In this study, the effects of heat input on the distribution of microhardness of tungsten inert gas (TIG) arc welded hot-extruded AZ61 magnesium alloy joints were investigated. The results show that with an increase of heat input, the distributions of microhardness at the top and bottom of the welded joints are different because they are determined by both the effect of grain coarsening and the effect of dispersion strengthening. With an increase of the heat input, the microhardness of the heat-affected zone (HAZ) at the top and bottom of welded joints and the fusion zone (FZ) at the bottom of welded joints decreased gradually, while the microhardness of the FZ at the top of welded joints decreased initially and then increased sharply. The reason for the abnormal distribution of microhardness of the FZ at the top of the welded joints is that this area is close to the heat source during welding and then large numbers of hard {beta}-Mg{sub 17}(Al,Zn){sub 12} particles are precipitated. Hence, in this case, the effect of dispersion strengthening dominated the microhardness.
This study aims to investigate the effect of machining parameters on the surface topography and composition of Ti-6Al-4V after micro-EDM as well as the effect of elemental composition on the surface microhardness. The surface topography has been studied in terms of quality of machined surface, crater sizes, and the presence of surface defects. Statistical analysis was carried out to study the influence of micro-EDM process parameters, i.e., voltage, capacitance, discharge energy, electrode rotational speed, and the electrode coating, on the elemental composition of the machined surface. It was found that the crater size, and hence the surface finish, was dependent on the electrical parameters only, with more pronounced effect of capacitance over voltage. The 60 V and 30 pF combination resulted in crater size as small as 1 µm, whereas crater size of 12 µm was obtained using a combination of 4700 pF and 112 V. Although smaller capacitance resulted in smaller crater sizes, it also increased the chances of defects or deposition of debris on the machined surface. There was migration of material from the tool electrode, dielectric oil, and atmosphere to the workpiece surface, which influenced the surface topography, crater sizes, and surface microhardness. The effects of non-electrical parameters on the relative percentage of various elements were found to be statistically insignificant. The surface microhardness was found to increase slightly due to the surface modification after EDM. The reason for increase in surface microhardness was identified as the migration of tungsten from the tool electrode and carbon from the dielectric. The maximum surface microhardness of 455 HV was obtained at a surface composition after micro-EDM containing 7.96% C and 9.69% W, where non-machined Ti-6Al-4V surface does not have any carbon or tungsten on the surface.
The effect of carbon on (111) p-type Czochralski silicon is examined. The preparation of the silicon and microhardness test procedures are described, and the equation used to determine microhardness from indentations in the silicon wafers is presented. The results indicate that as the carbon concentration in the silicon increases the microhardness increases. The linear increase in microhardness is the result of carbon hindering dislocation motion, and the effect of temperature on silicon deformation and dislocation mobility is explained. The measured microhardness was compared with an analysis which is based on dislocation pinning by carbon; a good correlation was observed. The Labusch model for the effect of pinning sites on dislocation motion is given.
A quaternary material Cd 1-x ZnxTe 1-y Sey (CZTS) is currently under investigation for its application as a material for hard X-ray and gamma ray detectors. The addition of selenium was found to be very effective in suppressing the formation of sub-grain boundaries and their networks. The CZTS crystals were grown by the THM technique at Brookhaven National Laboratory. The ingots are ~52 mm in diameter, weighting about 1.0-1.2 kg. In general, the ingots were crack-free except near the Te-CZTS interface. The goal of the presented work is to increase our understanding of key factors influencing the crystal quality and its suitability for radiation detection by a study of its mechanical properties, namely the microhardness and its dependence on crystal composition. Microhardness is closely connected to dislocations and their mobility. We report here on a detailed microhardness characterization and its correlation to the crystal composition of quaternary material Cd 1-x ZnxTe 1-y Se y . Measurements of the Vickers microhardness, resistivity mapping, photoluminescence, and Zn and Se composition analysis were employed along the crystal growth axis. The microhardness values, bandgap and Zn and Se composition along the crystal axis have been correlated. We also performed comparative study of a set of CdTe and CdZnTe samples prepared in the crystal growth laboratory of the Institute of Physics of Charles University or originating from commercial sources.
