Macrosegregation and nucleation in undercooled Pb-Sn alloys

A technique resulting in large undercoolings in bulk samples (23g) of lead-tin alloys was developed. Samples of Pb-12.5 wt percent Sn, Pb-61 wt percent Sn, and Pb-77 wt percent Sn were processed with undercoolings ranging from 4 to 34 K and with cooling rates varying between 0.04 and 4 K/sec. The nucleation behavior of the Pb-Sn system was found to be nonreciprocal. The solid Sn phase effectively nucleated the Pb phase of the eutectic; however, large undercoolings developed in Sn-rich eutectic liquid in the presence of the solid Pb phase. This phenomenon is believed to be mainly the result of differences in interfacial energies between solid Sn-eutectic liquid, and solid Pb-eutectic liquid rather than lattice misfit between Pb and Sn. Large amounts of segregation developed in the highly undercooled eutectic ingots. This macrosegregation was found to increase as undercooling increases. Macrosegregation in these undercooled eutectic alloys was found to be primarily due to a sink/float mechanism and the nucleation behavior of the alloy. Lead-rich dendrites are the primary phase in the undercooled eutectic system. These dendrites grow rapidly into the undercooled bath and soon break apart due to recalescence and Sn enrichment of the liquid. These fragmented Pb dendrites are then free to settle to the bottom portion of the ingot causing the macrosegregation observed in this study. A eutectic Pb-Sn alloy undercooled 20 K and cooled at 4 K/sec had a composition of about Pb-72 wt percent Sn at the top and 55 percent Sn at the bottom.

Degroh, Henry C., III↗

Macrosegregation and nucleation in undercooled Pb-Sn alloys

A novel technique resulting in large undercoolings in bulk samples (23 g) of lead-tin alloys was developed. Samples of Pb-12.5 wt percent Sn, Pb-61.9 wt.% Sn, and Pb-77 wt.% Sn were processed with undercoolings ranging from 4 to 34 K and with cooling rates varying between 0.04 and 4 K/s. The nucleation behavior of the Pb-Sn system was found to be nonreciprocal. The solid Sn phase effectively nucleated the Pb phase of the eutectic; however, large undercoolings developed in Sn-rich eutectic liquid in the presence of the solid Pb phase. This phenomenon is believed to be mainly the result of differences in interfacial energies between solid Sn-eutectic liquid, and solid Pb-eutectic liquid rather than lattice misfit between Pb and Sn. Large amounts of segregation developed in the highly undercooled eutectic ingots. This macrosegregation was found to increase as undercooling increases. Macrosegregation in these undercooled eutectic alloys was found to be primarily due to a sink/float mechanism and the nucleation behavior of the alloy. Lead-rich dendrites are the primary phase in the undercooled eutectic system. These dendrites grow rapidly into the undercooled bath and soon break apart due to recalescence and Sn enrichment of the liquid. These fragmented Pb dendrites are then free to settle to the bottom portion of the ingot causing the macrosegregation observed in this study. A eutectic Pb-Sn alloy undercooled 20 K and cooled at 4 K/s had a composition of about Pb-72 wt.% Sn at the top and 55% Sn at the bottom.

Degroh, Henry C., III↗

Channel formation in Pb-Sn, Pb-Sb, and Pb-Sn-Sb alloy ingots and comparison with the system NH4Cl-H2O

The formation of segregation channels during the unidirectional solidification of base chilled ingots has been studied as a function of composition in binary Pb-Sn and Pb-Sb and ternary Pb-Sn-Sb alloys. The patterns of channel distribution were characterized in the binary and ternary systems and are described as functions of temperature gradients, growth rates, dendrite spacings, and interdendritic permeabilities. Channels appear to nucleate at random across a dendritic front and subsequently to interact as they propagate, decreasing in density across the front. Assuming that the interdendritic spacing is the characteristic distance for a liquid perturbation, yields critical effective Rayleigh numbers which lie within a factor of x 40 for both metallic and aqueous systems. This correlation is close, considering the sensitivity to any assumed dimension and the range of material properties involved, and is taken to support a model for channel nucleation occurring close to the dendritic growth front.

