Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “IMPACT STRENGTH”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 19 records

The effect of aging treatment on the fracture toughness and impact strength of injection molded Ni-625 superalloy parts

In this study, the effect of aging heat treatment on fracture toughness and impact strength of Ni-625 superalloy fabricated by using powder injection molding (PIM) method was examined. After a feedstock was prepared by mixing the prealloyed Ni-625 superalloy powder, which was fabricated by gas atomisation, with a polymeric binder system and then it was granulated, it was shaped through the use of injection. The molded specimens were sintered at 1300 °C for 3 h after a two-stage debinding process. Once the sintered specimens were treated in the solution at 1150 °C for 2 h, they were quenched. Aging treatment was performed by keeping specimens at 745 °C for 22 h. Fracture toughness and impact tests were performed on sintered and aged specimens. Microstructure examinations were performed by using optical microscope, scanning electron microscope, and transmission electron microscope. The results revealed that aging heat treatment led to the formation of some carbides and intermetallic phases in the microstructure. While the hardness of the aged specimens increased due to these phases, their fracture toughness and impact strength values decreased. - Highlights: • Ni-625 superalloy components were produced by means of powder injection molding. • The produced components were subjected to aging treatment. • Aging process provided approximately 50% increase in the hardness of components. • Intermetallic precipitates, carbides and TCP phases occurred within the aged parts. • Fracture toughness and impact strength values decreased due to the hard phases.

36 MATERIALS SCIENCE↗

The Selection of Heat Treatment Parameters to Obtain Austempered Ductile Iron with the Required Impact Strength

The effect of austempering parameters on impact energy of non-alloyed cast iron with nodular graphite was examined. The analysis involved the austenitizing temperature in the range of 830-950 °C for the time of 60 min and the austempering temperature in the range of 300-400 °C for the time of 8, 16, 32 and 64 min. The value of the impact energy KV was determined. It has been found that the austenitizing temperature and austempering conditions affect the impact energy of ADI. The conducted analytical studies helped to develop a method for the selection of heat treatment parameters to obtain the ausferritic ductile iron with appropriate impact energy KV. The applied machine learning methods included support vector machine, decision trees, artificial neural networks and the method of variational component analysis.

36 MATERIALS SCIENCE↗

IMPACT STRENGTH OF GLASS AND GLASS CERAMIC

Strength of glass and glass ceramic was measured with a bar impact technique. High-speed movies show regions of tensile and compressive failure. The borosilicate glass had a compressive strength of at least 2.2 GPa, and the glass ceramic at least 4 GPa. However, the BSG was much stronger in tension than GC. In ballistic tests, the BSG was the superior armor.

36 MATERIALS SCIENCE↗

Development of Advanced Geopolymerized Brine Sludge Based Composites

For the first time in the world, geopolymerized brine sludge has been developed as it leads to the formation of enhanced geopolymeric gel which not only helps in further improving the interfacial binding of the conventional geopolymeric matrix using jute and glass fiber as reinforcement but also helps in making the toxic elements non-leachable from the geopolymerized brine sludge due to enhanced geopolymerization reaction taking place in the brine sludge incorporated advance matrix. The advanced geopolymerized matrix is capable of providing improved interfacial binding due to formation of additional C–S–H gel along with Na–S–H gel of conventional geopolymeric matrix in the geopolymeric brine sludge system. The simultaneous presence of desired components and constituents in the single matrix of geo polymeric brine sludge lead to the enhanced homogeneity among the reinforcement and matrix. The geo polymerized brine sludge was further used for making advance composites (AC) using closed mold fabrication system, with hand layup manual technique (a) without any fiber reinforcement, (b) with jute fiber reinforcement (c) and with glass fiber reinforcement of dimensions 12 in. × 12 in. × 6 in. The morphologies of all the three developed AC were examined using SEM and were also tested for their various mechanical properties like tensile strength, flexural strength, impact strength, abrasion resistance. The results indicate that fiber reinforced based AC shows the increase in the mechanical properties as compare to non-fiber reinforced AC. Further, the glass fiber reinforced AC showed better results than jute fiber reinforced AC. This remarkable enhancement is due to the unique properties of fiber in tolerating greater bending and fracture forces than the non reinforced matrix based materials. Graphical Abstract: .

