At least 19 records

Investigating the Chemical Reactivity of Lithium Silicate Model SEI Layers

Silicon anodes suffer from an unstable solid electrolyte interphase (SEI) layer that contributes to undesirable capacity fade with cycling. A key part to addressing this unstable SEI formation is to examine how certain components of the SEI react with the electrolyte over time. One SEI component that has not been thoroughly studied in the context of the chemical reactivity against the electrolyte is lithiated silicate. Four model silicate thin films with increasing lithium content were deposited by radio frequency (RF) magnetron sputtering to study how the lithiation of the native oxide on a silicon anode affects the chemical stability of the anode surface. SiO2, Li2Si2O5, Li2SiO3, and Li3SiOx films were exposed to 1.2 M LiPF6 in the 3:7 wt% ethylene carbonate/ethyl methyl carbonate (EC/EMC) electrolyte for periods of time that are representative of the amount of time it takes to undergo cell formations. Soaked samples were rinsed, dried, and characterized by a combination of attenuated total reflectance-infrared spectroscopy (ATR-IR), focused ion beam-secondary electron microscopy (FIB-SEM), and X-ray photoelectron spectroscopy (XPS) depth profiling. It was found that the rate of the decrease in film thickness of the silicates exposed to the electrolyte over time increases as a function of the lithium content in the thin film. This reaction involves HF etching and LiPF6 salt degradation leading to silicate loss and fluorination throughout the bulk. Understanding this chemical instability is critical to determining the overall mechanism of SEI degradation over time.

ADVANCED PROPULSION SYSTEMS,ENERGY STORAGE↗

Robust Solid/Electrolyte Interphase (SEI) formation on Si Anodes Using Glyme-based Electrolytes

Silicon (Si) is the most naturally abundant element possessing 10-fold theoretical capacity than graphitebased anodes. The practicality of implementing Si anodes is, however limited by the unstable solidelectrolyte interphase (SEI) and anode fracturing during continuous lithiation/delithiation. We demonstrate that glyme-based electrolytes (GlyEls) assure a conformal SEI on Si and keep the Si ‘fracture-free’. Benchmarking against the optimal, commonly-used carbonate electrolyte with the fluoroethylene carbonate (FEC) additive, Si anode cycled in a GlyEl exhibits reduced early parasitic current (by 62.5%) and interfacial resistance (by 72.8%), while the cell capacity retention is promoted by >7% over a course of 110 cycles. The mechanistic investigation by X-ray photoelectron spectroscopy (XPS) and energy-dispersive X-ray spectroscopy (EDX) indicates GlyEl enriches Si SEI with elastic polyether but diminishes its carbonate species. Glyme-based electrolytes prove viable in stabilizing the SEI on silicon for future high energy density lithium-ion batteries.

Yang, Guang↗

A quantitative figure of merit for battery SEI films and their use as functional solid-state electrolytes

As a key passivation film that governs battery operation, the solid electrolyte interphase (SEI) has long been credited for enabling high-performance batteries or blamed for their eventual death. However, qualitative descriptions of the SEI often found in the literature (e.g., “conductive,” “passivating”) highlight our incomplete understanding of this layer, where even the most basic properties foundational to SEI function remain difficult to measure. Here, we quantify SEI conductivities and SEI transference numbers using a separator-free Cu|SEI|Li architecture that treats the SEI as a functional solid-state electrolyte (SSE). We find that while any SEI property alone (e.g., electronic conductivity) is weakly correlated (R 2 < 0.67) with battery performance (e.g., Coulombic efficiency), a strong correlation (R 2 > 0.99) can be achieved by defining the “SEI cT number” as a product between the SEI transference number (T) and the ratio of SEI conductivities (c). Analogous to the thermoelectric figure of merit (i.e., zT ), SEI cT quantitatively benchmarks the holistic impact of SEI properties on battery performance and underscores the pitfalls of citing such properties in isolation. Perhaps most strikingly, we demonstrate that Li metal deposition and stripping at room temperature is possible in our separator-free Cu|SEI|Li cell, confirming that the SEI can function precisely as an SSE. Together, these results enrich our understanding of the SEI, not just as a passivation layer but as a functional structure that can potentially have important implications for solid-state batteries.

