Effects of Slag Composition on H{sub 2} Generation and Magnetic Precipitation from Molten Steelmaking Slag–Steam Reaction
In this paper, the effects of slag composition (slag basicity CaO/SiO{sub 2} and FeO concentration) on the amounts of H{sub 2} gas generated and the magnetic spinel phase precipitated as a result of the reaction between synthetic steelmaking slag and steam at 1873 K (1600 °C) were studied by thermodynamic simulation (using Thermodynamic Package FactSage 7.0) and laboratory experiments. The thermodynamic calculation showed that, upon increasing slag basicity (CaO/SiO{sub 2}) from 1.0 to 2.5, for the reaction of 100 g of slags with 100 g of H{sub 2}O gas, the accumulated amount of the produced H{sub 2} gas increased from 0.17 to 0.27 g, while the amount of magnetic spinel phase first increased and then decreased, with the maximum precipitation of 16.71 g at the basicity of 1.5. When the FeO concentration increased from 15 to 30 pct for the slag with basicity of 2.0, the accumulated amount of the produced H{sub 2} gas increased from 0.17 to 0.28 g, and the amount of magnetic spinel phase increased from 5.88 to 10.59 g. The laboratory experiments were conducted in confocal laser scanning microscope to verify the reaction between 0.2 g of slag and 3.75 L of H{sub 2}O-Ar gas (P{sub H{sub 2O}} =0.2 atm). The results indicated that, for 100 g of slags, upon increasing slag basicity (CaO/SiO{sub 2}) from 1.0 to 2.5, both the produced H{sub 2} gas and magnetic spinel phase first increased and then decreased, with the maximum amounts being 0.09 g of gas and 37.00 g of magnetic spinel phase at the slag basicity of 1.50. For the FeO concentration increasing from 15 to 30 pct, the amounts of both the produced H{sub 2} gas and magnetic spinel phase increased from 0.04 to 0.10 g and from 18.00 to 27.00 g, respectively. The reaction rate between the molten CaO-SiO{sub 2}-FeO-MnO-Al{sub 2}O{sub 3}-MgO slag and the moisture (P{sub H{sub 2O}} =0.2 atm) increased with the increasing FeO activity in the slag. The dependence of the reaction rate (mol/cm{sup 2}/s) on FeO content can be expressed as r =(7.67(a{sub FeO})−2.99)×10{sup −7}.
Slag Penetration into Refractory Lining of Slagging Coal Gasifier
The impurities in coal are converted into molten slag typically containing SiO2, FeO, CaO, and Al2O3 when coal feedstock is burned in slagging gasifiers. The slag flows down the gasifier sidewalls, dissolves, and penetrates and reacts with the refractory lining that protects the stainless steel shell of the gasifier from elevated temperatures (1300–1600°C). Refractories composed primarily of Cr2O3 have been found most resistant to slag corrosion, but they continue to fail performance requirements because of low resistance to spalling. Post-mortem analysis of high-chromia refractory bricks collected from commercial gasifiers suggests that the spalling is affected by the depth of slag penetration that is in turn affected by the wettability and interconnected porosity of the refractory as well as the slag viscosity. Laboratory tests were conducted to measure the viscosity of slags (Wyoming Powder River Basin [PRB], Pocahontas #3, and Pittsburgh #8), their contact angle on refractories (chromia-alumina [Aurex 75SR] and high-chromia [Serv 95 and Aurex 95P]), and the apparent porosity of selected refractories. In addition, the depth of slag penetration as a function of time and temperature was determined for various refractory-slag combinations. The results of laboratory tests were used to develop a refractory material that has high resistance to penetration by molten slag and thus has a potential to have a substantially longer service life than the materials currently being used.