36 MATERIALS SCIENCE↗

Electron impact collision strengths and transition rates for extreme ultraviolet emission from Xe{sup 10+}

The energy levels, oscillator strengths, and electron impact collision strengths are calculated for the Xe{sup 10+} ion using the configuration interaction scheme implemented by the Flexible Atomic Code. These data pertain to the 3917 levels belonging to the following configurations: 4s{sup 2}4p{sup 6}4d{sup 8}, 4s{sup 2}4p{sup 6}4d{sup 7}4f, 4s{sup 2}4p{sup 6}4d{sup 7}5l (l = s, p, d, or f), 4s{sup 2}4p{sup 5}4d{sup 9}, 4s{sup 2}4p{sup 5}4d{sup 8}4f, 4s{sup 2}4p{sup 5}4d{sup 8}5l, 4s{sup 2}4p{sup 6}4d{sup 6}5s5p, 4s{sup 2}4p{sup 6}4d{sup 6}5p5d. Configuration interactions among these configurations are included in the calculation. Collision strengths are obtained at 10 scattered electron energies (1-1000 eV) and are tabulated here at five representative energies of 10, 50, 100, 500, and 1000 eV. Effective collision strengths are obtained by assuming a Maxwellian electron velocity distribution at 10 temperatures ranging from 10 to 100 eV, and are tabulated at five representative temperatures of 10, 30, 50, 70 and 100 eV in this work. The whole data set should be useful for research involving extreme ultraviolet emission from Xe{sup 10+}.

74 ATOMIC AND MOLECULAR PHYSICS↗

Use of polypropylene fibers coated with nano-silica particles into a cementitious mortar

Fiber reinforced cementitious composite (FRCC) materials have been widely used during last decades in order to overcome some of traditional cementitious materials issues: brittle behaviour, fire resistance, cover spalling, impact strength. For composite materials, fiber/matrix bond plays an important role because by increasing fiber/matrix interactions is possible to increase the behaviour of the entire material. In this study, in order to improve fiber to matrix adhesion, two chemical treatments of polypropylene fibers were investigated: alkaline hydrolysis and nano-silica sol-gel particles deposition. Treatmtents effect on fibers morphology and mechanical properties was investigated by scanning electron microscopy (SEM) and tensile tests. SEM investigations report the presence of spherical nano-silica particles on fiber surface, in the case of sol-gel process, while alkaline hydrolysis leads to an increase of fibers roughness. Both treatments have negligible influence on fibers mechanical properties confirming the possibility of their use in a cementitious mortar. Pullout tests were carried out considering three embedded length of fibers in mortar samples (10, 20 and 30 mm, respectively) showing an increase of pullout energy for treated fibers. The influence on fiber reinforced mortar mechanical properties was investigated by three-point flexural tests on prismatic specimens considering two fibers length (15 and 30 mm) and two fibers volume fractions (0.50 and 1.00 %). A general increase of flexural strength over the reference mix was achieved and an overall better behaviour is recognizable for mortars containing treated fibers.

36 MATERIALS SCIENCE↗

Microstructure and Mechanical Characterization of Friction-Stir-Welded 316L Austenitic Stainless Steels

Fusion welding of austenitic stainless steels (ASSs) causes undesirable metallographic changes. An attempt has been made to join 3-mm-thick 316L ASS plates using friction stir welding and correlate the microstructural evolution and the mechanical properties under various welding conditions. Tungsten alloy (W-Re) tool was employed for welding. Successful joints were obtained within a range of traverse speeds (45-85 mm/min) used in this work. Various zones were observed across the joint line. The stir zone exhibited considerable grain refinement and traces of delta ferrite phase. EBSD images showed a decreasing grain size with increased traverse speed. XRD patterns and TEM images confirmed the existence of delta ferrite. The mechanical properties of the joints including microhardness, tensile strength, impact toughness and bending were further reported.

