Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “Microstructural Refinement”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 19 records

Phase transformations, microstructural refinement and defect evolution mechanisms in Al-Si alloys under non-hydrostatic diamond anvil cell compression

Non-hydrostatic compression of materials using a diamond anvil cell (DAC) can transform equilibrium microstructure of an alloy to novel, potentially metastable states. In this study, in situ synchrotron X-ray diffraction (XRD) during compression up to 24 GPa and subsequent ex situ, high resolution analytical electron microscopy (AEM) after decompression of an Al-Si alloy provided insight into the crystallographic changes during the compression as well as microstructural refinement, and defect structures caused by such a high pressure compression-decompression process. Pressure resolved in-situ synchrotron XRD was used to detail the phase transformation pathway of the eutectic Si phase in Al-Si alloy, from Si-I → Si-XI → Si-V during compression, and a final transformation predominantly to Si-III after decompression. Using scanning and transmission electron microscopy (S/TEM), site specific analysis of the alloy immediately underneath the anvil contact surface demonstrated a highly complex microstructure. A narrow region of thick amorphous Al oxide interspersed with nanocrystalline grains was found at the top surface. Underneath this Al oxide, while the majority the eutectic Si was transformed into highly-deformed, polycrystalline (PC) Si-III, a complex intermediate layer was discovered at the interface between Al and Si, comprised of a small fraction of Al nanocrystals and a majority of nanocrystalline Si-I. This combination of pressure resolved in-situ synchrotron XRD coupled with subsequent high resolution, electron microscopy resolved the phase transformation as well as non-equilibrium microstructures in a metallic alloy induced by a non-hydrostatic high pressure compression followed by decompression.

36 MATERIALS SCIENCE↗

Multimodal Analysis of Spatially Heterogeneous Microstructural Refinement and Softening Mechanisms in Three-Pass Friction Stir Processed Al4Si Alloy

Multiple thermally and thermomechanically induced microstructural refinement mechanisms can be activated in metallic alloys when subjected to solid phase processing methods such as friction stir processing (FSP). In this work, we provide detailed descriptions of the relationship between region-specific microstructural refinement mechanisms and the variation in microhardness, through a systematic and multimodal microstructural characterization of an FSP-processed 75% cold-rolled Al-4 at.% Si model binary alloy. Spatially resolved high-energy synchrotron X-ray diffraction, electron backscattered diffraction, and scanning transmission electron microscopy were used to understand the spatially heterogeneous microstructural evolution due to FSP. Results provide insights into how mechanisms such as static recovery, static recrystallization, dynamic recovery and recrystallization, geometric and continuous dynamic recrystallization, and particle-stimulated static or dynamic grain nucleation may occur heterogeneously in the microstructure as a function of the distance from the stir zone in processed alloys, directly influencing the degree of softening. The systematic analysis of microstructures and hardness in the FSP-processed model binary alloy given in this work highlights the rich microstructural domains that can be uniquely harnessed through solid phase processing of metallic alloys.

Al4Si, Friction Stir Processing, Geometric Dynamic↗

In-Situ Synchrotron X-Ray Diffraction of Ultrasonic Microstructural Refinement During Solidification in a Commercial Al–Si–Mg Alloy

This study reports the first use of in-situ synchrotron X-ray diffraction (SXRD) to study the effects of ultrasonic melt processing (USMP) on phase and grain size evolution during solidification in a commercial Al–Si–Mg casting alloy. USMP is a technique that, when applied to aluminum as it solidifies, can be used to refine the local microstructure of large-scale castings. Analysis of the in-situ SXRD data to estimate the average grain size of primary α-Al grains during USMP demonstrates that USMP slows the growth rate of α-Al grains and reduces grain size by 36 pct. Furthermore, there is also evidence that USMP causes the primary α-Al grains to move relative to the X-ray beam; such motion increases the probability of primary α-Al grains colliding and fragmenting. This movement becomes constrained at the onset of the Al–Si binary eutectic, suggesting that USMP ceases to effectively refine the microstructure once the Al–Si binary eutectic begins to form. Complementary laboratory-scale X-ray diffraction (XRD) data were used to correlate the lattice parameters of the α-Al and Si (D-A4) phases with temperature to estimate cooling rate during solidification. Thus, this study can guide the design of novel castings with spatially distributed fine-grained regions produced using local ultrasonic processing.

