Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “PbSe”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 19 records

Heavily Doped PBSE with High Thermoelectric Performance

The present invention discloses heavily doped PbSe with high thermoelectric performance. Thermoelectric property measurements disclosed herein indicated that PbSe is high zT material for mid-to-high temperature thermoelectric applications. At 850 K a peak zT (is) greater than 1.3 was observed when n(sub H) approximately 1.0 X 10(exp 20) cm(exp -3). The present invention also discloses that a number of strategies used to improve zT of PbTe, such as alloying with other elements, nanostructuring and band modification may also be used to further improve zT in PbSe.

Snyder, G. Jeffrey↗

Phase equilibria and liquid phase epitaxy growth of PbSnSeTe lattice matched to PbSe

The necessary phase diagram data for growing lattice-matched layers of PbSnSeTe on PbSe are presented. Solid compounds of Pb(1-x)Sn(x)Se(1-y)Te(y) lattice-matched to PbSe were grown from liquid melts consisting of (Pb/1-x/Sn/x/)(1-z)(Se/1-y/Te/y/)(z); phase equilibria data were determined together with liquidus data for values of x(liquid) from 0 to 40 percent and y(liquid) from 0 to 40 percent for temperatures between 450 and 540 C. It was found that relatively large amounts of Te must be added to the melt to achieve lattice matching because of its low segregation coefficient relative to Se. A significant lattice-pulling effect was discovered for the 5-percent Sn case, and a similar effect is expected for the 10- and 20-percent Sn cases.

Mccann, Patrick J.↗

N-type Doped PbTe and PbSe Alloys for Thermoelectric Applications

The present invention demonstrates that weak scattering of carriers leads to a high mobility and therefore helps achieve low electric resistivity with high Seebeck coefficient for a thermoelectric material. The inventors demonstrate this effect by obtaining a thermoelectric figure of merit, zT, higher than 1.3 at high temperatures in n-type PbSe, because of the weak scattering of carriers in the conduction band as compared with that in the valence band. The invention further demonstrates favorable thermoelectric transport properties of n-type PbTe.sub.1-xI.sub.x with carrier concentrations ranging from 5.8.times.10.sup.18-1.4.times.10.sup.20 cm.sup.-3.

Snyder, G. Jeffrey↗

Method of fabricating a PbS-PbSe IR detector array

A silicon wafer is provided which does not employ individually bonded leads between the IR sensitive elements and the input stages of multiplexers. The wafer is first coated with lead selenide in a first detector array area and is thereafter coated with lead sulfide within a second detector array area. The described steps result in the direct chemical deposition of lead selenide and lead sulfide upon the silicon wafer to eliminate individual wire bonding, bumping, flip chiping, planar interconnecting methods of connecting detector array elements to silicon chip circuitry, e.g., multiplexers, to enable easy fabrication of very long arrays. The electrode structure employed, produces an increase in the electrical field gradient between the electrodes for a given volume of detector material, relative to conventional electrode configurations.

Barrett, John R.↗

PbS-PbSe IR detector arrays

A silicon wafer is provided which does not employ individually bonded leads between the IR sensitive elements and the input stages of multiplexers. The wafer is first coated with lead selenide in a first detector array area and is thereafter coated with lead sulfide within a second detector array area. The described steps result in the direct chemical deposition of lead selenide and lead sulfide upon the silicon wafer to eliminate individual wire bonding, bumping, flip chipping, planar interconnecting methods of connecting detector array elements to silicon chip circuitry, e.g., multiplexers, to enable easy fabrication of very long arrays. The electrode structure employed, produces an increase in the electrical field gradient between the electrodes for a given volume of detector material, relative to conventional electrode configurations.

Barrett, John R.↗

Summary of in situ epitaxial nucleation and growth measurements

In situ nucleation and growth measurements of Ag and Au on single-crystal PbSe thin films were made using a transmission electron microscope. Properties studied were polymorphism, crystalline perfection, and the stoichiometric composition of the initial and the autoepitaxially thickened PbSe substrates. The quantitative nucleation and cluster growth measurements were limited to low-saturation conditions. The epitaxial orientations are discussed, and evidence is presented as to the stage of deposition at which the epitaxial order for Ag is introduced. Strong substrate/overgrowth interaction manifested itself by alloying and interdiffusion.

Poppa, H.↗

Infrared heterodyne spectroscopy of astronomical and laboratory sources at 8.5 micron

The first infrared heterodyne spectrometer using tuneable semiconductor (PbSe) diode lasers has been constructed and was used near 8.5 micron to measure absorption line profiles of N2O in the laboratory and black body emission from the Moon and from Mars. Spectral information was recorded over a 200 MHz bandwidth using an 8-channel filter bank. The resolution was 25 MHz and the minimum detectable (black body) power was 1 x 10 to the minus 16th power watts for 8 minutes of integration. The results demonstrate the usefulness of heterodyne spectroscopy for the study of remote and local sources in the infrared.