Hellawell, A.↗

Densities of Pb-Sn alloys during solidification

Data for the densities and expansion coefficients of solid and liquid alloys of the Pb-Sn system are consolidated in this paper. More importantly, the data are analyzed with the purpose of expressing either the density of the solid or of the liquid as a function of its composition and temperature. In particular, the densities of the solid and of the liquid during dendritic solidification are derived. Finally, the solutal and thermal coefficients of volume expansion for the liquid are given as functions of temperature and composition.

Poirier, D. R.↗

Macrosegregation in undercooled Pb-Sn eutectic alloys

A novel technique resulting in large undercoolings in bulk samples (23g) of lead-tin eutectic alloy is described. Samples of eutectic composition were processed with undercoolings ranging from 4 to 20 K and with cooling rates varying between 0.04 to 4 K/sec. The final macrostructure of undercooled samples depends on both the initial undercooling of the melt and the cooling rate. Gravity-driven segregation is found to increase with increasing undercooling. A eutectic Pb-Sn alloy undercooled at 20 K and cooled at 4 K/sec had a composition of about Pb-72 wt pct Sn at the top and 55 pct Sn at the bottom. Macrosegregation in these undercooled lead-tin eutectic alloys is shown to be primarily due to a sink/float mechanism caused by the difference in density of the solid and liquid phases and the undercooling and nucleation behavior of the alloy.

De Groh, H. C., III↗

Compositional variations in the undercooled Pb-Sn eutectic solidified at various acceleration levels

Ingots of Pb-61.9 Sn were undercooled and solidified under increasing gravity levels in order to investigate the effects of segregation. The onset of convective flow subsequent to the nucleation of lead is demonstrated. It is shown that when material system in the molten state contains constituents of varying densities, the combination of gravitational forces on the nucleating species and the amount of undercooling of the melt will determine the resultant segregation.

Johnston, M. H.↗

Gravitational macrosegregation in binary Pb-Sn alloy ingots

A space shuttle experiment employing the General Purpose (Rocket) Furnace (GPF) in its isothermal mode of operation is manifested on MSL-3, circa 1989. The central aim of this experiment is to investigate the effect of reduced gravity levels on the segregation behavior in a slowly, and isothermally, cooled sample of a binary Pb-15 wt% Sn alloy. This experiment should be able to simulate, in a small laboratory sample, some aspects of the segragation phenomena occurring in large industrial ingots. Ground-based experiments conducted in the single-cavity simulator of the GPF, in support of the microgravity experiment are described in detail. The results of the MSFC experiments are compared with other related experiments conducted at Case Western Reserve University (CWRS), wherein the isothermal constraints were relaxed. The isothermally processed samples indicate a small and gradual increase in fraction eutectic, and a corresponding increase in tin content, from the bottom to the top of the ingot. The radial variations are minimal near the ingot bottom, but there are large radial variations in the top half. In the CWRU experiments, more severe segregations, including segregation defects known as freckles. Follow up experiments employing the GPF without the isothermal constraints, or other suitably modified space shuttle hardware are suggested.

Laxmanan, V.↗

Gravitational macrosegregation in binary Pb-Sn alloy ingots

A space shuttle experiment employing the General Purpose (Rocket) Furnace (GPF) in its isothermal mode of operation is manifested on MSL-3, circa 1989. The central aim of this experiment is to investigate the effect of reduced gravity levels on the segregation behavior in a slowly, and isothermally, cooled sample of a binary Pb-15 wt pct Sn alloy. This experiment should be able to simulate, in a small laboratory sample, some aspects of the segregation phenomena occurring in large industrial ingots. Ground-based experiments conducted in the single-cavity simulator of the GPF, in support of the microgravity experiment are described in detail. The results of the MSFC experiments are compared with other related experiments conducted at Case Western Reserve University (CWRS), wherein the isothermal constraints were relaxed. The isothermally processed samples indicate a small and gradual increase in fraction eutectic, and a corresponding increase in tin content, from the bottom to the top of the ingot. The radial variations are minimal near the ingot bottom, but there are large radial variations in the top half. In the CWRU experiments, more severe segregations, including segregation defects known as freckles. Follow up experiments employing the GPF without the isothermal constraints, or other suitably modified space shuttle hardware are suggested.

