Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “Ni superalloys”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 19 records

Development of a heterogeneous nanostructure through abnormal recrystallization of a nanotwinned Ni superalloy

This work explores the development of a heterogeneous nanostructured material through leveraging abnormal recrystallization, which is a prominent phenomenon in coarse-grained Ni-based superalloys. Additionally, through synthesis of a sputtered Inconel 725 film with a heterogeneous distribution of stored energy and subsequent aging treatments at 730°C, a unique combination of grain sizes and morphologies was observed throughout the thickness of the material. Three distinct domains are formed in the aged microstructure, where abnormally large grains are observed in-between a nanocrystalline and a nanotwinned region. In order to investigate the transitions towards a heterogeneous structure, crystallographic orientation and elemental mapping at interval aging times up to 8 h revealed the microstructural evolution and precipitation behavior. From the experimental observations and the detailed analysis of this study, the current methodology can be utilized to further expand the design space of current heterogeneous nanostructured materials.

36 MATERIALS SCIENCE↗

A defect-resistant Co–Ni superalloy for 3D printing

Abstract Additive manufacturing promises a major transformation of the production of high economic value metallic materials, enabling innovative, geometrically complex designs with minimal material waste. The overarching challenge is to design alloys that are compatible with the unique additive processing conditions while maintaining material properties sufficient for the challenging environments encountered in energy, space, and nuclear applications. Here we describe a class of high strength, defect-resistant 3D printable superalloys containing approximately equal parts of Co and Ni along with Al, Cr, Ta and W that possess strengths in excess of 1.1 GPa in as-printed and post-processed forms and tensile ductilities of greater than 13% at room temperature. These alloys are amenable to crack-free 3D printing via electron beam melting (EBM) with preheat as well as selective laser melting (SLM) with limited preheat. Alloy design principles are described along with the structure and properties of EBM and SLM CoNi-base materials.

36 MATERIALS SCIENCE↗

Characterization of Build Parameters and Microstructure in Low Heat Input WAAM of Ni-Based Superalloy Haynes 282

Ni-based superalloy Haynes® 282® is being targeted for various applications in advanced power generation systems for its superior fabricability, weldability, and excellent high temperature creep and corrosion performance. This process optimization study aims to use a low heat-input, high deposition rate, controlled Gas Metal Arc Welding (GMAW) process, Cold Metal Transfer (CMT) by Fronius, attempting to achieve fully dense fabrication and possibly avoid the need for HIP. Twenty-one multilayer blocks (~25x100x40 mm3) were deposited to explore a large set of build parameters variations that focused on varying the travel speed from 14 to 42 inches per minute (ipm) and wire feed speed from 150 to 450 ipm. A strong correlation has been observed between arc energy – controlled primarily by travel and wire feed speed. Initial visual inspection, internal microstructural examination, and computed tomography (CT) have been used to determine the effects of built parameters on evolution of internal porosity and defects. Scanning electron microscopy techniques enabled structural and compositional imaging of heterogeneity and changes in microstructural properties.

additive manufacturing↗

Characterization of Build Parameters and Microstructure in Low Heat Input WAAM of Ni-Based Superalloy Haynes 282

Ni-based superalloy Haynes® 282® is being targeted for various applications in advanced power generation systems for its superior fabricability, weldability, and excellent high temperature creep and corrosion performance. This process optimization study aims to use a low heat-input, high deposition rate, controlled Gas Metal Arc Welding (GMAW) process, Cold Metal Transfer (CMT) by Fronius, attempting to achieve fully dense fabrication and possibly avoid the need for HIP. Twenty-one multilayer blocks (~25x100x40 mm3) were deposited to explore a large set of build parameters variations that focused on varying the travel speed from 14 to 42 inches per minute (ipm) and wire feed speed from 150 to 450 ipm. A strong correlation has been observed between arc energy – controlled primarily by travel and wire feed speed. Initial visual inspection, internal microstructural examination, and computed tomography (CT) have been used to determine the effects of built parameters on evolution of internal porosity and defects. Scanning electron microscopy techniques enabled structural and compositional imaging of heterogeneity and changes in microstructural properties.