Numerical Simulation of Slag Eye Formation and Slag Entrapment in a Bottom-Blown Argon-Stirred Ladle
A transient mathematical model is developed for simulating the bubble-steel-slag-top gas four-phase flow in a bottom-blown argon-stirred ladle with a 70-ton capacity. The Lagrangian discrete phase model (DPM) is used for describing the moving behavior of bubbles in the steel and slag. To observe the formation process of slag eye, the volume of fluid (VOF) model is used to track the interfaces between three incompressible phases: metal/slag, metal/gas, and slag/gas. The complex multiphase turbulent flow induced by bubble-liquid interactions is solved by a large eddy simulation (LES) model. Slag eye area and slag droplet dispersion are investigated under different gas flow rates. The results show that the movement of bubbles, formation and collapse of slag eye, volatility of steel/slag interface and behavior of slag entrapment can be properly predicted in the current model. When the gas flow rate is 300 L/min, the circulation driven by the bubble plume will stir the entire ladle adequately and form a slag eye of the right size. At the same time, it will not cause strong erosion to the ladle wall, and the fluctuation of the interface is of adequate intensity, which will be helpful for improving the desulfurization efficiency; the slag entrapment behavior can also be decreased. Interestingly, with the motion of liquid steel circulation, the collision and coalescence of dispersed slag droplets occur during the floating process in the vicinity of the wall.
Modification of Inclusions in Molten Steel by Mg-Ca Transfer from Top Slag: Experimental Confirmation of the ‘Refractory-Slag-Metal-Inclusion (ReSMI)’ Multiphase Reaction Model
High-temperature experiments and Refractory-Slag-Metal-Inclusion (ReSMI) multiphase reaction simulations were carried out to determine the effect of the ladle slag composition on the formation behavior of non-metallic inclusions in molten steel. Immediately after the slag-metal reaction, magnesium migrated to the molten steel and a MgAl{sub 2}O{sub 4} spinel inclusion was formed due to a reaction between magnesium and alumina inclusions. However, the spinel inclusion changed entirely into a liquid oxide inclusion via the transfer of calcium from slag to metal in the final stage of the reaction. Calcium transfer from slag to metal was more enhanced for lower SiO{sub 2} content in the slag. Consequently, the spinel inclusion was modified to form a liquid CaO-Al{sub 2}O{sub 3}-MgO-SiO{sub 2} inclusion, which is harmless under steelmaking conditions. The modification reaction was more efficient as the SiO{sub 2} content in the slag decreases.
Optimization of Mineralogy and Microstructure of Solidified Basic Oxygen Furnace Slag Through SiO{sub 2} Addition or Atmosphere Control During Hot-Stage Slag Treatment
Valorization of basic oxygen furnace (BOF) slag is of significant importance for mitigation of the steel production’s environmental impact. The present work aims to investigate the influence of SiO{sub 2} addition and oxygen partial pressure on the mineralogical modification of a typical industrial BOF slag. The slag basicity (mass ratio of CaO/SiO{sub 2}) was varied from 1.8 to 4.4 by mixing specific amounts of SiO{sub 2} with the master BOF slag. The original and modified slags were remelted and solidified under argon or air atmosphere followed by slow cooling. The experimental observations were then compared with the results of thermodynamic modeling to achieve a thorough understanding. With decreasing the basicity, free lime was eliminated, as it forms dicalcium silicate (Ca{sub 2}SiO{sub 4}). With increasing oxygen partial pressure, wustite was oxidized to hematite, which combined with free lime to form calcium aluminoferrite (C{sub 2}AF). The effects of SiO{sub 2} addition and oxygen partial pressure were finally evaluated with respect to the energy consumption for the BOF slag valorization. The modified slag is suitable as a precursor for construction applications as binders.
Interactions of refractory materials with molten gasifier slags
Explore the source record for details and available documents.
Influence of slag chemistry on the hydration of alkali-activated blast-furnace slag - Part I: Effect of MgO
The hydration and the microstructure of three alkali activated slags (AAS) with MgO contents between 8 and 13 wt.% are investigated. The slags were hydrated in the presence of two different alkaline activators, NaOH and Na{sub 2}SiO{sub 3}.5H{sub 2}O (WG). Higher MgO content of the slag resulted in a faster reaction and higher compressive strengths during the first days. The formation of C(- A)-S-H and of a hydrotalcite-like phase was observed in all samples by X-ray diffraction (XRD), thermal analysis (TGA) and scanning electron microscopy (SEM) techniques. Increasing the MgO content of the slag from 8 to 13% increased the amount of hydrotalcite and lowered the Al uptake by C-S-H resulting in 9% higher volume of the hydrates and a 50 to 80% increase of the compressive strength after 28 days and longer for WG activated slag pastes. For NaOH activated slags only a slight increase of the compressive strength was measured.
