Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “PWSCC”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 19 records

Baseline Evaluation of Eddy Current Testing for PWSCC Susceptible Materials

This technical letter report (TLR) summarizes technical efforts focused on assessments of eddy current testing (ET) examinations using various mockups for obtaining baseline surface and subsurface conditions on materials susceptible to primary water stress corrosion cracking (PWSCC). The scope of this work included nondestructive evaluation characterization of weld surfaces on mockups that were identified for application of various surface peening approaches. All of the work reported here was conducted prior to planned peening of these surfaces to evaluate pre-peening conditions, and subsequently compare the baseline ET results with post-peening conditions. The overall objective of this work was to demonstrate the effectiveness of employing ET for detecting near/sub-surface defects on mockups in support of peening assessments for surface stress improvement and mitigation of PWSCC in these materials. The U.S. Nuclear Regulatory Commission has communicated their expectations to industry for eddy current inspections of peened, inlayed, and onlayed dissimilar metal welds and is interested in better understanding detection performance and sensitivity of ET techniques to support the development of a technical foundation for detection and sizing limits, effective ET qualification requirements, alternate inspections or programs for evaluating PWSCC mitigation processes, and development of ET acceptance standards that can be referenced in the appropriate American Society of Mechanical Engineers Section XI Code Case (N-770-X). This TLR provides a technical discussion focused on the ET data obtained, the analysis, and conclusions drawn from surface examinations of various plate standards and actual components extracted from cancelled nuclear power plants.

36 MATERIALS SCIENCE↗

Predicting Rupture Pressure and Leak Rate of Alloy 600 U-bend Tubes with PWSCC and Comparing with Test Results (Technical Letter Report)

This report summarizes structural integrity work performed for the US NRC that predicts the structural integrity of steam generator (SG) tubes with flaws in the U-bend. The work covers model development and validation for U-bend tubes containing lab-induced primary water stress corrosion cracks (PWSCC). Limit load models for plastic collapse predicting ligament rupture pressure and leak rate of cracked U-bend tubes were developed and validated with pressure tests and finite element analyses (FEAs). Failure pressure and leak rate tests were conducted at room temperature on Alloy 600 U-bend tubes containing flaws located at various locations around the U-bend. Existing models for predicting structural integrity of straight tubes with well defined, rectangular, electro-discharge-machined (EDM) flaws were modified and used to predict the ligament rupture and unstable burst pressures as well as leak rates for the PWSCC flaws in the U-bend section.

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

A Destructive Validation of NDE Responses of Service-Induced PWSCC Found in North Anna 2 Control Rod Drive Nozzle 31

Studies conducted at the Pacific Northwest National Laboratory (PNNL) in Richland, Washington focused on assessing the effectiveness of nondestructive examination (NDE) techniques for inspecting control rod drive mechanism (CRDM) nozzles and J-groove weldments. The primary objective of this work is to provide information to the United States Nuclear Regulatory Commission (NRC) on the effectiveness of NDE methods as related to the in-service inspection of CRDM nozzles and J-groove weldments, and to enhance the knowledge base of primary water stress corrosion cracking (PWSCC) through destructive characterization of the CRDM assemblies.

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

Assessment of the Mechanical Stress Improvement Process for Mitigating Primary Water Stress Corrosion Cracking in Nickel Alloy Butt Welds in Piping Systems Approved for Leak-Before-Break