Mumma, M.↗

Heterodyne spectroscopy of astronomical and laboratory sources at 8.5 microns using diode laser local oscillators

The first 8.5 microns infrared heterodyne spectrometer has been constructed using tuneable semiconductor (PbSe) diode lasers and was used to measure absorption line profiles of N2O in the laboratory, as well as black-body emission from the moon and from Mars. Spectral information was recorded over a 200 MHz bandwidth using an 8-channel filter bank. The resolution was 25 MHz (6 millionths of a micron), and the minimum detectable (black-body) power was approximately 1 times 10 to the minus 16th power W for 8 min of integration. The results demonstrate the usefulness of heterodyne spectroscopy for the study of remote and local sources in the infrared.

Mumma, M.↗

Tunable diode-laser heterodyne spectrometer for remote observations near 8 microns

A diode-laser-based, ultrahigh resolution IR heterodyne spectrometer for laboratory and field use has been developed for operation between 7.5 and 8.5 microns. The local oscillator is a PbSe tunable diode laser kept continuously at operating temperatures of 12-60 K using a closed-cycle cooler. The laser output frequency is controlled and stabilized using a high-precision diode current supply, constant temperature controller, and a shock isolator mounted between the refrigerator cold tip and the diode mount. The system largely employs reflecting optics to minimize losses from internal reflection and absorption and to eliminate chromatic effects. Spectral analysis of the diode-laser output between 0 and 1 GHz reveals excess noise at many diode current settings, which limits the IR spectral regions over which useful heterodyne operation can be achieved. Observations have been made of atmospheric N2O, O3, and CH4 between 1170 and 1200/cm, using both a single-frequency swept IF channel and a 64-channel RF spectral line receiver with a total IF coverage of 1600 MHz.

Glenar, D.↗

Tunable diode laser heterodyne spectrometer for remote observations near 8 microns

Infrared heterodyne spectroscopy is a passive technique employing coherent optical detection for the study of spectral features in remote sources. It employs optical components such as mirrors and lenses normally associated with incoherent optics, but because of it's coherent nature, it offers the advantages of ultrahigh spectral resolving power, high frequency precision, and diffraction limited field-of-view. Attention is given to the development of an ultrahigh resolution diode laser heterodyne spectrometer for observational and laboratory use. The instrument is designed for operation in the spectral range from 7.5 to 8.5 microns. A PbSe tuneable diode laser (TDL) is employed as local oscillator. A closed-cycle cooler is employed to keep the oscillator at operating temperatures in the range from 12 to 60 K. Attention is given to factors determining the TDL heterodyne sensitivity, the spectrometer design, and a survey of 8 micron observations, SiO could be detected in the sunspot spectrum.

Glenar, D. A.↗

Monolithic lead salt-silicon focal plane development

This paper is a summary of work done in the development of monolithic lead salt-silicon infrared focal plane technology. The photoconductive detector materials, PbS and PbSe are chemically deposited onto premetallized silicon MOSFET integrated circuit wafers. A variety of structures based on an implanted PMOS process were fabricated and evaluated. Operational results of an eight-element PbS array multiplexed on-chip are presented along with radiometric measurements on other integrated PbS-silicon MOSFET structures. PbS imagery is shown using one element of a 20-element array integrated on-chip.

Barrett, J. R.↗

Uniform Etching For Polycrystalline Photoconductor Films

Prewetting surface overcomes problem of nonuniformity of etching often occuring in polycrystalline films at PbS and PbSe. Believed prewetting causes etchant to attack film uniformly. Because process involves wet chemistry, inexpensive and easy to use.

Barrett, John↗

Time resolved spectra in the infrared absorption and emission from shock heated hydrocarbons

The wavelength range of a previously constructed multichannel fast recording spectrometer was extended to the mid-infrared. With the initial configuration, light intensities were recorded simultaneously with a silicon-diode array simultaneously at 20 adjacent wavelengths, each with a 20-micron time resolution. For studies in the infrared, the silicon diodes were replaced by a 20-element PbSe array of similar dimensions, cooled by a three-stage thermoelectric device. It is proposed that infrared emissions could be due to shock-heated low molecular-weight hydrocarbons. The full Swan band system appeared in time-integrated emission spectra from shock-heated C2H2; no soot was generated. At low resolution, the profiles on the high-frequency side of the black body maximum show no distinctive features. These could be fitted to Planck curves, with temperatures that declined with time from an initial high that was intermediate between T5 (no conversion) and T5(eq).