Science & Technology - Other Topics↗

Liquid state properties of SEI components in dimethoxyethane

The solid-electrolyte interphase (SEI) layer is a critical constituent of battery technology, which incorporates the use of lithium metals. Since the formation of the SEI is difficult to avoid, the engineering and harnessing of the SEI are absolutely critical to advancing energy storage. One problem is that much fundamental information about SEI properties is lacking due to the difficulty in probing a chemically complex interfacial system. One such property that is currently unknown is the dissolution of the SEI. This process can have significant effects on the stability of the SEI, which is critical to battery performance but is difficult to probe experimentally. Here, we report the use of ab initio computational chemistry simulations to probe the solution state properties of SEI components LiF, Li 2 O, LiOH, and Li 2 CO 3 in order to study their dissolution and other solution-based characteristics. Ab initio molecular dynamics was used to study the solvation structures of the SEI with a combination of radial distribution functions, discrete solvation structure maps, and vibrational density of states, which allows for the determination of free energies. From the change in free energy of dissolution, we determined that LiOH is the most likely component to dissolve in the electrolyte followed by LiF, Li 2 CO 3 , and Li 2 O although none were favored thermodynamically. Furthermore, this indicates that dissolution is not probable, but Li 2 O would make the most stable SEI with regard to dissolution in the electrolyte.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

The Effect of the SEI Layer Mechanical Deformation on the Passivity of a Si Anode in Organic Carbonate Electrolytes

The solid electrolyte interphase (SEI) on a Si negative electrode in carbonate-based organic electrolytes shows intrinsically poor passivating behavior, giving rise to unsatisfactory calendar life of Li-ion batteries. Moreover, mechanical strains induced in the SEI due to large volume changes of Si during charge-discharge cycling could contribute to its mechanical instability and poor passivating behavior. This study elucidates the influence that static mechanical deformation of the SEI has on the rate of unwanted parasitic reactions at the Si/electrolyte interface as a function of electrode potential. Further, the experimental approach involves the utilization of Si thin-film electrodes on substrates with disparate elastic moduli, which either permit or suppress the SEI deformation in response to Si volume changes upon charging-discharging. We find that static mechanical stretching and deformation of the SEI results in an increased parasitic electrolyte reduction current on Si. Furthermore, attenuated total reflection and near-field Fourier-transform infrared nanospectroscopy reveal that the static mechanical stretching and deformation of the SEI fosters a selective transport of linear carbonate solvent through, and nanoconfinement within, the SEI. These, in turn, promote selective solvent reduction and continuous electrolyte decomposition on Si electrodes, reducing the calendar life of Si anode-based Li-ion batteries. Finally, possible correlations between the structure and chemical composition of the SEI layer and its mechanical and chemical resilience under prolonged mechanical deformation are discussed in detail.

25 ENERGY STORAGE↗

Electrolyte Role in SEI Evolution at Si in the Pre-lithiation Stage vs the Post-lithiation Stage

The formation and evolution of the dynamic solid electrolyte interphase (SEI) at the Si anode/electrolyte interface are yet to be completely understood to solve irreversible capacity loss and increase battery cycle life. Herein, the evolution of SEI and its dynamic properties at the Si anode/electrolyte interface are investigated in two electrolyte systems, a 1.2 M LiPF6 in EC: EMC 3:7 (wt%) electrolyte (referred to as Gen2) and a 1.2 M LiTFSI in EC: EMC 3:7 (wt%) electrolyte (referred to as LiTFSI). Two lithiation stages are studied: the pre-lithiation (pre-Li) SEI stage and the post-lithiation (post-Li) stage. Findings reveal at the pre-Li, SEI formation starts at an early potential and contributes to the greater mass gain in the Si/Gen2, and it is dominated by the formation of a non-uniform F- and P-rich layer in Si/Gen2, in contrast to a homogeneous F- and C-containing layer at the Si/LiTFSI interphase. The initially formed SEI in LiTFSI further benefits the charge transfer kinetics. At the post-Li stage, a more substantial SEI evolution is observed at Si/LiTFSI. This paper offers a foundational understanding of the SEI dynamic evolution with electrolyte dependence. Findings from this report offer important insights into solving the complex SEI stability issues on Si.

