The recovery kinetics of deformed copper- palladium and gold-palladium alloys.
Recovery of deformed copper-palladium and gold- palladium alloys by isothermal and isochronal annealing, noting vacancy and interstitial migration
SEARCH · Engineering Papers
Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.
Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.
Recovery of deformed copper-palladium and gold- palladium alloys by isothermal and isochronal annealing, noting vacancy and interstitial migration
Literature search on hydrogen absorption effect on palladium alloys revealed existence of alloy compositions in which alpha--beta transition does not take place. Survey conclusions: 40 percent gold alloy of palladium should be used in place of palladium; alloy must be free of interstitial impurities; and metallic surfaces of tube must be clean.
Plastic deformation effect on resistivity and Hall effect of copper-palladium and gold- palladium alloys
States density in vicinity of Fermi surface obtained from values of paramagnetic susceptibility for gold-palladium alloys
Understanding and controlling the alloying properties of nanomaterials under electrochemical conditions are critically important for fields ranging from energy storage and catalysis to electrochromic window technology. Hydrogen-absorbing nanomaterials, like palladium, are especially interesting due to their ability to reversibly absorb and store hydrogen in their lattice at near-stoichiometric amounts. Palladium’s work function is also significantly deeper than that of most transition metals, which enables electrochemical underpotential deposition of conformal monolayer and submonolayer amounts of transition metals onto the palladium surface. The simultaneous existence of these two properties is unique and opens new and exciting avenues for electrochemical applications. However, the intersection of surface-modified, hydrogen-alloyed palladium nanomaterials is poorly understood, and specifically, how these structures evolve during electrochemical operating conditions remains an open question. Here, we synthesize {100}-terminated palladium nanocubes and deposit between 0.5 and 22 monolayers of copper at the palladium surface. We then electrochemically alloy these surface-modified structures with hydrogen. Using a combination of analytical electrochemistry, spectroscopy, and microscopy, we track the positional evolution of the Cu at the surface of Pd, its impact on palladium’s ability to absorb hydrogen, and copper’s effect on hydrogen evolution electrocatalysis. We show that Cu readily alloys into the palladium nanocube at potentials more negative than the Cu 2+/0 deposition, but a 0.5 monolayer thick copper layer remains at the Pd surface regardless of potential. Finally, we discuss the implications of these findings within the framework of CO 2 reduction catalysis for carbon–carbon bond-forming chemistry.
Metal foil pumps (MFPs) are a leading technology for the direct internal recycling (DIR) of hydrogen isotopes from the plasma exhaust of fusion devices. MFPs rely on the concept of superpermeation, where plasma-generated atomic hydrogen absorbs into the metal foil, rapidly diffuses, and desorbs downstream. To date, studies of superpermeation have predominantly employed pure hydrogen or in some cases trace levels of impurities. In practice the plasma exhaust may contain significant levels of plasma enhancement gases such as argon, an inert gas with metastable states that can enhance the plasma. In this work, we systematically study the impact of Ar addition on the performance of PdCu and PdAg MFPs at low temperature. Performance was strongly dependent on the DIR fraction. At negligible DIR levels Ar addition did not significantly improve the flux over dilution effects. However, under appreciable DIR operation the flux was enhanced up to 90 % relative to pure H 2 , with the optimal concentration range being 5–10 % Ar exiting the system. Beyond 15 % addition plasma enhancement benefits were offset by dilution. Performance correlated with the atomic H emission, and benefits were more pronounced for PdAg than PdCu. Operation at significant DIR levels dramatically alters the flow dynamics resulting in concentration gradients near the MFP, creating plasma conditions that promote H 2 dissociation.
Not Available
Alloying is well-known to improve the dehydrogenation selectivity of pure metals, but there remains considerable debate about the structural and electronic features of alloy surfaces that give rise to this behavior. To provide molecular-level insights into these effects, a series of Pd intermetallic alloy catalysts with Zn, Ga, In, Fe and Mn promoter elements was synthesized, and the structures were determined using in situ X-ray absorption spectroscopy (XAS) and synchrotron X-ray diffraction (XRD). The alloys all showed propane dehydrogenation turnover rates 5–8 times higher than monometallic Pd and selectivity to propylene of over 90%. Moreover, among the synthesized alloys, Pd 3 M alloy structures were less olefin selective than PdM alloys which were, in turn, almost 100% selective to propylene. This selectivity improvement was interpreted by changes in the DFT-calculated binding energies and activation energies for C–C and C–H bond activation, which are ultimately influenced by perturbation of the most stable adsorption site and changes to the d-band density of states. Furthermore, transition state analysis showed that the C–C bond breaking reactions require 4-fold ensemble sites, which are suggested to be required for non-selective, alkane hydrogenolysis reactions. These sites, which are not present on alloys with PdM structures, could be formed in the Pd 3 M alloy through substitution of one M atom with Pd, and this effect is suggested to be partially responsible for their slightly lower selectivity.
