Engineering PapersSearch

SEARCH · Engineering Papers

Results for “Low-cycle fatigue”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

DROP DURABILITY ASSESSMENT OF ELECTRONIC ASSEMBLIES UNDER OFF-AXIS LOADING WITH SKEWED FIXTURES

This thesis studies drop durability of electronic assemblies when the acceleration vector is oriented at 45° to the out-of-plane direction of the circuit card. The off-axis drop tests are accomplished with a skewed fixture and are conducted as a proxy for multiaxial drop testing. Advanced shock testing and vibration test methods have been developed over the last few decades to better represent real-world field environments during ground-based laboratory testing. However, many of these test methods require expensive and specialized equipment not available in most laboratories. An alternative approach for approximating simultaneous loading along multiple axes on conventional equipment utilizes skewed fixtures which have seen use in off-axis random vibration and drop impact testing. These methods generally rely on the conversion of a uniaxial input load from the test equipment (using a uniaxial drop tower or shaker) into a multiaxial load when resolved in the reference frame of the test article (mounted on a skewed fixture). Skewed fixture design is presented and recommendations for conducting skewed angle drop testing are introduced based on local measurements along the skewed face of the fixture to accurately monitor the impact event. Characterization tests were performed with a skewed fixture, at simultaneous acceleration loads from 500 to 3,000 g in two (in-plane and out-of-plane) directions, while meeting standard time domain tolerances. Upon experimental characterization, drop shock durability tests were conducted on a printed circuit assembly (PCA). Mean drops-to-failure were measured and quantified with Weibull statistics. Dominant solder joint failure modes were identified via failure analysis. Prior work on inclined angle impact testing is limited, and the majority of solder joint interconnect level fatigue studies are conducted considering perpendicular loading normal the circuit card. Low-cycle fatigue curves are generated based on plastic strain and plastic work density within the solder joint. A multiscale nonlinear finite element model is used to relate board-level flexure to solder joint interconnect level plastic strain. A high strain rate solder constitutive model allows for accurate modeling of solder plasticity resulting from high-impact drop shock. Fatigue parameters are computed from the Coffin-Manson relation and Palmgren-Miner damage accumulation. This work serves to apply established low-cycle fatigue methods for conventional drop shock loading (impact normal to circuit card) to non-perpendicular loading with a skewed fixture.

Hower, Jonathan [Kansas City National Security Cam

Heterogeneous fatigue damage in a nickel-based single-crystal superalloy unraveled using correlative 3D X-ray technology

Nickel-based single-crystal (Ni-SX) superalloys under cyclic stress are susceptible to cracking at stress-concentration sites, eventually leading to low-cycle fatigue (LCF) failure. LCF cracks typically originate from intrinsic defects (e.g., voids and carbides) within solidified dendrites. However, systematic quantitative experimental analyses of defect-mediated local damage remain limited. To thoroughly understand the microscopic origins and evolution of LCF damage, correlated 3D mapping of dendrites across various regions is essential. Here, in this study, macroscale micro-computed tomography (μ-CT) was initially used to capture internal interdendritic secondary cracks within bulk DD413 superalloy after LCF testing at 760 °C. Subsequently, a multimodal methodology combining synchrotron 3D microdiffraction (3D-μXRD), high-resolution μ-CT, and electron microscopy was established. This approach allowed precise localization of internal damage zones near interdendritic secondary cracks and detailed mapping of the 3D correlated distributions of dendrites, defects, and residual stress/strain fields within these zones at submicron spatial resolution. Finally, the same approach was applied to specimens subjected to interrupted loading at approximately 40 % of the fatigue life to uncover the early damage states of dendrites. The dendrite cores (DCs) and interdendritic regions (IDs) exhibit microscale heterogeneous mechanical responses: nearly defect-free DCs accumulate local irreversible slip along specific slip systems to generate slip bands, while the IDs containing various defects accommodate local microplasticity through the activation of multiple slip systems around these defects. The local tensile stress near defects in the IDs exceeds that in the DC slip band regions by more than threefold, leading to the generation of local damage zones within the IDs. Chain-like defect distributions facilitate the interconnection of these local zones into a continuous damage region, further elevating the overall tensile stress in the IDs. Additionally, geometrically necessary dislocations alone are insufficient as indicators of LCF damage; both the internal stress state and its magnitude must be considered. These experimental results provide critical data and insights for the development of multi-physics fatigue models.

