Burst pressure models and validations for thick-walled pipelines containing corrosion defects
Corrosion is one major threat to pipeline integrity. Over the past decades, many corrosion models have been developed for determining the remaining strength of corroded pipelines, including ASME B31.G, Modified B31.G, LPC, PCORRC and their modified models. All these corrosion models are applicable only to large diameter, thin-walled pipelines with a diameter to wall thickness ratio D/t ≥ 20. In practice, many pipelines have a small diameter and thick wall with a D/t ratio < 20, and thus an adequate corrosion model is needed for assessing remaining strength for corroded thick-walled pipelines. This paper briefly reviews the theoretical burst pressure models for defect-free thin and thick-walled pipelines and four representative corrosion assessment models for thin-walled corroded pipelines. On this basis, two modified corrosion models are proposed to thick-walled pipelines in terms of the average shear stress yield theory. To verify the proposed corrosion models, comprehensive validations are performed. Numerical validations include the elastic-plastic finite element analysis to determine burst pressure for pipelines without and with corrosion defects and the model evaluation using a large dataset of available FEA results of burst pressure for machined defects. Experimental validations include a set of burst pressure tests for defect-free thick-walled pipes with different thicknesses and the model evaluation using one large burst dataset for machined defects with flat bottoms and another large dataset for real corrosion defects with curved river bottom profiles. Both numerical and experimental validations show that the proposed corrosion models can more accurately predict the remaining strength for corroded thin and thick-walled pipelines.