Crystallization of synthetic coal-petcoke slag mixtures simulating those encountered in entrained bed slagging gasifiers
Commercial entrained bed slagging gasifiers use a carbon feedstock of coal, petcoke, or combinations of them to produce CO and H{sub 2}. These carbon sources contain mineral impurities that liquefy during gasification and flow down the gasification sidewall, interacting with the refractory linear and solidifying in the cooler zones of the gasifier. Proper slag flow is critical to good gasifier operation. A hot-stage confocal scanning laser microscope (CSLM) was used to analyze the kinetic behavior of slag crystallization for a range of synthetic coal-petcoke mixtures. On the basis of the observed precipitation during cool down studies in the 1200-1700{sup o}C temperature range, a time-temperature-transformation (TTT) diagram was created. The crystallization studies were conducted with a CO/CO{sub 2} (=1.8) corresponding to a gasification PO{sub 2} of approximately 10-8 atm at 1500{sup o}C. Ash chemistries were chosen such that they correspond to coal-petcoke feedstock mixtures with coal ash amounts of 0, 10, 30, 50, 70, and 100% (by weight), with the balance being petcoke ash. The TTT diagram exhibited two crystallization areas, one above and one below 1350{sup o}C. At the nose of the higher temperature curves, karelianite (V{sub 2}O{sub 3}) crystallization occurred and was fastest for a 30% coal-petcoke ash mixture. The second nose was located below 1350{sup o}C and had spinel-type phases that formed at 1200{sup o}C, in which preferred atomic occupation at the octahedral and tetrahedral sites varied depending upon the ash composition. At 1200{sup o}C, an Al-rich spinel formed for 100% coal slag and a Fe-rich spinel formed in petcoke-enriched slags. The addition of petcoke ash to coal ash promoted crystallization in the slag, with additional crystalline phases, such as V-rich spinel, forming at the lower temperatures. These phases were not predicted using commercially available databases. 30 refs., 18 figs.
Effect of Temperature Gradient on Industrial Gasifier Coal Slag Infiltration into Alumina Refractory
Explore the source record for details and available documents.
Slag Behavior in Gasifiers. Part II: Constitutive Modeling of Slag
The viscosity of slag and the thermal conductivity of ash deposits are among two of the most important constitutive parameters that need to be studied. The accurate formulation or representations of the (transport) properties of coal present a special challenge of modeling efforts in computational fluid dynamics applications. Studies have indicated that slag viscosity must be within a certain range of temperatures for tapping and the membrane wall to be accessible, for example, between 1,300 °C and 1,500 °C, the viscosity is approximately 25 Pa·s. As the operating temperature decreases, the slag cools and solid crystals begin to form. Since slag behaves as a non-linear fluid, we discuss the constitutive modeling of slag and the important parameters that must be studied. We propose a new constitutive model, where the stress tensor not only has a yield stress part, but it also has a viscous part with a shear rate dependency of the viscosity, along with temperature and concentration dependency, while allowing for the possibility of the normal stress effects. In Part I, we reviewed, identify and discuss the key coal ash properties and the operating conditions impacting slag behavior.
Influence of slag chemistry on the hydration of alkali-activated blast-furnace slag - Part II: Effect of Al{sub 2}O{sub 3}
The hydration and microstructural evolution of three alkali activated slags (AAS) with Al{sub 2}O{sub 3} contents between 7 and 17% wt.% have been investigated. The slags were hydrated in the presence of two different alkaline activators, NaOH and Na{sub 2}SiO{sub 3}{center_dot}5H{sub 2}O. The formation of C(-A)-S-H and hydrotalcite was observed in all samples by X-ray diffraction, thermal analysis and scanning electron microscopy. Higher Al{sub 2}O{sub 3} content of the slag decreased the Mg/Al ratio of hydrotalcite, increased the Al incorporation in the C(-A)-S-H and led to the formation of straetlingite. Increasing Al{sub 2}O{sub 3} content of the slag slowed down the early hydration and a lower compressive strength during the first days was observed. At 28 days and longer, no significant effects of slag Al{sub 2}O{sub 3} content on the degree of hydration, the volume of the hydrates, the coarse porosity or on the compressive strengths were observed.
