The effect of filament peaking on electron beam weld quality

Electron beam welding uses high intensity beams that are generated by an electron emitting cathode under high vacuum conditions. The cathode, typically a ribbon or wire filament of refractory metal, must be heated to sufficiently high temperatures for electron emission to occur and must be carefully controlled to produce the desired beam current while at the same time optimizing filament lifetime. Traditional methods for doing this in commonly used triode gun assemblies consist of first finding the filament knee point in the filament current versus beam current relationship that produces the desired beam current for a given beam voltage. The filament current is then increased by some amount, typically 5–10%, per conventional wisdom to produce a peaked beam. This investigation studies and quantifies the beam and weld quality produced by underkneed and overpeaked filaments using electron beam diagnostics to measure the power density distribution of these beams. Underkneed filaments are shown to have power densities that drop off very quickly below the traditional knee, resulting in poor weld penetration. Kneed filaments do not reach the full beam intensity and also produce shallow welds. Increasing the filament current 10% above the traditional knee was shown to produce a circular Gaussian-like beam with peaked intensity optimized for welding and for filament lifetime. Further increases in the filament current that produce overpeaked beams do not significantly change the beam or weld quality and would only contribute to a reduced filament lifetime.

Electron Beam Welding

Manufacturing Full-Scale High Gradient Copper Accelerators: Electron Beam Welding and Allied Processes

This DOE ARDAP-funded study examines the technical and business feasibility of manufacturing high-gradient normal conducting RF (NCRF) copper accelerating structures using electron beam welding (EBW) instead of conventional high-temperature brazing. The core motivation is material performance: brazing softens copper significantly, while hard copper alloys have demonstrated ~75% higher operational gradients in SLAC tests, making cold-joining techniques highly attractive. EBW, applied to split-cell (half or quadrant) structure designs, preserves copper hardness away from the weld joint and simplifies machining — but industrial process optimization remains immature and a substantial learning curve is expected. The business case was modeled for two scenarios: a greenfield EBW linac company (> $10M upfront costs, viable above ~30 units/year) and an EBW division added to an existing accelerator firm to reduce risk and upfront costs, at the expense of being less optimal structure for the higher volume production. The study concludes that without a significant increase in demand, private investment alone cannot sustain this capability, and recommends federal support through R&D grants, procurement incentives, and CAPEX cost-sharing to incubate domestic EBW-NCRF manufacturing — with the existing-company model.

43 PARTICLE ACCELERATORS

Microstructure and 77K mechanical properties of electron beam welded Cu101- Inconel 625 joints

In developing large-scale next-generation superconducting radio frequency (SRF) linear accelerators using superconducting films on Cu, the design and development of dissimilar welding and joining metals, such as Cu to Inconel, stainless steel, and Nb, are essential. In this talk, we present the development of procedures for electron-beam welding of Cu¿Inconel 625 and evaluation of the microstructure and 77K mechanical properties of the weld and base material in the welded condition and heat treatments in the 750°C ¿950°C heat treatment range. The results will be presented in the context of developing joining techniques for low-temperature applications where high conductivity and strength, vacuum hygiene, and magnetic properties of the material need consideration. The methods presented here are being deployed to thin film SRF Cu cavities at Jefferson Lab. Acknowledgment: This material is based upon work supported by the U.S. Department of Energy, Office of Science, Office of Nuclear

Khanal, Bashu

Welding investigation of a wrought FeMnAl steel for armor application

A new wrought FeMnAl steel contains high Mn content and high Al content. This steel has high strength. When it is compared to conventional steels with the similar strength, its density is lower. FeMnAl steels can be used in armor vehicle manufacturing, in which welding is a common practice to join the steel plates together. The welding of FeMnAl steels has not been sufficiently studied before. Here, this work studied the weldability and weld microstructure of an FeMnAl steel and provided useful data for the welding practice of FeMnAl steels. The influences of weld filler metals and shielding gases were studied, using single-pass bead-on-plate gas metal arc welding (GMAW) and gas tungsten arc welding (GTAW) two processes. The optimal filler metals and shielding gases have been determined to achieve the better weldability. Autogenous GTAW and electron beam welding were also conducted. Cracks were found in the HAZ in the GMAW welds and electron beam welds. Fewer or no cracks were found in the HAZ of GTAW welds. SEM, SEM/EDX, TEM, TEM/EDX, and EBSD were used to analyze the grain boundaries in the HAZ and the cracks. The grain boundaries of FeMnAl base metal are mostly high angle grain boundaries (HAGBs), which attract impurity and solute atoms and cause intergranular cracking. The proposed cracking mechanisms are liquation cracking and ductility-dip cracking. It was found that GTAW provides much better weldability for the FeMnAl steel than GMAW and EBW.

