Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “DIENES”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 19 records

Processing Conjugated-Diene-Containing Polymers

Diels-Alder reaction used to cross-linked thermoplastics. Process uses Diels-Alder reaction to cross-link and/or extend conjugated-diene-containing polymers by reacting them with bis-unsaturated dienophiles results in improved polymer properties. Quantities of diene groups required for cross-linking varies from very low to very high concentrations. Process also used to extend, or build up molecular weights of, low-molecular-weight linear polymers with terminal conjugated dienic groups.

Bell, Vernon L.↗

Process for crosslinking and extending conjugated diene-containing polymers

A process using a Diels-Alder reaction which increases the molecular weight and/or crosslinks polymers by reacting the polymers with bisunsaturated dienophiles is developed. The polymer comprises at least 75% by weight based on the reaction product, has a molecular weight of at least 5000 and a plurality of conjugated 1,3-diene systems incorporated into the molecular structure. A dienophile reaction with the conjugated 1,3-diene of the polymer is at least 1% by weight based on the reaction product. Examples of the polymer include polyesters, polyamides, polyethers, polysulfones and copolymers. The bisunsaturated dienophiles may include bis-maleimides, bis maleic and bis tumaric esters and amides. This method for expanding the molecular weight chains of the polymers, preferable thermoplastics, is advantageous for processing or fabricating thermoplastics. A low molecular weight thermoplastic is converted to a high molecular weight plastic having improved strength and toughness for use in the completed end use article.

Bell, Vernon L.↗

Addition polymers from 1,4,5,8-tetrahydro-1,4;5,8-diepoxyanthracene and Bis-dienes: Processable resins for high temperature application

1,4,5,8-Tetrahydro-1,4;5,8-diepoxyanthracene reacts with various anthracene endcapped polyimide oligomers to form Diels-Alder cycloaddition copolymers. The polymers are soluble in common organic solvents, and have molecular weights of approximately 21,000 to 32,000. Interestingly, these resins appear to be more stable in air then in nitrogen. This is shown to be due to a unique dehydration (loss of water ranges from 2 to 5 percent) at temperatures of 390 to 400 C to give thermo-oxidatively stable pentiptycene units along the polymer backbone. Because of their high softening points and good thermo-oxidative stability, the polymers have potential as processible, matrix resins for high temperature composite applications.

Meador, Mary Ann B.↗

Addition polymers from 1,4,5,8-tetrahydro-1,4;5,8-diepoxyanthracene and Bis-dienes. 2: Evidence for thermal dehydration occurring in the cure process

Diels-Alder cycloaddition copolymers from 1,4,5,8-tetrahydro-1,4;5,8-diepoxyanthracene and anthracene end-capped polyimide oligomers appear, by thermogravimetric analysis (TGA), to undergo dehydration at elevated temperatures. This would produce thermally stable pentiptycene units along the polymer backbone, and render the polymers incapable of unzipping through a retro-Diels-Alder pathway. High resolution solid 13C nuclear magnetic resonance (NMR) of one formulation of the polymer system before and after heating at elevated temperatures, shows this to indeed be the case. NMR spectra of solid samples of the polymer before and after heating correlated well with those of the parent pentiptycene model compound before and after acid-catalyzed dehydration. Isothermal gravimetric analyses and viscosities of the polymer before and after heat treatment support dehydration as a mechanism for the cure reaction.

Meador, Mary Ann B.↗

Processable, high temperature polymers from 1,4,5,8-tetrahydro-1,4;5,8-diepoxyanthracene and bis-dienes

1,4,5,8-tetrahydro-1,4;5,8-diepoxyanthracene reacts with various anthracene end-capped polyimide oligomers to form Diels-Alder cycloaddition copolymers. The polymers are soluble in common organic solvents, and have molecular weights of approximately 21,000 to 32,000. These resins exhibit lower weight loss in air than in nitrogen. This is suggested to be due to dehydration (loss of water ranges from 2 to 5 percent) at temperatures of 390 to 400 C to give thermooxidatively stable pentiptycene units along the polymer backbone. Because of their high softening points and good thermooxidative stability, the polymers have potential as processable, matrix resins for high temperature composite applications.

