Chemical Stability of Perfluorobis(sulfonyl)imide-Acid (PFIA) Ionomers in Open Circuit Voltage (OCV) Accelerated Test Conditions
Not Available
SEARCH · Engineering Papers
Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.
Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.
Not Available
Explore the source record for details and available documents.
The self discharge test at full state of charge, may not be a good one to detect subtle defects since the li-ion chemistry has the highest self discharge at full state of charge. One should characterize self discharge versus storage time for each cell manufacturer/design to differentiate between normal self discharge and that due to a subtle manufacturing defect. The various soft short test methods indicate that if this test is carried out at full discharge (0% SOC) with all capacity removed (by lowering the current load in a stepwise manner to the same end of discharge voltage), then the cells need to be placed in storage for more than 72 hours to get a good analysis on the presence of subtle defects since it takes more than 72 hours to achieve voltage stabilization. If the cells are to be charged up even to a small percentage (ex. 1%), 72 hours are sufficient to determine issues. However, the pass/fail criteria should be based on a valid OCV decline. Less than 10 mV voltage decline is not a good method to detect subtle defects. As mentioned in the first bullet, self discharge is a competing reaction when a charge is introduced and hence a characterization of the self discharge versus storage time is required to fully correlate voltage decline to a failure due to a subtle defect. Soft short test method cannot be relied on for defect detection because cells with and without voltage decline seemed to have similar defects and characteristics. Screening methods such as internal resistance and capacity as well as a 3-sigma range for OCV, mass and dimensions should be used to screen out outliers. A very critical aspect in the understanding of subtle defects is to carry out destructive analysis of cells from every lot to confirm the quality of production and screen all cells and batteries in a stringent manner to have a high quality set of flight cells. Self Discharge Test: Fully charged cells shall be placed in Open circuit stand for 72 hours (OCV measurement twice a day); continue for total of 14 days with 1 reading per day 2. Soft Short Test 1: Fully charge; cells discharged to manufacturer's end of disch. Voltage (EODV) cutoff at C/5 rate; stand for 30 minutes; discharge with C/500 to the same EODV. stand for another 30 minutes; discharge the cells again using C/1000 current to the same EODV. OCV measurements twice a day for 72 hours and then for total of 14 days (data collection same as in 1.) 3. Soft Short Test 2: Fully charge; cells discharged to the manuf. EODV with a C/13 constant current; provide a 10 hour rest, discharge again to the same EODV with a current of C/250, provide a 10 hour rest, discharge again using a C/250 rate, provide a 24 hour rest, charge using C/250 to 3.15 V (for ~12 hours). OCV measurements twice a day for at 72 hours. (data collection same as in 1.) 4. Soft Short Test 3: Fully charge; cells shall be discharged using C/10 current to manuf. EODV. Allow the cell to remain at Open circuit for 10 seconds. Discharge the cell at C/20 rate to the same EODV, hold open circuit for 24 hours. Discharge the cells at C/200 rate to the same end of voltage cutoff and hold open circuit for 24 hours. Discharge the cells one more time at C/200 rate to the same EODV and hold open circuit for 36 hours. Charge at C/200 rate to 3.15 V and hold for 3 days. Record OCV during the open circuit stand periods every 12 hours and at the beginning and end of the 3 day hold (include the 12 hour OCV recording during this time also). Capacity Cycling: Cells with declining voltages - one cell from each manufacturer chosen for cycling Destructive Physical Analysis (DPA): Cells with and without decline chosen from each lot for DPA.
