former NASA Enabling Propulsion Materials Program using stoichiometric Sylramic (trademark) silicon-carbide (SiC) fibers, 2D (two dimensional)-woven fiber architectures, chemically vapor-infiltrated (CVI) BN fiber coatings (interphases), and SiC-based matrices containing CVI SiC interphase over-coatings, slurry-infiltrated SiC particulate, and melt-infiltrated (MI) silicon. The objective of this paper is to discuss the property benefits of this SiC/SiC composite system for high-temperature engine components and to elaborate on further progress in SiC/SiC development made under the new NASA Ultra Efficient Engine Technology Program. This progress stems from the recent development of advanced constituent materials and manufacturing processes, including specific treatments at NASA that improve the creep, rupture, and environmental resistance of the Sylramic fiber as well as the thermal conductivity and creep resistance of the CVI SiC over-coatings. Also discussed are recent observations concerning the detrimental effects of inadvertent carbon in the fiber-BN interfacial region and the beneficial effects of certain 2D-architectures for thin-walled SiC/SiC panels.

DiCarlo, J. A.

Advanced Environmental Barrier Coatings Developed for SiC/SiC Composite Vanes

Ceramic components exhibit superior high-temperature strength and durability over conventional component materials in use today, signifying the potential to revolutionize gas turbine engine component technology. Silicon-carbide fiber-reinforced silicon carbide ceramic matrix composites (SiC/SiC CMCs) are prime candidates for the ceramic hotsection components of next-generation gas turbine engines. A key barrier to the realization of SiC/SiC CMC hot-section components is the environmental degradation of SiC/SiC CMCs in combustion environments. This is in the form of surface recession due to the volatilization of silica scale by water vapor. An external environmental barrier coating (EBC) is a logical approach to achieve protection and long-term durability.

Lee, Kang N.

Advanced Woven SiC/SiC Composites for High Temperature Applications

The temperature, stress, and environmental conditions of many gas turbine, hypersonic, and even nuclear applications make the use of woven SiC/SiC composites an attractive enabling material system. The development in SiC/SiC composites over the past few years has resulted in significant advances in high temperature performance so that now these materials are being pursued for several turbine airfoil and reusable hypersonic applications. The keys to maximizing stress capability and maximizing temperature capability will be outlined for SiC/SiC. These include the type of SiC fiber, the fiber-architecture, and the matrix processing approach which leads to a variety of matrix compositions and structure. It will also be shown that a range of mechanical, thermal, and permeability properties can be attained and tailored depending on the needs of an application. Finally, some of the remaining challenges will be discussed in order for the use of these composite systems to be fully realized.

Morscher, Gregory N.

Creep Behavior of Hafnia and Ytterbium Silicate Environmental Barrier Coating Systems on SiC/SiC Ceramic Matrix Composites

Environmental barrier coatings will play a crucial role in future advanced gas turbine engines because of their ability to significantly extend the temperature capability and stability of SiC/SiC ceramic matrix composite (CMC) engine components, thus improving the engine performance. In order to develop high performance, robust coating systems for engine components, appropriate test approaches simulating operating temperature gradient and stress environments for evaluating the critical coating properties must be established. In this paper, thermal gradient mechanical testing approaches for evaluating creep and fatigue behavior of environmental barrier coated SiC/SiC CMC systems will be described. The creep and fatigue behavior of Hafnia and ytterbium silicate environmental barrier coatings on SiC/SiC CMC systems will be reported in simulated environmental exposure conditions. The coating failure mechanisms will also be discussed under the heat flux and stress conditions.