additive manufacturing↗

Effect of alloying elements on the $γ$’ antiphase boundary energy in Ni-base superalloys

Mechanical and fatigue performance of γ-γ' Ni-base superalloys are strongly affected by the antiphase boundary energy (APBE) of the γ' precipitates which, in turn, is dictated by the alloy's composition. Due to the multicomponent character of these alloys, establishing composition-APBE relationships are challenging, even though the qualitative effect of individual solutes on the APBE may be known. This work attempts to utilize density functional theory-based cluster expansion calculations to systematically assess the effect of composition on the APBE of the γ' phases in Ni-base superalloys. We aim to elucidate the influence of not only one single element but also multiple coexisting alloying elements on the γ' APBE. By explicit consideration of configurational disorder via Monte Carlo sampling, the effect of temperature on the APBE has also been analyzed. Overall, this work reveals that (1) effects of individual solute element M on the APBE energy obtained in an isolated, ternary condition (i.e. in Ni 3-x Al 1-y M x+y ) does not directly translate to a multi-solute case and that (2) the mutual synergistic interactions among different solute elements are not negligible. Based on the present results, an empirical master equation that predicts the APBE based on the composition of the γ' phases has been obtained.

36 MATERIALS SCIENCE↗

Understanding the deformation mechanisms in Ni-based superalloys with using crystal plasticity finite element method

Nl-based superalloy is considered as a good candidate due to its excellent resistance to elevated temperature deformation for long term period application. Understanding the deformation and failure mechanisms of Ni-Based superalloys is very helpful for providing design guidelines for processing Ni-based superalloys. Experimental characterization indicates that the deformation mechanisms of Ni based superalloy is strongly microstructure dependent. Besides, damage transform from the void nucleation to the macro cracks by voids growth leading to the failure of the Ni-based superalloys are also showing strong microstructure sensitivity. Therefore, this work focuses on the prediction and comprehension of the deformation and void growth behavior in Ni based superalloy at different working conditions via crystal plasticity finite element modeling and simulation. Physically based crystal plasticity frameworks were developed for newly Ni- based superalloy Haynes 282. It was found that dislocation shearing through the precipitates were acting as the main contributor to the strength of Haynes 282 at room temperature and 815°C. Our analysis of the creeping behavior of Haynes 282 exhibited that resistance of general climb replaced by the resistance induced by the deposited climb dislocation density. In addition, in the study of void growth behavior, our simulation results demonstrated that as the main loading axis perpendicular to the grain boundary (GB), voids grow more slowly on tilt GBs in bicrystals than those in single and bicrystals with twist GBs. And tilt GBs would promote the void grow into irregular shape.

36 MATERIALS SCIENCE↗

Multi-scale microstructural investigation of a laser 3D printed Ni-based superalloy

The heterogeneous microstructure of a laser 3D printed Ni-based superalloy was examined at multiple length scales. The sub-millimeter-sized columnar crystal grains are composed of micron-sized cellular colonies. The crystal grains grow in epitaxy with the substrate under the large temperature gradient and high cooling rate. The cell boundaries, decorated with γ/γ' eutectics, μ-phase precipitates and high density of dislocations, show enrichment of γ' forming elements and low-angle misorientations. Dislocations trapped in the intra-cellular regions are characterized as statistically stored dislocations with no detectable contribution to lattice curvature, and are the results of the interaction between dislocations and γ' precipitates.

