Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “SILVER 111”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

The friction behavior of semiconductors Si and GaAs in contact with pure metals

The friction behavior of the semiconductors silicon and gallium arsenide in contact with pure metals was studied. Five transition and two nontransition metals, titanium, tantalum, nickel, palladium, platinum, copper, and silver, slid on a single crystal silicon (111) surface. Four metals, indium, nickel, copper and silver, slid on a single crystal gallium arsenide (100) surface. Experiments were conducted in room air and in a vacuum of 10 to the minus 7th power N/sq cm (10 to the minus 9th power torr). The results indicate that the sliding of silicon on the transition metals exhibits relatively higher friction than for the nontransition metals in contact with silicon. There is a clear correlation between friction and Schottky barrier height formed at the metal silicon interface for the transition metals. Transition metals with a higher barrier height on silicon had a lower friction. The same effect of barrier height was found for the friction of gallium arsenide in contact with metals.

Mishina, H.↗

Friction behavior of silicon in contact with titanium, nickel, silver and copper

Sliding friction experiments are conducted with the semiconductor silicon in contact with the metals titanium, nickel, copper, and silver. Sliding is on the (111) plane of single-crystal silicon in the 112 crystallographic direction both in dry and lubricated (mineral oil) sliding. The friction coefficient in dry sliding is controlled by adhesion and the surface chemical activity of the metal. The more active the metal the stronger the adhesion and the higher the friction. In lubricated sliding the lubricant absorbs to the surfaces and reduces the importance of metal chemical effects. In lubricated sliding, silicon ceases to behave in a brittle manner and undergoes plastic deformation under load.

Mishina, H.↗

Effect of barrier height on friction behavior of the semiconductors silicon and gallium arsenide in contact with pure metals

Friction experiments were conducted for the semiconductors silicon and gallium arsenide in contact with pure metals. Polycrystalline titanium, tantalum, nickel, palladium, and platinum were made to contact a single crystal silicon (111) surface. Indium, nickel, copper, and silver were made to contact a single crystal gallium arsenide (100) surface. Sliding was conducted both in room air and in a vacuum of 10 to the minus 9th power torr. The friction of semiconductors in contact with metals depended on a Schottky barrier height formed at the metal semiconductor interface. Metals with a higher barrier height on semiconductors gave lower friction. The effect of the barrier height on friction behavior for argon sputtered cleaned surfaces in vacuum was more specific than that for the surfaces containing films in room air. With a silicon surface sliding on titanium, many silicon particles back transferred. In contrast, a large quantity of indium transferred to the gallium arsenide surface.

Mishina, H.↗

Hyperthermal atomic oxygen generator

Characterization of the transport properties of oxygen through silver was continued. Specifically, experiments measuring the transport through Ag(111), Ag(110), Ag(100) single crystals and through Ag0.05 Zr alloy were completed. In addition, experiments using glow discharge excitation of oxygen to assist in the transport were completed. It was found that the permeability through the different orientations of single crystal Ag was the same, but significant differences existed in the diffusivity. The experimental ratio of diffusivities, however, was in reasonable agreement with theoretical estimates. Since the solubilities of orientations must be the same, this suggests some problems with the assumption K = DS. The glow discharge experiments show that there is a substantial increase in transport (factor of six) when the upstream pressure is dissociated to some fraction of atoms (which have a much higher sticking coefficient). These results indicate that there is a significant surface limitation because of dissociative adsorption of the molecules. Experiments with the Ag0.05 Zr alloy and its high-grain boundary and defect density show a permeability of greater than a factor of two over ordinary polycrystalline Ag, but it is unclear as to whether this is because of enhanced transport through these defects or whether the Zr and defects on the surface increased the sticking coefficient and therefore the transport.

Khandelwal, Govind S.↗

Thermal and oxidative degradation studies of formulated C-ethers by gel-permeation chromatography

Gel-permeation chromatography was used to analyze C-ether lubricant formulations from high-temperature bearing tests and from micro-oxidation tests. Three mu-styragel columns (one 500 and two 100 A) and a tetrahydrofuran mobile phase were found to adequately separate the C-ether degradation products. The micro-oxidation tests yielded degradation results qualitatively similar to those observed from the bearing tests. Micro-oxidation tests conducted in air yielded more degradation than did tests in nitrogen. No great differences were observed between the thermal-oxidative stabilities of the two C-ether formulations or between the catalytic degradation activities of silver and M-50 steel. C-ether formulation I did yield more degradation than did formulation II in 111- and 25-hour bearing tests, respectively.

Jones, W. R., Jr.↗