Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “NATURAL RUBBER”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 19 records

Friction characteristics of three 30 by 11.5-14.5, type 8, aircraft tires with various tread groove patterns and rubber compounds

A test program was conducted to evaluate friction performance and wear characteristics on wet runways of three 30 x 11.5-14.5, type, aircraft tires having two different tread patterns and natural rubber contents. All test tires had the standard three circumferential groove tread, but two had molded transverse grooves which extended from shoulder to shoulder. The tread rubber content of the two tires with transverse grooves differed in that one had a 100 percent natural rubber tread and the other had a rubber tread composition that was 30 percent synthetic and 70 percent natural. The third test tire had the conventional 100 percent natural rubber tread. Results indicate that the differences in tire tread design and rubber composition do not significantly affect braking and cornering friction capability on wet or dry surfaces. Braking performance of the tires decreases with increased speed, with increased yaw angle and, at higher speeds, with increased wetness of the surface.

Yager, T. J.↗

Evaluation of the Effect of Silicone Contamination on Various Bond Systems and the Feasibility of Removing the Contamination

Silicone is a contaminant that can cause catastrophic failure of a bond system depending on the materials and processes used to fabricate the bond system, Unfortunately, more and more materials are fabricated using silicone. The purpose of this testing was to evaluate which bond systems are sensitive to silicone contamination and whether or not a cleaning process could be utilized to remove the silicone to bring the bond system performance back to baseline. Due to the extensive nature of the testing attempts will be made to generalize the understanding within classes of substrates, bond systems, and surface preparation and cleaning methods. This study was done by contaminating various meta! (steel, inconel, and aluminum), phenolic (carbon cloth phenolic and glass cloth phenolic), and rubber (natural rubber, asbestos-silicone dioxide filled natural butyldiene rubber, silica-filled ethylene propylenediene monomer, and carbon-filled ethylene propylenediene monomer) substrates which were then bonded using various adhesives and coatings (epoxy-based adhesives, paints, ablative compounds, and Chemlok adhesives) to determine the effect silicone contamination has on a given bond system's performance. The test configurations depended on the bond system being evaluated. The study also evaluated the feasibility of removing the silicone contamination by cleaning the contaminated substrate prior to bonding. The cleaning processes also varied depending on bond system.

Stanley, Stephanie D.↗

Evaluation of the Effect of Silicone Contamination on Various Bond Systems and the Feasibility of Removing the Contamination

Silicone is a contaminant that can cause catastrophic failure of a bond system depending on the materials and processes used to fabricate the bond system. Unfortunately, more and more materials are fabricated using silicone. The purpose of this testing was to evaluate which bond systems are sensitive to silicone contamination and whether or not a cleaning process could be utilized to remove the silicone to bring the bond system performance back to baseline. Due to the extensive nature of the testing, attempts will be made to generalize the understanding within classes of substrates, bond systems, and surface preparation and cleaning methods. This study was done by contaminating various metal (steel, Inconel, and aluminum), phenolic (carbon-cloth phenolic [CCP] and glass-cloth phenolic [GCP]), and rubber (natural rubber, asbestos-silicone dioxide filled natural butyldiene rubber [ASNBR]; silica-filled ethylene propylenediene monomer [SFEPDM], and carbon-filled ethylene propylenediene monomer [CFEPDM]) substrates which were then bonded using various adhesives and coatings (epoxy-based adhesives, paints, ablative compounds, and Chemlok adhesives) to determine the effect silicone contamination has on a given bond system's performance. The test configurations depended on the bond system being evaluated. The study also evaluated the feasibility of removing the silicone contamination by cleaning the contaminated substrate prior to bonding. The cleaning processes also varied depending on bond system.