The effect of nanosized particles NiO addition on the Vickers microhardness of polycrystalline SmBa{sub 2}Cu{sub 3}O{sub 7-δ} was investigated. Various amounts of nanosized particles NiO (x = 0.00, 0.02, 0.04, 0.08, and 0.12 wt%) were added to SmBa{sub 2}Cu{sub 3}O{sub 7-δ} prepared by the solid-state reaction method. Sample characterizations were carried out using X-ray powder diffraction (XRD), particle induced X-ray emission (PIXE), Rutherford backscattering (RBS), and scanning electron microscopy (SEM). The nanosized particle addition does not influence the orthorhombic structure of SmBa{sub 2}Cu{sub 3}O{sub 7-δ}, whereas it affects the oxygen content δ. The electrical and mechanical properties of (NiO){sub x}SmBa{sub 2}Cu{sub 3}O{sub 7-δ} samples were measured using four-standard probe technique and Vickers microhardness in order to investigate the effect of NiO nanosized particles on superconducting transition temperature and Vickers microhardness number H{sub v}. The Vickers microhardness data were analyzed using Hays and Kendall (HK), elastic plastic deformation (EPD), and modified proportional specimen resistance (MPSR) models. The analysis showed that the MPSR model was found to be the best to describe the behavior of H{sub v}.
Disks of an Al-6061 metal matrix composite, reinforced with 10 vol.% Al{sub 2}O{sub 3} particles, were processed by high-pressure torsion (HPT) at room temperature for 1/4, 1/2, 1, 5 and 10 turns under an applied pressure of 6.0 GPa. The evolution of microstructure was investigated using optical microscopy and scanning electron microscopy. During HPT processing the average grain size within the aluminum matrix decreased from ∼ 35 μm in the unprocessed condition to ∼ 170 nm after processing through 10 turns but there was no significant effect on the size and distribution of the alumina particulate clusters. The values of the Vickers microhardness were recorded across the surface of each disk and then plotted as two-dimensional and three-dimensional color-coded contour maps. The results show the hardness increases from ∼ 56 Hv in the initial condition to ∼ 165 Hv after HPT for 10 turns. The results demonstrate that, as in many unreinforced metallic alloys, the evolution of hardness with strain exhibits strain hardening without any significant recovery. - Highlights: •The average grain size of the Al matrix was ~ 170 nm after processing for 10 turns. •No significant effect of HPT on the size and distribution of the Al{sub 2}O{sub 3} particles. •The evolution of microhardness demonstrates strain hardening without recovery. •The microhardness at low strains increases linearly from the center to the edge. •The microhardness at high strains becomes homogeneous with a saturation of ~ 170 Hv.
Highlights: cThe microstructure variation with build height of TiAl alloy was investigated. • The microhardness rapidly increased with build height increasing from 19 mm to 20 mm. • The mechanism of microstructure evolution was illuminated during SEBM. - Abstract: In this research, a Ti-47Al-2Cr-2Nb alloy was fabricated by selective electron beam melting (SEBM). The microstructures at different heights of SEBM-produced TiAl alloy sample and their contribution to microhardness were investigated. The results revealed that the last deposited layers displayed near lamellar structure with fine α{sub 2} lamellae. Lamellar colonies degraded at the height of 19 mm of the as-built sample, accompanied with the α{sub 2} lamellae decomposition and B2 precipitation along primary α{sub 2} lamellae. Meanwhile, equiaxed γ and blocky B2 phase dispersed on the colony boundaries. Lamellar colonies further degraded and colony boundaries further coarsen at the heights of 15 mm and 5 mm due to the in-situ heat treatment during SEBM process. Three kinds of phase transformations could be observed during SEBM process, which were α{sub 2} → γ, α{sub 2} → B2 and α{sub 2} + γ → B2. The microhardness exhibited slight fluctuation as the building height increased from 3 mm to 19 mm, and the microhardness rapidly increased with the building height increasing from 19 mm to 20 mm. Eventually, the mechanism of microstructure evolution during SEBM process was discussed in detail.
