Materials Data on K(FeP)2 by Materials Project

K(FeP)2 is alpha bismuth trifluoride-derived structured and crystallizes in the tetragonal I4/mmm space group. The structure is three-dimensional. K1+ is bonded in a body-centered cubic geometry to eight equivalent P3- atoms. All K–P bond lengths are 3.40 Å. Fe+2.50+ is bonded to four equivalent P3- atoms to form a mixture of edge and corner-sharing FeP4 tetrahedra. All Fe–P bond lengths are 2.19 Å. P3- is bonded in a 4-coordinate geometry to four equivalent K1+ and four equivalent Fe+2.50+ atoms.

36 MATERIALS SCIENCE↗

Manipulating Spin–Lattice Coupling in Layered Magnetic Topological Insulator Heterostructure via Interface Engineering

Induced magnetic order in a topological insulator (TI) can be realized either by depositing magnetic adatoms on the surface of a TI or engineering the interface with epitaxial thin film or stacked assembly of 2D van der Waals (vdW) materials. Herein, the observation of spin-phonon coupling in the otherwise non-magnetic TI Bi 2 Te 3 is reported, due to the proximity of FePS 3 (an antiferromagnet (AFM), T N ≈ 120 K), in a vdW heterostructure framework. Temperature-dependent Raman spectroscopic studies reveal deviation from the usual phonon anharmonicity originated from spin-lattice coupling at the Bi 2 Te 3 /FePS 3 interface at/below 60 K in the peak position (self-energy) and linewidth (lifetime) of the characteristic phonon modes of Bi 2 Te 3 (106 and 138 cm –1 ) in the stacked heterostructure. The Ginzburg-Landau (GL) formalism, where the respective phonon frequencies of Bi 2 Te 3 couple to phonons of similar frequencies of FePS 3 in the AFM phase, is adopted to understand the origin of the hybrid magneto-elastic modes. At the same time, the reduction of characteristic TN of FePS 3 from 120 K in isolated flakes to 65 K in the heterostructure, possibly due to the interfacial strain, which leads to smaller Fe-S-Fe bond angles as corroborated by computational studies using density functional theory (DFT). Besides, inserting hexagonal boron nitride within Bi 2 Te 3 /FePS 3 stacking regains the anharmonicity in Bi 2 Te 3 . As a result, controlling interfacial spin-phonon coupling in stacked heterostructure can have potential application in surface code spin logic devices.

36 MATERIALS SCIENCE↗

Performance test of a laboratory pump liquid transfer based on the fountain effect

A laboratory scale pump has been tested in detail in order to determine the flow characteristics of a heater-activated all-metal thermomechanical pump (fountain effect pump, FEP). The emphasis is on the functional dependence of the fountain pressure difference versus mass throughput. A modified Vote et al. (1971) power law approximation is employed for a simplified description of the flow rate as a function of the driving force. Flow rates of up to 10 liters/(hr/sq cm) have been obtained despite a large nominal pore size of the porous plug of 2 microns (filtration rating) used for the FEP.

Chen, W. E. W.↗

Accelerated Alpha-s deterioration in a geostationary orbit

Between the Teflon substrate and the interference filter a 2 micron varnish layer was sandwiched in. The bending radius of the SSM, measured on a cone, decreased from about 13 mm to 6 mm prior to interference filter fracture, due to increased tensile strength of its substrate. These samples, and for comparison samples of the same make but without varnish and a conductive layer were included in the test. Additionally 2 Teflon FEP samples without the protective interference filter, one of them with a conductive layer, were tested. The sample substrate was 125 micron Teflon FEP, with vapor deposited silver reflector and a thin Inconel film for corrosion protection.

Husmann, O. K.↗

Evaluation of Low Earth Orbit Environmental Effects on International Space Station Thermal Control Materials

Samples of International Space Station (ISS) thermal control coatings were exposed to simulated low Earth orbit (LEO) environmental conditions to determine effects on optical properties. In one test, samples of the white paint coating Z-93P were coated with outgassed products from Tefzel(R) (ethylene tetrafluoroethylene copolymer) power cable insulation as-may occur on ISS. These samples were then exposed, along with an uncontaminated Z-93P witness sample, to vacuum ultraviolet (VUV) radiation to determine solar absorptance degradation. The Z-93P samples coated with Tefzel(R) outgassing products experienced greater increases in solar absorptance than witness samples not coated with Tefzel(R) outgassing products. In another test, samples of second surface silvered Teflon(R) FEP (fluorinated ethylene propylene), SiO. (where x=2)-coated silvered Teflon(R) FEP, and Z-93P witness samples were exposed to the combined environments of atomic oxygen and VLTV radiation to determine optical properties changes due to these simulated ISS environmental effects. This test verified the durability of these materials in the absence of contaminants.

