Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “Na metal battery”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 19 records

Superior metal storage behavior of Zn-containing porous carbon nanostructures for Na and Li metal batteries

Na and Li metals are ideal anodes for high-energy rechargeable batteries. However, their poor coulombic efficiency and the associated safety issues due to dendritic metal deposition and large volume changes during metallic plating/stripping are the major causes that persistently hinder their practical energy-storage applications. Herein, Zn-containing carbon nanostructures derived from typical zeolitic imidazolate framework-8 (ZIF-8) are proposed as advanced metal anode materials for both Na and Li metal batteries. In this study; the three-dimensional interconnected porous surfaces confine metallic Na and Li within the nanostructures, filling the carbon scaffold, and covering the electrode surface to form stable solid electrolyte interphases. Based on the metal nucleation and growth results obtained through various electrochemical tests, Zn incorporation and pore morphology have been revealed to be the key factors that regulate the metal nucleation and metallic plating/stripping during cycling. Thus, the incorporation of Zn in the closed pores of a carbon nanostructure improves the cycle performance, even in carbonate electrolytes, and produces stable Na and Li metallic anodes for next-generation rechargeable batteries.

25 ENERGY STORAGE↗

Metallic Cu Surface Enables Reversible Na Metal Anodes and Stabilizes Anode-Free Sodium Metal Batteries

Anode free Na metal batteries are promising for future energy storage because they not only provide the highest energy densities but also eliminate the need of handling hazardous Na metals during battery manufacturing. However, they suffer from much faster degradation due to strong sensitivities even to trace levels of side reactions. In view of the crucial roles of surface chemistry on modulating electrochemical plating, this work systematically investigated a series of Cu surfaces for Na plating and stripping in the 1.0 M NaPF 6 diglyme electrolyte. Our results suggest that Na plating and stripping on pure Cu surface without Cu oxide species exhibits much better reversibility and smaller overpotentials across a wide range of current densities, especially for the first plating/stripping cycle. The high performance includes consistently higher than 99.8% Faradaic efficiencies, much more stable interfacial resistance, and negligible formation of mossy Na after 500 cycles. This improved performance can be explained based on the stronger Na-Cu affinity compared with the Na-CuO affinity. Anode-free Na metal batteries equipped with high-capacity sodium vanadium phosphate cathodes and pure Cu current collector exhibited at least 70% capacity retention for 100 cycles.

Electrochemistry↗

Directing High-Efficiency Na Plating with Carbon–Aluminum Junction Interfaces for Anode-Free Na Metal Batteries

Anode-free sodium metal batteries are highly promising for future energy storage but suffer from much faster cycling degradation as they are sensitive to even trace levels of irreversible side reactions. This work focuses on the most practical Al foil current collectors and systematically examined the effect of nano-sized carbon coating on improving the Na plating and stripping stability. We identified that the carbon-Al junction interface generated by carbon coating enabled more uniform Na depositing with lower overpotentials, delivering higher than 99.8% Faradaic efficiencies for a wide range of cycling currents between 0.5 and 3.0 mA cm -2 . This performance is much better than the 96.4% efficiency observed on uncoated Al foils under the same conditions, and was also confirmed under lean electrolyte and freezing electrolyte conditions, and can be attributed to the stronger interfacial binding and enhanced sodiophilic properties of the carbon-aluminum junction sites. Furthermore, these sites not only ensure uniform Na plating but also eliminates side reactions that would otherwise cause electrolyte depletion. As a result, Na-metal free full cells assembled with high capacity Na 3 V 2 (PO 4 ) 3 cathode delivered ~ 85% capacity retention for 100 cycles, higher than the 73% of retention of uncoated Al foil.

25 ENERGY STORAGE↗

Synergetic Dual‐Additive Electrolyte Enables Highly Stable Performance in Sodium Metal Batteries

Sodium (Na)-metal batteries (SMBs) are considered one of the most promising candidates for the large-scale energy storage market owing to their high theoretical capacity (1,166 mAh g -1 ) and the abundance of Na raw material. However, the limited stability of electrolytes still hindered the application of SMBs. Herein, sulfolane (Sul) and vinylene carbonate (VC) are identified as effective dual additives that can largely stabilize propylene carbonate (PC)-based electrolytes, prevent dendrite growth, and extend the cycle life of SMBs. The cycling stability of the Na/NaNi 0.68 Mn 0.22 Co 0.1 O 2 (NaNMC) cell with this dual-additive electrolyte is remarkably enhanced, with a capacity retention of 94% and a Coulombic efficiency (CE) of 99.9% over 600 cycles at a 5 C (750 mA g -1 ) rate. The superior cycling performance of the cells can be attributed to the homogenous, dense, and thin hybrid solid electrolyte interphase consisting of F- and S-containing species on the surface of both the Na metal anode and the NaNMC cathode by adding dual additives. Such unique interphases can effectively facilitate Na-ion transport kinetics and avoid electrolyte depletion during repeated cycling at a very high rate of 5 C. This electrolyte design is believed to result in further improvements in the performance of SMBs.