Molten alloys with 50-mol% In-Sb, Sn-Sb, Sb-Bi, and Sb-Pb were examined as anodes for solid oxide fuel cells at 973 K. The cells were operated in the battery mode, without added fuel, in order to understand the oxidation characteristics of these alloys at electrolyte interfaces. Cells using 50-mol% In-Sb and Sn-Sb mixtures exhibited open-circuit voltages (OCV) of 1.0 and 0.93 V, values that are identical to that of cell with pure In and Sn respectively. Also similar to the pure In and Sn anodes, the impedances of these cells were initially low but increased dramatically after drawing a small amount of charge, implying formation of In₂O₃ and SnO₂ layers at the electrolyte interface. The 50-mol% Sb-Bi cell had an OCV of 0.73 V initially, close to the OCV observed with pure Sb. The OCV remained constant until a charge identical to that required for oxidation of all the Sb had been passed, after which the OCV dropped to 0.43 V, similar to the value for pure Bi. SEM analysis of the cell after conversion of the Sb showed two distinct phases, with metallic Bi at the bottom and Sb₂O₃ at the top. The electrochemical oxidation of 50-mol% Sb-Pb alloys exhibited an OCV that changed continuously with conversion, from 0.73 V initially to 0.67 V following the addition of charge corresponding to oxidation of 120% the Sb. The total cell impedance remained low for this entire period. EDS measurements on the sectioned Sb-Pb cell suggested that both Sb and Pb were oxidized simultaneously to form a mixed oxide of Pb and Sb.
Polymer -electrolyte-fuel-cell open-circuit voltages (OCVs) are exactly defined by equation (1), where cathode and anode proton activities [(aH+)cathode and (aH+)anode, respectively] usually are identical, so the third term in the right-hand side of equation (2) is ignored. OCV=E0+RT/2F*ln(a1/2 O2*(a2 H+)cathode/aH2O)-RT/2F*ln((a2 H+)anode/aH2) (1) =E0+RT/2F*ln(a1/2 O2*aH2/aH2O)+RT/2F*ln((a2 H+)cathode/(a2 H+)anode) (2) Water vapor pressure is a colligative property that fundamentally correlates to electrolyte concentrations in aqueous solutions. Proton activity is a function of acid concentration, such as pH, when electrolytes are acids. In polymer-electrolyte membranes, water vapor pressure and acid concentration are understood as relative humidity (RH) and water uptake (λ), respectively, where λ represents number of water molecules per sulfonic acid molecule. Several investigations have reported the relationship between RH and λ, meaning that proton activities and associated water uptakes are intimately related to RH. In actual fuel cell operation, cathode RH is determined by ambient-atmosphere and/or humidifier RH(s), and anode RH depends on hydrogen-circulator RH. Therefore, RH is not always identical at both electrodes, and the difference between electrode RHs is considerable during dry operation of polymer electrolyte fuel cells. Therefore, the third term in the right-hand side of equation (2) may be significant for dry operation. We measured OCVs when hydrogen was supplied to both electrodes at 80°C. One electrode (A) was fixed at 30% RH, while RH at the other electrode (B) was varied (0, 5, 10, 20, and 30%). Measured OCVs varied from 0 to 75 mV. For fuel cell tests, electrode A was supplied with hydrogen at 30% RH; electrode B, oxygen at 0, 5, 10, 20, and 30% RH. OCVs deviated from that measured when RH at electrode B was 30%, increasing from 0 to 60 mV with decreasing RH at electrode B. Results are also shown in Figure 1. Proton activities of both electrodes were thermodynamically calculated. The Gibbs–Duhem relation was applied to obtain molar Gibbs free energies of water and sulfonic acid, and proton activity coefficient was calculated using the Gibbs free energy of sulfonic acid and the relationship between RH and λ1–4, assuming that protons and sulfonic anions show identical ionic-activity coefficients. OCVs were estimated using the third term in the right-hand side of equation (2). Results are shown in Figure 1. Fuel-cell current–voltage performance was poor when RHs at the anode and cathode were 30 and 20%, respectively. To determine kinetic current, we measured the oxygen-reduction reaction (ORR) using a rotating-disk electrode (RDE) in concentrated-acid aqueous solutions, which modeled catalyst-layer ionomers. Kinetic currents decreased with acid concentrations. References T. A. Zawodzinski, Jr., C. Derouin, S. Radzinski, R. J. Sherman, V. T. Smith, T. E. Springer and S. Gottesfeld , J. Electrochem. Soc., 140,1041 (1993) P. K. Das and A. Z. Weber, Proceedings of the ASME 2013 11th Fuel Cell Science, Engineering and Technology Conference, Fuel Cell 18010 (2013) V. A. Sethuraman, J. W. Weidner, A. T. Haug, S. Motupally,b and L. V. Protsailo, J. Electrochem. Soc., 155, B50 (2008) A. Kusoglu and A. Z. Weber, Chem. Rev., 117, 987 (2017) Figure 1
