Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “MOLYBDENUM 99”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

Experimental Observations of Nuclear Activity in Deuterated Materials Subjected to a Low-Energy Photon Beam

Exposure of highly deuterated materials to a low-energy (nom. 2 MeV) photon beam resulted in nuclear activity of both the parent metals of hafnium and erbium and a witness material (molybdenum) mixed with the reactants. Gamma spectral analysis of all deuterated materials, ErD2.8+C36D74+Mo and HfD2+C36D74+Mo, showed that nuclear processes had occurred as shown by unique gamma signatures. For the deuterated erbium specimens, posttest gamma spectra showed evidence of radioisotopes of erbium ((163)Er and (171)Er) and of molybdenum ((99)Mo and (101)Mo) and by beta decay, technetium (99mTc and 101Tc). For the deuterated hafnium specimens, posttest gamma spectra showed evidence of radioisotopes of hafnium (180mHf and 181Hf) and molybdenum ((99)Mo and (101)Mo), and by beta decay, technetium ((99m)Tc and (101)Tc). In contrast, when either the hydrogenated or non-gas-loaded erbium or hafnium materials were exposed to the gamma flux, the gamma spectra revealed no new isotopes. Neutron activation materials showed evidence of thermal and epithermal neutrons. CR-39 solid-state nuclear track detectors showed evidence of fast neutrons with energies between 1.4 and 2.5 MeV and several instances of triple tracks, indicating (is) greater than 10 MeV neutrons. Further study is required to determine the mechanism causing the nuclear activity.

Steinetz, Bruce M.↗

Effect of Prestraining of Recrystallization Temperature and Mechanical Properties of Commercial, Sintered, Wrought Molybdenum

Given three presumably identical lots of commercial, sintered, wrought molybdenum, the 1-hour recrystallization temperature of one lot remained above 2900 F by limiting the amount of effective restraining to 35 percent or less. Different recrystallization temperatures were obtained in various atmospheres, the highest in argon and the lowest in hydrogen. Metal thus fabricated and then stress-relieved possessed an ultimate tensile strength at room temperature within 10 percent of metal swaged 99 percent and also possessed equivalent ductility. At 1800 F, equivalent strength and ductility was obtained irrespective of the amount of swaging over the range of 10 to 99 percent. The amount of swaging greatly influenced the recrystallized grain size but the difference in grain size is not the major controlling factor which determines whether recrystallized molybdenum is ductile or brittle at room temperature.

MATERIALS, PROPERTIES - TENSILE↗

Containerless Liquid to Solid Nucleation Pathways in Two Representative Grades of Commercially Available Zirconium

Experimental measurements were conducted to determine the solid metal nucleation pathways of radiatively cooling, molten zirconium spheres of two different commercially available purity grades in a high-vacuum, high-temperature electrostatic levitator. The ensemble distribution of maximum undercooling temperatures was interpreted using Poisson statistics to determine the temperature dependence of the solid metal nucleation rate. For a sample of nominally 99.95% pure zirconium, the results are consistent with heterogeneous solid metal nucleation either on static catalyst particles at least ~30 nm diameter or on a surface coating. For a sample of nominally 99% pure zirconium, however, it appears that heterogeneous solid metal nucleation occurred either on a polydispersion of ~10 nm (mean diameter) static catalyst particles or on dynamic catalyst particles which precipitated from a solution which became supersaturated as the melt cooled. A quantitative analysis of the compositions of both samples suggests that the catalysts probably consisted of one or more of the following elements: niobium, molybdenum, hafnium, and oxygen.

containerless, nucleation, zirconium↗

Improving the Visible and Infrared Contrast Ratio of Microshutter Arrays

Three device improvements have been developed that dramatically enhance the contrast ratio of microshutters. The goal of a microshutter is to allow as much light through as possible when the shutters are in the open configuration, and preventing any light from passing through when they are in the closed position. The ratio of the transmitted light that is blocked is defined here as the contrast ratio. Three major components contribute to the improved performance of these microshutters: 1. The precise implementation of light shields, which protect the gap around the shutters so no light can leak through. It has been ascertained that without the light shield there would be a gap on the order of 1 percent of the shutter area, limiting the contrast to a maximum of 100. 2. The precise coating of the interior wall of each microshutter was improved with an insulator and metal using an angle deposition technique. The coating prevents any infrared light that finds an entrance on the surface of the microshutter cell from being emitted from a sidewall. Since silicon is in effect transparent to any light with a wavelength longer than .1 micrometer, these coatings are essential to blocking any stray signals when the shutters are closed. 3. A thin film of molybdenum nitride (MoN) was integrated onto the surface of the microshutter blade. This film provides the majority of light blockage over the microshutter and also ensures that the shutter can be operated over a wide temperature range by maintaining its flatness. These improvements were motivated by the requirements dictated by the James Webb Space Telescope NIRSpec instrument. The science goals of the NIRSpec require observing some of the very faintest objects in a given field of view that also may contain some very bright objects. To observe the faint objects, the light from the bright objects - which could be thousands of times brighter - must be completely blocked. If a closed microshutter is even slightly transmissive, a very bright object will still transmit a small signal, which can be larger than a signal from a very faint object transmitted through an open shutter. Since this situation can completely corrupt the results, it was necessary that the closed shutters be able to attenuate light by at least a factor of 2,000. There currently exist four flight-quality microshutter arrays that have been fully or are currently undergoing testing and the results support that the three improvements described above have successfully led to contrast levels greater than 50,000 in over 99 percent of the microshutters at an operating temperature of 35 K. Applications for these high-contrast microshutters are in the photomask generation and stepper equipment used to make integrated circuits and microelectromechanical (MEMS) devices. Since microshutters are a reconfigurable optical element, their versatility in these industries provides an improvement over printed masks and fixed projection alignment systems.

Jhabvala, Murzy↗