Two heats of G91 steel have been investigated in liquid sodium at 550- 650°C to understand their corrosion behaviour, microstructural evolution, and tensile properties. Sodium exposure experiments of subsized, sheet-type tensile specimens of G91 were performed in Argonne’s forced convection sodium materials testing loops, SMT-1 and SMT-2. Maximum exposure times of ~49,000 h at ~38,000 h, and ~20,000 h have been achieved at 550, 600, and 650°C, respectively. Thermal aging experiments of G91 steel were also conducted in parallel, and the results were compared with those of the sodium-exposed specimens to isolate the effect of thermal aging from the effect of sodium exposure. It was found that the yield stress and ultimate tensile strength of G91 were reduced by more than 50% after sodium exposures at 650°C due to decarburization. The reduction in tensile strength was accompanied by the dissolution of M 23 C 6 carbides and excessive grain growth. The effect of sodium at 550 and 600°C was insignificant for exposure times up to ~49,000 h and ~38,000 h, respectively. The effect of sodium on the microstructural stability and tensile properties of G91 is largely dependent on the carbon mass transfer in the alloy-sodium system.
22 GENERAL STUDIES OF NUCLEAR REACTORS↗