Dever, Joyce A.↗

Comparison of Hyperthermal Ground Laboratory Atomic Oxygen Erosion Yields With Those in Low Earth Orbit

The atomic oxygen erosion yields of 26 materials (all polymers except for pyrolytic graphite) were measured in two directed hyperthermal radio frequency (RF) plasma ashers operating at 30 or 35 kHz with air. The hyperthermal asher results were compared with thermal energy asher results and low Earth orbital (LEO) results from the Materials International Space Station Experiment 2 and 7 (MISSE 2 and 7) flight experiments. The hyperthermal testing was conducted to a significant portion of the atomic oxygen fluence similar polymers were exposed to during the MISSE 2 and 7 missions. Comparison of the hyperthermal asher prediction of LEO erosion yields with thermal energy asher erosion yields indicates that except for the fluorocarbon polymers of PTFE and FEP, the hyperthermal energy ashers are a much more reliable predictor of LEO erosion yield than thermal energy asher testing, by a factor of four.

Flight tests↗

A technique for synergistic atomic oxygen and vacuum ultraviolet radiation durability evaluation of materials for use in LEO

Material erosion data collected during flight experiments such as the Environmental Oxygen Interaction with Materials (EOIM)-3 and the Long Duration Exposure Facility (LDEF) have raised questions as to the sensitivity of material erosion to levels of atomic oxygen exposure and vacuum ultraviolet (VUV) radiation. The erosion sensitivity of some materials such as FEP Teflon used as a thermal control material on satellites in low Earth orbit (LEO), is particularly important but difficult to determine. This is in large part due to the inability to hold all but one exposure parameter constant during a flight experiment. This is also difficult to perform in a ground based facility, because often the variation of the level of atomic oxygen or VUV radiation also results in a change in the level of the other parameter. A facility has been developed which allows each parameter to be changed almost independently and offer broad area exposure. The resulting samples can be made large enough for mechanical testing. The facility uses an electron cyclotron resonance plasma source to provide the atomic oxygen. A series of glass plates is used to focus the atomic oxygen while filtering the VUV radiation from the plasma source. After filtering, atomic oxygen effective flux levels can still be measured which are as high as 7 x 10(exp 15) atoms/cm(exp 2)-sec which is adequate for accelerated testing. VUV radiation levels after filtering can be as low as 0.3 suns. Additional VUV suns can be added with the use of deuterium lamps which allow the VUV level to be changed while keeping the flux of atomic oxygen constant. This paper discusses the facility, and results from exposure of Kapton and FEP at pre-determined atomic oxygen flux and VUV sun levels.

Rutledge, Sharon K.↗

Solar array system for solar maximum mission

The paper describes the design of the solar array system (SAS) for the Solar Maximum Mission, the unique features of the SAS, and the results of its successful in-orbit operation. It is noted that the array was unique in that: (1) major weight concessions were made to produce a dynamically stiff array; (2) it was the first array designed to be compatible with the NASA Multimission Modular Spacecraft; (3) it is the first jettisonable solar array; and (4) it represents the first use of FEP-bonded overslides on a prime power array. It is concluded that the array performed as predicted with no evidence of the FEP causing any unusual array power degradations. In addition, the deployment and telemetry systems performed as designed.

Meese, R. A.↗

The Future of Astronaut Nutrition: Daily Production of Kefir Nutrient Packs in a Lunar Analog Mission