Aluminum Alloys↗

Improving the Mechanical Properties of Cast Aluminum Via Ultrasonication-Induced Microstructural Refinement

One barrier to the broader use of cast aluminum alloys in automotive applications is their poor mechanical properties, especially compared to wrought materials. This study investigates the use of ultrasound to refine the microstructure of cast aluminum alloys during solidification and thus improve their mechanical properties. An A356 aluminum alloy (Al-Si-Mg) with added Fe (to mimic a recycle-grade alloy) was cast in a graphite mold with the simultaneous application of ultrasound. Tensile specimens were extracted from the castings and heat treated to a T6 temper. Ultrasonication during casting transformed the morphology of primary aluminum grains from dendritic (~140 microns in size) to globular (~36 microns in size), increased the ultimate tensile strength by 10 %, and tripled the ductility compared to casting without ultrasound. This improvement in strength and ductility demonstrates the potential for ultrasonic processing to improve the performance of cast aluminum alloys without altering their chemistry or additional post-processing.

Aluminum, Solidification, Ultrasound, Grain refinm↗

Clarifying the formation of equiaxed grains and microstructural refinement in the additive manufacturing of Ti-Cu

Controlling microstructural evolution in metallic additive manufacturing (AM) is difficult, especially in producing refined as-built grains instead of coarse, directional grains. Traditional solutions involve adding inoculants to AM feedstocks, but titanium (Ti) alloys cannot employ this approach without producing detrimental secondary phases. Ti-Cu (Ti-copper) alloys offer a solution through constitutional supercooling and/or solid state thermal cycling under AM conditions. This work analyzes a compositionally graded directed energy deposition (DED) Ti-Cu build, single-melt laser tracks, and dilatometric heat treatments to evaluate if, when, and by what mechanism(s) microstructural refinement occurs. Refinement by inoculation of unmelted powder particles was also considered. Constitutional supercooling produced no net microstructural refinement as any equiaxed dendrites which form are remelted with new deposition. This finding agreed with solidification modeling of powder bed fusion-laser beam (PBF-LB) and DED builds. Solid state thermal cycling refined microstructures only during ex-situ dilatometric heat treatments, suggesting build parameter optimization is needed to achieve refinement in-situ. Accidental heterogeneous nucleation on unmelted Ti powder, originating from the different thermophysical properties of Ti and Cu, provided the most significant microstructural refinement. This work systematically assesses the microstructural refinement mechanisms of Ti-Cu in AM builds and offers insights into microstructural control in eutectoid alloys.

36 MATERIALS SCIENCE↗

Microstructure-refinement–driven enhanced tensile properties of high-pressure die-cast A380 alloy through friction stir processing

This work employs friction stir processing (FSP), a well-known severe plastic deformation technique, to selectively modify the microstructure of thin-walled, high-pressure die-cast (HPDC) aluminum alloy A380, a major HPDC alloy fabricated in the die casting sector. FSP effectively breaks down Al dendrites and acicular Si particles, creating a homogenized distribution of equiaxed Si particles in the aluminum matrix. After FSP, the refined Si particles (~1.5 µm) are smaller than the eutectic Si particles (3–8 µm) in HPDC condition. In addition, interparticle distance has decreased almost 50% compared to dendritic arm spacing, and FSP has reduced the aspect ratio of Si particles to ~2. Furthermore, FSP eliminates porosity, and breaks down needle-like second-phase Fe-Mn and Cu-rich particles, yielding a refined, homogeneous distribution. The FSP-induced microstructural refinement and porosity reduction improve bulk yield strength and ductility by 23% and 66%. Tensile properties are enhanced beyond those of the die skin of the HPDC plate, and the alloy possesses lower defect density and a highly refined microstructure. This study establishes the viability of FSP as a tool for microstructure modification and mechanical property improvement for HPDC Al alloys for the light-weighting goal of the automotive industries.

