Influence of Iron Ore Addition on Metallurgical Reaction Behavior of Iron Coke Hot Briquette
Utilization of iron coke hot briquette (ICHB) has been considered to be one effective countermeasure to achieve low-carbon blast furnace. Before its actual application, a series of extensive fundamental investigations on the ICHB are required. In this study, the influence of iron ore addition on the metallurgical reaction behavior of ICHB made from carbonizing coal–iron ore composite agglomeration were investigated based on Chinese raw material conditions, and the corresponding mechanisms were revealed. The results show that the addition of iron ore concentrate leads to the degradation of the compressive strength and drum strength of ICHB, but they are maintained at a relatively high level. Furthermore, by increasing the addition ratio of iron ore from 0 to 20 pct, the density of ICHB is enhanced from 1413 to 1637 kg/m{sup 3}, and the porosity is increased from 8.03 to 12.84 pct, and the optical texture index (OTI) is reduced from 58.1 to 25.3. The phase composition of ICHB mainly consists of C, Fe, SiO{sub 2}, Fe{sub 3}O{sub 4}, and FeO after the addition of the iron ore concentrate. Moreover, the reactivity of ICHB is accelerated from 46.74 to 69.54 pct due to the catalytic effects of metallic iron and iron oxide, which worked as oxygen transfer carriers, while the post-reaction strength is reduced from 74.08 to 36.81 pct. In addition, the starting temperature of the ICHB gasification reaction is decreased remarkably from 919 °C to 839 °C. The activation energy (E{sub a}) for the gasification reaction under nonisothermal conditions is reduced from 312.78 to 249.83 kJ/mol, and the preexponential factor (A) shows a decreasing trend as well. Simultaneously, E{sub a} and A display the kinetic compensation effect and present a good linear relationship.
Catalytic decomposition of tar derived from wood waste pyrolysis using Indonesian low grade iron ore as catalyst
Low grade iron ore can be used as an alternative catalyst for bio-tar decomposition. Compared to other catalysts, such as Ni, Rd, Ru, Pd and Pt, iron ore is cheaper. The objective of this research was to investigate the effect of using low grade iron ore as catalyst for tar catalytic decomposition in fixed bed reactor. Tar used in this experiment was pyrolysis product of wood waste while the catalyst was Indonesian low grade iron ore. The variables studied were temperatures between 500 – 600 °C and catalyst weight between 0 – 40 gram. The first step, tar was evaporated at 450 °C to produce tar vapor. Then, tar vapor was flowed to fixed bed reactor filled low grade iron ore. Gas and tar vapor from reactor was cooled, then the liquid and uncondensable gas were analyzed by GC/MS. The catalyst, after experiment, was weighed to calculate total carbon deposited into catalyst pores. The results showed that the tar components that were heavy and light hydrocarbon were decomposed and cracked within the iron ore pores to from gases, light hydrocarbon (bio-oil) and carbon, thus decreasing content tar in bio-oil and increasing the total gas product. In conclusion, the more low grade iron ore used as catalyst, the tar content in the liquid decrease, the H{sup 2} productivity increased and calorimetric value of bio-oil increased.
Studies on the reduction kinetics of hematite iron ore pellets with noncoking coals for sponge iron plants
In the present investigation, fired pellets were made by mixing hematite iron ore fines of -100, -16+18, and -8+10 mesh size in different ratios and studies on their reduction kinetics in Lakhanpur, Orient OC-2 and Belpahar coals were carried out at temperatures ranging from 850{sup o}C to 1000{sup o}C with a view toward promoting the massive utilization of fines in ironmaking. The rate of reduction in all the fired iron ore pellets increased markedly with an increase in temperature up to 1000{sup o}C, and it was more intense in the first 30min. The values of activation energy, calculated from integral and differential approaches, for the reduction of fired pellets (prepared from iron ore fines of -100 mesh size) in coals were found to be in the range 131-148 and 130-181 kJ mol{sup -1} (for =0.2 to 0.8), indicating the process is controlled by a carbon gasification reaction. The addition of selected larger size particles in the matrix of -100 mesh size fines up to the extent studied decreased the activation energy and slightly increased the reduction rates of resultant fired pellets. In comparison to coal, the reduction of fired pellets in char was characterized by significantly lower reduction rates and higher activation energy.
