Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “SURFACE FINISHING”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 19 records

SURFACE FINISHING AND ELECTROLESS NICKEL PLATING OF ADDITIVELY MANUFACTURED (AM) METAL COMPONENTS

This study investigates the application of electroless nickel deposition on additively manufactured stainless steel samples. Current additive manufacturing (AM) technologies produce metal components with a rough surface. Rough surfaces generally exhibit fatigue characteristics, increasing the probability of initiating a crack or fracture to the printed part. For this reason, the direct use of as-produced parts in a finished product cannot be actualized, which presents a challenge. Post-processing of the AM parts is therefore required to smoothen the surface. This study analyzes chempolish (CP) and electropolish (EP) surface finishing techniques for post-processing AM stainless steel components CP has a great advantage in creating uniform, smooth surfaces regardless of size or part geometry EP creates an extremely smooth surface, which reduces the surface roughness to the sub-micrometer level. In this study, we also investigate nickel deposition on EP, CP, and as-built AM components using electroless nickel solutions. Electroless nickel plating is a method of alloy treatment designed to increase manufactured component's hardness and surface resistance to the unrelenting environment. The electroless nickel plating process is more straightforward than its counterpart electroplating.. We use low-phosphorus (2-5% P), medium-phosphorus (6-9% P), and high-phosphorus (10-13% P). These Ni deposition experiments were optimized using the L9 Taguchi design of experiments (TDOE), which compromises the prosperous content in the solution, surface finish, plane of the geometry, and bath temperature. The pre-and post-processed surface of the AM parts was characterized by KEYENCE Digital MicroscopeVHX-7000 and Phenom XL Desktop SEM. The experimental results show that electroless nickel deposition produces uniform Ni coating on the additively manufactured components up to 20 μm per hour. Mechanical properties of as-built and Ni coated AM samples were analyzed by applying a standard 10 N scratch test. Nickel coated AM samples were up to two times scratch resistant compared to the as-built samples. This study suggests electroless nickel plating is a robust viable option for surface hardening and finishing AM components for various applications and operating conditions.

Keywords: additive manufacturing, fatigue, chempol↗

Review of internal and external surface finishing technologies for additively manufactured metallic alloys components and new frontiers

Surface finishing in additive manufacturing (AM) is a technological bottleneck. The field of surface finishing of AM parts is vast because it not only focuses on roughness reduction in the hard-to-access internal surfaces but also includes the scope of adding coatings and sensors. Even though metal AM component is reaching the density and bulk microstructure at par or even better than conventionally produced components, adverse impact of surface roughness and imperfections is becoming the major obstruction. It is observed that external and internal surface roughness of AM components is a high probability cause of many unavoidable issues such as corrosion, incorrect tolerance estimations during the build stage, and the fatigue failure of parts before the expected life cycle. At present, AM field mainly focuses on improving and enhancing the internal and external surface roughness to pass the stringent qualification requirements for actual applications. To address these challenges, researchers worldwide are conducting many experiments and developing different surface finishing techniques. This paper reviews the state-of-the-art knowledge and processes of different surface finishing technology that can be applied to AM metal components. This article mainly highlights several liquid-based surfaces finishing approaches to develop promising surface microstructures on interior and exterior surfaces as a micromachining tool. The future of making strong and self-monitoring AM component requires broadening of surface finishing field and including advanced topics such as coatings and adding sensor technology. We also discuss new frontiers and the scope of future work in the surface finishing field to bring attention to related concerns and possibilities associated with making smart and strong AM components for twenty-first-century integrated engineering systems.

36 MATERIALS SCIENCE↗

Alternating chempolishing and electropolishing for interior and exterior surface finishing of additively manufactured (AM) metal components

Additively manufactured (AM) components’ surface finishing is crucial in adopting them for intended applications in challenging environments involving fatigue, corrosion, high temperature, and nuclear radiation. In our prior research, chempolishing (C) was utilized as an electroless etching process that uniformly smoothens complex AM components’ accessible interior and exterior surfaces (Tyagi et al. Additive Manufacturing, 25:32–38, 22). A wide range of electropolishing (E) has been demonstrated for AM surface finishing. However, electropolishing can impact a surface that can be juxtaposed to counter electrode and can yield a very smooth surface to sub-micrometer level roughness. However, a knowledge gap exists about the impact of applying both approaches on the same surface one after another and what new advantages may arise because of combining two methods. This paper uses dual-stage liquid-based surface finishing strategies produced by alternating the chempolishing (C) and electropolishing (E) steps. Two dual-stage surface finishing approaches, i.e., chempolishing followed by electropolishing (CE) and electropolishing followed by chempolishing (EC), were performed on the 316 stainless AM steel component. Impacts of EC and CE approaches were compared with single-stage C and E surface finishing approaches. An optical microscope and mechanical profilometer were utilized to investigate the wide range of surface roughness parameters. CE and EC produced Ra ~ 1.4 µm and ~ 1.6 µm, respectively. Surface roughness on CE- and EC-treated AM samples was lower than those individually treated by C and E approaches. Scanning electron microscopy provided further insights into the microstructural difference between CE- and EC-treated AM samples. This paper reports a liquid contact angle study on CE- and EC-treated AM samples to provide insights into the relative difference in surface energy that is crucial for making coatings on AM parts. A spectroscopic reflectance study was also employed to register the difference in physical properties of AM components treated with CE and EC approaches. Further, this study reveals industrially practicable interior and exterior surface finishing approaches for complex AM metal components that require minimum tooling and real-time process monitoring.