25 ENERGY STORAGE↗

Combined, time-resolved, in situ neutron reflectometry and X-ray diffraction analysis of dynamic SEI formation during electrochemical N 2 reduction

One means of improving performance for electrochemical ammonia production through the Li-mediated N 2 reduction reaction (Li-NRR) is by cycling the current driving the reaction between open-circuit conditions and periods of applied current density. Herein, we have investigated the dynamics of the electrode–electrolyte interface under Li-NRR conditions during current cycling using in situ time-resolved neutron reflectometry and grazing-incidence synchrotron X-ray diffraction. During cycling, measured neutron reflectivity curves indicated bilayer formation in which Li-containing species such as LiOH, Li 2 O, and small quantities of Li 3 N and metallic Li primarily appeared in a thin layer at the cathode surface, above which formed a much larger, porous, ‘solid–electrolyte interface’ (SEI) layer. Upon return to open-circuit conditions, Li-containing species quickly moved out of the thin layer, leaving a compact, stable layer of decomposition products underneath the SEI layer. This SEI layer concomitantly filled with electrolyte or dissolved, becoming indistinguishable from the electrolyte via contrast in scattering-length density (SLD). During the second current cycle, Li-containing species again preferentially deposited directly atop the cathode, with the thick SEI-like layer again appearing within a minute. This SEI layer exhibited a lower SLD more quickly than in the first cycle, which might suggest that Li-containing species become distributed within the porous SEI layer. Furthermore, these time-resolved observations of SEI and plated layers during current cycling suggest that benefits associated with return to open-circuit conditions between periods of applied current density may be related to the concomitant loss of Li-containing species from a thin layer at the cathode surface into a porous SEI layer that becomes filled with electrolyte or dissolves.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Deconvoluting Effects of Lithium Morphology and SEI Stability at Moderate Current Density Using Interface Engineering

Lithium (Li)-morphology and solid electrolyte interphase (SEI) are among the most significant performance regulators in Li-metal batteries (LMBs). While both Li-morphology and SEI composition play key roles in the cyclability of LMBs, less is understood about the individual contributions of each factor to overall Li reversibility, particularly at a practical current density (1 mA cm −2 ) at which the kinetics of both factors are not naturally separated. Herein, an interface engineering approach is introduced to deconvolute the impacts of Li-morphology and SEI composition on battery performance. By using interfacial nanofilms with differing resistivity (resistive HfO 2 versus conductive ZnO), the morphology of Li is varied, and by virtue of similar acidic character of the nanofilms, the formation of anion-rich SEIs is maintained. It is established that although the surface acidity of the thin films enables preformation of a more anion-rich SEI, it is not preserved after Li plating. It is further shown that resistance-controlled, low-surface-area Li-morphology exhibits up to threefold increase in stable cycle life when tested in multiple electrolytes. Overall, these findings explain why Li-morphological control is more advantageous for performance improvement than preformed SEI modulation due to the inherent challenges in SEI preservation.

36 MATERIALS SCIENCE↗

Achieving SEI preformed graphite in flow cell to mitigate initial lithium loss

The irreversible lithium loss due to the formation of solid electrolyte interphase (SEI) in the initial cycle on the graphite anode greatly reduces the overall cell energy density of lithium ion batteries, that is, the lost Li ions from forming SEI lead to the decrease of Li ions for the intercalation. The method of cathode prelithiation has been widely explored to compensate this lithium loss. However, these cathode additives with high lithium contents inevitably lower the loading of the cathode active materials. In this work, we report a novel approach to solve this challenge, a facile graphite prelithiation method by preforming SEI layers on the surface of graphite powders (Pre-SEI graphite) utilizing a specially designed flow cell. The Li accommodation in the graphite anode can be controlled by the operating time and current density in the flow cell for the electrochemical SEI formation. As a result, we demonstrate a 10% initial Columbic efficiency increase of the LiFePO 4 electrode in a full cell configuration using the Pre-SEI graphite, compared with the pristine graphite anode. The electrochemical preformation of SEI on the graphite powders offers a complete solution to offset initial lithium loss without a sacrifice of active cathode material loading.