A combined chemical/mechanical accelerated stress test (AST) was developed for proton exchange membrane (PEM) fuel cells based on relative humidity cycling (RHC) between dry and saturated gases at open circuit voltage (OCV). Membrane degradation and failure were investigated using scanning electron microscopy and small- and wide-angle X-ray scattering. Changes to membrane thickness, hydrophilic domain spacing, and crystallinity were observed to be most similar between field-operated cells and OCV RHC ASTs, where local thinning and divot-type defects are the primary failure modes. While RHC in air also reproduces these failure modes, it is not aggressive enough to differentiate between different membrane types in >1,333 hours (55 days) of testing. Conversely, steady-state OCV tests result in significant ionomer morphology changes and global thinning, which do not replicate field degradation and failure modes. It is inferred that during the OCV RHC AST, the decay of the membrane's mechanical properties is accelerated such that materials can be evaluated in hundreds, instead of thousands, of hours, while replicating the degradation and failure modes of field operation; associated AST protocols are recommended as OCV RHC at 90°C for 500 hours with wet/dry cycle durations of 30s/45s and 2m/2m for automotive and bus operation, respectively.
Explore the source record for details and available documents.
The aim of this project was to leverage the low area specific resistance (ASR) of Redox’s GDC electrolyte-based cell architecture and increase solid oxide fuel cell (SOFC) efficiency (i.e., open circuit voltage, or OCV) without significantly increasing cell resistance. The key to achieving the increased SOFC efficiency is the introduction of a thin sputtered yttria stabilized zirconia (YSZ) electron-blocking layer and a thin sputtered gadolinia doped ceria (GDC) barrier layer on top of the half-cell substrate (i.e., anode and GDC electrolyte). A key initial effort of the project was to improve the quality of the half-cell substrate surface so that any remaining defects were significantly smaller than the desired film thickness. During lab-scale trials, we had to overcome challenges with film cracking during post-sputtering treatments (e.g., thermal anneals) as well as damage to the sputtering targets. After the initial lab-scale trials, the focus shifted toward the use of commercial scale sputtering equipment with a sputtering equipment manufacturer in the microelectronics industry. Using the commercial sputtering equipment, we deposited films with different variations of power, PO2, sputtering time, platen speed, etc. We then determined the combinations of sputtering conditions and post-sputtering treatments that yielded high-quality films without cracks or other significant defects. While thin films were deposited on cells as large as 10 cm by 10 cm, the processing was optimized using 4 cm by 4 cm cells. Cell performance was evaluated in stainless-steel test fixtures between 500 °C and 700 °C with hydrogen fuel fed to the anode and air fed to the cathode. Extensive studies allowed us to determine that modified cathode and cathode contact firing processes were required to achieve theoretical OCV. Moreover, use of the new firing processes resulted in the need for a modified cathode contact to achieve a low ASR. In summary, the project demonstrated the performance of high OCV (1.13 V at 650 °C) from sputtered layers and a low ASR (~0.25 Ohms-cm2 at 650 °C) resulting from a modification of cathode/contact processing and the introduction of alternative contact layers that are sufficient to yield a Gen-1 cell with a maximum power density of approximately 1.2 W/cm2. At an operating voltage of 0.74 V, this would yield a cell power density of ~1.1 W/cm2. While not utilized in this project, a Redox Gen-2 cell has a catalyst-infiltrated porous anode that reduces the ASR by more than 50% from that of the Gen-1 cells used in this project. Therefore, if the sputtered YSZ electron-blocking layer and GDC barrier layer are added to a Gen-2 half cell with a similar increase in OCV to the theoretical value of ~1.13 V at 650 °C, and if the same improvement in ASR (from that demonstrated in this project) is achieved when using the Gen-2 half-cell architecture as a sputtered cell substrate, then the power density at 0.74 Vop could be as high as ~2.6 W/cm2. The impact of such power density gains, while still maintaining high cell efficiency, and thus high system efficiency, is a dramatic decrease in system cost because the stack represents ~30-40% of the SOFC system cost.