Astronaut nutrition will need to be supplemented with fresh nutrients and probiotics for long duration space travel. Kefir is a fermented milk beverage that provides probiotic bacteria, protein, calcium, and vitamin K. It has been historically cultured for thousands of years and is a modern-day health food. During the BioNutrients-2 experiment, one generation of kefir was cultured by astronauts on the ISS in fluorinated ethylene propylene (FEP) bags. This follow-on experiment aimed to test the hypothesis that kefir can be produced at ambient temperatures and safely passaged to make a series of nutrient packs in an analog environment. The Hawaiian Space Exploration Analog and Simulation (HI-SEAS) is a semi-controlled habitat located on the Mauna Loa volcano on the island of Hawaii at 2,500 m elevation. The recent EMMIHS (EuroMoonMars, International MoonBase Alliance, HI-SEAS) missions comprised of interdisciplinary, international crews for mock lunar missions. During a six-day mission in March 2024, crew members tested continuous passaging of kefir cultures (C-FIR commercial strain). After approximately 24 hours of growth, a portion of culture was used to seed the next generation of culture bags for four passages. A color board and pH indicator allowed the crew to easily determine when the culture had reached optimal pH. Laboratory analysis at NASA Ames Research Center showed that the pH met Kefir standards (<5). The yeast and lactic acid bacteria were in normal range and no contamination was detected in the final passage. By successfully accomplishing this experiment the team has demonstrated the ability to safely produce daily cultures of kefir in a microgravity applicable growth system.

Astronaut nutrition↗

Experimental verification of a tank to tank He II transfer model with trade study results

A computer program has been developed to study the thermodynamics of tank to tank superfluid helium transfer. The model includes a supply and a receiver tank connected by a transfer line. The convey of He II from one tank to the other is controlled by a fountain effect pump (FEP). Phase separators are present in both the supply and receiver tank to regulate the bath temperature. Description of this model has been published elsewhere. In the present paper, data from a transfer experiment are used to verify the accuracy of this model. The experiment consisted of an FEP made of a 2-micron sintered stainless steel porous plug. Superfluid has been transferred from a liquid helium bath into a glass beaker. Bath temperatures, flowrate and heater power records are available. These results are compared to the predictions of the computer program and good agreement is found between the two. This model is very useful for the study and design of superfluid transfer systems, e.g., the Superfluid Helium Tanker (SFHT) and the Particle Astrophysics Magnet Facility (ASTROMAG).

Yuan, S. W. K.↗

Solar maximum: Solar array degradation

The 5-year in-orbit power degradation of the silicon solar array aboard the Solar Maximum Satellite was evaluated. This was the first spacecraft to use Teflon R FEP as a coverglass adhesive, thus avoiding the necessity of an ultraviolet filter. The peak power tracking mode of the power regulator unit was employed to ensure consistent maximum power comparisons. Telemetry was normalized to account for the effects of illumination intensity, charged particle irradiation dosage, and solar array temperature. Reference conditions of 1.0 solar constant at air mass zero and 301 K (28 C) were used as a basis for normalization. Beginning-of-life array power was 2230 watts. Currently, the array output is 1830 watts. This corresponds to a 16 percent loss in array performance over 5 years. Comparison of Solar Maximum Telemetry and predicted power levels indicate that array output is 2 percent less than predictions based on an annual 1.0 MeV equivalent election fluence of 2.34 x ten to the 13th power square centimeters space environment.

Miller, T.↗

MISSE PEACE Polymers Atomic Oxygen Erosion Results

Forty-one different polymer samples, collectively called the Polymer Erosion and Contamination Experiment (PEACE) Polymers, have been exposed to the low Earth orbit (LEO) environment on the exterior of the International Space Station (ISS) for nearly 4 years as part of Materials International Space Station Experiment 2 (MISSE 2). The objective of the PEACE Polymers experiment was to determine the atomic oxygen erosion yield of a wide variety of polymeric materials after long term exposure to the space environment. The polymers range from those commonly used for spacecraft applications, such as Teflon (DuPont) FEP, to more recently developed polymers, such as high temperature polyimide PMR (polymerization of monomer reactants). Additional polymers were included to explore erosion yield dependence upon chemical composition. The MISSE PEACE Polymers experiment was flown in MISSE Passive Experiment Carrier 2 (PEC 2), tray 1, on the exterior of the ISS Quest Airlock and was exposed to atomic oxygen along with solar and charged particle radiation. MISSE 2 was successfully retrieved during a space walk on July 30, 2005, during Discovery s STS-114 Return to Flight mission. Details on the specific polymers flown, flight sample fabrication, pre-flight and post-flight characterization techniques, and atomic oxygen fluence calculations are discussed along with a summary of the atomic oxygen erosion yield results. The MISSE 2 PEACE Polymers experiment is unique because it has the widest variety of polymers flown in LEO for a long duration and provides extremely valuable erosion yield data for spacecraft design purposes.

deGroh, Kim, K.↗

Effect of Air and Vacuum Storage on the Degradation of X-Ray-Exposed Aluminized-Teflon Investigated