36 MATERIALS SCIENCE↗

Effect of Surface Finish on High-Temperature Oxidation of Steels in CO 2 , Supercritical CO 2 , and Air

Current and future power systems require steels resistant to high-temperature oxidation in CO 2 -rich environments. The introduction of structural defects by various surface treatments can profoundly affect the oxidation/corrosion behavior of steels in many environments. This effect is largely unexplored for steels exposed to high-temperature CO 2 , which is the focus of this work. We prepared Grade 22, Grade 91, 347H, and 310S steels with three different surface finishes, ranging from little to substantial surface damage, and exposed the steels to 1 bar CO 2 , 200 bar supercritical CO 2 , and laboratory air at 550 °C for up to 1500 h. Surface finish had little impact on the oxidation behavior of low-Cr (2 wt%) Grade 22 and high-Cr (25 wt%) 310S steels. In contrast, intermediate-Cr steels Grade 91 (8 wt%) and 347H (17 wt%) generally showed improved oxidation and carburization resistance with increasing extent of surface damage, which was attributed to the delay or prevention of the onset of Fe-rich oxide nodule growth. Comparison between exposure environments suggests that this effect is more complex for CO 2 compared to air and that it is additionally affected by CO 2 pressure. In conclusion, the results suggest that surface treatments should be considered as one approach to achieve improved corrosion resistance in high-temperature CO 2 , particularly for steels containing Cr levels near the transition that is required to form and maintain a protective Cr-rich oxide scale.

36 MATERIALS SCIENCE↗

Surface Finishing and Coating Parameters Impact on Additively Manufactured Binder-Jetted Steel–Bronze Composites

In this paper, electroless nickel plating is explored for the protection of binder-jetting-based additively manufactured (AM) composite materials. Electroless nickel plating was attempted on binder-jetted composites composed of stainless steel and bronze, resulting in differences in the physicochemical properties. We investigated the impact of surface finishing, plating solution chemistry, and plating parameters to attain a wide range of surface morphologies and roughness levels. We employed the Keyence microscope to quantitatively evaluate dramatically different surface properties before and after the coating of AM composites. Scanning electron microscopy revealed a wide range of microstructural properties in relation to each combination of surface finishing and coating parameters. We studied chempolishing, plasma cleaning, and organic cleaning as the surface preparation methods prior to coating. We found that surface preparation dictated the surface roughness. Taguchi statistical analysis was performed to investigate the relative strength of experimental factors and interconnectedness among process parameters to attain optimum coating qualities. The quantitative impacts of phosphorous level, temperature, surface preparation, and time factor on the roughness of the nickel-plated surface were 17.95%, 8.2%, 50.02%, and 13.21%, respectively. On the other hand, the quantitative impacts of phosphorous level, temperature, surface preparation, and time factor on the thickness of nickel plating were 35.12%, 41.40%, 3.87%, and 18.24%, respectively. The optimum combination of the factors’ level projected the lowest roughness of Ra at 7.76 µm. The optimum combination of the factors’ level projected the maximum achievable thickness of ~149 µm. This paper provides insights into coating process for overcoming the sensitivity of AM composites in hazardous application spaces via robust coating.