FeMnAl steel

Non-circular electron beam spot welds in stainless steel alloys

Circularly symmetric-shaped spot welds are desirable for welding applications as they relate to heat and fluid flow conditions in the melt pool with predictable weld penetrations and repeatable results. Non-circular spot welds on the other hand result in undesirable and unpredictable weld penetrations or non-bridging of the liquid melt pool across the joint. Two known causes for non-circular melt pools occur when welding dissimilar metals, or when welding with skewed electron or laser beams that are not perpendicular to the surface. A largely unexplored additional factor, shown here, is an asymmetric power density distribution within the beam that can create non-circular melt pools even though the beam dimensions are much smaller than the melt pool itself.

36 MATERIALS SCIENCE

Influence of fabrication on microstructure and heat affected zone width in weldments of nuclear reactor pressure vessel steel

Advanced manufacturing routes such as electron beam welding and powder metallurgy with hot isostatic pressing are increasingly used across energy and aerospace industries, where the reliable prediction of weld behavior and heat affected zone (HAZ) evolution is critical. This study examines how fabrication routes and post-weld heat treatments influence phase distribution, crystallite size, microstrain, and dislocation density in nuclear reactor pressure vessel steels using synchrotron X-ray diffraction (SXRD). Retained austenite occurs only in samples that did not undergo austenitization, whereas an austenitizing heat treatment fully eliminates retained austenite and produces a more uniform microstructure across the weldment in terms of phase fraction, dislocation density, and microstrain. The Rosenthal solution underestimates the HAZ width for powder metallurgy samples. A newly proposed modified Rosenthal solution, reducing density by accounting for porosity, matches the SXRD-measured HAZ width with a 0.65% error. Structure–property correlations reveal that dislocation density correlates strongly with nanohardness in homogenous microstructures, while in heterogenous weldments nanohardness is further influenced by the presence of dissimilar phase boundaries. These findings provide new insight into the thermal and microstructural response of powder metallurgy fabricated steels and offer a framework for optimizing welding procedures and heat treatments in advanced manufacturing applications.

73 NUCLEAR PHYSICS AND RADIATION PHYSICS

Gigacycle Fatigue Strength Evaluation of Welded 316L Stainless Steels for Mercury Target Vessel

At the Materials and Life Science Experimental Facility (MLF) in J-PARC, liquid mercury target for the pulsed spallation neutron source is in operation. An enclosure vessel for the liquid mercury target made of type 316L stainless steel (SS316L) suffers two kinds of cyclic stress during operation. One is the thermal stress due to the internal heating and swings by proton beam trip. The other is the impulsive stress by the pressure waves generated by the proton beam injection. The total number of loading cycles for the former is ∼104, and the latter is ∼4 × 108 for a year operation in the J-PARC mercury target vessel. The target vessel is assembled by an electron beam welding (EBW) and a gas tungsten arc welding (GTAW). However, fatigue data of welded SS316L up to gigacycle is limited. Ultrasonic fatigue testing, applying load cycles by utilizing ultrasonic resonance, for the welded SS316L was performed to investigate the effect of welding on fatigue behavior up to a gigacycle. The result showed that the fatigue strength degradation by EBW and EBW with GTAW were not recognized up to 109 cycles. Crack initiation in welded specimens nucliated at off-center areas of the specimen whereas the cracks in base metal specimen originated at the specimen center.

Naoe, Takashi [Japan Atomic Energy Agency (JAEA)]

Design of Silicide-Strengthened Nb–Si–Cr–(Mo) alloys for additive manufacturing

Three high–intermetallic volume Nb–Si–Cr–(Mo) alloys were designed using CALPHAD modeling with the goal of identifying high–specific strength, oxidation-resistant alloys that can be additively manufactured using powder bed fusion. The silicides Nb 5 Si 3 and Nb 9 Si 2 Cr3 were targeted as the primary strengthening phases, and the addition of Cr promoted the NbCr 2 phase. These alloys were cast and surface-processed with electron beam welding at different speeds to simulate additive manufacturing, and the phases and microstructures of both cast and welded regions were characterized. The weld processing was found to produce fine-grained microstructures in each alloy with fine-scale intermetallics uniformly distributed among a body-centered cubic Nb matrix. Microstructural refinement and hardness were found to increase with weld velocity; one alloy reached its highest hardness of approximately 16 GPa before the brittleness at higher velocities became detrimental. One alloy was found to be qualitatively the least brittle while also attaining a hardness of 13 GPa and was therefore identified as a good candidate for additive manufacturing.