Localized deformation

In situ Visible Light and Thermal Imaging Data from a Laser Powder Bed Fusion Additive Manufacturing Process Co-Registered to X-ray Computed Tomography and Fatigue Data

This dataset is comprised of in situ sensing data collected during a laser-based powder bed fusion additive manufacturing process, as well as rasterized scan path information, post-build X-ray computed tomography (XCT), and fatigue test results. A total of 64 cylinders, approximately 15 mm in diameter and 102 mm tall, were printed out of stainless steel 316H on a Colibrium Additive Concept Laser M2 Series 5 machine. Parameters known to produce dense material were used to construct 56 of these cylinders, while the remaining 8 cylinders were printed with relatively high energy density parameters prone to producing keyhole pores. In addition, two spatter generation blocks were constructed upstream of the 64 cylinders such that ejecta produced during the melting of the spatter generators were stochastically seeded onto the 64 cylinders. Based on previous experiments, these spatter particles were theorized to produce stochastic lack-of-fusion pores. During the construction of the build, high-resolution images of reflected light in the visible spectrum were captured both before and after recoating for each print layer. Additionally, temporally integrated thermal imaging in the near infrared spectrum produced integrated sum and max images on a layerwise basis. The multimodal in situ data has been co-registered to the build plate coordinate system, allowing for identification of process anomalies (e.g., spatter particles) apparent in the two sensors. Following construction of the build, the cylinders were subjected to XCT to identify internal flaws, and the resulting data have also been registered to the build plate coordinate system. Finally, 60 of the 64 cylinders were machined into fatigue coupons conforming to ASTM E466 and subsequently subjected to either high- or -low-cycle fatigue testing. The results of the fatigue tests have also been included in the dataset, and the XCT data corresponded to the approximate location of the gauge sections of the machine fatigue specimen geometry.

42 ENGINEERING

Dual-precipitates enhance fatigue resistance in an additively manufactured high-entropy alloy

To accomplish the intense desire of high-strength materials for enhanced energy-efficiency, recent research applies a combined strategy of additive-manufacturing and precipitation-strengthening in high entropy alloys. In a context, Al 0.2 Co 1.5 CrFeNi 1.5 Ti 0.3 nanoprecipitation-strengthened system was developed, demonstrating very convincing strength and toughness. Moreover, additive-manufacturing facilitated additional strength by well-decorated cell-boundaries with blocky L2 1 precipitates and homogeneously distributed L1 2 precipitates. However, fatigue research of this alloy remained unexplored despite being the main precursor for structural applications. In this study low-cycle fatigue behavior of this alloy in both as-built and precipitation-strengthened (aged) conditions has been explored, combined with in-situ neutron diffraction investigation. Findings revealed a substantial cyclic-stress profile and a notable fatigue-life below ±0.50% strain-amplitude, exceeding 10 5 cycles at ±0.30% strain-amplitude. These demonstrate the potential to carry higher payloads with marked engineering-reliability. Residual-stress estimation revealed strain-compatibility between the matrix and L1 2 precipitate, indicating a crack-initiation immune interface. A comparative examination of dislocation character revealed shifting towards pure edge-character in aged alloy indicates precipitates promoted planar-slip during deformation.

36 MATERIALS SCIENCE

In-situ observations of cyclic deformation in an extruded Mg-2Nd-1Y-0.1Zr-0.1Ca alloy

In this study, the evolution of deformation mechanisms during cyclic loading in an extruded, solution-treated Mg–2Nd–1Y–0.1Zr–0.1Ca alloy was investigated using a combination of in-situ loading, scanning electron microscopy (SEM), electron backscatter diffraction (EBSD), and focused ion beam (FIB) nanofabrication. The initial microstructure exhibited a random crystallographic texture with no preferred grain orientation. Flat, rectangular dog-bone specimens were subjected to load-controlled, fully reversed fatigue for 50 cycles, during which the same region was sequentially mapped to track microstructural changes. After 10 cycles of loading deformation twins were observed. During tensile reloading detwinning or narrowing of those twinned regions occurred. After 20 cycles, detwinning ceased and residual twins remained in the material. SEM imaging revealed numerous surface slip traces after cyclic loading. EBSD-assisted slip trace analysis identified the activation of prismatic and pyramidal < c+a> slip systems during low-cycle fatigue. Site-specific scanning transmission electron microscopy (STEM) further revealed that deformation was also accommodated by basal < a> slip and the dissociation of < c+a> dislocations. Center-of-symmetry (COS) analysis confirmed that the dissociation of < c+a> dislocations resulted in the formation of I₁ intrinsic stacking faults after cyclic loading. These findings provide new insights into the complex interplay of dislocation mechanisms governing fatigue deformation in rare-earth-containing Mg alloys.