36 MATERIALS SCIENCE↗

Influence of Oxidation Treatments and Surface Finishing on the Electrochemical Behavior of Ni-20Cr HVOF Coatings

The low-temperature electrochemical behavior of HVOF Ni-20Cr coatings was assessed. The coatings were evaluated in different conditions including as-sprayed, as-ground, and heat-treated in air and argon atmospheres. A detailed analysis of the coatings was carried out by means of XRD, SEM, and EPMA, prior and after the corrosion test. The corrosion rate was analyzed in a NaCl solution saturated with CO{sub 2}. Results demonstrate that the use of a low-oxygen partial pressure favors the formation of a Cr{sub 2}O{sub 3} layer on the surface of the coatings. According to the electrochemical results, the lower corrosion rates were obtained for the heat-treated coatings irrespective of the surface finishing, being the ground and argon heat-treated condition that shows the best corrosion performance. This behavior is due to the synergistic effect of the low-pressure heat treatment and the grinding processes. The grinding promotes a more homogeneous reaction area without surface heterogeneities such as voids, and the pre-oxidation treatment decreases the porosity content of the coating and also allows the growing of a Cr-rich oxide scale which acts as a barrier against the ions of the aqueous solution.

36 MATERIALS SCIENCE↗

Enhancing Surface Finish of Additively Manufactured 316L Stainless Steel with Pulse/Pulse Reverse Electropolishing

To improve the reliable integration of additively manufactured (AM) metal components, there is an urgent need for surface finishing methods capable of processing rough, “as-printed” surfaces. Here, we present a new and scalable electropolishing (EP) technique for use on AM 316L stainless steel (SS) that is capable of achieving a surface roughness equivalent to a machined finish, with arithmetic mean heights (S a ) as low as 1.0 µm. This technique utilizes the sequential application of a new, NaCl/H 2 O pulse/pulse reverse (P/PR) EP step along with a conventional DC (direct current) EP step, where P/PR expands the capability of EP by removing roughness features > 1 µm, which has been previously unattainable with DC EP alone without substantial material removal. This is achieved by independently varying pulse parameters, such as pulse width and height, allowing more control over electrodynamic processes at the part-electrolyte interface. Additionally, P/PR EP resulted in higher smoothing efficiency, where a higher degree of smoothing was achieved with less material removal when compared with conventional DC EP alone. This minimizes unwanted change in geometry from excessive metal dissolution.

36 MATERIALS SCIENCE↗

Selective laser melting of oxide dispersion strengthened MA956 alloy and its surface finishing by magnetic field assisted finishing

Selective laser melting (SLM) is a prominent metal additive manufacturing (AM) capable of processing a myriad of engineering materials with high precision and design freedom. However, similar to other AM processes, poor surface finishing has been an omnipresent problem in SLM technology. In this study, magnetic field assisted finishing (MAF) was used to finish SLM fabricated oxide dispersion strengthened (ODS) MA956, an iron-chromium-aluminum alloy. The effect of laser processing parameters on part density and surface roughness was first studied. Using a multi-objective optimization technique, the optimal parameters to obtain the highest density and lowest surface roughness were determined. Finally, MAF was applied to the parts built with the obtained optimal SLM parameters, but without significant improvement on the surfaces of as-printed samples. Hence, the surfaces of as-printed samples were post-processed (ground) to yield better initial surface conditions prior to MAF. The effect of initial roughness, iron particles size, and abrasive size on MAF performance was studied. Initial roughness had the most dominant effect followed by abrasive size. The underlying mechanism behind the dependency on initial roughness on final surface quality was analyzed by studying the change on the surface profiles with different starting initial roughness. The initial roughness required for MAF to be effective was determined. In conclusion, using the optimal processing conditions, MAF was applied to the post-processed samples to attain the final average surface roughness (R a ) as little as 0.36 μm starting from initial average roughness (R a ) of 1.53 μm.

36 MATERIALS SCIENCE↗

Finishing Surface Treatment of Potassium Titanyl Phosphate Single Crystals by Argon Cluster Ions

It is demonstrated that a argon cluster ion beam can be used for the finishing treatment of ultrasmooth surfaces (with initial root-mean-square roughness below 0.3 nm) of potassium titanyl phosphate single crystals. Analysis of the power spectral density function of surface roughness showed that cluster-ion irradiation leads to removal of residual chemical contaminations from the subsurface layer and produces additional smoothing of the crystal surface in a broad range of spatial frequencies (ν = 0.2–100 μm{sup –1}).

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Corrosion protection of ENIG surface finishing using electrochemical methods

Four types of thin film coating were carried out on copper for electronic materials by the electroless plating method at a pH range from 3 to 9. The coating performance was evaluated by electrochemical impedance spectroscopy and potentiodynamic polarization testing in a 3.5 wt.% NaCl solution. In addition, atomic force microscopy and X-ray diffraction were also used to analyze the coating surfaces. The electrochemical behavior of the coatings was improved using the electroless nickel plating solution of pH 5. The electroless nickel/immersion gold on the copper substrate exhibited high protective efficiency, charge transfer resistance and very low porosity, indicating an increase in corrosion resistance. Atomic force microscopy and X-ray diffraction analyses confirmed the surface uniformity and the formation of the crystalline-refined NiP {l_brace}1 2 2{r_brace} phase at pH 5.

