Hydrogen Isotope Labeling of Pharmaceuticals Via Dual Hydrogen Isotope Exchange Pathways Using CdS Quantum Dot Photocatalyst
Explore the source record for details and available documents.
SEARCH · Engineering Papers
Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.
Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.
Explore the source record for details and available documents.
Understanding the interaction of hydrogen with microstructural features in metallic materials is crucial for designing hydrogen-resistant alloys. Although thermal desorption spectroscopy (TDS) is widely used for investigating the hydrogen binding behavior of various microstructural features, its application to face-centered cubic (fcc) metals and alloys that exhibit low hydrogen diffusivity is limited due to the lumped TDS desorption signals. This paper shows that, by coupling a Sofronis–McMeeking type hydrogen transport model with a microstructure-informed finite-element model, TDS data can be deconvoluted to reveal the underlying adsorption–diffusion–desorption processes, hydrogen diffusivity, and trap-binding energies. In conclusion, the austenitic steel SS316L in solution-annealed condition is used as a demonstration material, and we focused on investigating the interaction of deuterium (hydrogen isotope) with grain boundaries, which is difficult to investigate from experiments alone but critical for design of alloys for hydrogen infrastructure.
Handbook of physical and thermal property data for hydrogen in region between triple point and critical point for study of hydrogen slush and/or hydrogen gel utilization
The NASA Safety Standard, which establishes a uniform process for hydrogen system design, materials selection, operation, storage, and transportation, is presented. The guidelines include suggestions for safely storing, handling, and using hydrogen in gaseous (GH2), liquid (LH2), or slush (SLH2) form whether used as a propellant or non-propellant. The handbook contains 9 chapters detailing properties and hazards, facility design, design of components, materials compatibility, detection, and transportation. Chapter 10 serves as a reference and the appendices contained therein include: assessment examples; scaling laws, explosions, blast effects, and fragmentation; codes, standards, and NASA directives; and relief devices along with a list of tables and figures, abbreviations, a glossary and an index for ease of use. The intent of the handbook is to provide enough information that it can be used alone, but at the same time, reference data sources that can provide much more detail if required.
Simplified design concepts were used to estimate gravimetric and volumetric energy densities for metal hydrogen battery cells for assessing the characteristics of cells containing metal hydrides as compared to gaseous storage cells, and for comparing nickel cathode and silver cathode systems. The silver cathode was found to yield superior energy densities in all cases considered. The inclusion of hydride forming materials yields cells with very high volumetric energy densities that also retain gravimetric energy densities nearly as high as those of gaseous storage cells.
A method has been developed for the determination of trapped hydrogen in metal alloys, involving the determination of mobile hydrogen using the electrochemical method and the determination of total hydrogen with the fusion method, the difference in hydrogen concentrations being due to trapped hydrogen. It has been found that hydrogen enters body-centered cubic structures through the grain bodies rather than through the grain boundaries. Hydrogen also diffuses much more rapidly in body-centered cubic structures on charging than in face-centered cubic structures, the hydrogen distribution being more uniform in nature. The energy necessary to cause hydrogen embrittlement is postulated to arise from the changes in crystal lattice energies brought about through interaction of hydrogen with atoms in the metal lattice. The total energy change is more negative for body-centered cubic structures, believed to be the cause of a greater tendency toward hydrogen embrittlement. Finally, the agreement of hydrogen concentrations obtained at 25 C by the electrochemical method with those obtained by the fusion method are taken as a strong indication of the power and validity of the electrochemical method.
It was long known that many strong metals can become weakened and brittle as the result of the accumulation of hydrogen within the metal. When the metal is stretched, it does not show normal ductile properties, but fractures prematurely. This problem can occur as the result of a hydrogen evolution reaction such as corrosion or electroplating, or due to hydrogen in the environment at the metal surface. High strength alloys such as steels are especially susceptible to hydrogen embrittlement. Nickel-hydrogen cells commonly use Inconel 718 alloy for the pressure container, and this also is susceptible to hydrogen embrittlement. Metals differ in their susceptibility to embrittlement. Hydrogen embrittlement in nickel-hydrogen cells is analyzed and the reasons why it may or may not occur are discussed. Although Inconel 718 can display hydrogen embrittlement, experience has not identified any problem with nickel-hydrogen cells. No hydrogen embrittlement problem is expected with the 718 alloy pressure container used in nickel-hydrogen cells.