In recent years, operating experience has shown that Alloy 82/182/600 materials used in reactor coolant system (RCS) pressure boundaries of pressurized water reactors (PWRs) are susceptible to primary water stress corrosion cracking (PWSCC). Cracking can initiate at the inside surface of these materials, in part, because of tensile residual stresses introduced by welding. These materials are present in piping systems that were approved by the U.S. Nuclear Regulatory Commission (NRC) for leak before-break (LBB) before PWSCC was found in RCS dissimilar metal butt welds. The identification of PWSCC led to concerns regarding the potential effect of this degradation on existing LBB analyses. In response to these concerns, the NRC Office of Nuclear Regulatory Research initiated a program entitled, “PWSCC in Leak-Before-Break Systems,” and a follow-on program entitled, “Degradation in Extremely Low Probability of Rupture (xLPR) Systems.” Under these programs, Pacific Northwest National Laboratory (PNNL) is assessing the various strategies being used by industry to manage potential or existing PWSCC in susceptible welds in piping systems approved for LBB. The commercial nuclear power industry has implemented strategies to manage potential or existing PWSCC at Alloy 82/182 dissimilar metal welds (DMW) in PWRs. One general strategy consists of management by a combination of mitigation plus inspection, where several mitigation techniques have been used by industry. The other general strategy is to manage potential PWSCC by inspection alone. At the request of the NRC, the American Society of Mechanical Engineers (ASME) took actions to develop improvements to the existing Code requirements to address the potential for PWSCC in Class 1 PWR piping butt welds fabricated with Alloy 82/182 weld materials. The ASME developed Code Case N-770, “Alternative Examination Requirements and Acceptance Standards for Class 1 PWR Piping and Vessel Nozzle Butt Welds Fabricated with UNS N06082 or UNS W86182 Weld Filler Material With or Without Application of Listed Mitigation Activities, Section XI, Division 1.” It was realized that the Code Case needed to be revised to address specific examinations such as welds with a design life of less than 10 years and post-weld preservice surface examinations. In general, the revised Code Case (N-770-1) has requirements for inspection of unmitigated as well as mitigated Alloy 82/182 RCS butt welds. As such, specific inspection requirements for welds mitigated by the Mechanical Stress Improvement Process (MSIP®), the subject of this technical letter report (TLR), are contained in the Code Case. The NRC incorporated ASME Code Case N-770-1 by reference into §50.55a (76 FR 36232, p. 36278) in June 2011.

MSIP↗

Analysis of Empirical Probability of Detection Data for Dissimilar Metal Welds

The U.S. Nuclear Regulatory Commission’s (NRC) Standard Review Plan (SRP) 3.6.3 describes leak-before- break (LBB) assessment procedures that can be used to assess compliance with the 10 CFR 50 Appendix A, General Design Criteria (GDC)-4 requirement that primary system pressure piping exhibit an extremely low probability of rupture. SRP 3.6.3 does not allow for assessment of piping systems with active degradation mechanisms, such as primary water stress corrosion cracking (PWSCC), which is currently occurring in systems that have been granted LBB approvals. To address those piping systems approved for LBB that are experiencing PWSCC, the NRC Office of Nuclear Regulatory Research (RES) working cooperatively with the Electric Power Research Institute (EPRI) conducted a multi-year project to develop a probabilistic fracture mechanics code called eXtremely Low Probability of Rupture (xLPR) that can be used to assess compliance with the regulations. xLPR is a probabilistic computational tool capable of evaluating degradation in reactor coolant piping welds leading to rupture with extremely low probabilities of occurrence. This tool models the effects of active degradation mechanisms and the inspection and mitigation activities that are being undertaken to manage PWSCC degradation. Crack initiation and growth due to fatigue and primary water stress corrosion, along with mitigation methods (mechanical mitigation as well as chemical mitigation) and the effects of in-service inspection (ISI) and leak detection can be analyzed using this tool.

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

Final Report - Inspection Limit Confirmation for Upper Head Penetration Nozzle Cracking