25 ENERGY STORAGE↗

Heterogeneous Solid Electrolyte Interphase Interactions Dictate Interface Instability in Sodium Metal Electrodes

Sodium (Na) metal batteries have attracted recent attention due to their low cost and high abundance of Na. However, the advancement of Na metal batteries is impeded due to key challenges such as dendrite growth, solid electrolyte interphase (SEI) fracture, and low Coulombic efficiency. This study examines the coupled electro‐chemo‐mechanical interactions governing the electrodeposition stability and morphological evolution at the Na/electrolyte interface. The SEI heterogeneities influence transport and reaction kinetics leading to the formation of current and stress hotspots during Na plating. Further, it is demonstrated that the heterogeneity‐induced Na metal evolution and its influence on the stress distribution critically affect the mechanical overpotential, contributing to a faster SEI failure. The analysis reveals three distinct failure mechanisms—mechanical, transport, and kinetic—that govern the onset of instabilities at the interface. Finally, a comprehensive comparative study of SEI failure in Na and lithium (Li) metal anodes illustrates that the electrochemical and mechanical characteristics of the SEI are crucial in tailoring the anode morphology and interface stability. This work delineates mechanistic stability regimes cognizant of the SEI attributes and underlying failure modes and offers important guidelines for the design of artificial SEI layers for stable Na metal electrodes.

25 ENERGY STORAGE↗

Solvent-free and low temperature synthesis of chalcogenide Na superionic conductors for solid-state batteries

Sodium chalcogenide ionic conductors are attractive candidates as solid electrolytes (SEs) in solid-state Na metal batteries. They show the advantages of high ionic conductivity of 10 –4 –10 –2 S cm –1 at room temperature and great chemical stability in air. However, simple, efficient, and scalable approaches for the synthesis of chalcogenide solid electrolytes (SEs) are required. In this work, we report a solvent-free mixing to form dry intermediate products, which are subjected to different treatments (electron-beam assisted method or low temperature heating (≤150 °C)) to produce pure phase of Na 3 SbS 4-y Se y (0 ≤ y < 2) chalcogenides. Heavy Se-doping in Na 3 SbS 4 results in the tetragonal-to-cubic phase transition as well as a significant change of Sb-S bonding in Raman spectra. Among all chalcogenide SEs, Na 3 SbS 3 Se showed the highest ionic conductivity of 3.75 × 10 –4 S cm –1 at room temperature, 47% higher than that of pristine Na 3 SbS 4 . Moreover, the Se-dopant also enhanced the electrochemical stability towards Na metal in solid-state batteries. The solid-state Na||FeS 2 battery with Na 3 SbS 3 Se SE displayed long-term cycling ability up to 1,000 cycles within the voltage window of 1.0–2.7 V and retained a specific capacity of 105 mAh g –1 after 600 cycles. As a result, this technique promotes the practical applications of chalcogenide SEs in solid-state batteries.

25 ENERGY STORAGE↗

Chemo‐Mechanics Interplay Dictates Interface Instability and Asymmetry in Plating and Stripping of Sodium Metal Electrodes

Abstract The development of practical sodium (Na) metal batteries is hindered by key challenges including dendrite growth, dead metal formation, and unstable solid electrolyte interphase (SEI) growth. A fundamental understanding of the chemo‐mechanical interactions at the Na/SEI interface is critical for designing stable Na metal electrodes. In this work, the coupled electrochemical‐mechanical processes governing the morphological evolution and stability of Na metal during plating and stripping are investigated. The heterogeneous nature of transport and morphological interactions at the Na/SEI interface is revealed to result in nonuniform mechanical overpotentials and reaction fronts, eventually leading to Na filaments or pits. The spatio‐temporal evolution of stress heterogeneities during Na plating and stripping is shown to be asymmetric, manifesting in varying morphological nonuniformities and instability modes. The crucial role of external pressure in modulating the electrochemical‐transport interactions, the mechanical response of Na, and the localized reaction currents and stresses at the Na/SEI interface is demonstrated. At different external pressure conditions, the correlation between transport heterogeneities in the SEI and the onset and propagation of interface instability has been delineated. This work highlights the need for synergistic tailoring of external pressure and SEI heterogeneity toward achieving stable electrodeposition and dissolution in Na metal electrodes.