Metalized Teflon FEP (fluorinated ethylene propylene, DuPont), a common thermal control material, has been found to degrade in the low-Earth-orbit space environment. The aluminized-FEP (Al-FEP) exterior layer on the Hubble Space Telescope has become extremely embrittled, with extensive cracking occurring on all sides of the telescope. This embrittlement has been primarily attributed to radiation exposure (x-rays from solar flares, electron/proton radiation, and possibly near-ultraviolet radiation) combined with thermal cycling. Limited samples of FEP tested after long-term exposure to low Earth orbit on the Hubble Space Telescope and on the Long Duration Exposure Facility indicated that there might be continued degradation in tensile properties over time. An investigation was conducted at the NASA Glenn Research Center to evaluate the effect of air and vacuum storage on the mechanical properties of x-ray-exposed FEP. Aluminized-FEP (5-mil-thick) tensile samples were x-ray exposed with 15.3-kV copper xrays for 2 hr, reducing the percent elongation to failure by approximately 50 percent in comparison to that for pristine Al-FEP. X-ray-exposed samples were stored in air or under vacuum for various time periods to see the effect of storage on tensile properties. Tensile results indicated that samples stored in air had larger decreases in tensile properties than samples stored under vacuum had, as seen in the graph. Samples stored under vacuum (for up to 400 hr) showed no further decrease in tensile properties over time, whereas samples stored in air (for up to 900 hr) appeared to show decreases in tensile properties over time. X-ray-exposed samples stored in air developed a hazy appearance in the exposed area, as seen in the photographs. When the source of the haziness was evaluated using scanning electron microscopy and atomic force microscopy, it was found to reside at the Al/FEP interface as witnessed by an increased surface roughness of the aluminized side of the material and a dramatic decrease in the adhesion between the Al and FEP. Optical properties of air-stored irradiated samples showed an increase in the diffuse reflectance, which is consistent with observed roughening that was characterized by AFM. These findings indicate that air exposure helps degrade x-ray-irradiated FEP. These results indicate that proper sample handling and storage is necessary with space-retrieved materials and with those exposed to ground-based irradiation simulation exposures.

deGroh, Kim K.↗

Erosion Data from the MISSE 8 Polymers Experiment After 2 Years of Space Exposure on the International Space Station

The Polymers Experiment was exposed to the low Earth orbit (LEO) space environment for 2.14 and 2.0 years as part of the Materials International Space Station Experiment 8 (MISSE 8) and the Optical Reflector Materials Experiment-III (ORMatE-III), respectively. The experiment contained 42 samples, which were flown in either ram, wake, or zenith orientations. The primary objective was to determine the effect of solar exposure on the atomic oxygen erosion yield (Ey) of fluoropolymers. This paper provides an overview of the experiment with details on the polymers flown, the characterization techniques used, the atomic oxygen fluence for each exposure orientation, and the LEO Ey results. The Ey values for the fluoropolymers range from 1.45 x 10(exp -25) cm(exp 3)/atom for white Tedlar Registered Trademark (polyvinyl fluoride with white titanium dioxide pigment) flown in the ram orientation to 6.32 x 10(exp -24) cm(exp 3)/atom for aluminized-Teflon Registered Trademark fluorinated ethylene propylene (Al-FEP) flown in the zenith orientation. Erosion yield data for FEP flown in ram, wake and zenith orientations are compared, and the Ey was found to be highly dependent on orientation, hence environmental exposure. Teflon FEP had an order of magnitude higher Ey when flown in the zenith direction (6.32 x10(exp -24) cm(exp3)/atom) as compared to the ram direction (2.37 x 10(exp -25) cm(exp 3)/atom). The Ey of FEP was found to increase with a direct correlation to the solar exposure/AO fluence ratio showing the effect of solar radiation and/or heating due to solar exposure on FEP erosion. In addition, back-surface carbon painted FEP (C-FEP) flown in the zenith orientation had a significantly higher Ey than clear FEP or Al-FEP further indicating that heating has a significant impact on the erosion of FEP, particularly in the zenith orientation.

