Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “Electromigration”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 19 records

In situ measurement of electromigration-induced transient stress in Pb-free Sn-Cu solder joints by synchrotron radiation based X-ray polychromatic microdiffraction

Electromigration-induced hydrostatic elastic stress in Pb-free SnCu solder joints was studied by in situ synchrotron X-ray white beam microdiffraction. The elastic stresses in two different grains with similar crystallographic orientation, one located at the anode end and the other at the cathode end, were analyzed based on the elastic anisotropy of the Beta-Sn crystal structure. The stress in the grain at the cathode end remained constant except for temperature fluctuations, while the compressive stress in the grain at the anode end was built-up as a function of time during electromigration until a steady state was reached. The measured compressive stress gradient between the cathode and the anode is much larger than what is needed to initiate Sn whisker growth. The effective charge number of Beta-Sn derived from the electromigration data is in good agreement with the calculated value.

36 MATERIALS SCIENCE↗

Purification of CdZnTe by electromigration

Electro-migration of ionized/electrically active impurities in CdZnTe (CZT) was successfully demonstrated at elevated temperature with an electric field of 20 V/mm. Copper, which exists in positively charged states, electro-migrated at a speed of 15 μm/h in an electric field of 20 V/mm. A notable variation in impurity concentration along the growth direction with the segregation tendency of the impurities was observed in an electro-migrated CZT boule. Notably, both Ga and Fe, which exist in positively charged states, exhibited the opposite distribution to that of their segregation tendency in Cd(Zn)Te. A CZT detector fabricated from the middle portion of the electro-migrated CZT boule showed an improved mobility-lifetime product of 0.91 × 10{sup −2} cm{sup 2}/V, compared with that of 1.4 × 10{sup −3} cm{sup 2}/V, observed in an as-grown (non-electro-migrated) CZT detector. The optimum radiation detector material would have minimum concentration of deep traps required for compensation.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

Characterization of nanoscale temperature fields during electromigration of nanowires

Quantitative studies of nanoscale heat dissipation (Joule heating) are essential for advancing nano-science and technology. Joule heating is widely expected to play a critical role in accelerating electromigration induced device failure. However, limitations in quantitatively probing temperature fields—with nanoscale resolution—have hindered elucidation of the role of Joule heating in electromigration. In this work, we use ultra-high vacuum scanning thermal microscopy to directly quantify thermal fields in nanowires during electromigration. Our results unambiguously illustrate that electromigration begins at temperatures significantly lower than the melting temperature of gold. Further, we show that during electromigration voids predominantly accumulate at the cathode resulting in both local hot spots and asymmetric temperature distributions. These results provide novel insights into the microscopic details of hot spot evolution during electromigration and are expected to guide the design of reliable nanoscale functional devices.

36 MATERIALS SCIENCE↗

Modeling of microstructural effects on electromigration failure

Current electromigration models used for simulation and analysis of interconnect reliability lack the appropriate description of metal microstructure and consequently have a very limited predictive capability. Therefore, the main objective of our work was obtaining more sophisticated electromigration tools. The problem is addressed through a combination of different levels of atomistic modeling and already available, continuum level macroscopic models. A novel method for an ab initio calculation of the effective valence for electromigration is presented and its application on the analysis of EM behavior is demonstrated. Additionally, a simple analytical model for the early electromigration lifetime is obtained. We have shown that its application provides a reasonable estimate for the early electromigration failures including the effect of microstructure. A simulation study is also applied on electromigration failure in tin solder bumps, where it contributed the understanding of the role of tin crystal anisotropy in the degradation mechanism of solder bumps.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Characterization of electromigration-induced short-range stress development in Al(0.25 at. % Cu) conductor line