36 MATERIALS SCIENCE↗

Microstructural refinement in ultrasonically modified A356 aluminum castings

Two A356 aluminum alloys (Al-Si-Mg), one with 0.09 wt.% Fe and one with 0.91 wt.% Fe, were cast in a graphite mold with the simultaneous application of local ultrasonic intensification to refine the as-cast microstructure. Ultrasonication during casting transformed the morphology of primary Al grains from dendritic (~140-290 microns in size) to globular (~33-36 microns in size). The alloy with high Fe exhibited globular grains at distances up to 45 mm away from the ultrasound probe, while the alloy with low Fe exhibited globular grains at distances only up to 6 mm away from the ultrasound probe. Near the location of the ultrasound probe (< 2 mm away), a second non-dendritic microstructural morphology was observed with fine aluminum grains (~9-25 microns in size). This unique fine-grained morphology has not been previously reported, contains a greater concentration of Si relative to the globular microstructure, and may be a large, fully eutectic region. Ultrasonication during casting also transformed the morphology of the ß-Al 5 FeSi phase particles (which are deleterious to the strength and ductility of the alloy) in the high Fe alloy from needle-like to rectangular, which could enable the greater use of secondary Al alloys. Thermodynamic simulations conducted to calculate the solidification paths of the two alloys studied predict that the ß-Al 5 FeSi phase begins to form earlier in the alloy with high Fe. Finally, data suggest that the ß-Al 5 FeSi phase (which is more abundant in alloys with high Fe content) may enhance ultrasonically-induced grain refinement.

36 MATERIALS SCIENCE↗

Microstructural refinement of an Al-Ce-Mg alloy via Shear Assisted Processing and Extrusion

Al-Ce alloys have attracted recent interest because of their high thermal stability due to the low solubility of Ce in the Al matrix. The Al 11 Ce 3 eutectic phase gives excellent strain hardening behavior and moderate high-temperature strength in the as-cast state. However, its strengthening effect is limited by its coarse as-cast structure. Therefore, alternative manufacturing methods such as additive manufacturing or equal channel angular pressing have been applied to refine the Al 11 Ce 3 phase to good effect. However, these techniques are both expensive and time-consuming. Therefore, this study aims to use Shear Assisted Processing and Extrusion (ShAPE), an emerging solid phase processing technique that is more easily scalable than the previously mentioned methods. ShAPE can produce useful cross-sections of an Al-8Ce-4Mg alloy while refining the Al 11 Ce 3 phase to produce a higher strength material. It was found that a low temperature ShAPE process can improve the room temperature yield strength by ~60 % compared to a binary Al-4Mg alloy. Additionally, the high-temperature yield strength of the Al-Ce alloys increased by 20%, with a simultaneous 15% improvement in ductility compared to the binary Al-Mg alloy. Finally, these results highlight the potential for ShAPE as a processing technique for Al-Ce alloys.

36 MATERIALS SCIENCE↗

In situ synchrotron X-ray diffraction analysis of ultrasonically assisted microstructure refinement during laser melting process

This work investigates the effect of ultrasonic treatment (UST) on the microstructure of AA4043 alloy during laser melting process. Here, the study utilizes in situ synchrotron X-ray diffraction (SXRD) and postmortem electron backscatter diffraction (EBSD) techniques to examine the ultrasonic grain refinement mechanism. The SXRD diffraction patterns exhibit higher continuity of major diffraction rings in the UST-test pattern, indicating a more refined grain structure. The presence of new diffraction spots in the post-test diffraction pattern with UST suggests the breakdown of epitaxial growth of columnar dendrites during solidification. Thermal profiles determined by analyzing the lattice parameter evolution show a faster cooling rate with UST. The inverse pole figures and aspect ratio distribution from EBSD reveal that the UST samples exhibit a refined, more equiaxed grain structure along the weld centerline. UST sample also develops more fine-sized low angle grain boundaries (LAGBs). These features offer better hot-cracking resistance in aluminum alloys.