Solar radiation↗

Contamination Results of MISSE 8 Wake and Nadir Samples After 2 Years of Space Exposure on the International Space Station

Spacecraft in low Earth orbit (LEO) are subjected to harsh environmental conditions, including radiation (cosmic rays, ultraviolet, x-ray and charged particle radiation), micrometeoroids and orbital debris, temperature extremes, thermal cycling, and atomic oxygen. In addition, on-orbit spacecraft contamination is a serious spaceflight issue, with silicone contamination being a particular concern. In an effort to understand on-orbit contamination of Materials International Space Station Experiment 8 (MISSE 8) flight samples and other International Space Station (ISS) payloads, contamination studies were conducted post-flight on retrieved Teflon fluorinated ethylene propylene (FEP) samples flown in the wake and nadir orientations on MISSE 8. The wake sample was Teflon FEP (M8-W11) flown as part of the Glenn MISSE 8 Polymers Experiment on the Optical Reflector Materials Experiment-III Ram/Wake (ORMatE-III R/W) tray and exposed to the LEO wake environment for 2.0 years. The nadir samples were silver-Teflon FEP radiator pieces taken from the MISSE 8 Single Events Upset Xilinx-Sandia Experiment II (SEUXSE II) Power Box and exposed to the LEO nadir environment for 2.14 years. The Teflon FEP flight materials were analyzed for changes in surface morphology and chemistry as compared to pristine control samples. The wake samples were also analyzed for changes in optical properties. There was no evidence of a molecular contamination layer present on the surface of the MISSE 8 wake or nadir facing Teflon FEP flight samples, although both the wake and nadir flight samples contained particulate contamination in some regions. The analyzed nadir particles were primarily zinc rich. The majority of analyzed wake particles were comprised of oxidized aluminum with small amounts of zinc and magnesium. The wake particles appear to have arrived early in the mission (or pre-flight) during a single event. This paper provides details of the MISSE 8 sample contamination analyses.

Erosion↗

Erosion Results of the MISSE 8 Polymers Experiment After 2 Years of Space Exposure on the International Space Station

Polymers and other oxidizable materials on the exterior of spacecraft in the low Earth orbit (LEO) space environment can be eroded due to reaction with atomic oxygen (AO). Therefore, in order to design durable spacecraft, it is important to know the LEO AO erosion yield (E(sub y), volume loss per incident oxygen atom) of materials susceptible to AO reaction. A spaceflight experiment, called the Polymers Experiment, which contained 42 samples, was developed to determine the effect of solar exposure on the AO E(sub y) of fluoropolymers flown in ram, wake, or zenith orientations. The Polymers Experiment was exposed to the LEO space environment on the exterior of the International Space Station (ISS) as part of the Materials International Space Station Experiment 8 (MISSE 8) mission. The MISSE 8 mission included samples flown in a zenith/nadir orientation for 2.14 years in the MISSE 8 Passive Experiment Container (PEC), and samples flown in a ram/wake orientation for 2.0 years in the Optical Reflector Materials Experiment-III (ORMatEIII) tray. The experiment included Kapton H (Registered Trademark) witness samples for AO fluence determination in each orientation. This paper provides an overview of the MISSE 8 mission, a description of the flight experiment with details on the polymers flown, the characterization techniques used, the AO fluence for each exposure orientation, and the LEO E(sub y) results. The E(sub y) of Teflon fluorinated ethylene propylene (FEP) samples flown in ram, wake, and zenith orientations have been compared, and the E(sub y) was found to be highly dependent on orientation and therefore environmental exposure. The FEP E(sub y) was found to directly correlate with the solar exposure/AO fluence ratio showing the effect of solar radiation and/or heating due to solar exposure on FEP erosion. In addition, back-surface carbon painted FEP (C-FEP) flown in the zenith orientation had a significantly higher E(sub y) than clear FEP or Al-FEP further indicating that heating has a significant impact on the erosion of FEP. This experiment provides valuable LEO flight data on the erosion of Teflon FEP, a commonly used spacecraft thermal insulation.

Teflon↗

Nuclear Criticality Safety Assessment of Criticality Control Containers without Moderation Control at the Waste Isolation Pilot Plant