Utilities need to recover value from baseload and some renewable assets even when the electricity is curtailed. The declining cost of renewables (particularly solar), the persistently low-cost of natural gas, and the declining electricity demand, have all worked to lower the price of electricity. Furthermore, the baseload assets have a high turndown cost, which is not reflected in the low market electricity prices. One option for utilizing the curtailed electricity is hydrogen generation. One important aspect of this project will be to provide a “go/no-go” recommendation on the economic feasibility of pursuing hydrogen generation vs. other markets that could offtake curtailed electricity or nuclear steam. This project will specifically assess the opportunities for hydrogen production and use in the service territories of Southern Company Services (SCS), Exelon SBC, and Xcel Energy. Each utility partner represents a different mix of generation fleets: Exelon has significant nuclear assets, Xcel is primarily renewables (wind) with some nuclear, and SCS represents both a renewables fleet and a heavily baseload fleet, which includes significant nuclear. The Contractors will conduct the study of hydrogen market opportunities by first considering the approximate electricity demand and price profiles for the year, and power generation capacity that can be used to produce hydrogen. Therefore, a profile for hydrogen generation will also be developed to better understand the quantity and timing of hydrogen production. Once the hydrogen production schedule is estimated, hydrogen storage requirements can be determined. This effort will provide sufficient information to make a go/no-go decision on moving ahead with a detailed regional case study for hydrogen production in any of the three utility areas.
Depleted oil and gas reservoirs, characterized by impermeable clay-rich caprocks, are promising sites for large-scale underground hydrogen storage (UHS), which is a key strategy to support hydrogen-based energy systems. However, experimental data on hydrogen storage in clay-rich geomaterials remain scarce. In this work, we experimentally investigated hydrogen adsorption and migration in clay-rich geomaterials in the presence of nitrogen and water under controlled temperatures. Experimental observations showed that hydrogen was adsorbed in dry illite. A dual-porosity transport model was developed to interpret hydrogen transport between large-pore and small-pore domains in illite. The large-pore domain is the space between clay particles (i.e., inter-particle space), whereas the small-pore domain is the nanoscale pore space between clay mineral layers (i.e., inter-layer or intra-particle space). In contrast, nitrogen showed no evidence of adsorption in dry illite because it cannot move into the small-pore domain due to the relatively large kinetic diameter, referred to as the molecular sieving effect. Here, we found that 0.7–1.3 nm is the length scale regulating this molecular sieving effect, matching the interlayer spacing in illite, suggesting that nitrogen is a promising cushion gas in UHS, which aims to maintain adequate pressure in the reservoir for economic operations. In wetted illite, hydrogen was not adsorbed into the interlayer space due to the occupation of adsorption sites by interlayer water, which highlights the critical role of the clay hydration state in controlling hydrogen-clay interactions. Additionally, hydrogen adsorption experiments on crushed shale indicated that the shale surface possessed adsorption sites more favorable for hydrogen than for nitrogen. Through these experiments, we provide new insights into hydrogen storage mechanisms in clay-rich geomaterials and offer valuable laboratory data for evaluating the performance of large-scale UHS systems.
Well characterized experimental data for consequence model validation is important in progressing the use of liquid hydrogen as an energy carrier. In 2019, the Health and Safety Executive (HSE) undertook a series of liquid hydrogen dispersion and combustion experiments as a part of the Pre-normative Research into the Safe Use of Liquid Hydrogen (PRESLHY) project. In partnership between the National Renewable Energy Laboratory (NREL) and HSE, time and spatially varying hydrogen concentration measurements were made in 25 dispersion experiments and 23 congested ignition experiments associated with PRESLHY WP3 and WP5, respectively. These measurements were undertaken using the hydrogen wide area monitoring system developed by NREL. During the 23 congested ignition experiments, high variability was observed in the measured explosion severity during experiments with similar initial conditions. This led to the conclusion that wind, including localized gusts, had a large influence on the dispersion of the hydrogen, and therefore the quantity of hydrogen that was present in the congested region of the explosions. Using the hydrogen concentration measurements taken immediately prior to ignition, the hydrogen clouds were visualized in an attempt to rationalize the variability in overpressure between the tests. Gaussian process regression was applied to quantify the variability of the measured hydrogen concentrations. This analysis could also be used to guide modifications in experimental designs for future research on hydrogen combustion behavior.