Metal foil pumps (MFPs) are key components in the direct internal recycling inner fuel cycle loop for the recovery of hydrogen isotopes from deuterium-tritium fusion exhaust. Operating under vacuum conditions, they utilize superthermal hydrogen as the feed gas in a process called superpermeation. A notable feature of MFPs is their ability to pump against a pressure gradient. This study examines the compression capabilities of PdAg and PdCu MFPs at low temperatures with a constant feed pressure of 10 Pa. At 75°C, compression ratios exceeding 200 were readily achieved, with downstream pressures exceeding 4500 Pa using PdCu. For both alloys, net fluxes decreased by only ~15% at downstream pressures of 1000 Pa, which offers potential simplifications for the downstream pump train. Performance declined markedly when the temperature was elevated to 200°C. Pump curves were constructed and advocated as the most appropriate manner to assess MFP performance. Separate pressure-driven-permeation experiments at relevant conditions were conducted, providing a direct measurement of the hydrogen dissociation constant $k$ d , which was found to be in good agreement with the previous literature. Further, these measurements were used to predict pump curves and maximum compression ratios by balancing superpermeation with pressure-driven permeation, achieving excellent agreement with experiment. Last, experiments using asymmetric MFPs revealed the detrimental impact that surface impurities have on performance in this system.
Abstract not provided.
Explore the source record for details and available documents.
Fusion fuel cycle designs depend on palladium and palladium-silver alloys. The selective permeability of these is used to separate hydrogen isotopes from other elements. Predicting the solubility of hydrogen isotopes in palladium-silver alloys is important for the design of key unit operations for tritium processing. This paper presents a model of hydrogen isotope solubility in palladium and palladium-silver alloys based on Guggenheim’s quasichemical lattice theory. The model parameters were determined as functions of isotope molecular weight and the silver content of the alloy. The model predicts reasonable values for the solubility of protium, deuterium, and tritium over a wide range of temperatures, pressures, and alloy compositions.
Hydrogen gas diffusion through palladium-silver alloy
Method for recovering powdered silver-palladium braze alloy from an acrylic spray binder and rubber masking adhesive used in spray brazing is devised. The process involves agitation and dissolution of masking materials and recovery of suspended precious metal particles on a filter.
Vapor pressure data obtained by the torsion-effusion method provides the thermodynamic properties of several transition-metal alloy systems. The vapor pressure of silver over solid silver and over palladium-silver alloys was measured and the results were more accurate than those found previously by other techniques.
Mass transfer of a gas through a selective, solid membrane is an effective method for separation of desired species. This selective permeability is evident in the flow of hydrogen and the isotope deuterium through palladium-silver metal alloy media. In this study, based upon Sieverts’s law and the Arrhenius diffusion equation, an empirical correlation was developed to determine the steady-state permeation rate R, dependence on media temperature T, gas supply pressure p(sub S), and gas backpressure p(sub B) on the lower pressure side. Because of an extensive range of experimental conditions and complete reporting of raw data, the research by Ackerman and Koskinas was used as a source for data allowing empirical equation fitting. Unfortunately, those authors reported best-fit equations that poorly represented their own results. To improve the modeling of the original data and demonstrate the quality of the measurements, the current study develops improved hydrogen and deuterium permeation rate equations: P = 4.22×10(exp −6) A[exp(−704/T)](sq. root p(sub S) − sq. root p(sub B))/t for hydrogen P = 2.12×10(exp −6) A[exp(−468/T )](sq. root p(sub S) − sq. root p(sub B))/t for deuterium for values of cross-sectional area A (sq.cm), medium thickness t (cm), pressure p (psia), and temperature T (Kelvin), giving a permeation rate in mole/minute. These equations model permeation rate data more closely than do several other existing literature sources.
Physical and chemical properties of platinum metals alloyed with tungsten, rhenium, osmium, and iridium
Adding small amounts of a more reactive dopant metal to a more selective host metal is a well-known strategy for promoting the catalytic reactivity of the latter without sacrificing its selectivity. While substantial attention has been given to coinage metal hosts for activating individual C–H or O–H bonds, less attention has been given to more exotic metals, such as indium, which is highly selective in the complex hydrogenation of CO 2 to methanol. Herein, we describe the synthesis and properties of Pd–In alloys containing Pd in various states of aggregation (isolated atom, small clusters, and extended clusters) assessed through various characterization methods. These materials exhibit unique catalytic behaviors, with Pd promoting both the reaction rate and methanol selectivity in all cases, though its efficacy is highest when Pd is present in small clusters. Here, the inefficiency of high Pd loadings is due in part to losses in Pd accessibility, while the importance of aggregated vs isolated Pd is theorized to result from accelerated H 2 activation. Methods used to synthesize more conventional dilute-limit and single-atom alloy catalysts can, therefore, be extended to non-coinage metal hosts to promote and control more complex chemistries, though the roles of ensemble size may greatly differ.