25 ENERGY STORAGE↗

Continuum-Level Modeling of Li-Ion Battery SEI by Upscaling Atomistically Informed Reaction Mechanisms

Understanding and controlling solid-electrolyte interphase (SEI) formation to stabilize cell performance is a significant challenge for next-generation Li-ion battery technologies. In recent years, computational modeling has become an essential tool in providing fundamental insights into SEI properties and dynamics. However, neither atomistic nor continuum-level approaches alone can capture the complexities of SEI chemistry across all relevant length and time scales. In this work, a continuum-level model is developed that is informed by reaction mechanisms obtained from first-principle calculations. The atomistically informed continuum-level model is used to understand electrolyte degradation, including the decomposition of ethylene carbonate (EC), ethyl methyl carbonate (EMC), and fluoroethylene carbonate (FEC). The model presented here is the most chemically complex continuum-level SEI model in the literature to date. The SEI model is calibrated against experimental irreversible leakage currents and shows qualitative agreement with expected SEI growth trends. The model framework is expected to accelerate fundamental understanding of SEI formation, facilitate mechanism development feedback, and dynamically interact with experimental insights.

continuum-level model↗

Revealing the effect of LiOH on forming a SEI using a Co magnetic “probe”

The solid-electrolyte-interphase (SEI) plays a critical role in lithium-ion batteries (LIBs) because of its important influence on electrochemical performance, such as cycle stability, coulombic efficiency, etc. Although LiOH has been recognized as a key component of the SEI, its influence on the SEI and electrochemical performance has not been well clarified due to the difficulty in precisely controlling the LiOH content and characterize the detailed interface reactions. Here, a gradual change of LiOH content is realized by different reduction schemes among Co(OH) 2 , CoOOH and CoO. With reduced Co nanoparticles as magnetic “probes”, SEI characterization is achieved by operando magnetometry. By combining comprehensive characterization and theoretical calculations, it is verified that LiOH leads to a composition transformation from lithium ethylene di-carbonate (LEDC) to lithium ethylene mono-carbonate (LEMC) in the SEI and ultimately results in capacity decay. This work unfolds the detailed SEI reaction scenario involving LiOH, provides new insights into the influence of SEI composition, and has value for the co-development between the electrode materials and electrolyte.

25 ENERGY STORAGE↗

The Importance of a Moving Boundary Approach for Modeling the SEI Layer Growth to Predict Capacity Fade

One of the contributing factors to the aging of lithium-ion batteries is the growth of the solid-electrolyte interphase (SEI) layer. The growth of the SEI layer leads to the irreversible loss of lithium available for cycling and increases the resistance of the battery. Physics-based models in literature model the kinetically limited or solvent diffusion-limited growth. In such models, the interface resistance is a constant, and the contribution to the overpotential of the intercalation reaction from the SEI layer is considered to be ohmic. In this study, we propose a model that describes the growth of the SEI layer on the electrode surface as a moving interface. The transport of lithium ions and the solvent in the electrolyte are affected by this moving interface. The equations that govern the species transport and the potential drop across the SEI layer are derived from dilute solution theory and solved by transforming the coordinates of the moving boundary. The ion transport induces changes in the conductivity across the SEI layer, which affects the potential drop that arises due to its growth. The effects of this potential on capacity fade are studied over cycling the battery.

25 ENERGY STORAGE↗

Insight into SEI Growth in Li-Ion Batteries using Molecular Dynamics and Accelerated Chemical Reactions

The performance of lithium-ion batteries (LIB) using organic electrolytes strongly depends on the formation of a stable solid electrolyte interphase (SEI) film. Elucidating the dynamic evolution and spatial composition of the SEI can be very useful to study the stability of SEI components and help optimize the formation cycles of LIB. We propose a classical molecular dynamics simulation protocol for predicting the first stages of SEI formation using a reaction method involving the decomposition of EC and LiPF 6 molecules in the electrolyte. We accelerate the formation of SEI components near the anode surface by increasing the probability of reactions, implemented through a geometry matching scheme, followed by a force-field reconfiguration. We observe the formation of gases (C 2 H 4 ), inorganic (Li 2 CO 3 and LiF) and organic (LEDC) components. Finally, this protocol shows promise to be able to evaluate the effects of varying electrolyte compositions and additives on SEI layer structure and composition.

25 ENERGY STORAGE↗

SEI Formation and Lithium-Ion Electrodeposition Dynamics in Lithium Metal Batteries via First-Principles Kinetic Monte Carlo Modeling

The stabilization and enhanced performance of lithium metal batteries (LMBs) depend on the formation and evolution of the Solid Electrolyte Interphase (SEI) layer as a critical component for regulating the Li metal electrodeposition processes. This study employs a first-principles kinetic Monte Carlo (kMC) model to simulate the SEI formation and Li + electrodeposition processes on a lithium metal anode, integrating both the electrochemical electrolyte reduction reactions and the diffusion events giving place to the SEI aggregation processes during battery charge and discharge processes. The model replicates the competitive interactions between organic and inorganic SEI components, emphasizing the influence of the cycling regime. Results indicate that grain boundaries within the SEI facilitate faster lithium-ion transport compared to crystalline regions, crucial for improving the performance and stability of LMBs. The findings underscore the importance of dynamic SEI modeling for further development of next-generation high-energy-density batteries.

