Color Change During Thermal Degradation of Polyolefin Electric Cable Insulations
Color change of electric cable insulations used in nuclear power plants (NPPs) is a non-destructive, quick and inexpensive technique to measure degradation. Quantification of color change is facilitated by a light booth of CIE D65 illuminant, a commercial camera and open-source software ImageJ with micaToolbox plugin. Yellowness index (YI) and total color difference (?E) are calculated from calibrated photos of a white cross-linked polyethylene (XLPE) and a black ethylene-propylene rubber (EPR) based specimens aged at 110°C, 121°C, 136°C and 150°C after 1~640 days. Using the same setup and software, pixelwise ?E profile is determined for the cross-sectional photo of a white EPR specimen, where heterogeneous aging is detected.