36 MATERIALS SCIENCE↗

Microstructural refinement of cement paste internally cured by polyacrylamide composite hydrogel particles containing silica fume and nanosilica

Supplementary cementitious materials were incorporated into hydrogel-based internal curing agents to improve the hydration, microstructure, and ultimately strength of internally cured high-performance cement paste. Polyacrylamide composite hydrogel particles containing amorphous silica – either silica fume or nanosilica – and two different polymer network crosslink densities were synthesized and incorporated into cement paste. The presence of silica and low crosslink density increased the absorption capacity of the particles in pore solution. Micrographs of internally cured paste indicated a significant improvement in hydrogel-related void-filling ability and an increase in void size for low crosslink density particles containing silica. Compressive strength and electrical resistivity increased at later ages for paste samples containing particles with higher silica dosage. The relationship between extent of hydration, void size, and void-filling activity was found to strongly influence the paste's long-term strength and is thus an important structure-property relationship to consider when selecting hydrogels for internal curing purposes.

36 MATERIALS SCIENCE↗

Refining Microstructures in Additively Manufactured Al/Cu Gradients Through TiB 2 Inclusions

Here, the additive manufacture of compositionally graded Al/Cu parts by laser engineered net shaping (LENS) is demonstrated. The use of a blue light build laser enabled deposition on a Cu substrate. The thermal gradient and rapid solidification inherent to selective laser melting enabled mass transport of Cu up to 4 mm from a Cu substrate through a pure Al deposition, providing a means of producing gradients with finer step sizes than the printed layer thicknesses. Divorcing gradient continuity from layer or particle size makes LENS a potentially enabling technology for the manufacture of graded density impactors for ramp compression experiments. Printing graded structures with pure Al, however, was prevented by the growth of Al 2 Cu 3 dendrites and acicular grains amid a matrix of Al 2 Cu. A combination of adding TiB 2 grain refining powder and actively varying print layer composition suppressed the dendritic growth mode and produced an equiaxed microstructure in a compositionally graded part. Material phase was characterized for crystal structure and nanoindentation hardness to enable a discussion of phase evolution in the rapidly solidifying melt pool of a LENS print.

36 MATERIALS SCIENCE↗

Microstructure refinement of hot deformed Dy-free NdFeB magnets through a novel cold sintering approach by pressure-assisted spark plasma sintering

Anisotropic fine-grained Dy-free NdFeB high-performance magnets were produced using a novel cold sintering approach by pressure-assisted spark plasma sintering (SPS). The NdFeB nanocrystalline ribbon powders were subjected to cold sintering below 450 °C using pressure-assisted SPS, followed by hot deformation at 710 °C and 810 °C via SPS. Results indicate that cold sintering below 450 °C effectively restricts grain growth in the NdFeB magnets, yielding sub-100 nm scale grains across both fine-grained regions and most coarse-grained regions. The refined grain structure achieved through cold sintering allows for a lower hot deformation temperature as compared with the magnet by conventional sintering, as finer grains allow easier deformation and grain sliding/rotation. This process produces a highly fine-grained and anisotropic microstructure to achieve high magnetic performance (i.e., high intrinsic coercivity, remanence, and maximum energy product) in the magnets. The cold sintering (at 350 °C) and lower hot deformation temperatures required (e.g., 710 °C) help control grain coarsening and limit grain size that is commensurate with the size of a single magnetic domain of the Nd 2 Fe 14 B magnetic matrix phase, resulting in high intrinsic coercivity (H ci =11.4 kOe). Furthermore, the reduced hot deformation temperature mitigates the formation of coarse grain bands, leading to improved magnetic properties, specifically an increased remanence (B r = 14.3 kGs) and a high maximum energy product ((BH) max = 48 MGOe). In conclusion, cold sintered hot deformed NdFeB magnet also shows good thermal stability with reversible temperature coefficient α(B r )= -0.097 %/K and α(H ci )= -0.616 %/K at elevated temperatures up to 400 K.