Bauer, S. H.↗

The Origin and Time Dependence of the Amount and Composition of Non-Constituent Gases Present in Crystal Growth Systems

Presence of different, non-constituent gases may be a critical factor in crystal growth systems. In Physical Vapor Transport processes the cras(es) can be used intentionally (to prevent excessively high, unstable growth conditions), or can evolve unintentionally during the course of the process (which may lead to undesired reduction in the -rowth rate). In melt growth, particularly under low gravity conditions (reduced hydrostatic pressure) the gas present in the system may contribute to formation of voids in the growing crystals and even to a separation of the crystal and the liquid phase [1]. On the other hand, some amount of gas may facilitate 'contactless' crystal growth particularly under reduced gravity conditions [2 - 6]. Different non-constituent gases may be present in growth ampoules, and their amount and composition may change during the crystallization process. Some gases can appear even in empty ampoules sealed originally under high vacuum: they may diffuse in from the outside, and/or desorb from the ampoule walls. Residual gases can also be generated by the source materials: even very high purity commercial elements and compounds may contain trace amounts of impurities, particularly oxides. The oxides may have low volatilities themselves but their reaction with other species, particularly carbon and hydrogen, may produce volatile compounds like water or carbon oxides. The non-constituent gases, either added initially to the system or evolved during the material processing, may diffuse out of the ampoule during the course of the experiment. Gases present outside (e.g. as a protective atmosphere or thermal conductor) may diffuse into the ampoule. In either case the growth conditions and the quality of the crystals may be affected. The problem is of a particular importance in sealed systems where the amount of the gases cannot be directly controlled. Therefore a reasonable knowledge and understanding of the origin, composition, magnitude, and change with time of gases present in sealed ampoules may be important for a meaningful control and interpretation of crystal growth processes. This problem is of a particular importance for processing of electronic materials in space because (i) safety considerations require using sealed systems only, and (ii) high cost of crystal growth experiments in microgravity calls for a throughout, accurate description of the processing conditions necessary for a meaningful, efficient, and conclusive interpretation of the space results. In this paper we present the results of our extensive studies on gases in closed crystal growth systems which include: (a) Degassing properties of fused silica; (b) Generation of inert gases by source materials (CdTe, ZnTe, CdZnTe, ZnSe, PbTe, PbSe, PbSeTe); (c) Diffusive cas losses from silica glass ampoules.

Palosz, Witold↗

Thermochemical Model and Experimental Studies on Physical Vapor Transport of Lead Telluride-Selenide

Mass transport rate and composition of the transported material as a function of different process parameters like temperature, undercooling, inert gas pressure, and the source compactness for different PbTe(1-x)Se(x), compositions were studied. With a proper preparation procedures mass transport rates suitable for growth at the rate of 0.5 - 1 mm/h were obtained. Different composition non-uniformities in the deposited material were observed. Due to deviation of the PbTe-PbSe solid solution from ideality, congruent mass transport of the material takes place around X = 0.3. For other compositions an improved and even good uniformity can be achieved when a solid, premelted source material is used.

Palosz, W.↗

Nanoengineered Materials for SWIR HOT Detectors

Heavy metal Selenide has been investigated for more than half century for high operating temperature (HOT) mid wave infrared (MWIR) applications. Most of the efforts have been devoted to make detector arrays on high-resistivity Si substrates for operating wavelengths in the 1.5 to 5.0 m region using physical vapor transport grown poly crystalline materials. For most of the biological spectral and imaging applications, short wave infrared (SWIR) detectors have shown better performance. Recent growth materials have shown variation in morphology with slight change in growth conditions and hence variation in performance parameters such as bandgap, mobility and resistivity from sample to sample. We have performed growth and optical characterization of pure and doped PbS and PbSe and have determined bandgap using available theoretical models for different morphologies.

Singh, N. B.↗

Design of Materials for IR Detectors Using High Z Elements for High Energy Radiation Environment

There is a strong need for rad hard and high operating temperature IR detectors for space environment. Heavy metal Selenides (high Z and large density) have been investigated for more than half century for high operating temperature mid wave infrared (MWIR) applications. Most of the efforts have been devoted to make detector arrays on high-resistivity Si substrates for operating wavelengths in the 1.5 to 5.0 m region using physical vapor transport grown poly crystalline materials. For most of the biological spectral and imaging applications, short wave infrared (SWIR) detectors have shown better performance. Recent growth materials have shown variation in morphology with slight change in growth conditions and hence variation in performance parameters such as bandgap, mobility and resistivity from sample to sample. We have performed growth and optical characterization of binary materials CdSe-PbSe to determine the suitability for IR detector. We have determined bandgap using several theoretical models for different morphologies observed during growth on silicon wafers.

Saraf, Sonali↗