Here, this study demonstrates a novel methodology that simultaneously exposes materials to both neutron irradiation and a hydrogen environment, enabling study on in pile interaction between radiation-induced defects and hydrogen in tungsten. The hydrogen environment was established by releasing hydrogen from vanadium hydride within an irradiation capsule. The hydrogen pressure during irradiation was estimated as 14.2 Torr. Post-irradiation thermal desorption spectroscopy analysis showed increased hydrogen retention in irradiated tungsten compared to unirradiated samples. Two dominant desorption peaks at ∼470 °C and ∼700 °C were observed in irradiated and unirradiated tungsten samples, suggesting similar trapping mechanisms between the two samples. However, an additional desorption peak at ∼800 °C in irradiated tungsten from the hydride capsule suggests an interplay between irradiation induced defects and hydrogen exposure, leading to the formation of additional hydrogen trapping sites. These findings provide critical insights into hydrogen retention in tungsten under fusion-relevant conditions and stimulate future studies to investigate the synergistic effects of neutron irradiation and hydrogen exposure.
Hydrogen bronzes can be used as hydrogen donors for the broad class of reactions involving proton-coupled electron transfer (PCET). Here, in this work, we describe a method to prepare platinum-decorated hydrogen tungsten bronzes, Pt@H x WO 3 · n H 2 O with n = 0, 1, and 2, by reacting the pristine oxides at modest temperatures with a mild reducing agent, H 3 PO 2 , and H 2 PtCl 6 in an aqueous solution. We explored the tunability and kinetics of this reaction and compared it with that of archetypal gas–solid hydrogen spillover. We demonstrate that the identity of the noble metal affects the extent of bronze reduction. This suggests that the mechanism proceeds via the adsorption of a hydrogen-atom species on the noble metal. Finally, we explored the ability of the Pt-decorated hydrogen tungsten bronzes to hydrogenate a model H + /e – acceptor, 2,2,6,6-tetramethyl-1-piperidinyloxyl (TEMPO). The bronze phases return to their fully oxidized states along with the subsequent reduction of TEMPO to TEMPOH. Overall, this work demonstrates a solution-phase method to obtain hydrogen bronzes, which can then be used to perform hydrogen transfer reactions, providing a pathway for the use of extended transition metal oxides as stoichiometric reagents for broad classes of hydrogenation reactions.
To reduce carbon emissions, the US natural gas infrastructure is seen as a primary solution for efficiently transporting hydrogen gas. Blending hydrogen gas with natural gas and transporting it across a national infrastructure could save significant infrastructure costs. To properly operate the infrastructure under the new gas system, it is critical to understand material compatibility with hydrogen under various conditions. The Blended Gas CRADA, a Hyblend project, is established to determine the material compatibility of existing natural gas pipes with hydrogen gas. In this study, we investigate the in-plane fracture behaviors of MDPEMarlex and HDPEGDB exposed to hydrogen and hydrogen-methane blended gas. Single-edge notch bending geometry is used. All tests are executed in-situ with the gas environment. The experimental results show a significant effect of the gas environment on HDPEGDB specimens, reducing 5% (H2) to 42% (Blended gas) of specific fracture energy compared to non-aged specimens. For the MDPEMarlex, the effects of the gas environment have increased the specific fracture energy by 10% (H2) to 15% (Blended gas). Fracture surfaces of the tested samples are observed using an electronic microscope. The in-plane fracture surface of HDPEGDB shows a pronounced dimple fracture pattern after exposure to hydrogen and blended gas. The expanded fracture pattern contributes to lower the specific fracture energy. These observations provide critical information for validating polymer pipeline materials when interact with hydrogen and hydrogen-blend gas.
An experimental study is conducted on 12.5-mm-thick SAE 1020 steel (plain carbon steel) plate to assess hydrogen attack at room temperature after specimen exposure at 525 C to hydrogen and a blend of hydrogen sulfide and hydrogen at a pressure of 3.5 MN/sq m for exposure times up to 240 hr. The results are discussed in terms of tensile properties, fissure formation, and surface scales. It is shown that hydrogen attack from a high-purity hydrogen environment is severe, with the formation of numerous methane fissures and bubbles along with a significant reduction in the room-temperature tensile yield and ultimate strengths. However, no hydrogen attack is observed in the hydrogen/hydrogen sulfide blend environment, i.e. no fissure or bubble formation occurred and the room-temperature tensile properties remained unchanged. It is suggested that the observed porous discontinuous scale of FeS acts as a barrier to hydrogen entry, thus reducing its effective equilibrium solubility in the iron lattice. Therefore, hydrogen attack should not occur in pressure-vessel steels used in many coal gasification processes.
