Results for “SHOT PEENING”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 19 records

Non-Destructive Characterization of Subsurface Residual Stress Fields and Correlation with Microstructural Conditions in a Shot-Peened Inconel Component

Shot-peening is an important surface treatment used in a preventative way to guard against fatigue failures. The residual stress state imparted by shot-peening deters the formation and propagation of surface cracks. In this paper, we describe the measurement of residual stresses in an Inconel, IN100, sample using lattice strains measured using High Energy X-ray Diffraction (HEXD) and a Bi-Scale Optimization Method (BSOM). HEXD enabled rapid, non-destructive lattice strain measurements over a large region of the sample. Subsurface strains were obtained using a conical slit setup. The BSOM utilizes a macroscale representation of the sample and a spherical harmonic-based crystal scale representation of crystal orientation space at each experimental point (diffraction volume). A roughly biaxial stress state was predicted with a von Mises equivalent stress between 300 MPa and 400 MPa near the surface. The layer of material with high residual stress induced by shot-peening was found to be approximately 1 mm thick. Diffraction peak width, EBSD, and microhardness measurements were also made on the same sample, which rendered more qualitative measures of the plasticity-related effects of the shot-peening induced residual stress field. All of these measurements show a dimishing shot-peening plasticity with the increasing depth.

42 ENGINEERING↗

RESONANT FREQUENCY EDDY CURRENT LIFTOFF MEASUREMENTS FOR SHOT PEENING INTENSITY ASSESSMENT IN MATERIALS

The shot peening intensity of nickel base materials has been examined with an innovative eddy current measurement. The goal is to provide a nondestructive tool to quantitatively evaluate the surface conditions after shot peening. Traditionally, the residual stress caused by the shot peening process can be examined by X-ray diffraction. Recent eddy current works have shown promising results in evaluating the small conductivity variation due to the residual stress. This study explores the feasibility of utilizing the cable which connects to a network analyzer and a conventional eddy current probe to monitor the surface conditions due to the shot peening.

36 MATERIALS SCIENCE↗

The Effect of Multiple Shot Peening on the Corrosion Behavior of Duplex Stainless Steel

Various types of shot peening treatments were applied to duplex stainless steel. The effects of shot peening intensity and working procedures on the microstructure were investigated. The domain size and microstrain evolution in the surface layer were characterized utilizing the Rietveld method. As the shot peening intensity increased, the surface roughness increased in the surface layer; however, it decreased after multiple (dual and triple) shot peening. The mole fraction of strain-induced martensite as a function of the intensity of shot peening was evaluated by XRD measurements. Both potentiodynamic polarization curves and salt spray tests of shot-peened samples in NaCl solution were investigated. The results indicate that traditional shot peening has negative effects on corrosion resistance with increasing shot peening intensity; however, the corrosion rate can be reduced by means of multiple shot peening.

36 MATERIALS SCIENCE↗

The Effect of Shot Peening on Steam Oxidation of 304H Stainless Steel

Shot peening is currently utilized in coal-fired power plant components to mitigate scale exfoliation issues from steamside oxidation of austenitic stainless steel superheater and reheater tubing. To focus on commercially available material, this study exposed quarter-ring specimens cut from two different commercially shot peened type 304H tubes and exposed to 1 bar steam for up to 15,000 h at 550°, 600°, 625°, and 650 °C. Specimens were removed at increments to characterize the oxide thickness and microstructure. The shot peened inner surface generally retained a thin, protective Cr-rich scale with occasional Fe-rich oxide nodules at 550–625 °C. The increased oxidation resistance from shot peening began to degrade at 650 °C after as little as 5,000 h. Cut and polished faces of these specimens formed thick, Fe-rich oxides similar to polished 304H coupons. Surprisingly, the mechanically machined outer surface of the tube specimens performed similarly to the shot peened inner diameter, suggesting it had sufficient cold work to achieve a similar benefit. As a result, electron backscatter diffraction and Vickers-hardness measurements were used to characterize post-exposure changes in underlying microstructure and mechanical properties, respectively, imparted by shot peening.

36 MATERIALS SCIENCE↗

Defect Density Mapping of Shot Peened Materials Using Positron Annihilation Spectroscopy

Shot peening is a technique used in industry to increase the fatigue life of components by creating compressive residual stresses in the near surface region. This compressive stress is pinned in the material by defects such as dislocations and monovacancies to which positrons are sensitive. Using a {sup 22}Na source S-parameter measurements were made using positron annihilation spectroscopy (PAS) on both non-peened and peened copper coupons. These measurements show that a correlation exists between copper coupons shot peened at different intensities that in principal can be used for verification of shot intensity. Finally a relative defect density map was produced to show that the shot peening uniformity can also be measured across the surface of a large component.