Scanning x-ray microbeam topography and fluorescence experiments were conducted in situ to study the electromigration behavior of a 0.5 μm thick, 10 μm wide, and 200 μm long Al(0.25 at. % Cu) conductor line with 1.5 μm-thick SiO2 passivation on a single crystal Si substrate. The strain sensitivity of x-ray topography measurement allowed detailed examination of the electromigration-induced stress distribution and evolution in the conductor line in response to the depletion of Cu solute early in the electromigration process. Upon electromigration at 0.4 MA/cm2 and 303 °C, a short-range stress gradient was quickly induced by Al migration in the Cu-depleted cathode region to counteract further Al flow. The stress gradient was fully developed during the 5.3 h incubation time, extending over the critical Blech length of about 66 μm from the cathode end. Plastic deformation then occurred at the downstream end of the Cu-depleted region. The preferential electromigration of Cu did not cause detectable stress change outside the Cu-depleted region, except for the significant stress development from the Al2Cu precipitation at the anode end which appeared to initiate the fracture in the passivation. Preliminary finite difference modeling was undertaken to simulate the experimental observations, from which important parameters dictating electromigration in Al(Cu) line were extracted: an apparent effective valence of −5.6 and −1.9 for Cu and Al in Al(Cu), respectively, and a critical Cu concentration of 0.16 at. % above which Al grain boundary diffusion is effectively blocked.

Physics↗

Resonantly Enhanced Electromigration Forces for Adsorbates on Graphene

We investigate the electromigration forces for weakly bonded adsorbates on graphene by using density-functional based calculations. We find that the nature of electromigration forces on an adsorbate critically depends on the energy level alignment between the adsorbate state and the Fermi level of the graphene. For a resonant adsorbate, whose frontier orbitals lie close to the Fermi level, the electromigration force is dominated by the electron wind force that is strongly enhanced along the electron flow direction, irrespective of the sign of the adsorbate charge. For a nonresonant adsorbate, the electromigration force is essentially the direct force that depends on the adsorbate charge. We also show that the magnitude of electromigration forces can be continuously tunable through electrostatic gating for resonant adsorbates. Our results provide new insight for understanding and controlling how nanoscale objects behave in or on host materials.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Synchrotron X-Ray Microdiffraction Studies of Electromigration in Interconnect lines at the Advanced Light Source

Synchrotron polychromatic X-ray microdiffraction is a particularly suitable technique to study in situ the effect of electromigration in metal interconnects as add spatial resolution to grain orientation and strain sensitivity. This technique has been extensively used at the Advanced Light Source to monitor changes in aluminum and copper interconnect test structures while high-density current is passed into them during accelerated tests at elevated temperature. One of the principal findings is the observation of electromigration-induced plasticity in the metal lines that appear during the very early stages of electromigration. In some of the lines, high density of geometrically necessary dislocation are formed leading to additional diffusion paths causing an enhancement of electromigration effect at test temperature. This paper presents an overview of the principal results obtained from X-ray microdiffraction studies of electromigration effects on aluminum and copper interconnects at the ALS throughout continuous efforts that spanned over a decade (1998-2008) from approximately 40 weeks of combined beamtime.

36 MATERIALS SCIENCE↗

Highly selective ion separations based on counter-flow electromigration in nanoporous membranes

Highly selective ion separations are vital for recovering important salts, and membrane-based techniques may enable environmentally friendly ion separations that operate continuously. This study demonstrates that simply opposing convective flow with electromigration in track-etched membranes leads to remarkable selectivities among monovalent ions. Because the membrane-pore diameters are orders of magnitude larger than the ion diameters, advection moves all ions at the same velocity, whereas electrophoretic velocities are proportional to ion mobilities. Thus during counter-flow cation electromigration, less mobile cations have lower electromigration velocity components and pass through porous membranes more rapidly than more mobile cations. Using membranes with 400 nm pores, counter-flow electromigration gives Li + /K + selectivities of 100 and Li + /Na + selectivities around 30 in mixed-salt studies. In this work, numerical simulations based on the extended Nernst-Planck equation agree with trends in experimental data and highlight the importance of high Péclet numbers, high current-to-flow ratios, and uniform current distributions for achieving high selectivities. Importantly, experimental separations give high selectivities at 0.3 M ionic strength and low Li + /K + ratios, which suggest these methods may also work in brine solutions. Nevertheless, energy costs for such separations are high.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Synchrotron X-Ray Microdiffraction Studies of Electromigration in Interconnect lines at the Advanced Light Source

Synchrotron polychromatic X-ray microdiffraction is a particularly suitable technique to study in situ the effect of electromigration in metal interconnects as add spatial resolution to grain orientation and strain sensitivity. This technique has been extensively used at the Advanced Light Source to monitor changes in aluminum and copper interconnect test structures while high-density current is passed into them during accelerated tests at elevated temperature. One of the principal findings is the observation of electromigration-induced plasticity in the metal lines that appear during the very early stages of electromigration. In some of the lines, high density of geometrically necessary dislocation are formed leading to additional diffusion paths causing an enhancement of electromigration effect at test temperature.