The Waste Isolation Pilot Plant (WIPP) provides for safe, permanent disposal of government-owned transuranic (TRU) and TRU mixed wastes. Receipt and disposal of waste at the WIPP site began in March 1999. The Sandia report, Consideration of Nuclear Criticality When Disposing of Transuranic Waste at the Waste Isolation Pilot Plant, addressed potential nuclear criticality safety issues based on the projected inventory characteristics known at the time [1]. As designs for inventory, waste forms, and disposal packages have changed, new analyses have been performed, and updates have been made to address any potential effects to the WIPP safety basis. New analyses performed include Saylor 2017 [2] and Brickner 2019 [3], which address certain waste containers with specified loadings under post-closure conditions. Both examined several hypothetical scenarios and included analyses to bound (from a criticality potential standpoint) credible configurations that could occur at WIPP during the repository regulatory post-closure disposal time period for feature, event, and process (FEP) considerations—10,000 years. During this post-closure period at WIPP, the screening of FEPs is governed by the risk-based standards and implementing regulations of the US Environmental Protection Agency (EPA) (i.e., 40 CFR 191 and 40 CFR 194, respectively) [4,5]. An FEP screening can be based on either a low-consequence or low-probability rationale. A low-probability rationale includes either (a) a qualitative rationale that the FEP is not credible or (b) a quantitative demonstration that the probability is less than 10-4 in 104 years. In this evaluation, a qualitative lowprobability rationale of not credible is used by demonstrating that bounding configurations of the waste are not critical. The demonstration of subcriticality is through quantitative calculations, but a probability of criticality is not evaluated. Rather, the rationale for this evaluation is that bounding configurations with an effective neutron multiplication factor (keff) well below the upper subcriticality limit (USL) make criticality incredible. Reference [2] documented a nuclear criticality assessment of the WIPP repository for disposal of dilute surplus plutonium materials using the Dilute and Dispose Approach and packaging in criticality control overpacks (CCOs). The CCO is the waste disposal container recently designed to allow for up to 380 fissile gram equivalent (FGE) 239 Pu per drum, which is a higher fissile loading than typical waste containers. The CCO consists of a criticality control container (CCC) positioned by upper and lower plywood spacers within a standard 55 gal drum. The CCC is used to establish a geometry control for fissile materials during transportation and WIPP emplacement operations. The current WIPP waste acceptance criteria for CCO payloads limit beryllium to less than or equal to 1% by weight of the waste contents and require the waste form to be non-machine compacted. Reference [2] considered two scenario progressions—room closure from salt creep, hereafter referred to as the reconfigured dry scenario, and flooding with brine, hereafter referred to as the reconfigured wet scenario. The subsequent drying out of the reconfigured wet scenarios was also considered. For all scenarios, subcriticality was maintained when 50 g of B 4 C (acting as a neutron absorber) per CCC was intermixed within the plutonium disposition waste form. The analysis used a waste form description that limits the amount of moderation that could be present within the waste form (i.e., it limits the amount of water and polyethylene that could be present based on planned processing conditions). This analysis to evaluate increased limits on the amount of moderation that could be present was performed as a companion to Reference [2] to address concerns associated with verifying moisture and/or plastic contents of waste materials following packaging of dilute surplus plutonium in the CCO. To that end, this analysis used the models and methods from Reference [2] to evaluate a more generic base waste form consisting of water and polyethylene that is more similar (and nearly identical) to the generic waste forms utilized in other models/analyses supporting the TRU Package Transporter Model II (TRUPACTII) safety analysis [6] (all are without moderation controls). The waste form in this analysis uses a base mixture of 75% water and 25% polyethylene, the total amount of which is varied to determine the optimum moderation to fissile material (H/Pu) ratio. The fissile loading is maintained at up to 380 FGE 239 Pu (modeled as PuO 2 ) per CCO with an additional 545 g of beryllium (to bound the 1% by weight contents restriction) and 50 g of B 4 C intermixed per CCO. The beryllium content (1% by weight) is based on the total allowed waste weight (this does not include packaging and container weights). Figures ES-1 and ES-2 display summary results, showing that with this model including 50 g of B 4 C per CCO, the system keff remains under 0.85 for all moderator amounts and provides a significant margin against post-closure criticality under postulated bounding conditions for compaction. Figure ES-1 compares an infinite model with a room model at the initial emplacement spacing and under full radial compaction. Full radial compaction places each CCC in direct contact and does not credit any anticipated spacing associated with current post-closure geomechanical modeling of the repository [7]. The effects of variations in the H/Pu ratio were evaluated by varying the amount of the water/polyethylene component of the waste model, with fissile loading maintained at 380 239 Pu FGE. Similarly, Figure ES-2 illustrates how various amounts of B 4 C per CCO influence k eff at different radial compactions, all at the H/Pu ratio of 200 (in the room array model). Therefore, while the results from Saylor 2017 [2] modeled more realistic process limits associated with packaging of dilute surplus plutonium, this analysis demonstrates that limits on moderation (plastic and water content) are not necessary to ensure subcriticality in the WIPP repository, provided the requisite B 4 C absorber is present.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