36 MATERIALS SCIENCE↗

Machine Learning Enhanced Development of Functionally Graded Materials Enabled by Directed Energy Deposition

The ability to functionally grade materials provides designers with a new dimension of design flexibility that can be leveraged to improve functionality, reduce cost, or improve efficiency in a wide range of applications. This program was specifically focused on FGMs for hot and harsh gas path environments. These environments are common for the hot sections of jet engines and gas turbines, where parts undergo high temperature and mechanical loads in a corrosive environment. Expensive high γ' strengthened Ni superalloys such as René 41 (R41) and René 80 (R80) are generally used exclusively for a whole part, although only a section of the part demands such superalloys. To minimize cost, low/no γ' strengthened Ni superalloys such as Inconel 718 (INC718) could be used at less-demanding sections of the part could be welded to the high γ' strengthened Ni superalloys. However, the welding typically is a failure site due to the low durability at the welding interface. Functionally grading provides a welding alternative that can allow cost reduction without sacrificing mechanical performance.

32 ENERGY CONSERVATION, CONSUMPTION, AND UTILIZATI↗

Design and development of a high-performance Ni-based superalloy WSU 150 for additive manufacturing

This work proposes a design and development strategy of a new nickel-based superalloy for additive manufacturing. A new Ni-based superalloy has been developed by the application of the combinatorial alloy development technique coupled with CALPHAD based solidification modeling by effectively suppressing the precipitation kinetics. The suppression of precipitation during processing paved a way for prevention of cracks during deposition. The new alloy "WSU 150" revealed excellent room temperature mechanical properties with a yield strength of 867 MPa, an ultimate tensile strength of 1188 MPa, and an elongation of 27.9% in the as-deposited condition. The mechanical properties of the heat-treated alloy were improved significantly to 1114 MPa yield strength, 1396 MPa ultimate tensile strength, and an elongation of 16.1%. Improvement in the mechanical properties is attributed to the additional precipitation and coarsening of γ' and carbides during heat-treatment. Microstructural investigation of the alloy revealed spherical γ' with a rippled size distribution from the center to the interdendritic region. The average size of the γ' particles in the as-deposited condition was found to be around 48 nm in the interdendritic region. Heat-treatment promoted the coarsening of γ' which is explained in the paper.

36 MATERIALS SCIENCE↗

Quantification of room temperature strengthening of laser shock peened Ni-based superalloy using synchrotron microdiffraction

Laser shock peening (LSP), a surface modification technique, is promising to enhance the strength and wear resistance for Ni-based superalloys. To understand the strengthening mechanism in a laser shock peened Ni-based superalloy DZ417G, we utilize synchrotron poly- and monochromatic X-ray microdiffraction, as well as electron microscopy and microhardness to quantify the local microstructures and mechanical properties at various depths. In the 1.2-mm-deep hardened layer, the microhardness increases monotonically by ~50% from the unaffected interior to the surface. Quantitative microdiffraction analysis shows that large amounts of dislocations are introduced by LSP. High densities of 7.1 × 10 15 m -2 and 11.8 × 10 15 m -2 are seen close to the peened surface for the γ- and γ'-phases, respectively, which are 5 and 20 times of those in the unaffected region. Different gradients of dislocation density are observed for the two phases from interior to surface, and their combined effect accounts well for the hardness increment. Due to the unaltered γ'-precipitates and chemical composition in the LSP affected zone, the large density of dislocations dominates the observed strengthening. Combined poly- and monochromatic X-ray microdiffraction allows quantifying the local microstructures of plastic deformation over a large sampling scale that can hardly be achieved using other materials characterization techniques.

36 MATERIALS SCIENCE↗

A transport-based framework for solidification cracking in Ni-based superalloys processed by laser powder bed fusion