Anode-supported SOFC button cells with LSCF-6428 cathodes were operated at various temperatures under constant current conditions for hundreds of hours in dry or humid (~3% water) cathode air while continuously collecting 1 hour XRD scans throughout the test duration. Additionally, one cell in dry air was held at OCV, and 12% CO2 was added to the humid air for another cell. Long cumulative XRD count times allowed minor phases in concentrations of less than 0.1 wt% to be identified. In humid air, cell performance increased during the first couple of hundred hours. XRD measured a gradual shift of Fe-rich Fe,Co spinel peaks to lower angles while post-mortem SEM discovered nano-nodules on the LSCF surfaces. When 12% CO2 was added to humid air, performance degradation was observed after the initial conditioning response, unlike in tests without CO2, which were stable after conditioning. XRD also measured a shift in the peaks of the major LSCF phase in the test with CO2 indicative of some degree of gradual decomposition. Cells tested at constant current in dry air exhibited fast initial degradation that decelerated over time, while the cell held at OCV maintained a stable voltage. XRD of the cathodes held at OCV at 750 °C and operated at constant current at 700 °C in dry air measured a slower shift of the Fe-rich spinel peaks to lower angles than was seen in tests in humid air, along with a shift in the peaks of a Co-rich Fe,Co spinel to higher angles. Post-mortem SEM of cells exposed to dry air discovered smaller nano-nodules on the LSCF surfaces than had been present in cells tested in humid air. Cells tested at constant current in dry air at 750 °C and 800 °C did not exhibit any gradual changes in the XRD patterns nor were nano-nodules discovered.
Present Li-ion battery (LIB) technology requires strong improvements in performance, energy capacity, charging-time, and cost to expand their application to e-mobility and grid storage. Li-metal is one of the most promising materials to replace commercial anodes such as graphite because of its 10 times higher specific capacity. However, Li-metal has high reactivity with commercial liquid electrolytes; thus, new solid materials are proposed to replace liquid electrolytes when Li-metal anodes are used. We present a theoretical analysis of the charging process in a full nanobattery, containing a LiCoO 2 cathode, a Li 7 P2S 8 I solid-state electrolyte (SSE), a Li-metal anode as well as Al and Cu collectors for the cathode and anode, respectively. In addition, we added a Li 3 P/Li 2 S film as a solid electrolyte interphase (SEI) layer between the Li-anode and SSE. Thus, we focus this study on the SEI and SSE. We simulated the charging of the nanobattery with an external voltage by applying an electric field. We estimated temperature profiles within the nanobattery and analyzed Li-ion transport through the SSE and SEI. Here, we observed a slight temperature rise at the SEI due to reactions forming $PS_{3}^{–}$ and $P_{2}S_{7}^{4}$$^{–}$ fragments at the interfaces; however, this temperature profile changes due to the charging current under the presence of the external electric field ε = 0.75 V Å –1 . Without the external field, the calculated open-circuit voltage (OCV) was 3.86 V for the battery, which is within the range of values of commercial cobalt-based LIBs. This voltage implies a spontaneous fall of available Li-ions from the anode to the cathode (during discharge). The charge of this nanobattery requires overcoming the OCV plus an additional voltage that determines the charging current. Thus, we applied an external potential able to neutralize the OCV, plus an additional 1.6 V to induce the transport of Li + from the cathode up to the anode. Several interesting details about Li + transport paths through the SSE and SEI are discussed.