Tubes of CG-27 alloy, filled with hydrogen doped with various amounts of carbon dioxide and carbon monoxide, were heated in a diesel fuel fired Stirling engine simulator materials test rig for 100 hours at 820 C and at a gas pressure of 15 MPa to determine the effectiveness of the dopants in reducing hydrogen permeation through the hot tube wall. This was done for clean as-heat treated tubes and also for tubes that had previously been exposed for 100 hours to hydrogen doped with 1.0 volume percent carbon dioxide to determine if the lower levels of dopant could maintain a low hydrogen permeation through the hot tube wall. Carbon dioxide, as a dopant in hydrogen, was most effective in reducing hydrogen permeation through clean tubes and in maintaining low hydrogen permeation after prior exposure to 1.0 volume percent carbon dioxide. Only the lowest level of carbon dioxide (0.05 volume percent) was not as effective in the clean or prior exposed tubes. Carbon monoxide as a dopant in hydrogen was less effective than carbon dioxide at a given concentration level. Of the four dopant levels studied; 1.0, 0.5, 0.2, and 0.05 volume percent carbon monoxide, only the 1.0 and 0.5 volume percent were effective in reducing and maintaining low hydrogen permeation through the CG-27.
The activities presented are a broad based approach to advancing key hydrogen related technologies in areas such as fuel cells, hydrogen production, and distributed sensors for hydrogen-leak detection, laser instrumentation for hydrogen-leak detection, and cryogenic transport and storage. Presented are the results from research projects, education and outreach activities, system and trade studies. The work will aid in advancing the state-of-the-art for several critical technologies related to the implementation of a hydrogen infrastructure. Activities conducted are relevant to a number of propulsion and power systems for terrestrial, aeronautics and aerospace applications. Hydrogen storage and in-space hydrogen transport research focused on developing and verifying design concepts for efficient, safe, lightweight liquid hydrogen cryogenic storage systems. Research into hydrogen production had a specific goal of further advancing proton conducting membrane technology in the laboratory at a larger scale. System and process trade studies evaluated the proton conducting membrane technology, specifically, scale-up issues.
HydroGEN Energy Materials Network (EMN) is an U.S. Department of Energy (DOE) EERE Hydrogen and Fuel Cell Technologies Office (HFTO)-funded consortium that aims to accelerate the discovery and development of advanced water splitting materials (AWSM) for clean, low-cost hydrogen production. Materials innovations are key to enhancing performance, durability, and cost of hydrogen generation technologies. HydroGEN is focused on low technology readiness level AWS technologies, including low- (alkaline exchanged membrane electrolysis) and high-temperature electrolysis (proton-conducting solid oxide electrolysis), photoelectrochecmical (PEC) and thermochemical (TCH) water splitting. The AWS technologies in this consortium study proton conduction in solid oxide electrolysis and hydroxide conduction in polymer electrolysis, and proton transport in photoelectrochemical water splitting. This presentation will provide an overview of the HydroGEN EMN and technical highlights of a few lab-led and DOE-awarded "seedling" R&D projects. HydroGEN continues to grow its community of industry, university, and national laboratories, forming a national innovation ecosystem focused on renewable hydrogen production.
Combined modeling and experimental studies are reported of the fueling of a large (28 kg capacity) 250-bar Type IV hydrogen tank of the type being deployed on early hydrogen ferries, such as the MV Sea Change. The primary goal was to determine how such tanks can be successfully fueled with hydrogen (state of charge greater than 97%) within 45 minutes without exceeding the 82 °C temperature limit for such tanks. The modeling studies show that a gas injector is needed to avoid thermal stratification during hydrogen fueling which can result in potential hot spots. Empirically, precooling of the hydrogen to 0 °C was found to be needed in some of the cases examined, as ambient conditions greatly affected the need for a precooling to achieve the 45-minute fill time desired by end users. The experimental results afforded a calibration of the engineering model SOFIL for these large 250-bar tanks, which now enables using SOFIL to predict volume-averaged hydrogen fueling temperatures to an accuracy of ±2.7°C for these tanks. The model can therefore be used to evaluate potential scenarios for development of a standardized fueling methodology for ferries utilizing large Type-IV tanks.