The ASME Code Case N-729-1 defines alternative examination requirements for the Control Rod Drive Mechanism (CRDM) upper head penetration nozzle welds. The basis for these examination requirements was developed as part of an Industry program conducted by the Materials Reliability Program (MRP) through the Electric Power Research Institute (EPRI). The results of this program were published in MRP-95 Rev. 1 and document a set of finite element weld residual stress analyses conducted on a variety of upper head penetration nozzles. The inspection zone selected by the industry was based on the stress where it was assumed that primary water stress corrosion cracking (PWSCC) would not initiate. As explained in MRP-95 Rev. 1, it has been illustrated that PWSCC does not occur in the Alloy 600 tube when the stresses are below the yield strength of that tube. Typical yield strengths at operating conditions for Alloy 600 range from 35 ksi to 65 ksi. A stress less than 20-ksi tension was chosen as a conservative range where PWSCC would not initiate. Over the last several years, Engineering Mechanics Corporation of Columbus (Emc2) has conducted welding residual stress analyses on upper head penetration J-welds made from Alloy 182 weld metal for the U.S. Nuclear Regulatory Commission (NRC) staff. These efforts were performed as a confirmatory evaluation of the industry’s analyses conducted as part of their MRP-95 Rev. 1 effort. To this point, the analyses conducted by Emc2 have not been compared to the MRP-95 Rev. 1 results or the examination zones defined in the Code Case. Therefore, this report summarizes the past Emc2 CRDM welding analyses and investigates the regions where the welding stresses may be sufficiently high to promote stress corrosion cracking (SCC). In all, 90 welding residual stress analyses were conducted by Emc2 and the largest distance below the weld where the stress drops below 20 ksi was 5 inches for the uphill weld of the 53-degree nozzle case. For the largest distance above the weld where stress drops below 20 ksi, the worst case was 1.5 inches above the downhill side of the 25-degree nozzle case. The inspection zones described in both MRP-95 Rev. 1 and Code Case N-729-1 were set at 1.0 inch for nozzle angles greater than 30 degrees or 1.5 inches for nozzle angles less than 30 degrees, above the highest or below the lowest point on the weld. In all cases analyzed by Emc2 in this effort, there was only one case where the stress was above 20 ksi outside of this inspection zone. For that case, the stresses were very close to 20 ksi at the inspection zone limit and were considered acceptable.

36 MATERIALS SCIENCE↗

Out-of-reactor test of corrosion and hydrogen pickup in fuel cladding materials in contact with nickel metal - 2016-0038

Increased reactor coolant hydrogen concentration in pressurized water reactors (PWRs) is under consideration for potential benefits in reducing primary water stress corrosion cracking (PWSCC) crack growth rate as well as increasing PWSCC crack initiation time in nickel-based alloys. Potential concerns related to fuel performance include possible increases in hydrogen pickup (HPU) by zirconium based alloys and the enhancement of the pickup through the so-called nickel-window effect. Although the risk of this occurrence may be low, the consequences of increased HPU could be substantial. We examined the impact of dissolved hydrogen (DH) concentrations on Zircaloy-4 corrosion and HPU when the samples are in contact with nickel sources. The work was completed in conjunction with a large project that evaluated the impact of dissolved hydrogen on various fuel cladding and spacer weld specimens of M5{sup R}, ZIRLO{sup R}, Optimized ZIRLO{sup TM}, Low-Tin ZIRLO{sup TM}, Optimized Low-Tin Zircaloy-4, and Zircaloy-2 in either as-received or pre-oxidized conditions for exposures up to 730 days in high-pressure, out-of-reactor autoclave systems operating with a simulated PWR coolant at three different DH concentrations: 30, 100, and 500 cm{sup 3} (cc) H{sub 2}/kg H{sub 2}O. A significant increase in HPU was observed for some Zircaloy-4 specimens in contact with synthetic crud at elevated DH levels. The HPU increased with increasing DH and a metallic nickel fraction in the synthetic crud. The formation of metallic nickel in the synthetic crud samples at elevated DH levels was confirmed. (authors)

36 MATERIALS SCIENCE↗

Crack-Free 30% Chromium-Nickel Alloy Welding Products for Nuclear Service

We report prior research in the development of 30% chromium-nickel alloy nuclear welding wires has resulted in the resolution of primary water stress corrosion cracking (PWSCC) and ductility dip cracking (DDC) as well as improvement in solidification cracking (SC) resistance. The resolution of DDC exhibits some Laves phase, which has a negative effect on SC resistance. In this study, the use of an alternate carbide former, tantalum (Ta), in combination with niobium (Nb) was researched. Three heats of recently designed Filler Metal 52MSS-Ta (i.e., HV1648, HV1673A, and VX131WXW) were melted, fabricated, and systematically studied. DDC and SC were evaluated with thermodynamic modeling using the Scheil solidification simulation model, two types of varestraint tests, and strain-to-fracture (STF) testing. The varestraint and STF test results showed an improved SC resistance with reduced Laves phase and concurrent excellent DDC resistance. Optimized compositions with low Laves phase also exhibited high threshold strain values (TSVs) in the STF test. VX131WXW — which contains 2.81 wt-% Ta, 0.6 wt-% Nb, and 6 wt-% iron (Fe) - exhibited a TSV of 24%. Thermo-Calc computed the Laves phase to be 0.24% for VX131WXW compared to 0.06% in HV1673A. This difference in Laves phase resulted in the lower SC resistance of VX131WXW compared to HV1673A when measured with longitudinal varestraint testing. The maximum crack distance for HV1673A was about 0.6 mm while that of heat VX131WXW was about 1.0 mm. The typical diluted weld deposit made with VX131WXW was also resistant to PWSCC due to the chromium content exceeding 24%. These simultaneous results mark progress toward crack-free welds and provide direction for further optimization of Ta-containing filler metals.