36 MATERIALS SCIENCE

Unveiling the Interplay: Cold Work, Recrystallization, and Flux Expulsion in SRF Cavities

The fabrication of SRF cavities from sheet materials includes deep-drawing, electron beam welding, chemical and mechanical polishing, high-temperature heat treatment, and material diffusion. The performance of these cavities is frequently limited by magnetic flux trapping giving rise to additional rf loss. In this presentation, we thoroughly examine how recrystallization influences flux expulsion in SRF cavities, using cold-worked niobium sheets from various suppliers. Our findings reveal that cold-worked sheets enhance flux expulsion, especially at lower heat treatment temperatures, by promoting improved recrystallization. In particular, a traditionally fabricated Nb cavity half-cell from an annealed poly-crystalline Nb sheet after an 800 C heat treatment leads to a bi-modal microstructure that ties in with flux trapping and inefficient flux expulsion. This non-uniform microstructure is related to varying strain profiles along the cavity shape. A novel approach to prevent this non-uniform microstructure is presented by fabricating a 1.3 GHz single cell Nb cavities with a cold-worked sheet and subsequent heat treatment leading to better flux expulsion after 800 C/3h

Dhakal, P. [Old Dominion Univ., Norfolk, VA (Unite

Non-Intrusive Load Monitoring of EBW Processes A Second Study [Slides]

The Objective is to Determine if induced off-nominal welding disturbances: (1) Beam arc out (weld on high vapor pressure aluminum plate); (2) Pulsed beam voltage; (3) Pulsed beam current; and (4) Pulsed beam focus current can be observed in the input power to the high-voltage cabinet powering the EB gun, ie Non-Instrusive Load Monitoring (NILM).

36 MATERIALS SCIENCE

Time-Dependent 600 °C Post-Weld Heat Treatment Response of Laser-Wire-Directed Energy Deposited Austenitic Stainless Steel Claddings on Carbon Steel

Austenitic stainless steel overlay claddings are often used to protect nuclear reactor pressure vessels from corrosion. Arc welding processes are traditionally employed, which require a high heat input to bond the dissimilar metals, creating a large heat-affected zone and high residual stress that demands a lengthy stress-relieving post-weld heat treatment, up to 48 hours. High energy beam (e.g., laser, electron beam) directed energy deposition-based overlay cladding processes show promise for fabricating claddings with superior performance compared to arc welded ones because of their localized heat input; however, their necessity and time of post-weld heat treatment are currently unclear. In this research, we investigate the time dependence of a 600 C stress-relieving post-weld heat treatment of austenitic stainless steel clad on low carbon steel by laser-wire-directed energy deposition, comparing the microstructure and mechanical properties of the as-fabricated condition to 2-, 10-, and 48-hour heat treatment times. Diffusion simulations and microscopy show a gradual carburization of the stainless steel cladding and decarburization of the heat-affected zone/base metal. Nanoindentation testing shows up to a 1.8–2.69 embrittlement in the cladding and a 0.33 to 0.69 softening in the heat-affected zone after the 48-hour post-weld heat treatment. Tensile testing of the cladding composites reveals that increasing post-weld heat treatment time raises clad cracking susceptibility due to intergranular carbide formation and shows that laser-wire-directed energy deposition claddings may not require post-weld heat treatment.

Coating

High-Speed and High-Quality Field Welding Repair Based on Advanced Non-Destructive Evaluation and Numerical Modeling

