Engineering PapersSearch

SEARCH · Engineering Papers

Results for “Preferred growth direction”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 19 records

Which way does the dendrite grow? Competition among epitaxy, preferred growth direction, and thermal gradients in powder bed fusion additive manufacturing

The as-processed microstructure of metal alloy parts manufactured through laser powder bed fusion (LPBF) is heavily derived from the cellular dendritic solidification. The growth direction of dendrites within the melt pool is determined through competition among epitaxial growth, preferred growth directions, and maximum thermal gradients. However, the dominant factor and the specific role of each in developing melt pool microstructures remain unknown. Here, in this study, we performed single laser track scans on an SS316L single crystal substrate and combined experimental characterization of microstructure and crystal orientations with Computational Fluid Dynamics simulations of thermal gradients to evaluate the role of each factor in determining dendritic growth direction and evolution. Our results reveal that epitaxial growth dominates microstructure development by preferentially growing along a single 〈100〉 variant of the single crystal substrate adjacent to the melt pool boundary. Under LPBF’s highly curved and rapidly evolving thermal field, this preferential dendrite variant selection and its continued growth from the melt pool boundary to the centerline are governed by the local temperature gradient magnitude at the solid-liquid interface, rather than by the instantaneous maximum temperature gradient direction alone. Using these findings, we successfully predict changes in the dendrite growth direction with changing laser scan direction on a single crystal substrate, and show that the geometric melt pool centerline can deviate from the microstructural centerline because asymmetric local temperature gradient magnitudes transiently limit growth, resulting in different dendrite travel distances on each side of the melt pool.

36 MATERIALS SCIENCE

Contactless Growth of ZnSe Single Crystals by Physical Vapor Transport

ZnSe crystals were grown by self-seeded physical vapor transport (PVT) technique in the horizontal configuration. The source materials were heat treated by H2 reduction to remove the oxide followed by baking under dynamic vacuum to adjust the source composition toward that of congruent sublimation. Contactless growth of ZnSe single crystals have been performed consistently using three different source materials. The crystals grew away from the wall during the later stage of the growth with large (110) facets tend to align parallel to the gravity direction. The Scanning Electron Micrography (SEM) micrographs and the Atomic Force Microscope (AFM) images showed that large (110) terraces and steps dominate the as-grown facets. The measured residual gas pressures in the processed ampoules agree well among various source materials and the major components were CO and H2. No preferred growth direction was found. The one-dimensional diffusion model on the mass flux of a multi-species PVT system was employed to analyze the conditions for contactless growth. The calculated thermal profile for supersaturation is very close to the thermal profile measured inside the empty furnace bore in the region of contactless growth. The effects of convective flows in the vapor phase inside the ampoule on the growth processes are discussed.

Su, Ching-Hua

Phase-field model of freeze casting

Directional solidification of water-based solutions has emerged as a versatile technique for templating hierarchical porous materials. However, the underlying mechanisms of pattern formation remain incompletely understood. In this work, we present a detailed derivation and analysis of a quantitative phase-field model for simulating this nonequilibrium process. The phase-field model extends the thin-interface formulation of dilute binary alloy solidification with antitrapping to incorporate the highly anisotropic energetic and kinetic properties of the partially faceted ice-water interface. This interface is faceted in the basal plane normal to the ⟨0001⟩ directions and atomically rough in other directions within the basal plane. On the basal plane, the model reproduces a linear or nonlinear relationship between the interface growth rate and the kinetic undercooling that can be linked to experimental measurements. In both cases, spontaneous parity breaking of the solidification front is observed when the preferred growth direction is aligned with the temperature gradient. This phenomenon leads to the formation of partially faceted ice lamellae that drift laterally in one of the ⟨0001⟩ directions. Here, we demonstrate that the drifting velocity of the ice lamellae is controlled by the kinetics on the basal plane and converges as the thickness of the diffuse solid-liquid interface decreases. Furthermore, we examine the effect of the form of the kinetic anisotropy, which is chosen here such that the inverse of the kinetic coefficient varies linearly from a finite value in the ⟨0001⟩ directions to zero in all other directions within the basal plane, consistent with the assumption that the interface grows in local thermodynamic equilibrium in this plane. Our results indicate that the drifting velocity of ice lamellae is not affected by the slope of this linear relation, and the radius and undercooling at the tip of an ice lamella converge at relatively small slope values. Consequently, the phase-field simulations remain quantitative with computationally tractable choices of both the interface thickness and the slope assumed in the form of the kinetic anisotropy.

