Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “Fe7C3”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

Materials Data on Fe7C3 by Materials Project

Fe7C3 crystallizes in the hexagonal P6_3mc space group. The structure is three-dimensional. there are three inequivalent Fe sites. In the first Fe site, Fe is bonded in a distorted L-shaped geometry to two equivalent C atoms. Both Fe–C bond lengths are 2.04 Å. In the second Fe site, Fe is bonded in a 3-coordinate geometry to three equivalent C atoms. There is one shorter (1.93 Å) and two longer (2.00 Å) Fe–C bond length. In the third Fe site, Fe is bonded in a 3-coordinate geometry to three equivalent C atoms. All Fe–C bond lengths are 1.98 Å. C is bonded in a 6-coordinate geometry to six Fe atoms.

36 MATERIALS SCIENCE↗

Materials Data on Fe7C3 by Materials Project

Fe7C3 crystallizes in the orthorhombic Pnma space group. The structure is three-dimensional. there are five inequivalent Fe sites. In the first Fe site, Fe is bonded in a 3-coordinate geometry to three C atoms. There are a spread of Fe–C bond distances ranging from 1.97–2.04 Å. In the second Fe site, Fe is bonded in a 3-coordinate geometry to three C atoms. There is one shorter (1.93 Å) and two longer (1.98 Å) Fe–C bond length. In the third Fe site, Fe is bonded in a water-like geometry to two equivalent C atoms. Both Fe–C bond lengths are 1.98 Å. In the fourth Fe site, Fe is bonded in a distorted trigonal planar geometry to three C atoms. There is one shorter (1.96 Å) and two longer (1.99 Å) Fe–C bond length. In the fifth Fe site, Fe is bonded in a 4-coordinate geometry to four C atoms. There are a spread of Fe–C bond distances ranging from 2.02–2.44 Å. There are two inequivalent C sites. In the first C site, C is bonded in a 7-coordinate geometry to seven Fe atoms. In the second C site, C is bonded in a 6-coordinate geometry to eight Fe atoms.

36 MATERIALS SCIENCE↗

Carbonate stability in the reduced lower mantle

Carbonate minerals are important hosts of carbon in the crust and mantle with a key role in the transport and storage of carbon in Earth’s deep interior over the history of the planet. Whether subducted carbonates efficiently melt and break down due to interactions with reduced phases or are preserved to great depths and ultimately reach the core-mantle boundary remains controversial. In this study, experiments in the laser-heated diamond anvil cell (LHDAC) on layered samples of dolomite (Mg,Ca)CO3 and iron at pressure and temperature conditions reaching those of the deep lower mantle show that carbon-iron redox interactions destabilize the MgCO3 component, producing a mixture of diamond, Fe7C3, and (Mg,Fe)O. However, CaCO3 is preserved, supporting its relative stability in carbonate-rich lithologies under reducing lower mantle conditions. These results constrain the thermodynamic stability of redox-driven breakdown of carbonates and demonstrate progress towards multiphase mantle petrology in the LHDAC at conditions of the lowermost mantle.

58 GEOSCIENCES↗

The iron spin transition of deep nitrogen-bearing mineral Fe3N1.2 at high pressure

Abstract Nitrogen is an essential element for life, one of the most abundant volatiles in the atmosphere, and an important component in the Earth’s interior, where iron nitride is an essential host of deep nitrogen. Here, we investigate the pressure-induced electronic spin-pairing transition of iron in siderazot (Fe3N1.2) at pressures up to 45.8 GPa at room temperature, using diamond-anvil cell techniques coupled with synchrotron X-ray emission spectroscopy. The integrated intensity of the satellite emission peak (K′β) decreases upon compression but remains unchanged at pressures greater than 30.5 GPa. In other words, the high-spin to low-spin transition of iron in Fe3N1.2 starts immediately at very low pressures and completes at ~30.5 GPa. The iron spin transition completion pressures increase with the nitrogen concentration of hexagonal close-packed iron nitrides (i.e., Fe3N1.2, Fe7N3, and Fe2N). Moreover, the identity and concentration of light elements in binary iron-rich compounds such as Fe3N, Fe3C, Fe3P, Fe3S, Fe7C3, and Fe7N3, together with their crystal structure, could affect the iron spin transition pressures. The spin transition of iron-rich alloys could alter the bonding nature and the physical properties, including the thermal and electrical conductivity, thereby influencing the thermal state and evolution of planetary interiors.

Geochemistry & Geophysics↗