30% chromium-nickel alloy↗

STRESS CORROSION CRACK GROWTH RESPONSE FOR ALLOY 152/52 DISSIMILAR METAL WELDS IN PWR PRIMARY WATER

As part of ongoing research into primary water stress corrosion cracking (PWSCC) susceptibility of alloy 690 and its welds, SCC tests have been conducted on alloy 152/52 dissimilar metal (DM) welds with cracks positioned with the goal to assess weld dilution and fusion line effects on SCC susceptibility. No increased crack growth rate was found when evaluating a 20% Cr dilution zone in alloy 152M joined to carbon steel (CS) that had not undergone a post-weld heat treatment (PWHT). However, high SCC crack growth rates were observed when the crack reached the fusion line of that material where it propagated both on the fusion line and in the heat affected zone (HAZ) of the carbon steel. Crack surface and crack profile examinations of the specimen revealed that cracking in the weld region was transgranular (TG) with weld grain boundaries not aligned with the geometric crack growth plane of the specimen. The application of a typical pressure vessel PWHT on a second set of alloy 152/52 – carbon steel DM weld specimens was found to eliminate the high SCC susceptibility in the fusion line and carbon steel HAZ regions. PWSCC tests were also performed on alloy 152-304SS DM weld specimens. Constant K crack growth rates did not exceed 5x10-9 mm/s in this material with post-test examinations revealing cracking primarily on the fusion line and slightly into the 304SS HAZ.

alloy 152↗

Inspection of Nickel Alloy Welds: Results from Five Year International Program

The U.S. Nuclear Regulatory Commission established and coordinated the international Program for the Inspection of Nickel alloy Components (PINC). The goal of PINC was to evaluate the capabilities of various nondestructive examination (NDE) techniques to detect and characterize primary water stress corrosion cracking (PWSCC) in dissimilar metal welds. Round-robin results showed that a combination of conventional and phased-array ultrasound provide the highest performance for flaw detection and depth sizing in dissimilar metal piping welds. The effective detection of flaws in bottom-mounted instrumentation penetrations by eddy current and ultrasound shows that it may be possible to reliably inspect these components in the field.

36 MATERIALS SCIENCE↗

New International Program to Asses the Reliability of Emerging Nondestructive Techniques (PARENT)

The Nuclear Regulatory Commission (NRC) established the Program to Assess the Reliability of Emerging Nondestructive Techniques (PARENT) to follow on from the successful Program for the Inspection of Nickel alloy Components (PINC). The goal of the PARENT is to conduct a confirmatory assessment of the reliability of nondestructive evaluation (NDE) techniques for detecting and sizing primary water stress corrosion cracks (PWSCC) and applying the lessons learned from PINC to a series of round-robin tests. These open and blind round-robin tests will comprise a new set of typical pressure boundary components including dissimilar metal welds (DMWs) and bottom-mounted instrumentation penetrations. Open round-robin tests will engage research and industry teams worldwide to investigate and demonstrate the reliability of emerging NDE techniques to detect and size flaws with a wide range of lengths, depths, orientations, and locations. Blind round-robin tests will utilize various testing organizations, whose inspectors and procedures are certified by the standards for the nuclear industry in their respective countries, to investigate the ability of established NDE techniques to detect and size flaws whose characteristics range from relatively easy to very difficult for detection and sizing. Blind and open round-robin testing started in late 2011 and early 2012, respectively. This paper will present the work scope with reports on progress, NDE methods evaluated, and project timeline for PARENT.

Bottom Mounted Instrumentation↗

Development, analysis, and evaluation of a commercial software framework for the study of Extremely Low Probability of Rupture (xLPR) events at nuclear power plants.