Laxmanan, V.↗

Bulk undercooling, nucleation, and macrosegregation of Pb-Sn alloys

Preliminary ground-based studies on the undercooling behavior of large samples (23 g) of lead-tin alloys are presented. Evidence of gravity-related segregation effects is found, and a possible area for future microgravity experimentation is thus identified. Detailed descriptions of the experimental procedure used to achieve bulk undercoolings of between 0.5 and 34 K, depending on composition, are given. The bulk undercoolings obtained in this study are comparable with those found in small droplets. The large size of the present samples enabled the observation of sedimentation and other macrosegregation processes.

Degroh, H. C., III↗

Enthalpies of a binary alloy during solidification

The purpose of the paper is to present a method of calculating the enthalpy of a dendritic alloy during solidification. The enthalpies of the dendritic solid and interdendritic liquid of alloys of the Pb-Sn system are evaluated, but the method could be applied to other binaries, as well. The enthalpies are consistent with a recent evaluation of the thermodynamics of Pb-Sn alloys and with the redistribution of solute in the same during dendritic solidification. Because of the heat of mixing in Pb-Sn alloys, the interdendritic liquid of hypoeutectic alloys (Pb-rich) of less than 50 wt pct Sn has enthalpies that increase as temperature decreases during solidification.

Poirier, D. R.↗

Directional solidification of eutectic composites in space environment

The Ni-Ni3Ta eutectic and a nickel-base alloy containing 30 wt pct Ta were solidified unidirectionally in an electron beam floating zone melting apparatus. It was found that the volume fraction of the Ni3Ta phase in the Ni-Ni3Ta eutectic mixture was increased from 7.6 to 36 volume pct in agreement with the theory as predicted. Tensile properties of the randomly solidified and unidirectionally solidified Ni-Ni3Ta eutectic were determined as function of solidification rate and temperature. It was found that the ultimate tensile strength decreased as both the test temperature and solidification rate increased. An elongation of 40 pct was obtained for a nickelbase alloy containing 30 wt at room temperature. This unusually large elongation was attributed to the superplastic behavior of the alloy. The critical currents versus the external fields at 2.5, 3.0, 3.5 and 4.2 deg for the unidirectionally solidified Pb-Sn eutectic were measured. The values of critical fields at zero critical currents were obtained by extrapolation.

Yue, A. S.↗

NBS: Materials measurements

Measurements in an Auger spectrometer of surface impurity concentrations on liquid gallium showed that the principle impurities were oxygen and carbon. The impurities showed a tendency to collect into plates or clumps. In Pb rich Pb-Sn off eutectic alloys, macrosegration caused by solutal convection was not reduced by vertical or horizontal fields of 0.1 T, but downward solidification virtually eliminated macrosegration in small diameter samples. Phase assemblages of selected compositions on the joints K(Fe0.5 Si-0.5) O2 -SiO2 and KFeO2 - SiO2 were determined over a large range of oxygen partial pressures and the temperature range 800 C to 1400 C.

Source record↗

Solutal convection induced macrosegregation and the dendrite to composite transition in off-eutectic alloys

The effect of solute gradient induced convection during vertical solidification on the macrosegregation of Pb-rich Pb-Sn off-eutectic alloys is determined experimentally as a function of composition and growth rate. In many cases macrosegregation is sufficient to prevent the plane front solidification of the alloy. The transition from dendritic to composite structure is found to occur when the composition of the solid is close enough to the eutectic composition to satisfy a stability criterion based on the ratio of the liquid temperature gradient to growth rate. A vertical or horizontal magnetic field of 0.1 T (1 kilogauss) does not reduce macrosegregation, but downward solidification (liquid below solid) virtually eliminates macrosegregation in small (3 mm) diameter samples.