Singla, Aditya [School of Mechanical Engineering P↗

In situ probing the origin of interfacial instability of Na metal anode

The unstable and fragile solid electrolyte interphase (SEI) has restricted the application of Na metal anodes. Despite numerous research efforts being put into understanding its chemical composition and physical properties, direct observation of its formation remains a challenge due to the lack of temporal and spatial resolution. Here, through combined in situ probing techniques, we exhibit two pivotal stages associated with SEI instability during the often -neglected formation process. It is revealed that Na metal that is not uniformly passivated at the initial (passivating) stage will trigger unrestricted electrolyte decomposition and homogeneous components distribution during the subsequent (growing) stage. SEI with homogenously distributed components is found to have higher solubility than that with a layered structure evolved from a compact passivation layer. Furthermore, through demonstrating an SEI dissolution model that is closely related to its formation process and compositional distribution, this work sheds light on an uncharted territory of Na metal batteries.

25 ENERGY STORAGE↗

Highly efficient interface stabilization for ambient-temperature quasi-solid-state sodium metal batteries

Solid-state sodium (Na) batteries (SSSBs) using sulfide-based solid electrolytes (SSEs) hold tremendous promise due to their high theoretical specific capacity, enhanced safety and abundant resources. However, detrimental interfacial issues between SSEs and Na metal present a major challenge to the advancement of sulfide-based SSSBs. To address interfacial issues, we demonstrate an efficient approach by incorporating an ionic liquid electrolyte ((PYR/Na)TFSI) as interlayer to stabilize the Na metal/SSE interface. The presence of the (PYR/Na)TFSI interlayer enables the formation of a stable solid electrolyte interphase (SEI) to prevent the harmful reactions and inhibit Na dendrites. Combination of ab initio molecular dynamics simulations and X-ray photoelectron spectroscopy revealed that this stable SEI is largely composed of reduced products of TFSI -, such as NaF and CF 3 . As a result, the symmetric cells exhibited stable Na plating/striping cycling for 300 h at 0.1 mA cm -2 . In addition, FeS2||Na quasi-solid-state batteries delivered an impressive specific capacity of over 300 mAh g -1 under the current density of 20 mA g -1 at room temperature. Under a higher current density (100 mA g -1 ), such batteries performed with long-term cycling stability and maintained a specific capacity of around 103 mAh g -1 after 330 cycles. This work demonstrates the novel perspective of using an ionic liquid interlayer to address interfacial issues, contributing to the advancement of high-performance SSSBs for the next-generation energy storage systems.

25 ENERGY STORAGE↗

Understanding ion-selective Li/Na metal plating behavior in hybrid Li-Na battery

This study investigates ion-selective Li/Na metal plating behavior in hybrid Li-Na battery systems, revealing the critical role of electrolyte solvents in these processes. Using a hybrid battery design with a LiFePO 4 cathode, Na metal anode, and NaPF 6 -based electrolytes, we observed contrasting effects of carbonate- and ether-based electrolyte solvents. While ether-based electrolytes showed expected Na plating/stripping, carbonate-based electrolytes surprisingly favored a Li-dominant plating/stripping reaction despite the Na-rich environment. X-ray photoelectron spectroscopy revealed that this selectivity is linked to the composition of the solid electrolyte interphase (SEI) layer, with carbonate electrolytes forming Li-based inorganic-rich SEI layers that facilitate Li-ion diffusion while screening Na ions. In conclusion, these findings challenge the conventional understanding of metal plating in multi-ion environments and offer insights for designing future hybrid battery systems.