Cyclic deformation

Evaluation of thermal energy storage for central receiver concentrating solar power plants under charging cycles through structural assessment

Electricity production by concentrated solar power (CSP) systems has stood out among energy transition alternatives due to their large generation capacity (between 30 MW and 400 MW) and high capacity factor (80%) when incorporating thermal storage systems (TES). Although TES tanks in operation worldwide are made of austenitic steels with remarkable mechanical and anticorrosive properties, operational failures have been reported due to low-cycle fatigue, creep, and the abrupt release of residual stresses generated during tank manufacturing. A critical operation for salt tanks is the initial daily charging operation, given the low fluid level and the thermal gradients between the inventory and the salt entering the tank. This study presents a structural simulation of a 39.6 m-diameter molten salt tank for central receiver CSP plants, accounting for temperature and pressure variations during charging and different sparger ring inlet configurations. The initial pre-stressed condition of the floor, resulting from the manufacture of welded plates, is used as a boundary condition. The fatigue and creep life analyses were performed in accordance with the ASME BPVC and API standards. It was found that the tank's floor is in a less favourable mechanical condition than the wall, due to its initial manufacturing condition and the maximum temperature differences during charging. A critical zone was identified in an area affected by residual stress on the floor and under the sparger ring. The baseline sparger ring configuration, with 52 2-inch-diameter orifices and a flow direction of 90 degrees , results in an average floor stress of approximately 25 MPa and creep damage after 1.2 years of tank operation.

14 SOLAR ENERGY

Advanced Materials & Manufacturing Technology (AMMT): Process understanding for qualifying LPBF 316H SS

Investigations were conducted in fiscal years (FY) 2023 and 2024 to gather relevant data sets addressing challenges related to qualifying 316H stainless steel (SS) for use in future nuclear reactors. This work was a collaborative effort involving researchers from Idaho National Laboratory (INL), Argonne National Laboratory (ANL), and Oak Ridge National Laboratory (ORNL). Key outcomes included: • Development of process-structure-property data sets to better understand the relationships between manufacturing processes, material structure, and performance characteristics. • Establishment of an in-situ monitoring system to link these various data sets together. • Detailed characterization of the raw material feedstock to further strengthen the understanding of process-structure and process-property relationships. Building on this foundation, in FY25 there was interest in exploring the behavior of additively manufactured 316H SS under different test conditions to support the overall material qualification process. Los Alamos National Laboratory (LANL) was tasked with providing specimen samples to the collaborating labs, who then conducted a round-robin study examining factors like selective heat treatment, low-cycle fatigue (LCF), and tensile-creep (T-C) properties. Additionally, high-temperature differential scanning calorimetry (DSC) was performed by LANL to better understand how the material's thermal characteristics change as it is heated up to the melting point. This provided a more comprehensive understanding of the material's behavior. The combined results from these investigations could potentially be used to support the inclusion of 316H stainless steel in Section III, Division 5 of the relevant codes and standards, allowing its use in future nuclear reactor applications.

36 MATERIALS SCIENCE

Microstructural Evolution and Mechanical Properties of LP-DED NASA HR-1 – A Hydrogen Resistant AM Superalloy for Space Propulsion Applications