36 MATERIALS SCIENCE↗

Local fields in conductor surface electromigration: A first-principles study in the low-bias ballistic limit

Utilizing first-principles quantum transport calculations, we investigate the role of local fields in conductor surface electromigration. A nanometer-thick Ag(100) thin film is adopted as our prototypical conductor, where we demonstrate the existence of intense local electric fields at atomic surface defects under an external bias. It is shown that such local fields can play an important role in driving surface electromigration and electrical breakdown. The intense fields originate from the relatively short (atomic-scale) screening lengths common to most elemental metals. This general short-range screening trend is established self-consistently within an intuitive picture of linear response electrostatics. The findings shed new light on the underlying physical origins of surface electromigration and point to the possibility of harnessing local fields to engineer electromigration at the nanoscale.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

In-situ scanning electron microscope observation of electromigration-induced void growth in 30 nm ½ pitch Cu interconnect structures

In-situ electromigration tests have been performed inside a scanning electron microscope on 30 nm wide single damascene interconnects without vias, where a good resolution was obtained and drift velocities during void growth could be measured at 300 °C. These tests showed direct evidence that the cathode end of the line, where a polycrystalline grain cluster encounters a bigger grain, can act as a flux divergent point of Cu diffusion. Moreover, it was found that a thicker barrier suppresses barrier/interface diffusivity of Cu atoms, thereby slowing down electromigration-induced void growth. It was also demonstrated that Cobalt based metal caps are beneficial to electromigration for advanced interconnects where thinner barriers are required.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

In situ electrical characterization of palladium-based single electron transistors made by electromigration technique

We report the fabrication of single electron transistors (SETs) by feedback-controlled electromigration of palladium and palladium-nickel alloy nanowires. We have optimized a gradual electromigration process for obtaining devices consisting of three terminals (source, drain and gate electrodes), which are capacitively coupled to a metallic cluster of nanometric dimensions. This metal nanocluster forms into the inter-electrode channel during the electromigration process and constitutes the active element of each device, acting as a quantum dot that rules the electron flow between source and drain electrodes. The charge transport of the as-fabricated devices shows Coulomb blockade characteristics and the source to drain conductance can be modulated by electrostatic gating. We have thus achieved the fabrication and in situ measurement of palladium-based SETs inside a liquid helium cryostat chamber.

36 MATERIALS SCIENCE↗

Thermoreflectance imaging of electromigration evolution in asymmetric aluminum constrictions

Electromigration (EM) is a phenomenon whereby the flow of current in metal wires moves the underlying atoms, potentially inducing electronic interconnect failures. The continued decrease in commercial lithographically defined feature sizes means that EM presents an increasing risk to the reliability of modern electronics. To mitigate these risks, it is important to look for novel mechanisms to extend lifetime without forfeiting miniaturization. Typically, only the overall increase in the interconnect resistance and failure voltage are characterized. However, if the current flows non-uniformly, spatially resolving the resulting hot spots during electromigration aging experiments may provide better insights into the fundamental mechanisms of this process. Here in this study, we focus on aluminum interconnects containing asymmetric reservoir and void pairs with contact pads on each end. Such reservoirs are potential candidates for self-healing. Thermoreflectance imaging was used to detect hot spots in electrical interconnects at risk of failure as the voltage was gradually increased. It reveals differential heating with increasing voltage for each polarity. We find that while current flow going from a constriction to a reservoir causes a break at the void, the identical structure with the opposite polarity can sustain higher current (J = 21 × 10 6 A/cm 2 ) and more localized joule heating and yet is more stable. Ultimately, a break takes place at the contact pad where the current flows from narrow interconnect to larger pads. In summary, thermoreflectance imaging with submicron spatial resolution provides valuable information about localized electromigration evolution and the potential role of reservoirs to create more robust interconnects.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

A First-Principles Quantum Transport Theory of the Enhanced Wind Force Driving Electromigration on Ag(111) Surfaces

