The derivation of CRSS in pure Ti and Ti-Al alloys

The work focuses on the determination of the critical resolved shear stress (CRSS) in titanium (Ti) and titanium-aluminum (Ti-Al) alloys, influenced by an array of factors such as non-symmetric fault energies and minimum energy paths, dislocation core-widths, short-range order (SRO) effects which alter the local atomic environment, and tension-compression (T-C) asymmetry affected by intermittent slip motion. To address these multifaceted complexities, an advanced theory has been developed, offering an in-depth understanding of the mechanisms underlying slip behavior. The active slip systems in these materials are basal, prismatic, and pyramidal planes, with the latter involving both $\langle$a$\rangle$ and $\langle$c + a$\rangle$ dislocations. Each slip system is characterized by distinct Wigner-Seitz cell configurations for misfit energy calculations, varying partial dislocation separation distances, and unique dislocation trajectories—all critical to precise CRSS calculations. The theoretical CRSS results were validated against a comprehensive range of experimental data, demonstrating a strong agreement and underscoring the model's efficacy.

Critical stress↗

Cross-slip and easy-glide CRSS in titanium: Theoretical predictions and in-situ TEM measurements

This study investigates the mechanics of prismatic and first-order pyramidal $\langle$a$\rangle$ slip in titanium (Ti), elucidating the physics of easy-glide and cross-slip through a combination of theory and experiments. Screw-character prismatic (Pr) dislocations in Ti are of particular interest because their complex cores can be stable or unstable, leading to activation by either cross-slip or planar glide. To investigate these mechanisms, site-specific micro tensile samples were prepared using focused ion beam (FIB) milling and mounted on a push-to-pull (PTP) device for in-situ transmission electron microscopy (TEM) tensile testing. The in-situ experiments provide direct observations of the onset of dislocation motion and the precise determination of the critical resolved shear stress (CRSS) for the activated mechanisms, and its evolution with load cycling. A comprehensive theory has been developed to predict the CRSS values for easy glide, cross-slip, and multiplication of dislocations. Predicted critical stresses for pyramidal (π)-to-Pr and reverse cross-slip agree closely with the experimental measurements. The latter cross-slip stress is a factor of two higher than that of unobstructed planar slip. The model accounts for overlapping dislocation cores and employs a Wigner-Seitz based cell to evaluate misfit energies. By combining ab initio density functional theory (DFT) with anisotropic elasticity, the framework identifies minimum energy pathways for dislocation glide, which can be intermittent and zig-zag. A simplified expression utilizing (π) and Pr Schmid factor ratios is proposed for critical stress corresponding to (π)-to-Pr cross-slip transition. The results are strongly dependent on crystal orientation, underscoring non-Schmid behavior. Overall, this study explores key critical stress parameters essential for informing higher-scale simulations of plasticity in Ti.

Critical stress↗

Assessment of surface and bulk-dominated methodologies to measure critical resolved shear stresses in hexagonal materials

We present that crystallographic slip in hexagonal metals involves a number of geometrically distinct slip families characterized by their slip direction and slip plane (basal, prismatic, and pyramidal). Owing to the low symmetry of hexagonal lattices, each of these slip families only have a few symmetrically equivalent slip systems (family members). Furthermore, different slip families become active at different resolved shear stress, i.e., they have different critical resolved shear stress values (CRSS). The plastic anisotropy of hexagonal materials makes the numerical prediction of their plastic behavior challenging and depends critically on the knowledge of CRSS values. The present contribution assesses the reliability of three proposed methods (with additional variations) to quantify CRSS values of the different hexagonal slip families. Those methods (a to c) rely on: (a) the statistics of observed surface slip traces in a (slightly) deformed polycrystal; (b) an iterative adjustment of CRSS values until a simulated single crystal indentation matches the corresponding experiment in terms of load–displacement response and residual surface topography of the indent; (c) in-situ high-energy X-ray diffraction to measure the evolution of resolved stress (from lattice strains) in grains for which single-family slip is probable based upon specific lattice reorientation conditions. Virtual experiments are performed on synthetic microstructures such that the (extracted) CRSS values resulting from simulating the different methodologies can be rigorously compared against the (target) CRSS values that are installed in the phenomenological constitutive material description used in the simulations. The resulting CRSS values of methods (a) exhibit a strong dependence on, and deterioration with, decreasing level of slip trace observability, which is an uncertain quantity in experimental measurements. For the inverse indentation method (b), the predicted CRSS values are within 8 % of their reference CRSS values for the two investigated cases. Lastly, the high-energy X-ray diffraction method (c) most reliably determines CRSS values for basal and prism slip, but lacks a strict grain selection criterion to assess pyramidal slip.