A Generalized Grain-Scale Model for the Non-Plasma and Plasma-Assisted Hydrogen Direct Reduction of Iron Ore
Direct Reduction of Iron ore using hydrogen (H-DRI) is a promising pathway towards efficient steelmaking and accurate predictive models are a necessity for scale-up and optimization of this technology. However, accurate models of this process remain limited because existing models oversimplify grain-scale phenomena, such as nonlinearity inside grain, self-sufficient porosity, surface reactions, and the role of plasma species. These phenomena are important for flash steelmaking and plasma-assisted H-DRI processes. To address this need, we present a phenomenological model for simulating H-DRI at the scale of a single micron-sized grain of the iron ore. We call this the Transient Reactive Grain Model (TRGM). TRGM incorporates key physical process: gas species transport, a chemical kinetics of material conversion, nanopore structural evolution and, adsorption-desorption surface kinetics at the reactive nanopore surface. The important contribution of this work is that the model provides a dependence on different reductant species, specifically hydrogen atoms versus molecules, so that role of hydrogen plasma reduction can be clarified compared to the use of pure hydrogen gas reduction. TRGM predictions agree well with experimental data for both molecular H2 reduction of Fe2O3 and plasma hydrogen reduction of Fe3O4. Results reveal species concentration gradients with a diffuse reaction zone, and enhanced hydrogen diffusion at the grain outer surface due to evolving porosity. These findings challenge common assumptions in existing models, including sharp reaction fronts, quasi-steady diffusion and kinetics, and the neglect of surface chemistry. As a generalized grain-scale model for H-DRI processes, TRGM has practical applications in flash steelmaking and in-flight reduction using both molecular and plasma hydrogen.
Effect of rare earth Ce on the far infrared radiation property of iron ore tailings ceramics
Highlights: • Detailed process proposed for preparation of iron ore tailings ceramics. • Replace natural minerals with iron ore tailings as raw materials for preparing functional ceramics. • Impact mechanism of Ce on far infrared ceramics, as well as its optimum addition amounts can be obtained. • Propose a new perspective on considering the mechanism of far infrared radiation. - Abstract: A kind of far infrared radiation ceramics was prepared by using iron ore tailings, CaCO{sub 3} and SiO{sub 2} as main raw materials, and Ce as additive. The result of Fourier transform infrared spectroscopy showed that the sample exhibits excellent radiation value of 0.914 when doping 7 wt.% Ce. Ce{sup 4+} dissolved into iron diopside and formed interstitial solid solution with it sintered at 1150 °C. The oxidation of Fe{sup 2+} to Fe{sup 3+} caused by Ce{sup 4+} led to a decrease of crystallite sizes and enhancement of Mg–O and Fe–O vibration in iron diopside, which consequently improved the far infrared radiation properties of iron ore tailings ceramics.
Bridging the Gap in Carbon Free Iron Making: How Hydrogen Affects the Reduction of Iron Ore between 900 and 1590 °C
Hydrogen-based reduction of iron ore for iron and steel production has emerged as a promising alternative to coal and natural gas. Unlike other hydrogen-based iron ore reduction studies, this research focuses on a wide temperature range across 900–1590 °C, encompassing reduction in solid, mixed, and liquid (slag) phases. For a 20 min exposure to hydrogen, the reduction degree increased monotonically from ∼35% at 900 °C to >90% at 1550 °C, except between 1100 °C and 1400 °C, where it stagnated ∼60%. This experimental work challenges the widely accepted notion that higher temperatures enhance the reduction process. Instead, it reveals an overlooked kinetic bottleneck, suggesting complex thermodynamic and mass transfer limitations influenced by phase transformations, diffusion barriers, and microstructural changes. Density functional theory-based molecular dynamics simulations indicate that oxygen diffusivity in BCC iron is 3.88 × 10 –5 cm 2 /s which is ∼5–10 times higher than that in FCC iron. This study reports that this stagnant reduction degree in the mixed solid–liquid phase is due to competition of multiple mechanisms, such as surface- and bulk-diffusion, pore collapse mechanisms, and crystallographic transitions.