36 MATERIALS SCIENCE↗

Improvement of Al/Steel Tungsten Inert Gas Welding–Brazing Joint by High-Energy Shot Peening

High-energy shot peening treatment was applied to improve the Al/steel tungsten inert gas welding–brazing lap joint. The mechanical properties and microstructure evolution of the joint were investigated. Results showed that the mechanical properties of weld were evidently reinforced due to microstructure transformation of joint surface layer. The grain structure in the joint surface layer was distorted and refined. Large compressive residual stress was introduced into the joint surface, and its hardness obviously increased due to strain hardening. When the peening pressure was 0.15 MPa, the tensile shear strength of the joint reached the maximum value (199.6 MPa), which was 16.5% higher than that of the as-welded joint.

36 MATERIALS SCIENCE↗

A Comparison of the Fatigue Life of Shot-Peened 4340M Steel with 100, 200, and 300% Coverage

Shot peening has been widely used for improving the fatigue performance of structural components. The objectives of this study are to increase the fatigue life of 4340M steel by shot peening and to compare performance at three different shot-peening coverages (100, 200, and 300%). The results show that the optimum coverage for 4340M steel is 200% in this experiment. Scanning electron microscopy (SEM) was used to evaluate the microstructural properties and estimate the depth and length of the resulting cracks. A proposed innovative technique, which still needs further verification, was applied to enable SEM to differentiate between the appearances of the three coverages. Residual stresses measured using x-ray diffraction showed that 200% coverage had comparatively the highest residual compressive stresses.

36 MATERIALS SCIENCE↗

Very High-Cycle Fatigue Properties and Residual Stress Relaxation of Micro-shot-Peened EA4T Axle Steel

In this paper, EA4T alloy railway axle steel was shot peened with steel balls and ceramic balls with a diameter of 50 μm, and 10{sup 9}-cycle fatigue tests of unpeened and peened specimens were carried out. The fatigue properties and the surface compression residual stress relaxation processes were investigated. The results of surface fracture observation indicated that all the cracks initiated from the surface, and both peened and unpeened specimens have conventional fatigue limits in the very high-cycle fatigue regime. Moreover, compared with unpeened (UP) specimens, the fatigue limits were improved by 31 and 28% for ceramic shot-peened (CSP) and steel shot-peened (SSP) specimens, respectively. The improvement of fatigue limit is related to the surface compressive residual stresses (SCRS) and the surface-hardened layer. The SCRS and full-width half-maximum (FWHM) values during the relaxation processes have been analyzed. At stress amplitudes lower than the cyclic yield strength, the residual stress of SSP specimens relaxed quickly in the first loading cycle and then remained stable, while the residual stress of CSP specimens relaxed quickly in the first loading cycle and relaxed slowly afterward, then remained stable. For all SSP and CSP specimens with applied stress amplitudes larger than the cyclic yield strength, the residual stress relaxed quickly in the initial cycles, and then remained stable after the first loading cycle.

36 MATERIALS SCIENCE↗

Effects of Fine Particle Shot Peening Treatment on Fatigue Properties of Al-7Si-0.3Mg Alloy

In this study, two different fine particle shot peening (FPSP) treatments were performed on Al-7Si-0.3Mg alloy specimens to evaluate their effects on fatigue properties. After the treatment, the microstructure morphology of the specimens was observed, and the surface roughness and residual stress distribution were measured. Rotating bending fatigue tests were conducted, and the fatigue fracture surfaces were observed using scanning electron microscopy (SEM). The crack initiation and propagation behavior were investigated using the replica method. The results indicate that FPSP can introduce residual stress on the surface layer of the material and refine the surface microstructure, and also change the surface roughness. At low stress amplitude levels, FPSP can improve fatigue life significantly. At 5 × 10{sup 7} cycles, the fatigue strength of shot-peened specimens increased by 33% compared to unpeened specimens. In unpeened and steel shot-peened (SSP) specimens, both crystal slip and casting defects can induce fatigue failure, while only casting defects can cause failure in the case of ceramic shot-peened (CSP) specimens. Moreover, FPSP can move the crack initiation site to the subsurface from the surface. The range of threshold stress intensity factor of the material can be improved significantly by this treatment. Casting defects have a significant influence on fatigue strength; the effect on fatigue strength can be well evaluated by the modified Murakami equation.