Meador, Mary Ann B.↗

Diels-Alder Trapping of Photochemically Generated Dienes with Acrylic Esters: A Novel Approach to Photocured Polymer Film Development

Diels-Alder cycloadditions have often been utilized in polymer synthesis as an alternative to condensation reactions. In our earlier efforts, we developed a new method for the preparation of linear aromatic polyimides, which employs o-quionodimethanes (o-QDMs), generated by a well-known photochemical reaction: the photoenolization of o-methylphenyl ketones. Photolysis of o-methylbenzophenone 1 produces hydroxy-o-quino- diemthane 2, which can be trapped with dienophiles, such as dimethyl acetylenedicarboxylate, to efficiently yield the corresponding cycloadduct (Scheme 1). Here we extend this approach to a novel photocuring process for development of polymer films. We synthesized a series of molecules with multi o-mehtylphenyl ketone functionalities. We further investigated these molecules as photoreactive monomers to obtain polyester films through Diels-Alder cycloadditions.

Ilhan, Faysal↗

Mixed solvent electrolytes for ambient temperature secondary lithium cells

The present invention comprises an improved electrolyte for secondary lithium-based cells as well as batteries fabricated using this electrolyte. The electrolyte is a lithium containing salt dissolved in a non-aqueous solvent, which is made from a mixture of ethylene carbonate, ethylene propylene diene terpolymer, 2-methylfuran, and 2-methyltetrahydrofuran. This improved, mixed solvent electrolyte is more conductive than prior electrolytes and much less corrosive to lithium anodes. Batteries constructed with this improved electrolyte utilize lithium or lithium alloy anodes and cathodes made of metal chalcogenides or oxides, such as TiS.sub.2, NbSe.sub.3, V.sub.6 O.sub.13, V.sub.2 O.sub.5, MoS.sub.2, MoS.sub.3, CoO.sub.2, or CrO.sub.2, dissolved in a supporting polymer matrix, like EPDM. The preferred non-aqueous solvent mixture comprises approximately 5 to 30 volume percent ethylene carbonate, approximately 0.01 to 0.1 weight percent ethylene propylene diene terpolymer, and approximately 0.2 to 2 percent 2-methylfuran, with the balance being 2-methyltetrahydrofuran. The most preferred solvent comprises approximately 10 to 20 volume percent ethylene carbonate, about 0.05 weight percent ethylene propylene diene terpolymer, and about 1.0 percent 2-methylfuran, with the balance being 2-methyltetrahydrofuran. The concentration of lithium arsenic hexafluoride can range from about 1.0 to 1.8 M; a concentration 1.5 M is most preferred. Secondary batteries made with the improved electrolyte of this invention have lower internal impedance, longer cycle life, higher energy density, low self-discharge, and longer shelf life.

Shen, David H.↗

Thermal rearrangements in 1,2-poly/1,4-hexadiene/s

The work described was carried out to study the thermal rearrangements of two unsaturated diene polymers - 1,2-poly(cis-1,4-hexadiene) (CHD) and 1,2-poly(trans-1.4-hexadiene) (THD). It is shown that both CHD and THD have a predominatly 1,8 diene structure and seem to cyclize mainly by the (2 + 2) thermal cycloaddition of double bonds, and to a small extent also by sigmatropic rearrangement with hydrogen shift.

Golub, M. A.↗

Thermal rearrangements of unsaturated polymers

Thermal anaerobic uncatalyzed cyclizations and cis-trans isomerizations observed in unsaturated hydrocarbon polymers are surveyed. Three main types of cyclizations are described. Type I is a radical reaction which is caused by chain rupture and gives rise to six-membered rings; this reaction occurs during pyrolysis of polymers with double bonds in a 1,5- or 1,6-diene configuration. Type II is a (2 + 2) thermal cycloaddition of double bonds in certain polymers with a 1,6-diene structure; bicycloheptane structures result. Type III is an intramolecular ene reaction. Many polymers containing a double bond linking CH units display thermal cis-trans isomerization. The common activation energy is approximately 130 kJ/mol, and the initial rate constants are lower, for homologous polymers, the greater the separation of the carbon-carbon double bonds.

Golub, M. A.↗

Reversible Thermoset Adhesives

Embodiments of a reversible thermoset adhesive formed by incorporating thermally-reversible cross-linking units and a method for making the reversible thermoset adhesive are provided. One approach to formulating reversible thermoset adhesives includes incorporating dienes, such as furans, and dienophiles, such as maleimides, into a polymer network as reversible covalent cross-links using Diels Alder cross-link formation between the diene and dienophile. The chemical components may be selected based on their compatibility with adhesive chemistry as well as their ability to undergo controlled, reversible cross-linking chemistry.