Boettinger, W. J.↗

Substrate heating rates for planar and cylindrical-post magnetron sputtering sources

Results are presented for the substrate heating energy/atom required in the planar magnetron sputtering of Al, Cr, Ni, Cu, Mo, In, Ta, W, and Pt in Ar, as well as Al and Cr in O2. Data are also obtained for cylindrical magnetron sputtering of Nb, Ag, Ta, W, and Pb-Sn in Ar, and Mo sputtered in Ne, Ar, Kr, and Xe. Planar and cylindrical magnetron heating rates were comparable. Special experiments were conducted to examine the contributions to substrate heating of plasma species and ion neutralization and reflection at the cathode; the results obtained indicate that charged plasma species do not significantly contribute to the heating, but that neutralized and reflected ions play a significant role in the planar as well as cylindrical cases despite the differences in cathode geometry.

Thornton, J. A.↗

Cellular-dendritic transition in directionally solidified binary alloys

The microstructural development of binary alloys during directional solidification is studied. Cellular growth data for the Al-Cu and Pb-Sn binary alloy systems are analyzed in order evaluate the criteria of Kurz and Fisher (1981) and Trivedi (1984) for cellular-dendritic transition. It is observed that the experimental growth values do not correlate with the Kurz and Fisher or Trivedi data.

Tewari, S. N.↗

Local convective flows in partly solidified alloys

Channel formation in a dendritic mushy zone is examined with reference to experimental results obtained for an acqueous system, NH4Cl-H2O, and a low-melting metallic system, Pb-Sn. The problems of channel nucleation, propagation, and prevention are considered for a configuration in which heat flow is directed downwards and growth occurs upwards into a positive temperature gradient. It is found that channels nucleate at the growth front by double diffusive perturbations into the quiescent bulk liquid, and not by perturbations within the dendritic framework of the mushy zone.

Hellawell, A.↗

Computer simulation of macrosegregation in directionally solidified circular ingots

The formulation and employment of a computer code designed to simulate the directional solidification of lead-rich Pb-Sn alloys in the form of an ingot with a uniform and circular cross-section are described. The formulation is for steady-state solidification in which convection in the all-liquid zone is ignored. Particular attention was given to designing a code to simulate the effect of a subtle variation of temperature in the radial direction. This is important because a very small temperature difference between the center and the surface of the ingot (e.g., less than 0.5 C ) is enough to cause substantial convection within the mushy-zone when the solidification rate is approximately 0.001 to 0.0001 cm/s.

Yeum, K. S.↗

Primary arm spacing in directionally solidified Pb-10 wt percent Sn alloys

The dependence of primary arm spacings on growth speed was investigated for cellular and dendritic arrays in Pb-10 wt percent Sn samples directionally solidified under a constant positive thermal gradient in the melt. The gradient of constitutional supercooling was varied from almost zero (near the break-down of the planar liquid-solid interface at small growth speeds, cellular morphology) to near unity (large growth speeds, dendritic morphology). The spatial arrangements of cells and dendrites, as given by their coordination number, are not very different from each other. It appears that primary arm spacing maxima and the cell to dendrite transition are strongly influenced by the magnitude of the solute partition coefficient. The planar to cellular bifurcation is supercritical in Pb-Sn which has a high partition coefficient, as compared to the subcritical behavior reported in Al-Cu and succinonitrile-acetone, both of which have low partition coefficients. The primary arm spacing model due to Hunt agrees with the experimentally observed trend for the whole growth regime. There is a good quantitative agreement at higher gradients of supercooling. However, the model overpredicts the primary arm spacings at low gradients of constitutional supercooling.

Chopra, M. A.↗