The main aim of this study is to produce copper reinforced metal matrix composite (MMC) layers using micron sized SiC particles via friction stir processing (FSP) in order to enhance surface mechanical properties. Microstructural evaluation using optical microscopy (OM) and scanning electron microscopy (SEM) indicated that an increase in traverse speed and a decrease in rotational speed cause a reduction in the grain size of stir zone (SZ) for the specimens friction stir processed (FSPed) without SiC particles. With the aim of determining the optimum processing parameters, the effect of traverse speed as the main processing variable on microstructure and microhardness of MMC layers was investigated. Higher traverse speeds resulted in poor dispersion of SiC particles and consequently reduced the microhardness values of MMC layers. It was found that upon addition of SiC particles, wear properties were improved. This behavior was further supported by SEM images of wear surfaces. Results demonstrated that the microcomposite produced by FSP exhibited enhanced wear resistance and higher average friction coefficient in comparison with pure copper. Tensile properties and fracture characteristics of the specimens FSPed with and without SiC particles and pure copper were also evaluated. According to the results, the MMC layer produced by FSP showed lower strength and elongation than pure copper while a remarkable elongation was observed for FSPed specimen without SiC particles. Research Highlights: {yields} Decrease in traverse speed leads to good dispersion of SiC particles in composites. {yields} No distinct TMAZ in side regions of SZ of FSPed specimens with SiC particles. {yields} Microhardness of FSPed specimens with SiC particles shows a remarkable increase. {yields} Reinforcement of Cu with SiC particles improves wear and friction behavior of surface. {yields} A weak bonding in tensile due to probable agglomeration for SiC containing samples.
The effect of cooling rate on the microstructure and microhardness of the Cu{sub 40}Zr{sub 44}Ag{sub 8}Al{sub 8} (at.%) alloy has been studied. The crystalline phases were characterized by X-ray diffraction, optical microscopy and scanning electron microscopy with energy dispersive X-ray spectroscopy, and identified as AlCu{sub 2}Zr, Cu{sub 10}Zr{sub 7} and CuZr{sub 2}. The solidification sequence was established as following: the Cu{sub 10}Zr{sub 7} phase forms first in the periphery of the rod, then following with AlCu{sub 2}Zr phase in the rod center and finally CuZr{sub 2} crystals in Cu-depleted areas. The effect of crystals on the mechanical properties of the Cu{sub 40}Zr{sub 44}Ag{sub 8}Al{sub 8} alloy was also estimated through the microhardness. According to the value of microhardness, inhomogeneous structure of the amorphous matrix is more easily formed for the alloy in the low cooling rate (i.e., 9 mm) as compared with the alloy with fully amorphous state in the large cooling rate (i.e., 3 mm). This inhomogeneous structure was attributed to the composition change of amorphous matrix arising from the forming of crystalline phases due to the low cooling rate. - Highlights: Black-Right-Pointing-Pointer The crystalline phases in the Cu{sub 40}Zr{sub 44}Ag{sub 8}Al{sub 8} alloy were identified. Black-Right-Pointing-Pointer The solidification sequence of Cu{sub 40}Zr{sub 44}Ag{sub 8}Al{sub 8} alloy was verified. Black-Right-Pointing-Pointer The softening and hardening of alloy could be observed due to the crystallization.
This paper reports the effect of the deformation path on the microstructure, microhardness, and texture evolution of interstitial free (IF) steel processed by differential speed rolling (DSR) method. For this purpose, total height reductions of 50% and 75% were imposed on the samples by a series of differential speed rolling operations with various height reductions per pass (deformation levels) ranging from 10 to 50% under a fixed roll speed ratio of 1:4 for the upper and lower rolls, respectively. Microstructural observations using transmission electron microscopy and electron backscattered diffraction measurements showed that the samples rolled at deformation level of 50% had the finest mean grain size (∼ 0.5 μm) compared to the other counterparts; also the samples rolled at deformation level of 50% showed a more uniform microstructure. Based on the microhardness measurements along the thickness direction of the deformed samples, gradual evolution of the microhardness value and its homogeneity was observed with the increase of the deformation level per pass. Texture analysis showed that, as the deformation level per pass increased, the fraction of alpha fiber and gamma fiber in the deformed samples increased. The textures obtained by the differential speed rolling process under the lubricated condition would be equivalent to those obtained by the conventional rolling. - Highlights: • Effect of DSR deformation path on microstructure of IF steel is significant. • IF steel rolled at deformation level of 50% has the ultrafine grains of ∼ 0.5 μm. • Rolling texture components are pronounced with increasing deformation level.