Mac Murray, Benjamin C.↗

Photochromism of heterocyclic systems

The preparations of photochromic dimers of a 2-aryl-4,5-di-phenylimidazyl radical and of a 2,5-diphenyl-3,4-isobenzopyrrole with different substituents in the homocyclic ring are reported. Of the dienes investigated, only 1-4-diphenyl-1,3-butadiene and 2,3-dimethyl-1,3-butadiene gave isolable amounts of the Diels-Adler adducts.

Silversmith, E. F.↗

Interstellar molecules - Origin by catalytic reactions on grain surfaces

To determine the compound distribution formed by surface catalysis, mixtures of CO, D2, and ND2 were heated with nickel-iron or montmorillonite clay catalysts for 49-214 hours at 250 to 300 C. Compounds identified include most of the known polyatomic interstellar molecules, as well as homologous series of acetylenes, dienes, alcohols, aldehydes, ketones, ethers, esters, nitriles, amines, etc., and cyclic compounds such as furans and pyrroles. These homologous series are uniquely characteristic of surface catalysis. A search for the heavier members of these series, predicted to occur at 1/10th to 1/1,000th the abundance of the lightest members, thus comprises a crucial test of this mechanism.

Anders, E.↗

Toxicity of Pyrolysis Gases from Elastomers

The toxicity of the pyrolysis gases from six elastomers was investigated. The elastomers were polyisoprene (natural rubber), styrene-butadiene rubber (SBR), ethylene propylene diene terpolymer (EPDM), acrylonitrile rubber, chlorosulfonated polyethylene rubber, and polychloroprene. The rising temperature and fixed temperature programs produced exactly the same rank order of materials based on time to death. Acryltonitrile rubber exhibited the greatest toxicity under these test conditions; carbon monoxide was not found in sufficient concentrations to be the primary cause of death.

Hilado, Carlos J.↗

Effect of heating rate on toxicity of pyrolysis gases from some elastomers

The effect of heating rate on the toxicity of the pyrolysis gases from six elastomers was investigated, using a screening test method. The elastomers were polyisoprene (natural rubber), styrene-butadiene rubber (SBR), ethylene propylene diene terpolymer (EPDM), acrylonitrile rubber, chlorosulfonated polyethylene rubber, and polychloroprene. The rising temperature and fixed temperature programs produced exactly the same rank order of materials based on time to death. Acrylonitrile rubber exhibited the greatest toxicity under these test conditions, and carbon monoxide was not found in sufficient concentrations to be the primary cause of death.

Hilado, C. J.↗

Impact-induced energy partitioning, melting, and vaporization on terrestrial planets

The reported investigation was conducted in connection with the desirability to obtain information regarding the response of a solidified planetary surface to the primary impact of a meteoroid whose dimensions are small compared to that of the planet. The investigation is an extension of studies conducted by Ahrens and O'Keefe (1977) concerned with a calculation via finite-difference techniques of the entire flow field, the energy partitioning, and the quantity of melt and vapor produced upon impact of an iron object on a gabbroic anorthosite half-space at 15 km/sec. The assumptions used in these calculations are summarized. Calculations based on an equation of state for the low- and high-pressure mineral assemblage of gabbroic anorthosite, initial density 2.94 g/cu cm are considered. An algorithm is formulated for the description of the phase transformation upon shock loading. It is shown that the relative volume of melt and the equivalent volume of shock-induced vapor is proportional to the meteoroid kinetic energy (at high speeds) using the similarity scaling of projectile and target properties as suggested by Dienes and Walsh (1970).

Okeefe, J. D.↗

Concentration-time data in toxicity tests and resulting relationships

Periodic analyses for carbon monoxide and methane in the animal exposure chamber during pyrolysis of polyethylene at 800 C without forced air flow showed that the concentrations of these compounds increased with exposure time. These observations, and similar observations for polyurethane flexible foam, permitted the calculation of carbon monoxide toxicity in terms of a DP (Death Product Concentration) value, in addition to flammability in terms of HC (Hydro Carbon) value. Observed DP values exceeding the critical DP(CO) value of 47,200 ppm-min for carbon monoxide may indicate that lethal exposures were reached earlier but not immediately manifested because of the time delay involved in physiological processes. On the basis of this DP(CO) value, carbon monoxide could have been the sole toxicant in the case of polyethylene, polypropylene, polyoxymethylene, polystyrene, polycarbonate, ethylene propylene diene rubber, and wood.

Hilado, C. J.↗