36 MATERIALS SCIENCE↗

Direct measurement of critical resolved shear stress of prismatic and basal slip in polycrystalline Ti using high energy X-ray diffraction microscopy

Knowledge of the critical resolved shear stress (CRSS) values of different slip modes is important for accurately modeling plastic deformation of hexagonal materials. Here, we demonstrate that CRSS can be directly measured with an in-situ high energy X-ray diffraction microscopy (HEDM) experiment. A commercially pure Ti tensile specimen was deformed up to 2.6% strain. In-situ far-field HEDM experiments were carried out to track the evolution of crystallographic orientations, centers of masses, and stress states of 1153 grains in a material volume of 1.1mm×1mm×1mm. Predominant prismatic slip was identified in 18 grains, where the orientation change occurred primarily by rotation around the c-axis during specimen deformation. By analyzing the resolved shear stress on individual slip systems, the estimated CRSS for prismatic slip is 96±18 MPa. Predominant basal slip was identified in 22 other grains, where the 2 orientation change occurred primarily by tilting the c-axis about an axis in the basal plane. The estimated CRSS for basal slip is 127±33 MPa. The ratio of CRSS basal /CRSS prismatic is in the range of 1.7-2.1. From indirect assessment, the CRSS for pyramidal < c+a > slip is likely greater than 240MPa. Lastly, grain size and free surface effects on the CRSS value in different grains are also examined.

46 INSTRUMENTATION RELATED TO NUCLEAR SCIENCE AND ↗

Distorted dislocation cores and asymmetric glide resistances in titanium

The determination of Critical Resolved Shear Stress (CRSS) in titanium for basal, prismatic, and pyramidal slip-planes without empirical constants is presented by combining Density Functional Theory (DFT) and anisotropic elasticity. A new mechanism leading to tension-compression (T-C) asymmetry in the CRSS levels has been revealed for the first time. The conditions for this asymmetry are established, involving a complex interplay between the dislocation core-structure and core-advance behavior. The three conditions for T-C asymmetry that need to be simultaneously satisfied can be summarized as: (1) a medium stacking fault width, d, (3 < d/b F < 10, where b F is the magnitude of the Burgers vector of the full dislocation), (2) an asymmetric core-structure of the extended dislocation (ξ 1 ≠ ξ 2 , where ξ 1 and ξ 2 are the core-widths of the first and second partials, respectively), and (3) intermittent motion of the partials (Δd/b F ≠ 0, where Δd is the magnitude of fluctuation in stacking fault width during intermittent motion). Pyramidal-slip in titanium satisfies all three conditions, resulting in significant T-C asymmetry. The CRSS theory considers a Wigner-Seitz (W-S) cell based domain area assigned to each lattice site for the calculations of core-energies accurately capturing the slip-plane lattice. The W-S based approach is essential due to the lower symmetry of the HCP crystal circumventing potential errors associated with the one-dimensional atomic-row approximation. Dislocation core structures are obtained for all the slip-systems in titanium showing significant distortion of the disregistry profile governing the core-advance behavior. The CRSS values predicted from the theory show agreement with the experimental CRSS levels reported in the literature.

Dislocation core↗

Plastic deformation of single crystals of the equiatomic Cr-Mn-Fe-Co-Ni high-entropy alloy in tension and compression from 10 K to 1273 K

In this report the plastic deformation behavior of single crystals of the quinary, equiatomic Cr-Mn-Fe-Co-Ni high-entropy alloy (HEA) with the face-centered cubic structure has been investigated in tension and compression as a function of crystal orientation and temperature from 10 K to 1373 K. The critical resolved shear stress (CRSS) for {111}<110> slip at room temperature is 42-45 MPa. It does not depend much on crystal orientation (i.e., the Schmid law holds true) and the sense (tension vs. compression) of the applied load. The CRSS for {111}<110> slip increases with the decrease in temperature, without showing any significant inertia effects at cryogenic temperatures below 77 K. Extrapolation from the measured yield stresses down to 10 K yields a CRSS value at 0 K of 168 MPa. At cryogenic temperatures, the measured strain-rate sensitivity of flow stress is consistent with a very small activation volume. The concept of stress equivalence holds true both for the temperature dependence of CRSS and the stress dependence of activation volume, indicating that solid-solution hardening is the major strengthening mechanism. Deformation twinning occurs at 77 K but not at room temperature, resulting in higher tensile elongation to failure at 77 K than at room temperature. Deformation twinning at 77 K occurs at a shear stress of 378 MPa on conjugate ($\bar1\bar11$) planes in the form of Lüders deformation after large plastic strain (about 85%) achieved by the stage I (easy glide) and stage II (linear work-hardening) deformation.