Sandia National Laboratories (SNL) participated in a Pilot Study to examine the process and requirements to create a software system to assess the extremely low probability of pipe rupture (xLPR) in nuclear power plants. This project was tasked to develop a prototype xLPR model leveraging existing fracture mechanics models and codes coupled with a commercial software framework to determine the framework, model, and architecture requirements appropriate for building a modular-based code. The xLPR pilot study was conducted to demonstrate the feasibility of the proposed developmental process and framework for a probabilistic code to address degradation mechanisms in piping system safety assessments. The pilot study includes a demonstration problem to assess the probability of rupture of DM pressurizer surge nozzle welds degraded by primary water stress-corrosion cracking (PWSCC). The pilot study was designed to define and develop the framework and model; then construct a prototype software system based on the proposed model. The second phase of the project will be a longer term program and code development effort focusing on the generic, primary piping integrity issues (xLPR code). The results and recommendations presented in this report will be used to help the U.S. Nuclear Regulatory Commission (NRC) define the requirements for the longer term program.

21 SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLANTS↗

Evaluation of Manual Ultrasonic Examinations Applied to Detect Flaws in Primary System Dissimilar Metal Welds at North Anna Power Station

During a recent inservice inspection (ISI) of a dissimilar metal weld (DMW) in an inlet (hot leg) steam generator nozzle at North Anna Power Station Unit 1, several axially oriented flaws went undetected by the licensee's manual ultrasonic testing (UT) technique. The flaws were subsequently detected as a result of outside diameter (OD) surface machining in preparation for a full structural weld overlay. The machining operation uncovered the existence of two through-wall flaws, based on the observance of primary water leaking from the DMW. Further ultrasonic tests were then performed, and a total of five axially oriented flaws, classified as primary water stress corrosion cracking (PWSCC), were detected in varied locations around the weld circumference.

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

Pacific Northwest National Laboratory Investigation of the Stress Corrosion Cracking in Nickel-Base Alloys (Volume 2)

The objective of this program is to evaluate the primary water stress corrosion cracking (PWSCC) susceptibility of high chromium alloy 690 and its weld metals, establish quantitative measurements of crack-growth rates and determine relationships among cracking susceptibility, environmental conditions and metallurgical characteristics. Stress-corrosion, crack-growth rates have been determined for 12 alloy 690 specimens, 11 alloy 152/52/52M weld metal specimens, 4 alloy 52M/182 overlay specimens and 2 alloy 52M/82 inlay specimens in simulated PWR primary water environments. The alloy 690 test materials included three different heats of extruded control-rod-drive mechanism (CRDM) tubing with variations in the initial material condition and degree of cold work for one heat. Two cold-rolled (CR) alloy 690 plate heats were also obtained and evaluated enabling comparisons to the CR CRDM materials. Weld metal, overlay and inlay specimens were machined from industry mock ups to provide plant-representative materials for testing. Specimens have been tested for one alloy 152 weld, two alloy 52 welds and three alloy 52M welds. The overlay and inlay specimens were prepared to propagate stress-corrosion cracks from the alloy 182 or 82 material into the more resistant alloy 52M. In all cases, crack extension was monitored in situ by direct current potential drop (DCPD) with length resolution of about +1 µm making it possible to measure extremely low growth rates approaching 5x10 -10 mm/s. Most SCC tests were performed at 325-360°C with hydrogen concentrations from 11-29 cc/kg; however, environmental conditions were modified during a few experiments to evaluate the influence of temperature, water chemistry or electrochemical potential on propagation rates. In addition, low-temperature (~50°C) cracking behavior was examined for selected alloy 690 and weld metal specimens. Extensive characterizations have been performed on material microstructures and stress-corrosion cracks by optical and electron microscopy techniques and linked to crack-growth test results to help define material and environmental parameters controlling SCC susceptibility.