36 MATERIALS SCIENCE↗

Investigation of shot peening residual stress on alloy 718 leaf springs for primary water stress corrosion cracking analysis

This paper investigates the residual stress distributions from shot peening of Nickel Alloy 718 fuel assembly hold down spring material of PWR. Precision X-Ray Diffraction (XRD) testing has been performed to quantify residual stress versus depth on shot peened Nickel Alloy 718 samples that have been plastically deformed to different levels of stress. The results from these XRD tests have been used to benchmark a finite element model (FEM) that includes the effects of the residual compressive stress layer from shot peening. The benchmarked method of applying shot peening residual stresses can be applied to FEMs of Nickel Alloy 718 fuel assembly hold down springs to investigate the stress distributions in the springs at different loading conditions. XRD test results with a comparison to the benchmarked FEM are presented. (authors)

36 MATERIALS SCIENCE↗

EXPERIMENTAL-BASED DISCUSSION FOR THE SEPARATION OF RESIDUAL STRESSES AND COLD WORK IN SHOT PEENED IN718 USING HIGH FREQUENCY EDDY CURRENT SPECTROSCOPY

Typical aero engine alloys, such as IN718, can be surface-treated by shot peening to induce near-surface compressive strains. To calculate the remaining operation time for those critical aero engine components, a quantitative nondestructive determination of near-surface strain gradients has to be developed. We have demonstrated in the past, that it is possible to obtain a characteristic depth profile (surface and sub-surface) of the electrical conductivity of shot peened specimen by using high-frequency eddy current techniques. The measured conductivity profile is resulting from residual stresses, cold work, surface roughness, and the microstructure of the material. The objective is to measure residual stresses (separately from other material properties) in such components after a defined life time. It can be assumed, that surface roughness and microstructure remain unchanged in IN718 materials over their lifetime, but cold work and residual stresses can change independently. Consequently, there is a need to clearly separate the information from both material properties of received eddy current conductivity signals in order to obtain specific information related to residual stresses. This paper presents results acquired from different experiments, conducted to separate both effects by using the eddy current technique on shot peened IN718 materials. We present different physical approaches and illustrate the experiments to solve them. In addition, we will demonstrate that there is a need to use additional techniques, for example ultrasonic time-of-flight measurements, to separate the effects of residual stresses from compound (mixed) signals obtained on cold work samples.

36 MATERIALS SCIENCE↗

Residual Stress Asymmetry in Thin Sheets of Double-Sided Shot Peened Aluminum

The local mechanical properties and residual stresses of a double-sided shot-peened aluminum alloy AA7050-T7451 sheet were measured by nanoindentation and simulated by the finite element method (FEM). The variation of the pileup area around the indentation due to residual stresses, as well as changes in hardness as a function of cold working, was assessed. Numerical simulations were conducted to investigate the residual stress profile. When the indentation contact area was corrected to account for pileup induced from residual stresses, the hardness increased about 10% over the range of depths at which compressive residual stresses exist, indicating some strain hardening did occur. The maximum compressive residual stress for the second shot-peened surface is on the order of 10% higher than the first surface; this is ascribed to the sequencing during the peening process, in which the first side peening influenced the stress throughout the part thickness for these thin plate structures. The ability to couple FEM simulations and rapid experimental assessments of residual stresses and hardness allows for future prediction of part thickness effects in double-sided peening processes.

36 MATERIALS SCIENCE↗

The grain refinement mechanisms of various phases in shot-peened Nickel-Aluminum bronze (NAB) alloy

Highlights: • There exist two grain refinement mechanisms at the same time in the α phase. • The refinement of β' phase is attributed to the formation of dense and ordered nano twins. • The brittle strip-shape κ{sub iii} phases are fragmented after large deformation. • The κ{sub iv} and κ{sub ii} phases exhibit the twinning and dislocation deformation modes, separately. • The microhardness increases significantly owing to work hardening effect and grain refinement. - Abstract: In this study, coarse-grained Nickel-Aluminum bronze (NAB) alloy is subjected to shot-peening (SP) treatment, and the grain refinement mechanisms of various phases in shot-peened NAB alloy are investigated separately. The results show that severe deformation layers are produced on the surface. Meanwhile, refined grains with the average size below 100 nm are induced through SP treatment indicated by the results of X-ray diffraction (XRD) patterns. Various phases in NAB alloy including α, β' and three intermetallic phases (κ{sub ii}, κ{sub iii} and κ{sub iv}) display different grain refinement mechanisms. The grain refinement in the α phase involves dislocation segmentation in the precipitation-free zone and the twinning intersection in the precipitation zone. The formation of nanotwins by emitting partial dislocations at the grain boundary is found to be responsible for the grain refinement in the β' phase. As for the κ phases, the strip-shaped κ{sub iii} phases are fragmented after severe deformation, and the κ{sub iv} and κ{sub ii} phases exhibit the twinning and dislocation deformation modes, respectively. Also, the microhardness is significantly enhanced after SP treatment, which is mainly attributed to the work hardening effect and grain refinement.