Materials science

Hot forming of silicon sheet, silicon sheet growth development for the large area silicon sheet task of the low cost silicon solar array project

The hot workability of polycrystalline silicon was studied. Uniaxail stress-strain curves are given for strain rates in the range of .0001 to .1/sec and temperatures from 1100 to 1380 C. At the highest strain rates at 1380 C axial strains in excess of 20% were easily obtainable without cracking. After deformations of 36%, recrystallization was completed within 0.1 hr at 1380 C. When the recrystallization was complete, there was still a small volume fraction of unrecyrstallized material which appeared very stable and may degrade the electronic properties of the bulk materials. Texture measurements showed that the as-produced vapor deposited polycrystalline rods have a 110 fiber texture with the 110 direction parallel to the growth direction and no preferred orientation about this axis. Upon axial compression perpendicular to the growth direction, the former 110 fiber axis changed to 111 and the compression axis became 110 . Recrystallization changed the texture to 110 along the former fiber axis and to 100 along the compression axis.

Graham, C. D., Jr.

Parametric Experimental Study of the Formation of Glaze Ice Shapes on Swept Wings

An experiment was conducted to study the effect of velocity and sweep angle on the critical distance in ice accretion formation on swept wings at glaze ice conditions. The critical distance is defined as the distance from the attachment line to the beginning of the zone where roughness elements develop into glaze ice feathers. Icing runs were performed on a NACA 00 1 2 swept wing tip at velocities of 75, 100, 150, and 200 miles per hour. At each velocity and tunnel condition, the sweep angle was changed from 0 deg to 45 deg at 5 deg increments. Casting data, ice shape tracings, and close-up photographic data were obtained. The results showed that at given velocity and tunnel conditions, as the sweep angle is increased from 0 deg to 25 deg the critical distance slowly decreases. As the sweep angle is increased past 25 deg, the critical distance starts decreasing more rapidly. For 75 and 100 mph it reaches a value of 0 millimeters at 35 deg. For 150 and 200 mph it reaches a value of 0 millimeters at 40 deg. On the ice accretion, as the sweep angle is increased from 0 deg to 25 deg, the extent of the attachment line zone slowly decreases. In the glaze ice feathers zone, the angle that the preferred direction of growth of the feathers makes with respect to the attachment line direction increases. But overall, the ice accretions remain similar to the 0 deg sweep angle case. As the sweep angle is increased above 25 deg, the extent of the attachment line zone decreases rapidly and complete scallops form at 35 deg sweep angle for 75 and 100 mph, and at 40 deg for 150 and 200 mph.

Vargas, Mario

Method for the growth of large low-defect single crystals

A method and the benefits resulting from the product thereof are disclosed for the growth of large, low-defect single-crystals of tetrahedrally-bonded crystal materials. The process utilizes a uniquely designed crystal shape whereby the direction of rapid growth is parallel to a preferred crystal direction. By establishing several regions of growth, a large single crystal that is largely defect-free can be grown at high growth rates. This process is particularly suitable for producing products for wide-bandgap semiconductors, such as SiC, GaN, AlN, and diamond. Large low-defect single crystals of these semiconductors enable greatly enhanced performance and reliability for applications involving high power, high voltage, and/or high temperature operating conditions.

Powell, J. Anthony

Pulsed Laser Deposition of High Temperature Protonic Films

Pulsed laser deposition has been used to fabricate nanostructured BaCe(0.85)Y(0.15)O3- sigma) films. Protonic conduction of fabricated BaCe(0.85)Y(0.15)O(3-sigma) films was compared to sintered BaCe(0.85)Y(0.15)O(3-sigma). Sintered samples and laser targets were prepared by sintering BaCe(0.85)Y(0.15)O(3-sigma) powders derived by solid state synthesis. Films 1 to 8 micron thick were deposited by KrF excimer laser on porous Al2O3 substrates. Thin films were fabricated at deposition temperatures of 700 to 950 C at O2 pressures up to 200 mTorr using laser pulse energies of 0.45 - 0.95 J. Fabricated films were characterized by X-ray diffraction, electron microscopy and electrical impedance spectroscopy. Single phase BaCe(0.85)Y(0.15)O(3-sigma) films with a columnar growth morphology are observed with preferred crystal growth along the [100] or [001] direction. Results indicate [100] growth dependence upon laser pulse energy. Electrical conductivity of bulk samples produced by solid state sintering and thin film samples were measured over a temperature range of 100 C to 900 C. Electrical conduction behavior was dependent upon film deposition temperature. Maximum conductivity occurs at deposition temperature of 900 oC; the electrical conductivity exceeds the sintered specimen. All other deposited films exhibit a lower electrical conductivity than the sintered specimen. Activation energy for electrical conduction showed dependence upon deposition temperature, it varied

Dynys, Fred W.