The National Aeronautics and Space Administration (NASA) has actively pursued metal additive manufacturing (AM) technologies for spaceflight applications since the late 2000s. AM offers transformative advantages in cost, schedule, part consolidation, and design flexibility. Among the various AM techniques, laser powder directed energy deposition (LP-DED) is particularly well suited for fabricating complex geometries with fine feature resolution. In propulsion systems that utilize high-pressure gaseous hydrogen—such as liquid hydrogen rocket engines—hydrogen environment embrittlement (HEE) presents a serious threat to material performance 1,2 . Mechanical property degradation under these conditions can compromise component reliability, especially under cyclic loading. To address this challenge, NASA developed NASA HR-1 (Hydrogen Resistant-1) as a solution for liquid rocket engine components operating in hydrogen-rich environments, using the LP-DED technique 3-9 . A key component in a liquid rocket engine is the exhaust nozzle, which is typically regeneratively cooled (regen) due to the high heat flux. NASA HR-1 was specifically developed for regen nozzle applications using hydrogen as a propellant, providing resistance to HEE, a critical issue for many materials. The AM version of NASA HR-1 was also formulated to achieve high ultimate tensile strength, along with high yield strength and ductility in this environment 5,6 . Low-cycle fatigue (LCF) is another important consideration in nozzle design, as components are expected to endure multiple starts and missions. Additionally, the LP-DED version of the alloy exhibits improved thermal conductivity compared to its wrought counterpart, which benefits nozzle cooling. Overall, NASA HR-1 offers an excellent balance of high strength, HEE resistance, LCF performance, thermal conductivity, and ductility to meet the demanding requirements of channel-cooled nozzles and other components used with hydrogen and other propellants. The LP-DED–processed NASA HR-1 requires several post-processing heat treatment steps to achieve the material properties desirable for its intended application 6 . These steps include stress relief, homogenization, solution annealing, and aging for precipitation hardening. The stress relief treatment mitigates residual stresses accumulated during the LP-DED process and minimizes the potential for distortion. Homogenization, a common step for AM materials, reduces elemental segregation and promotes recrystallization to develop a more equiaxed grain structure. The subsequent solution annealing treatment heats the part to a solid solution temperature to dissolve the undesirable η-phase that forms during cooling from homogenization, followed by rapid cooling to retain an η-phase–free microstructure. Finally, aging promotes precipitation of the strengthening γ′ phase in the alloy. The integration of compositional design and optimized thermal processing enables high-quality LP-DED NASA HR-1 components with excellent microstructural and mechanical stability. Improved chemical and microstructure homogeneity enhances ductility and fatigue resistance—both critical for safe and reliable operation in high-pressure hydrogen environments. NASA has successfully fabricated and hot-fire tested multiple subscale and full-scale channel wall nozzles using LP-DED NASA HR-1 5,6, 9-14 . These efforts included process refinements to support thin-wall construction and various channel geometries. Throughout development, several key observations emerged. After homogenization, the as-built columnar grain structure transforms into a fully equiaxed microstructure. However, subsequent treatments—such as solution annealing and aging—result in changes that are more difficult to track. The grain structure remains largely unchanged, and the γ′ precipitates, typically 5–10 nm in diameter, are beyond the resolution of scanning electron microscopy (SEM). While transmission electron microscopy (TEM) can resolve these fine precipitates, TEM sample preparation is time-consuming and difficult for LP-DED material. As an alternative, differential scanning calorimetry (DSC) offers a useful, qualitative approach to monitor precipitate evolution throughout different stages of heat treatment. The overall goal is to improve the understanding of how heat treatment affects the microstructure and mechanical performance of LP-DED NASA HR-1. This paper presents heat treatment design considerations, microstructural characterization, mechanical testing – including tensile and LCF testing in both air and hydrogen environments.

Superalloy

A Combined Computational and Mathematical Analysis of Interconnect Fatigue Potential in Photovoltaic Modules

A finite element model of a 60-cell monocrystalline silicon glass-polymer photovoltaic module was simulated with ±1.0 kPa and ±2.4 kPa loads applied to the glass to calculate the deformation under load. Cell-to-cell displacements were used to approximate interconnect strain and stress. A mathematical fatigue cycle life relation was fitted to data for the interconnect material (copper), to generate a life prediction at each interconnect location based on the local stress means, reversal extents, and amplitudes. Interconnect stress was found to be significantly asymmetric about zero despite symmetric positive and negative module loads due to laminate thickness offsets about the neutral plane and the effects of module framing. Cycle life results indicated that interconnect fatigue failure was unlikely to occur over a 30-year lifetime of conservative wind and snow load cycles since the typical cell design feature of leaving some unconstrained length between the cell edge and first solder pad increases the effective gauge length and decreases the stress levels below the material endurance limit. Follow-up analyses found that 3.6 mm and 6.4 mm were the minimum unconstrained lengths required to survive the assumed lifetime of wind and snow cycles, respectively, confirming that typical industrial module constructions with 8–15 mm unconstrained lengths should survive conservatively. Notably, large magnitude, low-cycle snow loading was consistently the limiting factor requiring a longer unconstrained interconnect length. Finally, insights and workflows from this study inform module interconnection design limits for survival against mechanical fatigue in deployment environments.

14 SOLAR ENERGY