36 MATERIALS SCIENCE↗

Laser Shot Peening System Final Report CRADA No. TC-1369-96

This CRADA project was established with a primary goal to develop a laser shot peening system which could operate at production throughput rates and produce the desired depth and intensity of induced shots. The first objective was to understand all parameters required for acceptable peening, including pulse energy, pulse temporal format, pulse spatial format, sample configuration and tamping mechanism. The next objective was to demonstrate the technique on representative samples and then on representative parts. The final objective was to implement the technology into a meaningful industrial peen.

36 MATERIALS SCIENCE↗

Laser Shot Peening Final Report CRADA No. TC-02059-03

This was a collaborative effort between The Regents of the University of California, Lawrence Livermore National Laboratory (LLNL) and Metal Improvement Company, Inc. (MIC), to further develop the laser shot peening technology. This project had an emphasis on laser development and government and military applications including DOE’s natural gas and oil technology program (NGOTP), Yucca Mountain Project (YMP), F-22 Fighter, etc.

36 MATERIALS SCIENCE↗

Enhanced Fatigue Behavior in Quenched and Tempered High-Strength Steel by Means of Double Surface Treatments

The aim of this study is to maximize the fatigue life of a high-strength steel. For this purpose, two different kinds of double surface treatments were studied: shot peening plus vibratory finishing and shot peening plus grit blasting. First, a high-intensity peening treatment was applied, with the aim of inducing a deep region submitted to high compressive residual stresses, and a second surface treatment was followed, to reduce the roughness induced in the first treatment and mitigate the damage produced on the specimen surface. The use of such double treatments was demonstrated to be a good choice to achieve high surface hardening and deep compressive residual stress profiles and to minimize surface defects. The fatigue life of the steel was greatly enhanced following the application of both double surface treatments. A vibratory treatment applied for 24 h after the application of a previous shot peening treatment was able to increase the average fatigue life of the single shot-peened samples almost sevenfold, but a much greater fatigue enhancement was produced using grit blasting for only 60 s. Anyway, both second treatments are able to remove the damaged surface layer produced in the first high-intensity shot peening treatment. The obtained results also revealed that an appropriate combination of surface treatments (shot peening + secondary treatment) avoided the initiation of cracks at the surface of the specimens under cyclic bending loads. Instead, crack initiation took place beneath the compressive residual stress field, induced in alumina inclusions that acted as stress concentrators.

36 MATERIALS SCIENCE↗

Study of the scale formed on super 304H boiler tube steels after long-term steam oxidation at high temperatures

Highlights: • Steam oxidation tests were performed on the conventional and shot-peened Super304H boiler tube. • A continuous amorphous SiO{sub 2} layer separated the metal from the scale in shot-peened specimen. • The SiO{sub 2} layer enhanced the formation of dense Cr{sub 2}O{sub 3} and FeCr{sub 2}O{sub 4} layers. • The scale on shot-peened specimens is stable upon steam temperature and time increase. Steam oxidation of a Super 304H boiler tube was performed at steam temperatures of 650 °C and 700 °C for time durations up to 5000 h. The oxidation scale outcomes which formed on as-received untreated and shot-peened (SP) tubes were studied using X-ray diffraction (XRD), scanning electron microscopy (SEM), electron backscatter diffraction (EBSD), and transmission electron microscopy (TEM). γ-Grain nanocrystallization on the surface of the SP specimen generated an abundant fraction of grain boundary that guaranteed the formation of a continuous amorphous SiO{sub 2} layer at the metal-scale interface that enhanced the formation of dense Cr{sub 2}O{sub 3} and FeCr{sub 2}O{sub 4} in the scale. Scale breakaway along defects in the outer layer of the scale was accelerated by the steam temperature in the untreated specimens, whereas the scale that formed on the SP specimens appeared to be stable.

36 MATERIALS SCIENCE↗