Abstract A comprehensive investigation of PFSA membrane chemical degradation rates as a function of thickness (8-20 µm) is reported. The two-pronged study was conducted on bare membranes and as components of chemically-mitigated and mechanically-reinforced, state-of-the-art (SOA) membrane electrode assemblies (MEAs). The bare membranes were subjected to H2O2 vapor test and MEAs were degraded under OCV conditions, both at 90°C. Both test types employed fluoride release rates (FRR) to monitor chemical degradation rates. Vapor tests revealed that area-specific degradation rates were positively correlated with membrane thickness, but thickness normalized degradation rates were independent of thickness. Open-circuit voltage (OCV) investigations spanning the membrane thickness series of MEAs was probed via a 27-experiment 3(4-1) fractional factorial experimental design. Statistical analysis of the FRR values revealed that chemical degradation rates were dominated by the relative humidity value and that the area-specific degradation rates of MEAs were independent of membrane thickness. The OCV chemical durability insensitivity to membrane thickness is supported by on-load membrane chemical durability studies at the stack level. The results suggest that ,despite smaller ionomer inventory, SOA thin membranes and MEAs are not greatly disadvantaged relative to thicker membranes from a chemical durability perspective, provided oxidative stress levels are controlled throughout application lifetime.
The photoelectrochemical responses of a TiO 2 nanotube anode in ethylene glycol (EG), glycerol, ammonia, ethanol, urea, and Na 2 S electrolytes with different concentrations were investigated. The TiO 2 nanotube anode was highly efficient in photoelectrocatalysis in these solutions under UV light illumination. The photocurrent density is obviously affected by the concentration change. Na 2 S generated the highest photocurrent density at 0, 1, and 2 V bias voltages, but its concentration does not significantly affect the photocurrent density. Urea shows high open circuit voltage at proper concentration and low photocurrent at different concentrations. Externally applied bias voltage is also an important factor that changes the photoelectrochemical reaction process. In view of the open circuit voltage, EG, ammonia, and ethanol fuel cells show the trend that the open circuit voltage (OCV) increases with the increase of the concentration of the solutions. Glycerol has the highest OCV compared with others, and it deceases with the increase in the concentration because of the high viscosity. The OCV of the urea and Na 2 S solutions did not show obvious concentration effect.
This procedure provides instructions for performing inner containment vessel (ICV) and outer containment vessel (OCV) maintenance leakage rate testing on the following packaging seals and corresponding seal surfaces using a nondestructive helium(He) leak test: ICV upper main O-ring seal, ICV outer vent port plug O-ring seal, OCV upper main O-ring seal, and OCV vent port plug O-ring seal.
There is increasing interest in hydrogen-bromine fuel cells as both primary and regenerative energy storage systems. One promising design for a hydrogen-bromine fuel cell is a negative half cell having only a gas phase, which is separated by a cationic exchange membrane from a positive half cell having an aqueous electrolyte. The hydrogen gas and the aqueous bromide solution are stored external to the cell. In order to calculate the energy storage capacity and to predict and assess the performance of a single cell, the open circuit potential (OCV) must be estimated for different states of change, under various conditions. Theoretical expressions were derived to estimate the OCV of a hydrogen-bromine fuel cell. In these expressions temperature, hydrogen pressure, and bromine and hydrobromic acid concentrations were taken into consideration. Also included are the effects of the Nafion membrance separator and the various bromide complex species. Activity coefficients were taken into account in one of the expressions. The sensitivity of these parameters on the calculated OCV was studied.
