Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “MnCr2O4”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

Materials Data on MnCr2O4 by Materials Project

Computed materials data using density functional theory calculations. These calculations determine the electronic structure of bulk materials by solving approximations to the Schrodinger equation. For more information, see https://materialsproject.org/docs/calculations

36 MATERIALS SCIENCE↗

Chromium Poisoning Mitigation Strategy in Strontium-Doped Lanthanum Manganite-Based Air Electrodes in Solid Oxide Fuel Cells

Abstract Chromium poisoning of the air electrode remains an obstacle to the long-term performance of solid oxide fuel cells (SOFCs). In Sr-doped LaMnO3 (LSM) air electrodes, the poisoning process results in two types of deposits, chromium oxide (Cr2O3), and Mn, Cr spinel (MnCr2O4). The former forms electrochemically and the latter forms via a chemical reaction. By applying a small anodic reverse bias, Cr2O3 deposits can be removed because their formation is electrochemical in nature. However, MnCr2O4 deposits remain because their formation is chemical, rather than electrochemical, in nature. In situ chemical decomposition of the Mn, Cr spinel was investigated as an alternate removal method as thermodynamics supports its decomposition into constituent oxides below ∼540 °C in pure oxygen. The spinel decomposition process was characterized using thermogravimetric and X-ray diffraction analyses. The experimentally determined rate of spinel decomposition was undetectable (very slow) with isolated MnCr2O4 powders. The addition of 10 mol% gadolinia doped ceria (GDC) and silver powders significantly increased the rate of decomposition. However, the rate is limited by the diffusion of oxygen through the decomposed oxide layer. Although one strategy may be the addition of GDC and silver to the LSM air electrode to enhance spinel decomposition, the more effective mitigation strategy would be to prevent the formation of MnCr2O4 spinel in the first place through the removal of the reactants: Cr2O3 via electrochemical cleaning and mobile Mn ions in the zirconia electrolyte by incorporating a diffusion barrier layer such as GDC between the air electrode and electrolyte.

Electrochemistry↗

Cyclic and isothermal oxidation behavior at 1100 and 1200 C of Ni-20Cr, Ni-20Cr-3Mn, Ni-20Cr-3Si, and Ni-40Cr alloys

Alloys of Ni-20Cr, Ni-20Cr-3Mn, Ni-20Cr-3Si, and Ni-40Cr were cyclically oxidized at 1100 and 1200 C for up to 100 hours. Oxidation behavior was judged by sample thickness and weight change, metallography, diffraction, and microprobe analysis. The least attacked were Ni-40Cr and Ni-20Cr-3Si. The alloy Ni-20Cr-3Mn was much less attacked than Ni-20Cr, but more than the other alloys. The formation of Cr2O3 accounted for the increased resistance of Ni-Cr and Ni-20Cr-3Si, and the formation of MnCr2O4 accounts for the improvement in Ni-20Cr-3mn over Ni-20Cr.

Lowell, C. E.↗

Cyclic and isothermal oxidation behavior on some Ni-Cr alloys

It is shown experimentally that 3 wt.% Si and 3 wt.% Mn additions can substantially improve the oxidation resistance of Ni-20Cr under both isothermal and cyclic conditions at 1100 and 1200 C. This is especially true in cyclic oxidation. In all cases, Si offers a greater improvement than Mn; however, the advantage of Si is substantial only during cyclic oxidation at 1200 C. The Si additions which lead to alloys of improved oxidation resistance suppress the formation of NiO and NiCr2O4 even under the most severe test conditions. The mechanism of improvement afforded by Mn appears to be the formation of MnCr2O4 at the expense of NiO and NiCr2O4.

Lowell, C. E.↗