36 MATERIALS SCIENCE↗

Temperature-dependent phase-specific deformation mechanisms in a directionally solidified NiAl-Cr(Mo) lamellar composite

Phase-specific thermal expansion and mechanical deformation behaviors of a directionally solidified NiAl–Cr(Mo) lamellar in situ composite were investigated by using real-time in situ neutron diffraction during compression at elevated temperatures up to 800 °C. Tensile and compressive thermal residual stresses were found to exist in the NiAl phase and Crss (solid solution) phase, respectively. Then, based on the evolution of lattice spacings and phase stresses, the phase-specific deformation behavior was analyzed qualitatively and quantitatively. Moreover, estimates of phase stresses were derived by Hooke's law on the basis of a simple method for the determination of stress-free lattice spacing in in situ composites. During compressive loading, the NiAl phase yields earlier than the Crss phase. The Crss phase carries much higher stress than the NiAl phase, and displays consistent strain hardening at all temperatures. The NiAl phase exhibits strain hardening at relatively low temperatures and softening at high temperatures. During unloading, the NiAl phase yields in tension whereas the Crss phase unloads elastically. Additionally, post-test microstructural observations show phase-through cracks at room temperature, micro cracks along phase interfaces at 600 °C and intact lamellae kinks at 800 °C, which is due to the increasing deformability of both phases as temperature rises.

36 MATERIALS SCIENCE↗

Twin nucleation and migration in FeCr single crystals

Tension and compression experiments were conducted on body-centered cubic Fe -47.8 at pct. Cr single crystals. The critical resolved shear stress (CRSS) magnitudes for slip nucleation, twin nucleation and twin migration were established. We show that the nucleation of slip occurs at a CRSS of about 88 MPa, while twinning nucleates at a CRSS of about 191 MPa with an associated load drop. Following twin nucleation, twin migration proceeds at a CRSS that is lower than the initiation stress ( Almost-Equal-To 114-153 MPa). The experimental results of the nucleation stresses indicate that the Schmid law holds to a first approximation for the slip and twin nucleation cases, but to a lesser extent for twin migration particularly when considerable slip strains preceded twinning. The CRSSs were determined experimentally using digital image correlation (DIC) in conjunction with electron back scattering diffraction (EBSD). The DIC measurements enabled pinpointing the precise stress on the stress-strain curves where twins or slip were activated. The crystal orientations were obtained using EBSD and used to determine the activated twin and slip systems through trace analysis. - Highlights: Black-Right-Pointing-Pointer Digital image correlation allows to capture slip/twin initiation for bcc FeCr. Black-Right-Pointing-Pointer Crystal orientations from EBSD allow slip/twin system indexing. Black-Right-Pointing-Pointer Nucleation of slip always precedes twinning. Black-Right-Pointing-Pointer Twin growth is sustained with a lower stress than required for nucleation. Black-Right-Pointing-Pointer Twin-slip interactions provide high hardening at the onset of plasticity.

36 MATERIALS SCIENCE↗

Role of alloying elements on twin growth and twin transmission in magnesium alloys

A spatially-resolved crystal plasticity Fast Fourier Transform (FFT)-based model is employed to study the effect of alloying addition on twin thickening and twin transmission in hexagonal close packed (HCP) magnesium. In the simulations, the influence of alloying additions is represented through the differences in the critical resolved shear stress (CRSS) of different slip and twinning modes. The results show that for the same grain orientation, twin type and boundary conditions, anisotropy in the CRSS values have a significant effect on twin thickening and twin transmission. Those with large differences in CRSS favor both twin thickening and twin transmission, and vice versa for those with small differences. Furthermore, less difference among the CRSS values enhances the dependence of thickening and transmission on the neighboring grain orientation.