Modeling Isothermal Reduction of Iron Ore Pellet Using Finite Element Analysis Method: Experiments & Validation
Iron ore pellet reduction experiments were performed with pure hydrogen (H2) and mixtures with carbon monoxide (CO) at different ratios. For direct reduction processes that switch dynamically between reformed natural gas and hydrogen as the reductant, it is important to understand the effects of the transition on the oxide reduction kinetics to optimize the residence time of iron ore pellets in a shaft reactor. Hence, the reduction rates were studied by varying experimental parameters such as the temperature (800, 850 & 900 °C), reactant gas flow rate (100, 150 & 200 cm3/min), pellet size and composition of the reactant gas mixture. The rate of reduction was observed to increase with an increase in temperature and reactant gas flow rate, but it decreased with an increase in pellet size. SEM greyscale analysis was performed to analyze the porosity and phase composition of partially reduced pellets. The porosity of the pellets was observed to increase from 0.3 for unreacted pellet to 0.42 for a completely reduced pellet. Energy-dispersive X-ray spectroscopy (EDAX) analysis was performed to identify the phases observed in the SEM images. The fraction of iron phase was observed to increase from the shell region of the pellet to the core region with an increase in the degree of reduction. A 2D-axisymmetric numerical model was developed on COMSOL Multiphysics, and it was validated using the conversion (X) vs. time curves obtained from each experiment. The model was able to accurately predict the total time needed for the complete conversion of a single iron ore pellet for multiple experiments. Effects of changes in the porosity and tortuosity of the pellet on the model were also studied and the rate of reduction was observed to be sensitive to changes in both porosity and tortuosity. The SEM analysis and the model results show that tortuosity is higher for pellets reduced with H2 than for pellets reduced with H2-CO gas mixtures.
Assessment of reduction behavior of hematite iron ore pellets in coal fines for application in sponge ironmaking
Studies on isothermal reduction kinetics (with F grade coal) in fired pellets of hematite iron ores, procured from four different mines of Orissa, were carried out in the temperature range of 850-1000C to provide information for the Indian sponge iron plants. The rate of reduction in all the fired iron ore pellets increased markedly with a rise of temperature up to 950C, and thereafter it decreased at 1000C. The rate was more intense in the first 30 minutes. All iron ores exhibited almost complete reduction in their pellets at temperatures of 900 and 950C in 2 hours' heating time duration, and the final product morphologies consisted of prominent cracks. The kinetic model equation 1-(1-a){sup 1/3}=kt was found to fit best to the experimental data, and the values of apparent activation energy were evaluated. Reductions of D. R. Pattnaik and M. G. Mohanty iron ore pellets were characterized by higher activation energies (183 and 150 kJ mol{sup -1}), indicating carbon gasification reaction to be the rate-controlling step. The results established lower values of activation energy (83 and 84 kJ mol{sup -1}) for the reduction of G. M. OMC Ltd. and Sakaruddin iron ore pellets, proposing their overall rates to be controlled by indirect reduction reactions.
High-Fidelity Arc-Discharge Model for Hydrogen-Plasma-Smelting-Reduction of Iron Ore
Electrification and use of renewable hydrogen is currently a necessity for decarbonizing the iron-and-steel industry. In this regard, hydrogen plasma smelting reduction (HPSR) is a novel pathway that is being explored for reduction of iron ore. HPSR provides several decarbonization merits compared to conventional blast furnaces. Firstly, the use of renewable hydrogen drastically reduces the CO2 emissions compared to the use of coke. Secondly, renewable electricity in the form of a thermal plasma for making reactive hydrogen species (radicals, ions) are more efficient at reducing iron ore compared to neutral H2. Thirdly, a molten product compatible with downstream processes is obtained from the intense heat transfer from the plasma. However, the scale-up of this technology requires fundamental exploration of hydrogen plasma dynamics and its interaction with complex solid material that include phase changing iron-ore and slag. In this work, we present a first principles continuum scale model for thermal plasmas in Ar/H2 gas mixtures typically used for HPSR. The thermal plasma governing equations for mass, momentum and energy with Lorentz force and Joule heating source terms are solved along with electromagnetic equations for electrostatic and magnetic vector potential. Our solver will be based on Pele, a suite of reacting flow solvers designed for advanced scientific computing architectures (Henry De Frahan et al., Proceedings of SIAM Parallel Processing, 13-25, 2024), and will utilize adaptive mesh generation for enhanced resolutions at locations of intense physicochemical interactions. This study will present the impact of Ar to H2 ratios on excited/dissociated hydrogen species concentrations, plasma temperature and conductivity along with the impact of outgassed species (water, metal vapor, O, OH radicals) from ore surface on gas phase chemistry. Furthermore, the heat and species flux to the surface will be quantified as a function of applied voltages in a transferred arc configuration.