Solidification cracking remains a persistent barrier to laser powder bed fusion (LPBF) processing of solid-solution-strengthened (SSS) Ni-based superalloys and is commonly attributed to carbide formation, liquation-type failure, or elemental segregation. In this work, the cracking behavior of three SSS Ni-based superalloys—Inconel 625 (625), Inconel 617 (617), and Haynes 230 (230)—is examined under comparable LPBF conditions to evaluate the origins of their cracking susceptibility. Carbides were present in both 625 and 230, yet cracking behavior differed significantly. MC-type carbides in 625 remain discrete and preserve liquid connectivity, whereas Cr-rich M23C6 carbides in 230 form at cellular triple junctions that bottleneck the interdendritic liquid network, influencing cracking through liquid connectivity rather than as an independent cause. Alloy 617 exhibited anomalous segregation without resolvable secondary phases yet cracked mildly, indicating that extensive carbide formation is not a prerequisite for cracking. To rationalize these observations, a transport-limited framework is proposed in which cracking occurs when terminal-liquid feeding cannot accommodate solidification-induced strain; among the mechanisms evaluated, this framework is most consistent with the physical constraints imposed by LPBF solidification. Transport-based crack-susceptibility indexes incorporating permeability, viscosity, and solidification kinetics distinguish the alloy hierarchy; permeability ratios Krat increased from approximately 7 (625) to 11.5 (617) and 14.5 (230), with corresponding increases in the μ-weighted mushy zone risk index (CSIMZRM). These results are consistent with transport-limited liquid feeding as a rate-limiting contributor to solidification cracking in LPBF-processed SSS Ni-based superalloys, providing a physically grounded basis for alloy and process design.

Hyer, Holden [ORNL] (ORCID:0000000343915561)↗

Employing sequential experiments to gain insights on the interaction between creep and fatigue damage in Ni‐base superalloys

Abstract The interaction between creep and fatigue damage in Ni‐base superalloy CMSX‐8 was explored using a sequential workflow that decouples creep and fatigue steps to quantify how accumulated creep damage interacts with subsequent isothermal low‐cycle fatigue (LCF) and vice versa. Two workflows were considered: creep followed by LCF and LCF followed by creep. For the first workflow, the subsequent LCF was evaluated at temperatures of 20°C, 750°C, and 1100°C. It was found that the extent of deleterious interaction of prior creep on LCF depended on increasing subsequent fatigue test temperature. For the LCF followed by creep, fatigue tests were first conducted at 20°C and 1100°C to 60% of life, and then creep was conducted at 800°C, where primary creep is promoted, or 900°C, where primary creep is absent. LCF damage accumulated at 1100°C accelerated creep and decreased ductility, while fatigue damage at room temperature had minimal effect on the creep behavior.

Gorgannejad, Sanam↗

Process-Microstructure-Property Relationships in Low Heat Input Wire-Arc Additive Manufacturing (WAAM) of Ni-Based Superalloy Haynes 282

Conference presentation on WAAM process optimization on Ni-based superalloy Haynes® 282®. This alloy is targeted for advanced power generation systems for its superior high temperature mechanical properties. Wire-arc additive manufacturing (WAAM) offers attractive cost and materials savings with high deposition rates. Based on initial build process optimization, WAAM blocks were made, and screened for defects using high-throughput CT scanning. The microstructural evolution in arc energy range of 250-700 J/mm was characterized in the as-built and aged conditions, using electron microscopy. Results showed self-consistent microstructure across conditions, with grain size dependence on arc energy, MC and M6C carbides in as-built, and blocky grain boundary M23C6 in as-heat-treated condition. Further reductions in as-built porosity were explored through 20+ combinations of H2 and CO2 additions to shielding gas. Initial results show improved wetting behavior, and bead overlap with up to 1% H2 and up to 0.25% CO2. Combination of experimentally determined datasets provided comprehensive understanding of process-structure-property relationships in WAAM Haynes 282.

Haynes 282↗

Science-Based Acceleration of the Full Value Stream for Metal Additive Manufacturing: Expedited Powder Development and Additive Manufacturing Deployment in the Areas of Ni-Base Superalloy and Custom Alloy Powders for AM (Final Report)

The overall Science-based Acceleration of the Full Value Stream for Metal Additive Manufacturing (AM): Expedited Powder Development and Additive Manufacturing Deployment (“X-P4AM”) project objective is to drastically reduce the time-to-market barriers for new additive alloys of interest in automotive and aerospace applications, through computational alloy design with rapid screening and down- selection via synthesis of candidate alloys with rapid solidification. The project will also refine the technology in high pressure gas atomization to improve the production of commercial quantities of selected powders with high powder yields and enhanced powder quality. Production of modified nickel-based superalloys and a Ni-containing alloy based on a high entropy composition, enhanced powder production methods, and optimized AM build parameterization provided critical steps in widespread adoption of AM technology for aerospace applications, in this case. The individual backgrounds and capabilities of the Parties are ideally suited to the successful execution of this work. The included work enhanced the Contractors’ AM capabilities, a core competency of the Contractors, and develop a close working relationship with the Participant in the area of nickel-based powder superalloys and custom alloys and their end use.