Herein we examine the low bias electromigration wind force acting on quasi one-dimensional nanoscale features within the Landauer-B uttiker conduction picture. Ordinarily the electromigration force is calculated under the approximation that the non-equilibrium carrier distribution in the vicinity of a defect is the same as that in the bulk. However, this approximation is rooted in the assumption that atomic scale defects scatter all incident electrons weakly (just as electrons weakly and diusely scatter in the bulk). We examine this assumption by calculating the mode resolved transmission against Ag(111) step edges and atomic wires using density functional theory (DFT) and the Keldysh non-equilibrium Green's function (NEGF) formalism. Furthermore we show that those modes that scatter strongly give rise to a non-equilibrium electrochemical potential drop across a defect and an increased wind force. The results quantitatively explain previously not understood experimental observations of an enhanced electron wind force against Ag(111) step edges [O. Bondarchuk et al., Phys. Rev. Lett. 99, 206801 (2007)]. In general, the results underscore the challenging nanoscale reliability problem posed by surface electromigration in nanosturctures and the need for a non-equilibrium quantum transport description of the electron wind force.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Flow through negatively charged, nanoporous membranes separates Li + and K + due to induced electromigration

Flow through negatively charged nanopores separates Li + and K + with selectivities of up to 70 and Li + passages from 20% to above 100%. Remarkably, both the Li + /K + selectivity and Li + passage initially increase with flow rate, breaking the permeability/selectivity trade-off. Modelling demonstrates that flow through the membranes creates electric fields that retard transport of cations. Selectivity increases with flow rate because the K + electromigration velocity exceeds its convective velocity, but for Li + electromigration is weaker than convection. Here, modelling also shows the importance of controlling concentration polarization. With further work, related separations might provide highly pure Li salts for battery manufacturing.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Electromigration study of copper lines on steps prepared by a plasma-based etch process

The electromigration phenomenon of the copper line etched with a plasma-based process over the SiN{sub x} step has been investigated. Two important factors, i.e., the dielectric topography and the stress temperature, were examined using the accelerated isothermal electromigration method. The activation energy of 0.73 eV to 0.89 eV indicates two possible mass transport pathways: interfacial and copper surface diffusions. The copper line on the SiN{sub x} step has a shorter lifetime and a smaller activation energy than the copper line on the flat surface has. For the former, voids were formed at the cusp region and perpendicular to the current flow direction. For the latter, voids were formed in series and parallel to the current flow direction. The ''neck'' structure at the cusp region, which is a result of the inappropriate etching condition, further decreased the lifetime and the activation energy. The lifetime of the ''neck-free'' copper line over the SiN{sub x} step was estimated to be 7.1 x 10{sup 9} s under the high-speed IC operation condition. The thermal stress mismatch between the copper layer and TiW barrier layer as well as the underneath dielectric layer facilitated the void formation. The step effect on the lifetime was reduced when the test temperature was high because of the change of the local stress. In summary, the topography and the test temperature are critical factors for the copper line's lifetime.

36 MATERIALS SCIENCE↗

Lattice dependent motion of voids during electromigration

The influence of the crystal lattice configuration to electromigration processes, e.g., void formation and propagation, is investigated in suitable test structures. They are fabricated out of self-assembled, bi-crystalline Ag islands, grown epitaxially on a clean Si(111) surface. The {mu}m-wide and approximately 100 nm thick Ag islands are a composition of a Ag(001) and a Ag(111) part. By focused ion beam milling, they are structured into wires with a single grain boundary, the orientation of which can be chosen arbitrarily. In-situ scanning electron microscopy (SEM) allows to capture an image sequence during electrical stressing and monitors the development of voids and hillocks in time. To visualize the position and motion of voids, we calculate void maps using a threshold algorithm. Most of the information from the SEM image sequence is compressed into one single image. Our present electromigration studies are based on in-situ SEM investigations for three different lattice configurations: Ag(001) (with electron current flow in [110] direction), Ag(111) (with electron current flow in [112] direction), and additionally 90 Ring-Operator rotated Ag(111) (with electron current flow in [110] direction). Our experimental results show that not only the formation and shape but also the motion direction of voids strongly depends on the crystal orientation.

36 MATERIALS SCIENCE↗