25 ENERGY STORAGE↗

Probing Operando Electrochemical Strain Generation in α-NaFeO 2 Composite Cathodes during Cycling of Na-Ion Batteries

The transition metal oxide (TMO) cathodes in Na-ion batteries suffer from low-capacity retention. Chemo-mechanical instabilities lead to the deterioration of the electrochemical performance of TMO cathodes in Li-ion batteries. However, there is not much known about the chemo-mechanical instabilities in the TMO cathodes for Na-ion batteries. Understanding the governing forces behind the interplay between the electrochemical performance and mechanical stability in TMO cathodes is critical for the development of Na-ion batteries. Here, we synchronize the digital image correlation (DIC) technique with electrochemical analysis to capture the real-time deformation behavior of the α-NaFeO 2 cathodes during cycling. When the charge cutoff voltage is 3.6 V, the cathode experiences reversible deformations (except for the first cycle). There is negative strain (shrinkage) generation during Na extraction and positive strain (expansion) generation during the subsequent Na insertion. A detailed analysis of the potential-dependent strain rate evolution points out complicated phase transformations and nonequilibrium conditions in the α-NaFeO 2 cathodes during cycling. When the charge cutoff voltage was increased to 4.2 V, there was a rapid capacity loss and large plastic deformations in the α-NaFeO 2 cathodes. We provide an in-depth discussion about the possible mechanisms behind the chemo-mechanical instabilities in the α-NaFeO 2 . In conclusion, the correlation is critical to develop material-based strategies to mitigate instability mechanisms in TMO cathodes for Na-ion batteries.

Wable, Minal [University of Maryland Baltimore Cou↗

Intermetallics Based on Sodium Chalcogenides Promote Stable Electrodeposition–Electrodissolution of Sodium Metal Anodes

Sodiophilic micro-composite films of sodium-chalcogenide intermetallics (Na 2 Te and Na 2 S) and Cu particles are fabricated onto commercial copper foam current collectors (Na 2 Te@CF and Na 2 S@CF). For the first time a controllable capacity thermal infusion process is demonstrated. Enhanced wetting by the metal electrodeposition leads to state-of-the-art electrochemical performance. For example, Na 2 Te@CF-based half-cells demonstrate stable cycling at 6 mA cm -2 and 6 mAh cm -2 , corresponding to 54 µm of Na electrodeposited/electrodissolved by geometric area. Sodium metal batteries with Na 3 V 2 (PO 4 ) 3 cathodes are stable at 30C (7 mA cm -2 ) and for 10 000 cycles at 5C and 10C. Cross-sectional cryogenic focused ion beam (cryo-FIB) microscopy details deposited and remnant dissolved microstructures. Sodium metal electrodeposition onto Na 2 Te@CF is dense, smooth, and free of dendrites or pores. On unmodified copper foam, sodium grows in a filament-like manner, not requiring cycling to achieve this geometry. Substrate–metal interaction critically affects the metal–electrolyte interface, namely the thickness and morphology of the solid electrolyte interphase. Density functional theory and mesoscale simulations provide insight into support-adatom energetics, nucleation response, and early-stage morphological evolution. On Na 2 Te sodium atomic dispersion is thermodynamically more stable than isolated clusters, leading to conformal adatom coverage of the surface.

36 MATERIALS SCIENCE↗

Elastic NaxMoS2-carbon-BASE triple interface direct robust solid-solid interface for all-solid-state Na-S batteries

The promises of all-solid-state (ASS) sodium batteries for the next generation energy storage are widely recognized but their developments have been severely constrained by the difficulties to design favorable solid-solid interfaces for unhindered Na-ion transport. Using the most promising ß?-Al2O3 solid state electrolyte (BASE) as a platform, we demonstrate here a triple nanojunction strategy that provides simultaneous strong Na adhesion and continuous Na-ions diffusion at solid-solid interface. Such triple junctions (NaxMoS2-carbon-BASE) were constructed by adhering ternary composite Na anodes containing dispersed 3 wt% MoS2 and 3 wt% carbon on BASE, and provide nearly complete adhesion of Na on BASE with a much smaller contact angle (~ 45o vs. 120o of pristine Na). The composite Na anodes exhibited ~ 3 times improved elastic property and the synergy of NaxMoS2 and carbon provides the required ionic and electronic diffusion channels at solid-solid interface, which significantly improve Na utilization and resist premature failure due to loss of solid-solid contact as Na shrink during high capacity stripping. As a result, Na metal at the triple junction exhibited more than five time reduced charge transfer resistance and at least 200 hours stable battery cycling at practical current densities. The novel anode architecture also enabled high capacity cycling of prototype ASS sodium sulfur batteries when coupled with advanced sulfur cathodes containing intrinsic Na-ions diffusion channels and redox catalytic mediators, leading to stable cycling with specific capacity of 1110 mAh g-1.