Elucidating key reducing species beyond ions in hydrogen plasma smelting reduction of iron ore
Hydrogen plasma smelting reduction (HPSR) of iron ore has attracted significant attention over the past decade due to its high-temperature operation, rapid plasma mediated reduction kinetics, and simpler density-based separation of molten iron product, compared to H2-based solid-state reduction. All of these attributes enable processing of low-grade ores for downstream use in electric-arc furnaces, as virgin iron with low gangue content is required for high quality steel and improved furnace operation. While positive ions exist within the plasma arc, this work demonstrates that near the anodic ore surface, hydrogen radicals and vibrationally excited hydrogen species dominate and their densities correlate well with observed reduction rates. Species concentrations in the transferred plasma arc and at the plasma-ore interface are evaluated using coupled thermal plasma and near-wall non-equilibrium plasma models. The thermal plasma model is validated against experimental voltage data and spectroscopic measurements of plasma temperature and density for varying current inputs. Modeling of the near surface thermochemical non-equilibrium and micrometer scale anode sheath layer reveals, in addition to the expected H + , significant concentrations of ArH + and H$^+_3$ ions, typically not observed in thermal plasmas under thermodynamic equilibrium. Our results show that the inverted sheath structure at the anodic ore surface strongly suppresses reactive positive ion fluxes, while non-equilibrium electron-impact processes generate abundant hydrogen radicals and vibrationally excited species. These findings highlight the critical role of non-equilibrium effects in hydrogen arc-driven iron ore reduction and advance understanding beyond prevailing hypotheses centered on hydrogen ion-driven mechanisms.
Reduction of Iron‐Ore Pellets Using Different Gas Mixtures and Temperatures
Direct reduction of iron ore (DRI) is gaining an increased attention due to the growing need to decarbonize industrial processes. The current industrial DRI processes are performed using reformed natural gas, which results in CO 2 emission, although it is less than carbothermic reduction in the blast furnace. Carbon‐free reduction may be realized through the utilization of green H 2 as a reducing agent, in place of natural gas. Herein, the effects of various gas mixtures and temperature on the reduction kinetics of the hematite iron‐ore pellets are focused on in this work. Pellets are reduced at 700, 800, 850, and 900 °C in hydrogen and using various gas mixes at 850 °C. Morphology of the pellets is investigated with the help of scanning electron microscopy and mercury intrusion porosimetry. The effects of temperature and gas composition on the reduction kinetics and porosity of the pellets are discussed. A notable effect of reduction rate on the internal structure of the pellets is detected, slower reduction rate yielded bigger pores offsetting the gas composition. Higher temperature results in coarser pores and higher porosity. Finally, increase of CO content in the gas mix also leads to bigger pore size.
Synthesis of mesoporous silica materials (MCM-41) from iron ore tailings
Highly ordered mesoporous materials were successfully synthesized by using the iron ore tailings as the silica source and n-hexadecyltrimethyl ammonium bromide as the template. The samples were detail characterized by powder X-ray diffraction, scanning electron microscope, high-resolution transmission electron microscopy and N{sub 2} physisorption. The as-synthesized materials had high surface area of 527 m{sup 2} g{sup -1} and the mean pore diameter of 2.65 nm with a well-ordered two-dimensional hexagonal structure. It is feasible to prepare mesoporous MCM-41 materials using the iron ore tailings as precursor.
Grinding Wear Behaviour of Stepped Austempered Ductile Iron as Media Material During Comminution of Iron Ore in Ball Mills
An attempt has been made to evaluate the suitability of austempered ductile iron (ADI) as media material for grinding iron ore in a ball mill. Spheroidal graphite (S.G) iron balls are austenitised at 900 deg. C for 60 minutes and given stepped austempering treatment at 280 deg. C for 30 minutes and 60 minutes followed by 380 deg. C for 60 minutes in each case. These materials are characterised by measuring hardness, analysing X-ray diffraction (X-RD), studying microstructure using optical and scanning electron microscope (SEM). Grinding wear behaviour of these materials was assessed for wear loss in wet condition at different pH value of the mineral slurry and found that the wear rate of grinding media material decreases with increase in pH of the slurry. The wear resistance of ADI balls were compared with forged En31 steel balls and found that the stepped austempered ductile iron is superior to forged En31 steel balls.
