Physicochemical investigation of NiAl with small molybdenum additions
Specimens of four cast NiAl alloys, three of them containing 0.5, 1.0 and 1.5 at. % Mo., were homogenized for 10, 10, and 140 hr at 1373, 1523 and 1273 K, respectively, then kept at 1073, 1173 and 1323 K for 60, 120 and 3 hr, respectively, and quenched in icy water. The precipitation of a metastable Ni3Mo phase was observed at temperatures between 1073 and 1523 K. Molybdenum substituted for nickel was found to inhibit the lattice disordering in NiAl at 1073 and 1523 K.