Creep strength-enhanced ferritic (CSEF) steels such as Grade 91 (9Cr-1Mo-V) and Grade 92 (Fe-9Cr-2W-0.5Mo) steels are widely used in the fossil-fuel-fired and nuclear power plants. The weld integrity of these steels is crucial for power plants' safe and reliable operations. Due to harsh service conditions, the steel weld can become susceptible to environmental degradation. Field welding repair is used to restore the degraded weld’s performance where a controlled temper-bead welding technique is commonly used to temper the freshly formed martensite during welding. However, knowledge of weld repairability is limited and experimental trial and error optimization to achieve desired microstructure and joint properties is expensive and time-consuming. Many existing computational models, e.g., finite element models, are limited to solving heat conduction equation and ignoring convective heat transfer due to molten metal flow. These models can result in over-prediction of peak temperatures of weld pool and heat-affected zone (HAZ), which in turn can affect the accuracy of tempering prediction. Moreover, these finite element models require an input of the deposit profiles in advance and thus limits the usability of these models. Here, a molten pool-based, multi-pass multi-layer model has been developed based on computational fluid dynamics (CFD) approach with the Volume of Fluid (VOF) method. The model calculates the bead formation, thereby eliminating the need for pre-determined bead profiles required by finite element models. For computational efficiency, a coordinate system attached to the moving heat source is utilized. A subroutine is developed to convert the temperature profiles in the reference frame stationary to the heat source to that stationary to the workpiece. The converted thermal cycles are then imported into a microstructure model to compute the tempering kinetics and resultant hardness using a Johnson-Mehl-Avrami-Kolmogorov (JMAK), and modified Grange-Baughman parameter. The modeling approach is first developed and validated on single- and multi-pass deposition of stainless steel filler metal onto a SA-533 high strength steel substrate. The models are then applied to a multi-pass V-groove repair weld of Grade 91 steel plate as well as directed energy deposition of Grade 92 steel. Non-destructive characterization of microstructures was performed on Grade 91 and 92 steel welds. Two welding processes, cold metal transfer (CMT) and flux-cored arc welding (FCAW), were investigated for the Grade 91 steel weld samples. For the Grade 92 weld samples, three different heat inputs (low, medium, and high) of gas tungsten arc welding (GTAW) were utilized to replicate traditional field welding processes. The non-destructive evaluation (NDE) method used for this research was immersion ultrasonic testing (UT) using a micro-resolution ultrasonic imaging methodology specifically designed to operate in the through-transmission configuration operating at 20 MHz of frequency. The system used a focused ultrasonic beam spot size diameter between 250-300 μm, and a 6 μm laser vibrometer spot size for detection, to produce highly defined images with longitudinal and mode-converted shear waves. From the micro-resolution ultrasonic C-scan images, three microstructural regions, i.e., weld metal (WM), HAZ, and base metal (BM), were clearly identifiable. Various levels of ultrasonic amplitudes distributed over the three regions were correlated with electron beam backscattered diffraction (EBSD) images using grain size, grain boundaries, and dislocation densities. The results showed that areas with relatively higher ultrasonic amplitude levels were associated with smaller grains and higher dislocation densities, while areas with lower amplitude levels were associated with larger grains and lower dislocation densities. In addition, ultrasonic velocity data obtained across the three different weld microstructural regions of Grade 91 test samples were correlated with optical metallographic images and hardness measurements. The results showed distinctive decreases in ultrasonic velocity and hardness over the HAZ region, where weld failures often occur during service.

36 MATERIALS SCIENCE

Dissimilar metal joining of Ti-6Al-4V and Inconel 625

The dissimilar joining of Ti-6Al-4V and Inconel 625 by using a suitable interlayer shows potential design flexibility by avoiding the brittle intermetallic phases from direct welding. These phases include NiTi , NiTi 2 , and Ni 3 Ti . The objective of this work is to facilitate laser welding of Ti-6Al-4V and Inconel 625 through a vanadium interlayer to form an intermetallic free, strong, and corrosion resistant joint. Vanadium was chosen based on binary phase diagram solubilities, literature, and theoretical CalPhaD calculations in PanDat. Laser welding was systematically explored from based on beam mode, offset, power, and scan speed. Varied parameters include laser power from 325 to 650 watts, laser scan speed from 80 to 160 in/min, and beam offset up to a ¼ of the beam diameter. Parameters were chosen based on previous dissimilar joining research and those found in the literature. Metallography, including optical and scanning electron microscopy, was used to analyze the weld chemical composition, grain structure, and defects through both the fusion and heat affected zones. The results and discussion will examine the relationship between process parameters, microstructure, and observed weld defects. Our findings will not only assess the weldability of vanadium and Inconel 625 but also establish a transferable framework for studying other dissimilar material combinations, providing valuable insights for future research in this field.

36 MATERIALS SCIENCE

Laser repair welding of irradiated alloy 182

Welding repair of irradiated nickel-based alloys, such as Alloy 182, poses a significant challenge due to helium-induced cracking (HeIC) and grain boundary degradation (GBD) in the heat affected zone, driven by helium accumulation at grain boundaries and welding-induced tensile stresses. This study investigates the weldability of irradiated Alloy 182 up to 15 wppm doped boron using both conventional laser welding and the Auxiliary Beam Stress Improved (ABSI) laser welding technique. While HeIC was observed at the weld toe of the entry pass in both methods due to the higher effective heat input associated with the initial pass directly on the base metal, no additional cracking occurred elsewhere, even at elevated helium concentrations. Optical and scanning electron microscopy analysis revealed that the ABSI technique, which introduces additional compressive stresses to counteract solidification-induced tensile stresses, significantly reduced GBD formation, lowering its total count from 1,230 to 339 and decreasing both average and maximum GBD lengths. In conclusion, these results demonstrate that the ABSI technique is a promising approach to mitigate helium-induced damage and improve the weldability of irradiated Alloy 182, offering a viable solution for structural repairs for long-term operation of existing nuclear reactors.

grain boundary degradation