ß”-Al2O3 solid electrolyte, solid state batteries,↗

Stabilizing Metallic Na Anodes via Sodiophilicity Regulation: A Review

This review focuses on the Na wetting challenges and relevant strategies regarding stabilizing sodium-metal anodes in sodium-metal batteries (SMBs). The Na anode is the essential component of three key energy storage systems, including molten SMBs (i.e., intermediate-temperature Na-S and ZEBRA batteries), all-solid-state SMBs, and conventional SMBs using liquid electrolytes. We begin with a general description of issues encountered by different SMB systems and point out the common challenge in Na wetting. We detail the emerging strategies of improving Na wettability and stabilizing Na metal anodes for the three types of batteries, with the emphasis on discussing various types of tactics developed for SMBs using liquid electrolytes. We conclude with a discussion of the overlooked yet critical aspects (Na metal utilization, N/P ratio, critical current density, etc.) in the existing strategies for an individual battery system and propose promising areas (anolyte incorporation and catholyte modifications for lower-temperature molten SMBs, cell evaluation under practically relevant current density and areal capacity, etc.) that we believe to be the most urgent for further pursuit. Comprehensive investigations combining complementary post-mortem, in situ, and operando analyses to elucidate cell-level structure-performance relations are advocated.

25 ENERGY STORAGE↗

Non-fluorinated electrolyte for high-voltage anode-free sodium metal battery

Abundant sodium (Na) batteries are a sustainable alternative to resource-constrained lithium-ion batteries, offering huge cost advantages. However, developing high-voltage anode-free sodium metal batteries (SMBs) to narrow the energy density gap with lithium-ion batteries is hindered by a critical challenge: existing electrolytes cannot simultaneously achieve ultra-high Na coulombic efficiency and anodic stability. Here, in this study, we present a rationally designed non-fluorinated electrolyte (1.0 M NaPF 6 in 1,2-diethoxyethane/1,2-di-tert-butoxyethane) to address this key limitation, achieving Na coulombic efficiency of >99.95% and anodic stability of >4.8 V. For coin cells (2.0 mAh cm −2 , N/P = 1.7), our electrolyte design enables 4.0 V Na | |Na 3 V 2 (PO 4 ) 3 (NVP) at 5 C and 4.3 V Na | |NaNi 0.6 Mn 0.2 Co 0.2 O 2 (NMC622) at 0.3 C for 5,000 and 500 cycles with a capacity retention >80%. Remarkably, the 50 mAh anode-free pouch cells 4.0 V Al | |NVP and 4.3 V Al | |NMC622 also achieve 500 and 300 cycles (retention >75%) with a specific energy of >360 Wh kg (electrode) −1 . This work focuses on electrolyte optimization and conceptual advances, whereas critical aspects such as safety, large-scale manufacturability and practical feasibility of SMBs require further investigation. The electrolyte design using non-fluorinated solvents enhances the anodic stability without sacrificing Na efficiency, laying groundwork for advancing low-cost, high-energy SMBs and supporting the transition to sustainable battery technologies.

25 ENERGY STORAGE↗

Making Plasticized Polymer Electrolytes Stable Against Sodium Metal for High‐Energy Solid‐State Sodium Batteries

Solid polymer electrolytes based on plastic crystals are promising for solid-state sodium metal (Na 0 ) batteries, yet their practicality has been hindered by the notorious Na 0 -electrolyte interface instability issue, the underlying cause of which remains poorly understood. Here, in this study, by leveraging a model plasticized polymer electrolyte based on conventional succinonitrile plastic crystals, we uncover its failure origin in Na 0 batteries is associated with the formation of a thick and non-uniform solid electrolyte interphase (SEI) and whiskery Na 0 nucleation/growth. Furthermore, we design a new additive-embedded plasticized polymer electrolyte to manipulate the Na 0 deposition and SEI formulation. For the first time, we demonstrate that introducing fluoroethylene carbonate (FEC) additive into the succinonitrile-plasticized polymer electrolyte can effectively protect Na 0 against interfacial corrosion by facilitating the growth of dome-like Na 0 with thin, amorphous, and fluorine-rich SEIs, thus enabling significantly improved performances of Na//Na symmetric cells (1,800 h at 0.5 mA cm −2 ) and Na//Na 3 V 2 (PO 4 ) 3 full cells (93.0 % capacity retention after 1,200 cycles at 1 C rate in coin cells and 93.1 % capacity retention after 250 cycles at C/3 in pouch cells at room temperature). Our work provides valuable insights into the interfacial failure of plasticized polymer electrolytes and offers a promising solution to resolving the interfacial instability issue.

25 ENERGY STORAGE↗