It was found that strongly absorbed Nd:YAG laser radiation leads to a non-monotonous dependence of microhardness of p- and n-type Si crystals on laser radiation. This dependence is characterized by two maxima for p-Si and one maximum for n-Si crystals. In both cases the increase of microhardness at higher laser intensity is explained by formation of mechanically compressed layer at the irradiated surface due to concentration of the interstitial atoms of Si at the surface in temperature gradient field. The decrease of the microhardness is explained by formation of nano-cones as a result of plastic deformation of the mechanically stressed layer. The additional maximum at lower laser intensity for p-Si crystal is explained by p-n type inversion of Si conductivity.
FeSiB alloys have been fabricated by selective laser melting (SLM) using a laser scan rate of 0.1–1.5 m/s, laser power of 90 W, scan line spacing of 40 μ m, and layer thickness of 50 μ m. X-ray diffraction, scanning electron microscopy coupled with energy-dispersive X-ray spectroscopy, atomic force microscopy, profilometer, microdurometer, and vibrating sample magnetometer have been used to investigate the structural, microstructural, roughness, microhardness, and magnetic property changes during the laser melting process. The produced samples exhibit a nanocomposite structure consisting of nanocrystalline α-Fe{sub 0.95}Si{sub 0.05} and Fe{sub 2}B phases embedded into an amorphous ε-FeSi-type matrix. The selective laser-melted samples show high density, low surface roughness, higher microhardness values (1654–2273 Hv), and soft magnetic properties (M{sub s} = 188.6–199 emu/g and H{sub c} = 43.8–73 Oe).
Epitaxial CMSX-4{sup ®} deposition is achieved on CMSX-4{sup ®} substrates through the scanning laser epitaxy (SLE) process. A thorough analysis is performed using various advanced material characterization techniques, namely high-resolution optical microscopy, scanning electron microscopy, energy-dispersive x-ray spectroscopy, x-ray diffraction, and Vickers microhardness measurements, to characterize and compare the quality of the SLE-fabricated CMSX-4{sup ®} deposits to the CMSX-4{sup ®} substrates. The results show that the CMSX-4{sup ®} deposits have smaller primary dendritic arm spacing, finer γ/γ′ size, weaker elemental segregation, and higher microhardness compared to the investment cast CMSX-4{sup ®} substrates. The results presented here demonstrate that CMSX-4{sup ®} is an attractive material for laser-based AM processing and, therefore, can be used in the fabrication of gas turbine hot-section components through AM processing.
With standard T6 heat treatments, precipitate-hardened alloys such as Al7075 and Al6061 fabricated using Additive Friction Stir Deposition (AFSD) method restore to noticeablely different peak mechanical properties. Previous research observed similar results but did not provide a viable solution. This study proposes a new processing strategy, namely enhanced plastic deformation by subjecting the Al7075 feedstock to annealed softening treatments. Specifically, by annealing the standard T651-Al7075 feedstock and deposition substrate (179 HV), their Microhardness were first degraded to its lowest state (80 HV), which is called a Soft-to-Soft system. For the Soft-to-Soft system subjected to AFSD, after undergoing appropriate T6 heat treatment, the microhardness of the AFSD 7075 alloy was restored to its peak value (183.1 ± 1.8 HV). The results indicate that this softening strategy can effectively reduce the non-strengthening phase in the AFSD matrix, thereby increasing the strengthening phase (η′ phase). This addresses the issue of traditional AFSD-prepared aluminum alloys being unable to achieve peak performance through T6 heat treatment.