Cold Sintering↗

Material flow behavior and microstructural refinement of AA6061 alloy during friction extrusion

In this work we used friction extrusion (FE), a solid phase processing technique, to produce dense, fully consolidated 5?mm rods of aluminum alloy 6061 (AA6061). The combination of large shear stresses and high temperatures at the tool-billet interface during extrusion produced equiaxed, dynamically recrystallized grains and finely distributed precipitates. Texture and microstructure evolution during extrusion was investigated in detail using scanning electron microscopy, electron backscatter diffraction, and transmission electron microscopy. Smoothed particle hydrodynamics simulation was performed to study complex material flow during extrusion. Simulation results suggest spiral material flow during extrusion which corroborated experimental results. Advantages of friction extruded microstructure over conventionally extruded counterparts are also explored using flash annealing for solution treatment followed by artificial aging. Mechanical properties of the as-friction extruded, and the artificially aged specimens were evaluated using tensile testing and compared with conventional extruded material properties.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Mechanical Behavior of Al–Al2Cu–Si and Al–Al2Cu Eutectic Alloys

In this study, laser rapid solidification technique was used to refine the microstructure of ternary Al–Cu–Si and binary Al–Cu eutectic alloys to nanoscales. Micropillar compression testing was performed to measure the stress–strain response of the samples with characteristic microstructure in the melt pool regions. The laser-remelted Al–Al2Cu–Si ternary alloy was observed to reach the compressive strength of 1.59 GPa before failure at a strain of 28.5%, which is significantly better than the as-cast alloy with a maximum strength of 0.48 GPa at a failure strain of 4.8%. The laser-remelted Al–Cu binary alloy was observed to reach the compressive strength of 2.07 GPa before failure at a strain of 26.5%, which is significantly better than the as-cast alloy with maximum strength of 0.74 GPa at a failure strain of 3.3%. The enhanced compressive strength and improved compressive plasticity were interpreted in terms of microstructural refinement and hierarchical eutectic morphology.

36 MATERIALS SCIENCE↗

Melt-Pool Dynamics and Microstructure of Mg Alloy WE43 under Laser Powder Bed Fusion Additive Manufacturing Conditions

Magnesium-based alloy WE43 is a state-of-the-art bioresorbable metallic implant material. There is a need for implants with both complex geometries to match the mechanical properties of bone and refined microstructure for controlled resorption. Additive manufacturing (AM) using laser powder bed fusion (LPBF) presents a viable fabrication method for implant applications, as it offers near-net-shape geometrical control, allows for geometry customization based on an individual patient, and fast cooling rates to achieve a refined microstructure. In this study, the laser–alloy interaction is investigated over a range of LPBF-relevant processing conditions to reveal melt-pool dynamics, pore formation, and the microstructure of laser-melted WE43. In situ X-ray imaging reveals distinct laser-induced vapor depression morphology regimes, with minimal pore formation at laser-scan speeds greater than 500 mm/s. Optical and electron microscopy of cross-sectioned laser tracks reveal three distinct microstructural regimes that can be controlled by adjusting laser-scan parameters: columnar, dendritic, and banded microstructures. These regimes are consistent with those predicted by the analytic solidification theory for conduction-mode welding, but not for keyhole-mode tracks. The results provide insight into the fundamental laser–material interactions of the WE43 alloy under AM-processing conditions and are critical for the successful implementation of LPBF-produced WE43 parts in biomedical applications.