Interaction of Pure Alumina Refractory with FeO–SiO 2 and FeO–SiO 2 –CaO Slags Relevant to the Novel Flash Ironmaking Technology
Not provided.
The Effect of Propellant Variables on Slag in Subscale Spin Motors: Design and Qualification of a Slag Discrimination Motor - Part 1
The formation, collection, and expulsion of aluminum oxide slag is known to affect the performance of many solid rocket motor systems. Slag expulsion, in particular, is believed to be capable of causing pressure and thrust perturbations. Propellant combustion studies, performed and documented by many investigators, have shown that variations in propellant raw materials and processing affect the nature of alumina droplets at the burning propellant surface, and hence, may affect the quantity of slag retained in the motor chamber, available for expulsion. Thiokol has completed an experimental and analytical evaluation to determine the effects of several material and process variables on Space SHuttle propellant and its propensity to 'slag'. This paper describes the test article, a small scale spin motor with special nozzle, designed and qualified as a slag discriminating tool for use in the evaluation.
Iron speciation in blast furnace slag cements
Slag-containing pastes and concretes were analysed by element-specific synchrotron-based techniques to determine the speciation of iron on crushed materials through spatially resolved micro-spectroscopic studies. The investigated cement samples were hydrated either in the laboratory, or exposed to river or sea water. Metallic iron, along with minor proportions of iron sulphide and magnetite was detected in the laboratory sample. Iron sulphide, goethite, and siliceous hydrogarnet were discovered in the blended slag cements hydrated in contact with river water for up to 7 years. In contrast, no Fe(0) was observed in blended concretes exposed to sea water. Instead, iron sulphide, iron(II)-hydroxide and -oxide, hematite, magnetite, siliceous hydrogarnet, and goethite were detected as well as ilmenite (FeTiO{sub 3}) in the aggregates. The strong acceleration of Fe oxidation in samples exposed to sea water and the long-term passivation observed in the other samples indicate comparable processes as those occurring on steel bars.
Molecular structure of CaO?FeO[subscript x]?SiO[subscript 2] glassy slags and resultant inorganic po
Explore the source record for details and available documents.
Synthesis of Titanium Oxycarbide from Titanium Slag by Methane-Containing Gas
In this study, reaction steps of a process for synthesis of titanium oxycarbide from titanium slag were demonstrated. This process involves the reduction of titanium slag by a methane-hydrogen-argon mixture at 1473 K (1200 °C) and the leaching of the reduced products by hydrofluoric acid near room temperature to remove the main impurity (Fe{sub 3}Si). Some iron was formed by disproportionation of the main M{sub 3}O{sub 5} phase before gaseous reduction started. Upon reduction, more iron formed first, followed by reduction of titanium dioxide to suboxides and eventually oxycarbide.
Effect of Slag Composition on the Crystallization Kinetics of Synthetic CaO-SiO{sub 2}-Al{sub 2}O{sub 3}-MgO Slags
The crystallization kinetics of CaO-SiO{sub 2}-Al{sub 2}O{sub 3}-MgO (CSAM) slags was studied with the aid of single hot thermocouple technique (SHTT). Kinetic parameters such as the Avrami exponent (n), rate coefficient (K), and effective activation energy of crystallization (E{sub A}) were obtained by kinetic analysis of data obtained from in situ observation of glassy to crystalline transformation and image analysis. Also, the dependence of nucleation and growth rates of crystalline phases were quantified as a function of time, temperature, and slag basicity. Together with the observations of crystallization front, they facilitated establishing the dominant mechanisms of crystallization. In an attempt to predict crystallization rate under non-isothermal conditions, a mathematical model was developed that employs the rate data of isothermal transformation. The model was validated by reproducing an experimental continuous cooling transformation diagram purely from isothermal data.