36 MATERIALS SCIENCE↗

Power Cylinder Friction Reduction Through Coatings, Surface Finish and Design

About 7-10% of the total energy input in a vehicle is lost due to mechanical friction, and in an engine, about 50% of the total frictional losses occur at the interface between the cylinder and pistons and piston rings. Therefore, this interface offers great opportunities for friction reduction. The goal of this proposed study is to demonstrate friction reduction potential using advanced coatings, surface finish, and design on power cylinder system containing cylinder bore, piston rings, crankshaft, and advanced engine oils. Experience through years of research in this area lead us to believe that full benefit potential can be realized only by considering a systems approach.

33 ADVANCED PROPULSION SYSTEMS↗

Performance characterization of freeform finished surfaces of potassium dihydrogen phosphate using fluid jet polishing with a nonaqueous slurry

Abstract Potassium dihydrogen phosphate (KDP) and its deuterated analog (DKDP) are unique nonlinear optical materials for high power laser systems. They are used widely for frequency conversion and polarization control by virtue of the ability to grow optical-quality crystals at apertures suitable for fusion-class laser systems. Existing methods for freeform figuring of KDP/DKDP optics do not produce surfaces with sufficient laser-induced–damage thresholds (LIDT’s) for operation in the ultraviolet portion of high-peak-power laser systems. In this work, we investigate fluid jet polishing (FJP) using a nonaqueous slurry as a sub-aperture finishing method for producing freeform KDP surfaces. This method was used to selectively polish surface areas to different depths on the same substrate with removals ranging from 0.16 μm to 5.13 μm. The finished surfaces demonstrated a slight increase in roughness as the removal depth increased along with a small number of fracture pits. Laser damage testing with 351 nm, 1 ns pulses demonstrated excellent surface damage thresholds, with the highest values in areas devoid of fracture pits. This work demonstrates, for the first time, a method that enables fabrication of a waveplate that provides tailored polarization randomization that can be scaled to meter-sized optics. Furthermore, this method is based on FJP technology that incorporates a nonaqueous slurry specially designed for use with KDP. This novel nonaqueous FJP process can be also used for figuring other types of materials that exhibit similar challenging inherent properties such as softness, brittleness, water-solubility, and temperature sensitivity.

36 MATERIALS SCIENCE↗

Coating for improved surface finish

A ceramic matrix composite (CMC) component includes at least one seal surface, the at least one seal surface disposed adjacent an interfacing surface for providing a seal therebetween; and a coating disposed on the seal surface. The coating includes an aluminum oxide and/or a silicon dioxide.

Hafner, Matthew Troy↗

Processing aluminum alloy with hybrid wire arc additive manufacturing and ultrasonic nanocrystalline surface modification to improve porosity, surface finish, and hardness

Here, in this paper, a novel hybrid wire arc additive manufacturing (WAAM) and ultrasonic nanocrystal surface modification (UNSM) on porosity manipulation and surface properties of aluminum 5356 alloys was studied. The goal is to improve the quality of the WAAM-built part by eliminating bigger pores and reducing its size, reducing surface roughness, and increasing surface hardness. The as-built WAAM and WAAM-UNSM-treated samples were quantitatively studied for porosity using an X-ray micro-computed tomography (μ-CT). The surface roughness was measured on the surface profile of the same samples before and after UNSM treatment. Followed by the Vickers micro-hardness tests to evaluate the hardness modified by the influence of the UNSM treatment. It was found that the bigger pores in the as-built WAAM samples were eliminated and the medium-sized pores were shrunk to almost half the size after the UNSM treatment. Further, the UNSM treatment showed a significant improvement in both surface roughness and hardness on the WAAM Al5356 samples. This experimental work demonstrates the critical advantages of hybrid WAAM-UNSM in improving the qualities of the WAAM processed parts.

Hardness↗

Buffered Electropolishing – A New Way for Achieving Extremely Smooth Surface Finish on Nb SRF Cavities to be Used in Particle Accelerators

Future accelerators require unprecedented cavity performance, which is strongly influenced by interior surface nano-smoothness. Electropolishing (EP) is the technique of choice to be developed for high-field superconducting radio frequency (SRF) cavities. Electrochemical impedance spectroscopy (EIS) and related techniques point to the electropolishing mechanism of Nb in a sulphuric and hydrofluoric acid electrolyte controlled by a compact surface salt film under F- diffusion-limited mass transport control. These and other findings are guiding a systematic characterization to form the basis for cavities process optimization.

43 PARTICLE ACCELERATORS↗