36 MATERIALS SCIENCE↗

Effect of aging on impact properties of ASTM A890 Grade 1C super duplex stainless steel

Super duplex stainless steels in the solution annealed condition are thermodynamically metastable systems which, when exposed to heat, present a strong tendency to 'seek' the most favorable thermodynamic condition. The main purpose of this study was to characterize the microstructure of a super duplex stainless steel in the as cast and solution annealed conditions, and to determine the influence of aging heat treatments on its impact strength, based on Charpy impact tests applied to V-notched test specimens. The sigma phase was found to begin precipitating at heat treatment temperatures above 760 deg. C and to dissolve completely only above 1040 deg. C, with the highest peak concentration of this phase appearing at close to 850 deg. C. Heat treatments conducted at temperatures of 580 deg. C to 740 deg. C led to a reduction of the energy absorbed in the Charpy impact test in response to the precipitation of a particulate phase with particle sizes ranging from 0.5 {mu}m to 1.0 {mu}m, with a chromium and iron-rich chemical composition.

36 MATERIALS SCIENCE↗

Electron impact collision strengths in Sn XXIII

The energy levels, multipole (E1, M1, E2, and M2) transition rates, and electron-impact collision strengths are calculated for Sn XXIII. The data refer to 107 fine-structure levels belonging to the configurations (1s{sup 2}2s{sup 2}2p{sup 6})3s{sup 2}3p{sup 6}3d{sup 10}, 3s{sup 2}3p{sup 6}3d{sup 9}4l, 3s{sup 2}3p{sup 5}3d{sup 10}4l, and 3s3p{sup 6}3d{sup 10}4l(l = s, p, d, and f). The collision strengths are calculated with a 20-collision-energy grid in terms of the energy of the scattered electron between 37.5 and 8436 eV by using the distorted-wave approximation. Effective collision strengths are obtained at five electron temperatures, T{sub e} (eV) = 193.89, 387.78, 581.67, 775.57, and 969.46, by integrating the collision strengths over a Maxwellian electron distribution.

73 NUCLEAR PHYSICS AND RADIATION PHYSICS↗

Mechanical and tribological property comparison of melt-compounded nanocomposites of atomic-layer-deposition-coated polyamide particles and commercial nanofillers

Mechanical and tribological properties of melt-compounded titanium dioxide nanocomposites of atomic-layer-deposition (ALD)-coated polyamide particles and commercial nanofillers were compared. The nanofiller dispersion in the polyamide matrix was studied using transmission electron microscopy showing very different morphology for the ALD-created and the traditional nanocomposites: former appearing as ribbons in the matrix whereas latter composing from spherical clusters. The effect of such morphology change on the specimen's mechanical response subjected to tensile and impact loading was investigated. The results demonstrated that ALD-created nanocomposites possess significantly higher Young's modulus than pure and traditionally filled polyamide matrix. However, transition from ductile to brittle behavior occurs especially for the ALD-created nanocomposites. Notched impact strength experiments supported this, suggesting that the impact strength of ALD-created composites decreased significantly compared to pure polyamide matrix, whereas traditionally melt-compounded nanocomposites showed no significant changes. Furthermore, the tribological properties of the selected specimens were determined and the effect of the nanofiller on the friction and scratching properties of the polyamide matrix is discussed.

36 MATERIALS SCIENCE↗

Effects of Natural and Artificial Weathering on the Physical Properties of Recycled Poly(ethylene terephthalate)

In accelerated weathering tests, specimens are exposed to higher radiation intensity, temperature and humidity than is likely under natural weathering in order to achieve rapid degradation of the polymer in a convenient short time. In the current work, a correlation between the two environments is attempted so that a prediction of lifetimes in the natural environment can be achieved. During aging, surface flaws are created due to the chain scission process. This is initiated by the absorption of ultra-violet light and directly affects visual appearance and impact strength. After natural weathering, the material shows only plastic deformation in an impact test. However, after artificial weathering to 5000 h of UV exposure, there is a decrease of 85% in impact strength. Colour change occurs at a high rate in the early stages of UV exposure. Beyond 2000 h of exposure, the colour change approaches a steady state and a correlation between the changes under natural and artificial weathering becomes apparent for a potential prediction of lifetimes. From the analysis including the specular component (SCI), taking surface roughening into account, 1 year under natural weathering was found to be equivalent to 25 days under accelerated weathering.