Al-Ni-Nd-Si alloy with nominal composition of Al-8 wt.%Ni-5 wt.%Nd-4 wt.%Si was rapidly solidified by using melt-spinning technique to examine the influence of the cooling rate/conditions on microstructure and mechanical properties. The resulting conventional cast (ingot) and melt-spun ribbons were characterized by X-ray diffraction, optical microscopy, scanning electron microscopy together with energy dispersive spectroscopy, differential scanning calorimetry, differential thermal analysis and Vickers microhardness tester. The ingot alloys consists of four phases namely {alpha}-Al, intermetallic Al{sub 3}Ni, Al{sub 11}Nd{sub 3} and fcc Si. Melt-spun ribbons are completely composed of {alpha}-Al phase. The optical microscopy and scanning electron microscopy results show that the microstructures of rapidly solidified ribbons are clearly different from their ingot alloy. The change in microhardness is discussed based on the microstructural observations. - Highlights: Black-Right-Pointing-Pointer Rapid solidification allows a reduction in grain size, extended solid solution ranges. Black-Right-Pointing-Pointer We observed the matrix lattice parameter increases with increasing wheel speed. Black-Right-Pointing-Pointer Melt-spun ribbons consist of partly amorphous phases embedded in crystalline phases. Black-Right-Pointing-Pointer The solidification rate is high enough to retain most of alloying elements in the Al matrix. Black-Right-Pointing-Pointer The rapid solidification has effect on the phase constitution.
Microstructures and microhardness at fusion boundary of a weld joint were investigated in a 316 stainless steel/Inconel 182 dissimilar weldment. The results showed that there were two alternately distributed typical fusion boundaries, a narrow random boundary (possessed 15% in length) with a clear sharp interface and an epitaxial fusion one with (100){sub BM}//(100){sub WM} at the joint interface. The composition transition, microstructure and hardness across the fusion boundary strongly depended on the type of the fusion boundary. For the random boundary, there was a clear sharp interface and the composition transition with a width of 100 μm took place symmetrically across the grain boundary. For the epitaxial fusion one, however, there were Type-I and Type-II grain boundaries perpendicular and parallel to the epitaxial fusion boundary, respectively. The composition transition took place in the Inconel 182 weld side. Σ3 boundaries in the HAZ of 316SS side and Σ5 grain boundaries in weld metal were usually observed, despite the type of fusion boundary, however the former was much more in epitaxial fusion boundary. Microhardness was continuously decreased across the random fusion boundary from the side of Inconel 182 to 316SS, but a hardening phenomenon appeared in the epitaxial fusion boundary zone because of its fine cellular microstructure. - Highlights: • Two typical fusion boundaries alternately distributed in the fusion interface • The microstructure, composition and hardness across fusion boundary depended on its type. • Different regions in welded joint have different special CSL value boundaries. • Hardening phenomenon only appeared in the epitaxial fusion boundary.
Highlights: • Heat conduction strongly affects the microstructural development. • Heat conduction conditions changes with increasing part height. • Anisotropic microstructural development affects the microhardness of the part. • Anisotropic mechanical properties along the structure are assumed. - Abstract: Wire-based additive manufacturing has been increasingly investigated in recent years. Although it is possible nowadays to manufacture structures that are free from inner defects such as porosity and cracks using wire and arc additive manufacturing, there is still a lack of knowledge regarding wire-based laser metal deposition of aluminium and its alloys. In order to be able to produce locally tailored part properties, it is necessary to understand the process parameter to material property relationships. Using laser energy sources, it becomes possible to analyse in detail the heat input and to observe occurring microstructural evolutions. This work includes a microstructural and mechanical characterization of an AA5087 wall structure. Detailed analyses of the chemical composition, texture, and microhardness of the structure have been performed. The microstructure contains different grain orientations as well as grain shapes and sizes along the structure, resulting in locally different material properties. The results have been analysed and discussed in reference to fundamental theories such as the Hall–Petch and Orowan mechanisms.