Stanley, Stephanie D.↗

Transient permeation of organic vapors through elastomeric membranes

The permeation of benzene and acetone vapors through sulfur-cured natural rubber was studied by the time-lag method. The zero concentration diffusion coefficient, was obtained by the early-time method. The Frisch time lag equation was utilized to estimate both the solubility coefficient and the additional parameter required to define the concentration-dependence of the diffusion coefficient. This form of concentration dependence was manifested by the corresponding permeability coefficient values. At low entering penetrant pressure where the transport coefficients are constant, indirect evidence was obtained that zero diffusion coefficient is the mechanically correct diffusion coefficient. The solubility coefficient values calculated for benzene vapor in natural rubber are in reasonable agreement with published equilibrium sorption data for a similar rubber compound. At higher entering penetrant pressures, average diffusion coefficients obtained at steady state tended to be larger than the corresponding average diffusion coefficients derived from the time-lags.

Curry, J. E.↗

Friction characteristics of 20 x 4.4, type 7, aircraft tires constructed with different tread rubber compounds

A test program was conducted at the Langley aircraft landing loads and traction facility to evaluate the friction characteristics of 20 x 4.4, type, aircraft tires constructed with experimental cut-resistant, tread rubber compounds. These compounds consisted of different blends of natural rubber (NR) and an alfin catalyzed styrene-butadiene copolymer rubber (SBR). One tire having a blend of 30 SBR and 70 NR and another having a blend of 60 SBR and 40 NR in the tread were tested together with a standard production tire with no SBR content in the tread rubber. The results of this investigation indicated that the test tires constructed with the special cut-resistant tread rubber compositions did not suffer any significant degradation in tire friction capability when compared with the standard tire. In general, tire friction capability decreased with increasing speed and surface wetness condition. As yaw angle increased, tire braking capability decreased while tire cornering capability increased. Tread-wear data based on number of brake cycles, however, suggested that the tires with alfin SBR blends experienced significantly greater wear than the standard production tire.

Dreher, R. C.↗

Wear of steel by rubber

Wear of a steel blade used as a scraper to abrade rubber surfaces has been found to take place much more rapidly on a cis-polyisoprene (natural rubber) surface than on a cis-polybutadiene surface, and much more rapidly in an inert atmosphere than in air. These observations are attributed to the direct attack upon steel of free-radical species generated by mechanical rupture of elastomer molecules during abrasion.

Gent, A. N.↗

ODC-Free Solvent Implementation Issues for Vulcanized Rubber and Bond Systems

Thiokol Propulsion has worked extensively to replace 1,1,1-trichloroethane (TCA) with ozone depleting chemicals (ODC)-free solvents for use in the manufacture of the Reusable Solid Rocket Motor (RSRM) for the Space Shuttle Program. As Thiokol has transitioned from sub-scale to full-scale testing and implementation of these new solvents, issues have been discovered which have required special attention. The original intent of Thiokol's solvent replacement strategy was to replace TCA with a single drop-in solvent for all equivalent applications. We have learned that a single candidate does not exist for replacing TCA. Solvent incompatibility with process materials has caused us to seek for niche solvents and/or processing changes that provide an ODC-free solution for special applications. This paper addresses some of the solvent incompatibilities, which have lead to processes changes and possible niche solvent usage. These incompatibilities were discovered during full-scale testing of ODC-free solvents and relate to vulcanized rubber and bond systems in the RSRM. Specifically, the following items are presented: (1) Cure effects of d-limonene based solvents on Silica Filled Ethylene Propylene Diene Monomer (SF-EPDM) rubber. During full-scale test operations, Thiokol discovered that d-limonene (terpene) based solvents inhibit the cure of EPDM rubber. Subsequent testing showed the same issue with Nitrile Butadiene Rubber (NBR). Also discussed are efforts to minimize uncured rubber exposure to solvents; and (2) Cured bond system sensitivity to ODC-free solvents. During full scale testing it was discovered that a natural rubber to steel vulcanized bond could degrade after prolonged exposure to ODC-free solvents. Follow on testing showed that low vapor pressure and residence time seemed to be most likely cause for failure.