Objective of this investigation is to provide the necessary inputs for a thermal model of the Li-ion battery for the Mars 2001 Lander. Two alternate configurations of this battery are under development: a) prismatic parallel plate, and b) cylindrical spiral wound. Required thermal inputs for both consist of the following: a) heat generation rates, b) thermal mass, and c) thermal conductivity. Thermal mass and conductivity were computed on the basis of known properties and configuration of the cell components. The heat generation rates were taken as the product of current and difference between open circuit voltage (OCV) and operating voltages (CCV) at a given state-of charge (SOC). Herein, it was assumed that the enthalpy voltage was equal to the OCV. OCV vs SOC data were obtained experimentally and CCV vs SOC were taken from previously obtained discharge data.
An expert system manages a power grid wherein charging stations are connected to the power grid, with electric vehicles connected to the charging stations, whereby the expert system selectively backfills power from connected electric vehicles to the power grid through a grid tie inverter (if present) within the charging stations. In more traditional usage, the expert system allows for electric vehicle charging, coupled with user preferences as to charge time, charge cost, and charging station capabilities, without exceeding the power grid capacity at any point. A robust yet accurate state of charge (SOC) calculation method is also presented, whereby initially an open circuit voltage (OCV) based on sampled battery voltages and currents is calculated, and then the SOC is obtained based on a mapping between a previously measured reference OCV (ROCV) and SOC. The OCV-SOC calculation method accommodates likely any battery type with any current profile.
The formation of the solid electrolyte interphase (SEI) in an ionic liquid electrolyte of 0.5 m lithium bis(fluorosulfonyl)imide (LiFSI) in 1-ethyl-3-methylimidazolium bis(fluorosulfonyl)imide at high cell voltages (1.7–1.9 V) is investigated in ordered mesoporous carbon (OMC) based Li metal cells using an operando small-angle neutron scattering (SANS) technique coupled with electrochemical impedance spectroscopy and ex situ X-ray photoelectron spectroscopy (XPS). It is demonstrated that discharging the OMC Li metal cells to ≈2 V and holding the cell voltage constant induces a rapid current increase with time, confirming extensive reduction and SEI formation. XPS analysis reveals that LiF is formed at open cell voltage (OCV), which is attributed to the carbenes generated at the lithium negative electrode because of its reaction with EMIm cation diffusing to and initiating the reaction with FSI - anions at the carbon positive electrode. It is confirmed that the chemical reaction at OCV and electrochemical reduction at high cell voltage of the FSI - anion plays a protective role against EMIm cation co-intercalation into the carbon positive electrode during the initial discharge. Operando SANS studies also suggest that slight differences occur in the surface composition and reaction mechanism as a function of cell voltage.
As the demand for high-performance and reliable energy storage devices continues to rise, identifying new anode materials is crucial for advancing Li-ion battery (LIB) technology. Inspired by recent experimental breakthroughs in synthesizing two-dimensional transition metal carbo-chalcogenides (2D-TMCCs), density functional theory calculations are performed to systematically explore their sulfide variants (TM 2 S 2 C) spanning all 3d transition metals in three possible phases. Through comprehensive evaluations of thermodynamic, dynamic, mechanical, and thermal stabilities, seven stable 2D-TMCC candidates are identified, four of which exhibit superior battery performance. Notably, V-based 2D-TMCCs across all three phases deliver moderate open-circuit voltages (OCV), efficient Li diffusion, and substantial capacities, making them promising candidates for industrial applications without requiring specific phase controls. A Cr-based 2D-TMCC (with sulfur atoms above carbon atoms) offers the highest capacity of 515.40 mAh g −1 , the lowest Li diffusion barrier, and an optimal OCV, highlighting its appealing potential as an anode material for LIBs. Furthermore, significant Li–Li spacing and pronounced electron delocalization in these four 2D-TMCCs suggest a reduced risk of dendrite formation. This work expands the 2D-TMCC family and identifies up-and-coming candidates for next-generation LIB anodes.