The influence of acceleration forces on nucleation, solidification, and deformation processes in tin single crystals

An apparatus was designed and assembled to directionally solidify single crystals under the influence of acceleration forces of various magnitudes. The investigation conducted showed that acceleration gradients produce a preferred growth orientation effect not previously observed for tin. Convection currents at approximately 5-g encourage multiple nucleation and subsequent random orientation of growth direction. Deformation effects such as recrystallization and twinning are observed at acceleration levels greater than 2-g.

Johnston, M. H.

Tailoring-Orientated Deposition of Li 2 S for Extreme Fast-Charging Lithium–Sulfur Batteries

Precipitation/dissolution of insulating Li 2 S has long been recognized as the rate-determining step in lithium-sulfur (Li-S) batteries, which dramatically undermines sulfur utilization at elevated charging rates. Herein, we present an orientated Li 2 S deposition strategy to achieve extreme fast charging (XFC, ≤15 min) through synergistic control of porosity, electronic conductivity, and anchoring sites of electrode substrate. Via magnesiothermic reduction of a zeolitic imidazolate framework, a nitrogen-doped and hierarchical porous carbon with highly graphitic phase was developed. This design effectively reduces interfacial resistance and ensures efficient sequestration of polysulfides during deposition, leading to (110)-preferred growth of Li 2 S nanocrystalline between (002)-dominated graphitic layers. Our approach directs an alternative Li 2 S deposition pathway to the commonly reported lateral growth and 3D thickening growth mode, ameliorating the electrode passivation. Therefore, a Li-S cell capable of charging/discharging at 5C (12 min) while maintaining excellent cycling stability (82% capacity retention) for 1000 cycles is demonstrated. In conclusion, even under high S loading (8.3 mg cm -2 ) and low electrolyte/sulfur ratio (3.8 mL mg -1 ), the sulfur cathode still delivers a high areal capacity of >7 mAh cm -2 for 80 cycles.

25 ENERGY STORAGE

Temperature Dependent Early-Stage Oxidation Dynamics of Cu(100) Film with Faceted Holes

Fundamental understanding of surface oxidation dynamics is critical for rational corrosion protection and advanced manufacturing of nanostructured oxides. In situ environmental TEM (ETEM) provides high spatial (nano- to atomic- scale) and temporal (< 0.1 s) resolution to investigate the early-stage oxidation/corrosion dynamics of metals and alloys. Thin samples with facets are widely used to enable cross-sectional observation of the oxidation dynamics in ETEM. However, how different facet orientations oxidize under the same conditions, and how these facets change the oxidation process, has not been investigated before. Here, using in situ ETEM, we systematically compare the oxidation dynamics of Cu(001) thin films, with faceted holes exposing {100} and {110} facets at temperatures ranging from 250–600 °C under 0.03 Pa O 2 . Oxidation preference is observed to change, from Cu(110) facets at lower temperatures to Cu(100) facets at ~ 500 °C. Oxide growth mechanisms change from outward growth on Cu 2 O surfaces at low temperatures, to inward growth on Cu-Cu 2 O interfaces at high temperatures. At high temperatures (500–600 °C), a rod-like Cu 2 O morphology is observed, with side facets of ~ {024} and top facets of {100} on Cu(100). This differs from the square-shaped Cu 2 O exposing {110} facets formed on Cu(001) surfaces. Rod-like oxides exhibit directional growth along their lengths with linear growth rates, regardless of rod length and width. This suggests that O from Cu(001) surfaces, rather than Cu(100) facets, serves as an O source for oxide growth. These results show a direct comparison of oxidation at different orientations with temperature, underscoring the temperature dependence of oxidation preference. Our results also suggest future in situ ETEM experiments viewing oxidation corrosion cross-sectionally should be cautious when oxide size is comparable with sample thickness, as the oxidizing mechanism may change due to sample thickness.