Bruemmer, Stephen M.↗

Analysis of Phase Transformation Studies in Solute Addition Alloys

Components serving in a nuclear reactor plant must withstand a very harsh environment including extended time at elevated temperatures, neutron irradiation, stress, and/or corrosive media. The many modes of degradation are complex and very depending on material and service locations. However, understanding and managing materials degradation is paramount for the continued safe and reliable operation of nuclear power plants. For the reactor core and primary systems, several key areas have been identified. Thermomechanical considerations such as aging and fatigue must be examined. Irradiation-induced processes must also be considered for higher fluences under the life extension consideration of the current light water reactors (LWRs), which particularly includes the influence of radiation-induced segregation (RIS), swelling, and precipitation on component hardening and embrittlement. Corrosion takes many forms within the reactor core, although irradiation-assisted stress corrosion cracking (IASCC) and primary water stress corrosion cracking (PWSCC) are of high interest in extended life scenarios. Research in these areas can build upon other ongoing programs in the LWR industry as well as other reactor materials programs (such as fusion and fast reactors) to help resolve these issues for extended LWR life. Type 304 and 316 stainless steels are classic structural materials used in LWRs. A set of well designed type 304 and 316 variants by changing the amount of a single solute element were irradiated using the BOR-60 fast breeder reactor at ~320°C in Russia. This set of alloy samples has been used in this task to characterize detailed microstructural evolution and measure magnetic phase, swelling and hardness. This report summarizes the detailed microstructural results, characterized using conventional and scanning transmission electron microscopy (CTEM/STEM) and energy dispersive X-ray spectroscopy (EDS), and the newly developed model of strength factor for estimating radiation hardening. The results provide invaluable insights into understanding degradation mechanisms of key components and assists in the prediction of the life of similar materials and the base knowledge required to develop advanced radiation resistant alloys. The effect of solute elements on microstructural evolution under neutron irradiation is explored. The approximate correlation between microstructure changes and radiation hardening is established. The major results and implications are discussed below.

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

Insights Gained from Ultrasonic Testing of Piping Welds Subjected to the Mechanical Stress Improvement Process

Pacific Northwest National Laboratory (PNNL) is assisting the United States Nuclear Regulatory Commission (NRC) in developing a position on the management of primary water stress corrosion cracking (PWSCC) in leak-before-break piping systems. Part of this involves determining whether inspections alone, or inspections plus mitigation, are needed. This work addresses the reliability of ultrasonic testing (UT) of cracks that have been mitigated by the mechanical stress improvement process (MSIP). The MSIP has been approved by the NRC (NUREG-0313) since 1986 and modifies residual stresses remaining after welding with compressive, or neutral, stresses near the inner diameter surface of the pipe. This compressive stress is thought to arrest existing cracks and inhibit new crack formation. To evaluate the effectiveness of the MSIP and the reliability of ultrasonic inspections, flaws were evaluated both before and after MSIP application. An initial investigation was based on data acquired from cracked areas in 325-mm-diameter piping at the Ignalina Nuclear Power Plant (INPP) in Lithuania. In a follow-on exercise, PNNL acquired and evaluated similar UT data from a dissimilar metal weld (DMW) specimen containing implanted thermal fatigue cracks. The DMW specimen is a carbon steel nozzle-to-safe end-to-stainless steel pipe section that simulates a pressurizer surge nozzle. The flaws were implanted in the nozzle-to-safe end Alloy 82/182 butter region. Results are presented on the effects of MSIP on specimen surfaces, and on UT flaw responses.

21 SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLANTS↗

Microstructural Effects on SCC Initiation PWR Primary Water Cold-Worked Alloy 600

SCC initiation behavior of one mill annealed alloy 600 plate heat was investigated in simulated PWR primary water under constant load at yield stress with in-situ direct current potential drop (DCPD) monitoring for crack initiation. Twelve specimens were tested at similar cold work levels among which three showed much shorter SCC initiation times (<400 hrs) than the others (>1200 hrs). Post-test examinations revealed that these three specimens all feature an inhomogeneous microstructure where the primary crack always nucleated along the boundary of large elongated grains protruding normally into the gauge. In contrast, such microstructure was either not observed or did not extend deep enough into the gauge in the other specimens exhibiting ~3-6X longer initiation times. In order to better understand the role of this microstructural inhomogeneity in SCC initiation, high-resolution microscopy was performed to compare carbide morphology and strain distribution between the long grains and normal grains, and their potential effects on SCC initiation are discussed in this paper.

Alloy 600↗