36 MATERIALS SCIENCE↗

Material property characterization of 3D printed polypropylene wood plastic composites

Abstract Wood flour (WF) at 10 wt.% and 20 wt.% loadings was used as a reinforcing filler to enhance the applicability of polypropylene (PP) for 3D printing. After performing printability tests of PP wood plastic composites (WPCs), the mechanical properties of both injection‐molded and 3D‐printed PP WPC specimens were explored. Test specimens were prepared from 3D printed hexagons for analyzing the mechanical properties. Adding WF to neat PP increased the storage modulus and the glass transition temperature while decreasing the degree of crystallinity and the coefficient of thermal expansion, while enhancing the printability of neat PP. The tensile strength, tensile modulus of elasticity, flexural strength, and flexural modulus of elasticity of injection‐molded neat PP improved by up to 21%, 59%, 30%, and 56%, respectively, with 20 wt.% WF. However, the impact strength of injection‐molded neat PP decreased by 85%, with 20 wt.% WF. After 3D printing, the tensile strength and tensile modulus of elasticity of printed neat PP increased by up to 84% and 60%, respectively, with 20 wt.% WF. The flexural strength and flexural modulus of elasticity of neat printed PP remained unchanged compared to those of PP filled with 20 wt.% WF, while the impact strength decreased by 87%. Highlights WF was used as a reinforcement in polypropylene designed for 3D printing A pilot‐scale, pellet‐fed 3D printer was used to print hollow hexagons, and then test specimens were fabricated from these hexagons for mechanical properties The tensile and flexural properties of 3D printed neat polypropylene improved, while the impact strength decreased after adding 20 wt.% WF to the neat PP.

Hwang, Sungjun↗

Chemically Functionalized Plant Fibers and Carbon Nanotubes for High Compatibility and Reinforcement in Polylactic Acid (PLA) Composite

In this study, surface modification is used to improve the compatibility of Kenaf fibers (KFs) and multi-walled carbon nanotubes (MWCNTs) in a polylactic acid (PLA) matrix, as well as to enhance the mechanical properties. Through the use of a silane coupling agent, the KF is grafted with functional groups to generate a chemical bond with the PLA; the modified KF shows high compatibility in the PLA matrix. Compared to the bare PLA, the optimal KF/MWCNT/PLA composite (PC1F30-OX) shows increases of 58% in tensile strength, and 113% in impact strength. A small addition of MWCNTs (1 wt%) dramatically improves the antistatic ability by lowering the surface resistance to 3.47 GΩ. With the addition of hydrophilic KF into the PLA, the composite becomes much more environmentally friendly, and the biodegradation rate can be controlled by the amount of KF added. The addition of hydrophilic KF allowed the composite to accommodate more enzyme to hasten the biodegradation; almost complete decomposition occurred after 11 weeks.

38 RADIATION CHEMISTRY, RADIOCHEMISTRY, AND NUCLEA↗

Performance of Cow Dung Reinforced Biodegradable Poly(Lactic Acid) Biocomposites for Structural Applications

In this work, performance of cow dung (CD) reinforced poly(lactic acid) (PLA) biocomposites was investigated for the potential use in load bearing application. CD of average 4 mm size was blended with PLA at different CD ratios (0–50 wt%) and their effects on the biocomposite properties were studied. The results showed an improvement in the flexural properties, while the tensile and impact strength dropped by 20 and 28% with the addition of 50% CD. The decline in the tensile and impact strength was due to micro-cracking and voids formation at higher CD content. Also, the incorporation of CD slightly decreased the thermal stability of the biocomposite. However, dynamic mechanical properties of the biocomposites generally improved. SEM analysis of tensile and impact fractured surfaces indicated that the CD had a reasonable adhesion with matrix. Moreover, the SEM micrographs of soil burial studies showed an accelerated degradation of higher CD wt% biocomposites.