Studies on Highly Fluxed Iron Ore Pellets Hardened at 1100 °C to 1200 °C
The behaviors of highly fluxed (basicity 2, 4, 6, and 8) iron ore pellets heat hardened in the temperature range 1100 °C to 1200 °C were examined and are reported here. The highly fluxed (basicity 8) pellets exhibited 103 kg/pellet crushing strength and 43.65 pct porosity when heat hardened at 1180 °C. During heat hardening, calcium di-ferrite and calcium ferrite phases were observed; however, when they were heated at 1200 °C, high crushing strength (458.63 kg/pellet) with low porosity (4.57 pct) were noted due to low melting eutectic formation. In this study, it was possible to prepare highly fluxed pellets without sticking at 1180 °C with good strength and porosity.
Iron Ore Reduction by Hydrogen Using a Laboratory Scale Fluidized Bed Reactor: Kinetic Investigation—Experimental Setup and Method for Determination
The reduction kinetics of hematite iron ore fines to metallic iron by hydrogen using a laboratory fluidized bed reactor were investigated in a temperature range between 873 K and 1073 K, by measuring the weight change of the sample portion during reduction. The fluidization conditions were checked regarding plausibility within the Grace diagram and the measured pressure drop across the material during experiments. The apparent activation energy of the reduction was determined against the degree of reduction and varied along an estimated two-peak curve between 11 and 55 kJ mol{sup −1}. Conventional kinetic analysis for the reduction of FeO to metallic iron, using typical models to describe gas–solid reactions, does not show results with high accuracy. Multistep kinetic analysis, using the Johnson–Mehl–Avrami model, shows that the initial stage of reduction from Fe{sub 2}O{sub 3} to Fe{sub 3}O{sub 4}, and partly to FeO, is controlled by diffusion and chemical reaction, depending on the temperature. Further reduction can be described by a combination of nucleation and chemical reaction, whereby the influence of nucleation increases with an increasing reduction temperature. The results of the kinetical analysis were linked to the shape of the curve from apparent activation energy against the degree of reduction.
Reduction Enhancement Mechanisms of a Low-Grade Iron Ore–Coal Composite by NaCl
The reduction behavior of a low iron grade with high SiO{sub 2} content ore–coal composite was investigated in the temperature range of 1143 K to 1263 K (870 °C to 990 °C). Sodium chloride was chosen as an additive to promote this reduction process. The effect of the sodium chloride addition and its mechanism was also investigated. Results showed that the added sodium chloride could enhance the reduction of wustite to iron due to the decrease of fayalite, and a higher metallization ratio of reduced sample was obtained. Thermogravimetric–differential scanning calorimeter analysis showed that sodium chloride could greatly facilitate the gasification process of coal and, thus, provide sufficient carbon monoxide to the reduction process of iron oxides. Meanwhile, sodium chloride promoted the reduction process of iron ore pellets directly as the coal gasification effect was excluded. Microstructures of reduced sample revealed that sodium chloride broke the structure of ore and enhanced the growth of newly formed iron particles. As the ore–coal composite with mol (C/Fe = 1.4) and 3 mass pct sodium chloride addition was roasted at 1233 K (960 °C) for 55 minutes, a reduced sample with metallization ration of 74.45 pct could be obtained.
Numerical Methods for Simulating the Reduction of Iron Ore in Blast Furnace Shaft
The blast furnace process is a counter-current moving bed chemical reactor to reduce iron oxides to iron, which involves complex transport phenomena and chemical reactions. The iron ore and coke are alternatively charged into the blast furnace, forming a layer by layer structural burden which is slowly descending in the counter-current direction of the ascending gas flow. We proposed a new methodology to efficiently simulate the gas and solid burden flow in the counter current moving bed in blast furnace shaft. The gas dynamics, burden movement, chemical reactions, heat and mass transfer between the gas phase and solid phase are included. Furthermore, the new methodology has been developed to explicitly consider the effects of the layer thickness thermally and chemically in the CFD model.