36 MATERIALS SCIENCE↗

Mass transport in a highly immiscible alloy on extended shear deformation

Forced mixing to a single phase or supersaturated solid solution (SSS) and its prerequisite microstructure evolution in immiscible systems has been a focus of research for both fundamental science and a variety of applications. Controlling the formation of SSS by shear deformation assisted processing could enable a material design beyond conventional equilibrium microstructure in immiscible systems. Here, a highly immiscible (mixing enthalpy of ~ 20 kJ·mol -1 ) Cu-50 at. % Cr binary alloy was employed to investigate the microstructure evolution and localized tendencies of SSS during severe shear deformation. The present results demonstrate distinctive microstructure refinement process in each phase and how they lead to localized SSS as a function of shear strain. Preferential dynamic recrystallization occurs in the softer Cu phase due to strain localization, leading to substantial grain refinement. The refinement of Cr phase in the top-most layer, however, is enabled by the progressive evolution of grain lamination, splitting, and fragmentation as a function of shear strain. The eventual SSS is found to be strongly dependent on the local environments that affect the dislocation activity, including the level of microstructure refinement, the interfacial orientation relationship, hardness difference, and supposed stability of oxidation. Ab initio simulations comfirm that it is more favorable to oxidize Cr than Cu at incoherent Cu/Cr interfaces which then limits the mass transport on an incoherent boundary. Our results shed light on the underpinning mechanism for non-equilibrium mass transport in immiscible systems upon severe deformation that can be applicable to a variety of processing techniques aimed at producing immiscible alloys with superior mechanical properties.

36 MATERIALS SCIENCE↗

Effect of tool design and pass strategy on defect elimination and uniform, enhanced tensile properties of friction stir processed high-pressure die-cast A380 alloy

This work reports implementation of friction stir processing (FSP) to locally modify microstructure and create a defect-free processing zone with the aid of different tool designs and altering the passing strategy for two different process parameter combinations. Here, FSP is applied on high pressure die-cast (HPDC) A380 alloy, a widely used Al-Si alloy fabricated in the die casting sector for automotive and aerospace applications. However, the presence of gas and shrinkage porosity, brittle needle-shaped Fe-containing ß-FeSiAl 5 intermetallic compounds, Al-dendrites, coarse and acicular silicon particles, and large second-phase particulates have a detrimental influence on the uniformity of tensile properties across the thickness direction of an HPDC plate. FSP is able to eliminate porosity, refine microstructure and improve tensile properties. An FSP tool design and a passing strategy are identified for the best microstructure consolidation and uniform enhanced tensile properties. This study noted the importance of tool features such as scroll design and flats on tool pin and multiple pass orientation strategy to find best combination of defect-free refined microstructure and uniform tensile strength and ductility across the processing zone of HPDC Al alloys.

36 MATERIALS SCIENCE↗

Phase stability in cast and additively manufactured Al-rich Al-Cu-Ce alloys

Additively manufactured (AM) eutectic Al alloy systems have been studied extensively for advantageous thermal stability and mechanical properties due to their refined microstructures. Al-Cu-Ce alloys are one subset of these AM eutectic alloys. Here we studied phase stability in AM Al-Cu-Ce alloys and compared it to that of conventionally cast ones. A new phase, Al 8 Cu 3 Ce, was identified in the microstructures of both AM and cast Al-Cu-Ce alloys. This Al 8 Cu 3 Ce phase was not previously included on experimental or thermodynamically calculated phase diagrams of the Al-Cu-Ce system. Therefore, we performed additional thermodynamic modeling of the system. These models were experimentally validated with cast and subsequently heat-treated Al-Cu-Ce alloys. We found that despite the refined microstructure of the AM alloys, the phases formed were consistent with the cast alloys, suggesting that AM processing did not significantly alter the formation and stability of phases from that in the conventional alloys. In conclusion, this work has resolved inconsistent previous descriptions of the Al-Cu-Ce ternary phase diagram in the Al-rich region and resulted in the addition of the Al 8 Cu 3 Ce as an equilibrium phase above 500 °C.

36 MATERIALS SCIENCE↗