36 MATERIALS SCIENCE↗

Study on Mechanical and Thermal Properties of Poly(Lactic acid)/Poly(Butylene adipate-co-terephthalate)/Office Wastepaper Fiber Biodegradable Composites

Office wastepaper fibers(OWF)/poly(butylene adipate-co-terephthalate) (PBAT)/poly(lactic acid) (PLA) biodegradable composites with different mass ratio were made by melt blending and injection moulding process. At the same time, the use of MAPLA and KH560 was studied as a potential approach for improving interfacial adhesion between OWF, PBAT and PLA. The results revealed that with the increasing of PBAT, the notched impact strength of PLA/PBAT/OWF composites can be first increased and then decreased. When the content of PBAT was 20 wt%, the notch impact strength of PLA/PBAT/OWF composite was the highest, increased by 291% compared with pure PLA. TGA results revealed that the onset degradation temperature of the composites can be increased and its thermal decomposition step can be changed. According to the crystallization and melting performance table, OWF can act as nucleating agent to promote the crystallization properties of composites, while PBAT can prevent the crystallization and the higher the content is, the more obvious it is. It can be seen from the SEM figures that the addition of MAPLA and KH560 simultaneously makes the composites interface bond closer, thus improving the interface performance of PLA/20PBAT/OWF composite. Among the three kinds of modified composites, PLA/20PBAT/OWF/MK composite has the lowest water absorption and the best comprehensive performance.

36 MATERIALS SCIENCE↗

Polymeric materials from renewable resources

The goals of our studies have been the use of renewable raw materials in the preparation of polymeric materials with diversified properties. In this context, lignosulfonate, which is produced in large scale around the world, but not widely used in the production of polymeric materials, was used to replace phenol and polyols in the preparation of phenolic- (Ligno-PH) and polyurethane-type (Ligno-PU) polymers, respectively. These polymers were used to prepare composites reinforced with sisal lignocellulosic fibers. The use of lignosulfonate in the formulation of both types of polymers was beneficial, because in general composites with improved properties, specially impact strength, were obtained. Composites were also prepared from the so called “biopolyethylene” (HDPE), curaua lignocellulosic fiber, and castor oil (CO). All composites HDBPE/CO/Fiber exhibited higher impact strength, when compared to those of the corresponding HDBPE/Fiber. These results, combined with others (eg SEM images of the fractured surfaces) indicated that, in addition to acting as a plasticizer, this oil may have acted as a compatibilizer of the hydrophilic fiber with the hydrophobic polymer. The set of results indicated that (i) mats with nano (diameter ≤ 100nm) and/or ultrafine (submicron scale) fibers were produced, (ii) hybrid fibers were produced (bio-based mats composites), (iii) cellulosic pulp (CP) and/or lignin (Lig) can be combined with PET matrices to control properties such as stiffness and hydrophilicity of the respective mats. Materials with diversified properties were prepared from high content of renewable raw materials, thus fulfilling the proposed targets.

36 MATERIALS SCIENCE↗

Thermal and mechanical properties of TPU/PBT reinforced by carbon fiber

In this study, thermal, mechanical properties and processability were performed on a series of carbon fiber (CF) filled thermoplastic polyurethane (TPU)/poly (butylene terephthalate) (PBT) composites to identify the effect of CF weight fraction on the properties of TPU/PBT. Scanning Electronic Microscope (SEM) show that CFs are uniformly dispersed in TPU/PBT matrix and there are no agglomerations. Melt flow index (MFI) show that the melt viscosity increased with the CF loading. Thermogravimetric analysis (TGA) revealed that the introduction of CF into organic materials tend to improve their thermal stability. The mechanical properties indicated that tensile strength and modulus, flexural strength and modulus, improved with an increase in CF loading, but the impact strength decreased by the loading of CF.

36 MATERIALS SCIENCE↗