36 MATERIALS SCIENCE

High temperature electric arc furnace and method

An apparatus and process for improving the microstructure of electrically conducting materials is disclosed by the present invention. A revolving heat source applies heat to the surface of the material evenly and quickly. One or more heat sinks quickly cool the material. In the preferred embodiment, the cooling may be done in such a way as to promote as high a degree of directional grain growth as desired or completely nondirectional grain growth.

Richard M Poorman

Microstructural, Chemical and Mechanical Characterization of Polymer-Derived Hi-Nicalon Fibers with Surface Coatings

Room temperature tensile strengths of as-received Hi-Nicalon fibers and those having BN/SiC, p-BN/SiC, and p-B(Si)N/SiC surface coatings, deposited by chemical vapor deposition, were measured using an average fiber diameter of 13.5 microns. The Weibull statistical parameters were determined for each fiber. The average tensile strength of uncoated Hi-Nicalon on was 3.19 +/- 0.73 GPa with a Weibull modulus of 5.41. Strength of fibers coated with BN/SiC did not change. However, coat with p-BN/SiC and p-B(Si)N/SiC surface layers showed strength loss of approx. 10 and 35 percent, respectively, compared with as-received fibers. The elemental compositions of the fibers and the coatings were analyzed using scanning Auger microprobe and energy dispersive x-ray spectroscopy. The BN coating was contaminated with a large concentration of carbon and some oxygen. In contrast, p-BN, p-B(Si)N, and SiC coatings did not show any contamination. Microstructural analyses of the fibers and the coatings were done by scanning electron microscopy (SEM), transmission electron microscopy (TEM), and selected area electron diffraction. Hi-Nicalon fiber consists of the P-SIC nanocrystals ranging in size from 1 to 30 nm embedded in an amorphous matrix. TEM analysis of the BN coating revealed four distinct layers with turbostatic structure. The p-BN layer was turbostratic and showed considerable preferred orientation. The p-B(Si)N was glassy and the silicon and boron were uniformly distributed. The silicon carbide coating was polycrystalline with a columnar structure along the growth direction. The p-B(Si)N/SiC coatings were more uniform, less defective and of better quality than the BN/SiC or the p-BN/SiC coatings.

Bansal, Narottam P.

Performance, defect behavior and carrier enhancement in low energy, proton irradiated p+nn+ InP solar cells

The highest AMO efficiency (19.1 percent) InP solar cell consisted of an n+pp+ structure epitaxially grown on a p+ InP substrate. However, the high cost and relative fragility of InP served as motivation for research efforts directed at heteroepitaxial growth of InP on more viable substrates. The highest AMO efficiency (13.7 percent) for this type of cell was achieved using a GaAs substrate. Considering only cost and fracture toughness, Si would be the preferred substrate. The fact that Si is a donor in InP introduces complexities which are necessary in order to avoid the formation of an efficiency limiting counterdiode. One method used to overcome this problem lies in employing an n+p+ tunnel junction in contact with the cell's p region. A simpler method consists of using an n+ substrate and processing the cell in the p+ nn+ configuration. This eliminates the need for a tunnel junction. Unfortunately, the p/n configuration has received relatively little attention the best cell with this geometry having achieved an efficiency of 17 percent. Irradiation of these homoepitaxial cells, with 1 Mev electrons, showed that they were slightly more radiation resistant than diffused junction n/p cells. Additional p/n InP cells have been processed by some activity aimed at diffusion. Currently, there has been some activity aimed at producing heteroepitaxial p+nn+ InP cells using n+ Ge substrates. Since, like Si, Ge is an n-dopant in InP, use of this configuration obviates the need for a tunnel junction. Obviously, before attempting to process heteroepitaxial cells, one must produce a reasonably good homoepitaxial cell. In the present case we focus our attention on homoepitaxially on an n+ Ge substrate.

Weinberg, I.