36 MATERIALS SCIENCE↗

Study of slip activity in a Mg-Y alloy by in situ high energy X-ray diffraction microscopy and elastic viscoplastic self-consistent modeling

Slip activity from various slip modes largely determines the yield strength and ductility of Mg alloys. Solid solution elements in Mg can change the slip activity dramatically. In this paper, far-field high energy X-ray diffraction microscopy (FF-HEDM) is employed to study slip activity in a Mg-3wt%Y alloy during an in situ tensile experiment. The specimen was incrementally loaded up to 3% engineering strain along the rolling direction. At each load step, FF-HEDM data were collected to track the crystallographic orientation, center of mass, and stress tensor changes of nearly 1000 grains in the probed volume. By analyzing the change in orientation and stress tensor of individual grains at different load steps, it is possible to identify the activated slip systems and measure their critical resolved shear stress (CRSS) values. Prismatic slip and pyramidal I slip are found to be very active in this alloy. The estimated CRSS values for basal slip, prismatic slip and pyramidal I slip are 12 MPa, 38 MPa, and 36 MPa, respectively. These CRSS values were applied in a dislocation-based elastic viscoplastic self-consistent (EVPSC) model that successfully simulated the tensile stress-strain curve from the FF-HEDM experiment. The model also qualitatively predicted the crystal rotation in most of the selected grains, though it underestimated the internal stress and the magnitude of crystal rotation in these grains. Influence of solute Y on the strength and ductility of Mg alloys is discussed.

36 MATERIALS SCIENCE↗

A measure of plastic anisotropy for hexagonal close packed metals: Application to alloying effects on the formability of Mg

Mg is inherently plastically anisotropic and, over the years, alloying development efforts have sought to reduce the plastic anisotropy in order to enhance formability. To understand the relationship between alloy type and plastic anisotropy, we use a visco-plastic self-consistent (VPSC) polycrystal plasticity model to relate the macroscopic constitutive response to the underlying slip and twinning mechanisms in pure Mg and several Mg alloys. In the calculations, the influence of alloy type is represented by the differences in the CRSS values among the basal, prismatic, pyramidal slip and tensile twin systems. We show that for the same initial texture, this microscopic-level CRSS anisotropy can have a significant effect on the macroscopic indicators of formability, namely the anisotropy of the post-deformation polycrystal yield surface, tension-compression yield asymmetry, and Lankford coefficients. A plastic anisotropy (PA) measure is formulated to quantify the degree of single crystal plastic anisotropy acquired by the dissimilarities in the CRSS values of the slip and twinning modes for a given alloy. We demonstrate a strong correlation between the PA measure with the formability indicators mentioned above for multiple initial textures commonly enountered in processing. In conclusion, we find that alloys can be classified into two groups, those with a PA value below 2, which are more formable, less twinnable, and less sensitive to initial texture, where PA ~2 for pure Mg, and those with a PA value above 2, which possess the opposite deformation response.

36 MATERIALS SCIENCE↗

Phase field dislocation dynamics (PFDD) modeling of non-Schmid behavior in BCC metals informed by atomistic simulations

Body-Centered Cubic (BCC) metals exhibit anomalous mechanical properties such as twinning/anti-twinning and tension/compression asymmetry, which are attributed to asymmetric behavior of screw dislocations. Unlike Face-Centered Cubic (FCC) metals, the Critical Resolved Shear Stress (CRSS) of BCC metals deviates from the Schmid law. Here, we use a mesoscale modeling approach called Phase Field Dislocation Dynamics (PFDD) to understand the critical factors that control this non-Schmid behavior and reproduce atomistic predictions of the CRSS (Peierls stress). All inputs to the PFDD model are obtained from Molecular Statics (MS) simulations. Multiple pathways for modeling the non-Schmid behavior are investigated by incorporating the representative dislocation properties into different energy terms in the PFDD model. One way to understand non-Schmid behavior is to incorporate stress components projected on inclined planes into the external energy term within PFDD. Alternatively, we propose that non-Schmid behavior can also be accounted for by considering the variation of the {110} unstable stacking fault energy and the dislocation core width as a function of the applied tensorial stress field. The CRSS predicted using PFDD modeling is in excellent agreement with MS predictions.