Hodgson, James R.↗

Improved Methods for Hyperelastic Material Characterizations Based on Uniaxial, Radial-Biaxial, and Strip-Biaxial Test Data

This report concerns the different analytical methods used for material characterizations of hyperelastic silicone rubber, a potential candidate elastomer for aerospace applications. To establish the constitutive equations for the silicon rubber, strain-energy gradients (material constants) must be determined from experiments. Earlier experiments by Blatz-Ko showed that the material constants of natural rubber determined from different stress fields were different. Therefore, in the current material characterization, uniaxial, equalbiaxial, and strip-biaxial tensile tests were conducted. Based on the resulting stress-stretch data, the material constants were determined by using a trendline on the stress-difference plots and energy plots, and also the MSC-Marc ® curve-fitting method. The results confirm that the material constants determined from uniaxial and biaxial stress fields are indeed different. The material constants determined from the equal-biaxial energy plots and from the MSC-Marc ® combined-curve-fitting method were found to be extremely close, and can be considered as universal material constants for establishing the constitutive equations for the silicone rubber under any stress field. The results of this report show that a uniaxially stretched specimen became slightly anisotropic due to crystallization of polymer molecular chains, and that equal-biaxial and strip-biaxial testing must be conducted to fully understand the material properties of hyperelastic materials.

William L Ko↗

Manually operated elastomer heat pump

Device consisting of a rotating mechanism, a frame with multiple wide bands of rubber, and a fluid bath, demonstrates the feasibility of a human operated device capable of cooling or producing heat. This invention utilizes the basic thermodynamic properties of natural rubber.

Hutchinson, W. D.↗

Stored energy function and compressibility of compressible rubberlike materials under large strain

By using new invariants in the theory of finite elasticity an expression is obtained for the stored energy function of slightly compressible materials in which the effects of the distortional change (change of shape) and of the volume change are clearly separated. The volume-related terms are expressed as a function of the third invariant, the classical compressibility, and an induced anisotropy of the effective compressibility which is due to the large deformations. After evaluating the terms, using data on pressure, volume, uniaxial strain, and fractional volume change vs strain data on natural rubber from the literature, it is shown that the volume change contribution to the total stress observed in a simple tensile experiment can be clearly separated from the distortional contribution, even at finite strains.

Peng, S. T. J.↗

Developments in new aircraft tire tread materials

Comparative laboratory and field tests were conducted on experimental and state-of-the-art aircraft tire tread materials in a program aimed at seeking new elastomeric materials which would provide improved aircraft tire tread wear, traction, and blowout resistance in the interests of operational safety and economy. The experimental stock was formulated of natural rubber and amorphous vinyl polybutadiene to provide high thermal-oxidative resistance, a characteristic pursued on the premise that thermal oxidation is involved both in the normal abrasion or wear of tire treads and probably in the chain of events leading to blowout failures. Results from the tests demonstrate that the experimental stock provided better heat buildup (hysteresis) and fatigue properties, at least equal wet and dry traction, and greater wear resistance than the state-of-the-art stock.

Yager, T. J.↗

Toxicity of Pyrolysis Gases from Elastomers

The toxicity of the pyrolysis gases from six elastomers was investigated. The elastomers were polyisoprene (natural rubber), styrene-butadiene rubber (SBR), ethylene propylene diene terpolymer (EPDM), acrylonitrile rubber, chlorosulfonated polyethylene rubber, and polychloroprene. The rising temperature and fixed temperature programs produced exactly the same rank order of materials based on time to death. Acryltonitrile rubber exhibited the greatest toxicity under these test conditions; carbon monoxide was not found in sufficient concentrations to be the primary cause of death.

Hilado, Carlos J.↗

Effect of heating rate on toxicity of pyrolysis gases from some elastomers

The effect of heating rate on the toxicity of the pyrolysis gases from six elastomers was investigated, using a screening test method. The elastomers were polyisoprene (natural rubber), styrene-butadiene rubber (SBR), ethylene propylene diene terpolymer (EPDM), acrylonitrile rubber, chlorosulfonated polyethylene rubber, and polychloroprene. The rising temperature and fixed temperature programs produced exactly the same rank order of materials based on time to death. Acrylonitrile rubber exhibited the greatest toxicity under these test conditions, and carbon monoxide was not found in sufficient concentrations to be the primary cause of death.

Hilado, C. J.↗