Root-growth behavior of the Arabidopsis mutant rgr1. Roles of gravitropism and circumnutation in the waving/coiling phenomenon

In this study we investigated the kinetics of the gravitropic response of the Arabidopsis mutant rgr1 (reduced root gravitropism). Although the rate of curvature in rgr1, which is allelic to axr4, was smaller than in the wild type (ecotype Wassilewskija), curvature was initiated in the same region of the root, the distal elongation zone. The time lag for the response was unaffected in the mutant; however, the gravitropic response of rgr1 contained a feature not found in the wild type: when roots growing along the surface of an agar plate were gravistimulated, there was often an upward curvature that initiated in the central elongation zone. Because this response was dependent on the tactile environment of the root, it most likely resulted from the superposition of the waving/coiling phenomenon onto the gravitropic response. We found that the frequency of the waving pattern and circumnutation, a cyclic endogenous pattern of root growth, was the same in rgr1 and in the wild type, so the waving/coiling phenomenon is likely governed by circumnutation patterns. The amplitudes of these oscillations may then be selectively amplified by tactile stimulation to provide a directional preference to the slanting.

NASA Discipline Plant Biology

Solidification rate influence on orientation and mechanical properties of MAR-M-246+Hf

The influence of solidification rates on the orientation and mechanical properties of MAR-M-246+Hf was studied. The preferred orientation was found to be (001) for single crystals, with all samples with 45 degrees of (001). Tensile tests were performed at room temperature. The anisotropy of directionally solidified MAR-M-246+Hf was demonstrated by gage section deformation. Dendrite arm spacing and crystal growth were found to depend on solidification rates and source material conditions. The greatest strength occurred at lower solidification rates. Some single crystals were grown by control of growth rates without seeding.

Hamilton, D.

Hydrogen ejection from hydrocarbons: Characterization and relevance in soot formation and interstellar chemistry

Polycyclic aromatic hydrocarbons (PAHs) play a major role in the chemistry of combustion, pyrolysis, and the interstellar medium. Production (or activation) of radical PAHs and propagation of their resulting reactions require efficient dehydrogenation, but the preferred method of hydrogen loss is not well understood. Unimolecular hydrogen ejection (i.e., direct C─H bond fission) and bimolecular radical abstraction are two main candidate pathways. We performed a computational study to characterize the role of H ejection, particularly as a driver for radical-centric hydrocarbon-growth mechanisms and particle formation. Electronic structure calculations establish that C─H bond strengths span a broad range of energies, which can be weaker than 30 kcal/mol in some C 9 and C 13 PAH radicals. At T > 1200 K, calculated thermal rates for hydrogen ejection from weak C─H bonds at zigzag sites on PAH radicals are significantly larger than typical H-abstraction rates. These results are highly relevant in the context of chain reactions of radical species and soot inception under fuel-rich combustion conditions. Furthermore, calculated microcanonical rates that include the additional internal energy released by bond formation (e.g., ring closure to yield C 9 H 9 ) yield significantly higher rates than those associated with full thermalization. These microcanonical considerations are relevant to the astrochemical processes associated with hydrocarbon growth and processing in the low-density interstellar environment.

08 HYDROGEN

Mirror instability and origin of morningside auroral structure

Auroral optical imagery shows marked differences between auroral features of the evening and morning sectors: the separation between diffuse and discrete auroras in the evening sector is not distinct in the morning sector, which is dominated by auroral patches and multiple banded structures aligned along some direction. Plasma distribution function signatures also show marked differences: downward electron beams and inverted-V signatures prefer the evening sector, while the electron spectra on the morning sector are similar to the diffuse aurora. A theory of morningside auroras consistent with these features was constructed. The theory is based on modulation of the growth rates of electron cyclotron waves by the mirror instability, which is in turn driven by inward-convected ions that have become anisotropic. This modulation produces alternating bands of enhanced and reduced electron precipitation which approximate the observed multiple auroral bands and patches of the morning sector.

Chiu, Y. T.

Mirror instability and the origin of morningside auroral structure

Auroral optical imagery shows marked differences between auroral features of the evening and morning sectors: The separation between diffuse and discrete auroras in the evening sector is not distinct in the morning sector, which is dominated by auroral patches and multiple banded structures aligned along some direction. Plasma distribution function signatures also show marked differences: downward electron beams and inverted-V signatures prefer the evening sector, while the electron spectra on the morning sector are similar to the diffuse aurora. We have constructed a theory of morningside auroras consistent with these features. The theory is based on modulation of the growth rates of electron cyclotron waves by the mirror instability, which is in turn driven by inward-convected ions that have become anisotropic. This modulation produces alternating bands of enhanced and reduced electron precipitation which approximate the observed multiple auroral bands and patches of the morning sector.

Chiu, Y. T.