25 ENERGY STORAGE↗

The Chemistry, Formation and Passivation of Solid-Electrolyte Interphase (SEI) from FSI- Breakdown at Li-metal Potential

LiFSI-based liquid electrolytes are promising for realizing high Coulombic efficiency (CE) and long cycle life of next-generation high-energy Li metal battery. Nevertheless, the fundamentals of both the chemistry and formation of solid-electrolyte interphase (SEI) in these electrolytes have remained elusive. Herein, we extensively combine electrochemistry and X-ray photoelectron spectroscopy (XPS) to illustrate the reaction pathways of electrolyte decomposition, especially FSI- breakdown, as well as the dissolution trend of various inorganic SEI components. The SEI-forming reactions at Cu/electrolyte interface manifest a potential (E) dependence, driven by direct electron-transfer (ET) and Li underpotential-deposition (Li UPD) at high and low E regions, respectively. By closely correlating the XPS data obtained with and without solvent washing, we demonstrate that not all the products derived from SEI reactions are incorporated into forming a passivating surface layer, with a notable portion dissolving into liquid electrolyte instead. Importantly, high-CE electrolyte dictated by the chemical identity of solvent, is found to exhibit minimized interfacial reactivity of SEI formation enabling more effective interphasial passivation, via preferential integration of passivating ingredients such as LiF. Overall, this work formulates a systematic understating of bridging the SEI chemistry, formation and passivation while identifying key characteristics of high-performance electrolyte for guiding future design.

Bao, Zhenan [SLAC National Accelerator Laboratory ↗

A new mechanism of stabilizing SEI of Si anode driven by crosstalk behavior and its potential for developing high performance Si-based batteries

Stabilizing solid electrolyte interphase (SEI) is a key factor for determining cell performance of Silicon (Si) anode, such as safety, cycle lifetime, and calendar lifetime. Here, we found a new potential for stabilizing SEI of the Si anode, driven by crosstalk with cathode material. Here we investigated the effect of crosstalk on the chemistry of SEI of the Si anode as a function of three different, representative cathode materials: LiNi 0.5 Mn 0.3 Co 0.2 O 2 (NMC532), LiNi 0.8 Mn 0.1 Co 0.1 O 2 (NMC811), and LiFePO 4 (LFP). Specifically, we observed that crosstalk significantly affected the formation and growth mechanism of SEI layer on the Si anodes. Unexpectedly, dissolved Fe ions from the LFP cathode has a positive impact on the chemistry and electrochemical stability of the SEI layer of Si anode compared to the other cathodes, resulting in better electrochemical performance in terms of initial coulombic efficiency and capacity fade.

25 ENERGY STORAGE↗

Capacity and Coulombic Efficiency Measurements Underestimate the Rate of SEI Growth in Silicon Anodes

Capacity measurements and related quantities are the first layer of information acquired during testing of Li-ion cells. It is generally considered that elevated values of coulombic efficiency and capacity retention are absolute indicators of the existence of a stable solid electrolyte interphase (SEI). Here, we challenge this notion by analyzing how the effect of side reactions on cell capacity depends on the choice of electrodes. More specifically, we demonstrate that the extent of measurable capacity fade due to SEI growth is modulated by the shape of the voltage profile of the cathode and anode at the end of charge and discharge half-cycles. This shape-dependency creates a mismatch between SEI growth and cell capacity loss, which is relatively small for graphite anodes but sizable for silicon-containing electrodes. We illustrate this point by showing that, at the same coulombic efficiency and capacity retention, cells containing silicon-based materials could actually exhibit rates of SEI growth that are as much as ≥ 40% higher than graphite cells. The main implication of this behavior is that, for certain systems, capacity measurements may be an unreliable source of information about the extent of reactions at the SEI, allowing other consequences of these side reactions (such as electrolyte depletion) to proceed unchecked while the cell appears to be stable.