36 MATERIALS SCIENCE↗

Science-Based Acceleration of the Full Value Stream for Metal Additive Manufacturing: Expedited Powder Development and Additive Manufacturing Deployment in the Areas of Ni-Base Superalloy and Custom Alloy Powders for AM

The overall Science-based Acceleration of the Full Value Stream for Metal Additive Manufacturing (AM): Expedited Powder Development and Additive Manufacturing Deployment (“X-P4AM”) project objective is to drastically reduce the time-to-market barriers for new additive alloys of interest in automotive and aerospace applications, through computational alloy design with rapid screening and down- selection via synthesis of candidate alloys with rapid solidification. The project will also refine the technology in high pressure gas atomization to improve the production of commercial quantities of selected powders with high powder yields and enhanced powder quality. Production of modified nickel-based superalloys and a Ni-containing alloy based on a high entropy composition, enhanced powder production methods, and optimized AM build parameterization provided critical steps in widespread adoption of AM technology for aerospace applications, in this case. The individual backgrounds and capabilities of the Parties are ideally suited to the successful execution of this work. The included work enhanced the Contractors’ AM capabilities, a core competency of the Contractors, and develop a close working relationship with the Participant in the areas of nickel-based powder superalloys and custom alloys and their end use.

36 MATERIALS SCIENCE↗

Science-Based Acceleration of the Full Value Stream for Metal Additive Manufacturing: Expedited Powder Development and Additive Manufacturing Deployment in the Areas of Ni-Base Superalloy and Custom Alloy Powders for AM

The overall Science-based Acceleration of the Full Value Stream for Metal Additive Manufacturing (AM): Expedited Powder Development and Additive Manufacturing Deployment (“X-P4AM”) project objective is to drastically reduce the time-to-market barriers for new additive alloys of interest in automotive and aerospace applications, through computational alloy design with rapid screening and down- selection via synthesis of candidate alloys with rapid solidification. The project will also refine the technology in high pressure gas atomization to improve the production of commercial quantities of selected powders with high powder yields and enhanced powder quality. Production of modified nickel-based superalloys and a Ni-containing alloy based on a high entropy composition, enhanced powder production methods, and optimized AM build parameterization provided critical steps in widespread adoption of AM technology for aerospace applications, in this case. The individual backgrounds and capabilities of the Parties are ideally suited to the successful execution of this work. The included work enhanced the Contractors’ AM capabilities, a core competency of the Contractors, and develop a close working relationship with the Participant in the areas of nickel-based powder superalloys and custom alloys and their end use.

36 MATERIALS SCIENCE↗

Creep resistant Ni-based superalloy casting and method of manufacture for advanced high-temperature applications

One or more embodiments relates to a method of casting a creep-resistant Ni-based superalloy and a homogenization heat treatment for the alloy. The method includes forming a feed stock having Nickel (Ni) and at least one of Chromium (Cr), Cobalt (Co), Aluminum (Al), Titanium (Ti), Niobium (Nb), Iron (Fe), Carbon (C), Manganese (Mn), Molybdenum (Mo), Silicon (Si), Copper (Cu), Phosphorus (P), Sulfur (S) and Boron (B). The method further includes fabricating the creep-resistant Ni-based superalloy in a predetermined shape using the feed stock and at least one process such as vacuum induction melting (VIM), electroslag remelting (ESR) and/or vacuum arc remelting (VAR).

Jablonski, Paul D.↗