36 MATERIALS SCIENCE↗

Experimental determination of critical resolved shear stress for strain-induced phase transformation

The current investigation reports the first attempt to measure the critical resolved shear stress to initiates strain-induced phase transformation in a three-dimensional polycrystalline aggregate using high-energy diffraction microscopy (HEDM). In situ tensile testing was performed on a Fe38.5Mn20Co20Cr15Si5Cu1.5 metastable alloy exhibiting transformation-induced plasticity (TRIP). Grains with a higher propensity for strain-induced phase transformation were tracked using HEDM. A sharp drop in grain specific stress, coinciding with the appearance of a new ε-hcp grain oriented relative to the parent γ-fcc phase, was taken as evidence of grain-specific stress required to trigger phase transformation. The highest resolved shear stress on the potential transformation systems was identified as the critical resolved shear stress (CRSS) for strain-induced phase transformation. For the studied metastable alloy, CRSS for transformation was determined to be 86±3 MPa which was very close to theoretical CRSS value determined using Schmid factor (89±12 MPa) compared to the value determined using Taylor factor (62±7 MPa).

Jain, Roopam↗

Assessing Adaptive Irrigation Impacts on Water Scarcity in Nonstationary Environments—A Multi‐Agent Reinforcement Learning Approach

Abstract One major challenge in water resource management is to balance the uncertain and nonstationary water demands and supplies caused by the changing anthropogenic and hydroclimate conditions. To address this issue, we developed a reinforcement learning agent‐based modeling (RL‐ABM) framework where agents (agriculture water users) are able to learn and adjust water demands based on their interactions with the water systems. The intelligent agents are created by a reinforcement learning algorithm adapted from the Q‐learning algorithm. We illustrated this framework in a case study where the RL‐ABM is two‐way coupled with the Colorado River Simulation System (CRSS), a long‐term planning model used for the administration of the Colorado River Basin, for assessing agriculture water uses impacts on water scarcity. Seventy‐eight intelligent agents are simulated, which can be grouped into three categories based on their parameter values: the “aggressive” (swift actions; low regrets), the “forward‐looking conservative” (mild actions; high regrets; fast learning), and the “myopic conservative” (mild actions; median regrets; slow learning). The ABM‐CRSS results showed that the major reservoirs in the Upper Colorado Basin might experience more frequent water shortages due to the increasing water uses compared to the original CRSS results. If the drought continues, the case study also demonstrates that agents can learn and adjust their demands.

Hung, Fengwei↗

Size effect, critical resolved shear stress, stacking fault energy, and solid solution strengthening in the CrMnFeCoNi high-entropy alloy

High-entropy alloys (HEAs) comprise a novel class of scientifically and technologically interesting materials. Among these, equatomic CrMnFeCoNi with the face-centered cubic (FCC) structure is noteworthy because its ductility and strength increase with decreasing temperature while maintaining outstanding fracture toughness at cryogenic temperatures. Here we report for the first time by single crystal micropillar compression that its bulk room temperature critical resolved shear stress (CRSS) is ~33–43MPa, ~10 times higher than that of pure nickel. CRSS depends on pillar size with an inverse power-law scaling exponent of –0.63 independent of orientation. Planar ½<110>{111} dislocations dissociate into Shockley partials whose separations range from ~3.5–4.5nm near the screw orientation to ~5–8nm near the edge, yielding a stacking fault energy of 30±5mJ/m2. Dislocations are smoothly curved without any preferred line orientation indicating no significant anisotropy in mobilities of edge and screw segments. The shear-modulus-normalized CRSS of the HEA is not exceptionally high compared to those of certain concentrated binary FCC solid solutions. Its rough magnitude calculated using the Fleischer/Labusch models corresponds to that of a hypothetical binary with the elastic constants of our HEA, solute concentrations of 20–50 at.%, and atomic size misfit of ~4%.

36 MATERIALS SCIENCE↗

The effects of heat treatment on the response of WE43 Mg alloy: crystal plasticity finite element simulation and SEM-DIC experiment

The present report addressed the effects of heat treatment on the mechanical response of a WE43 Mg alloy using an integrated framework of SEM-DIC experiment and CPFE simulation. Both macroscopic responses including yield strength, ultimate strength, ductility, and microscopic responses, including local displacement and strain maps, were experimentally investigated. The focus of this work is to use the CPFE simulation as an integrated computational tool to study the effects of heat treatment. The CPFE framework was evaluated using the local fields of displacement and strain obtained from the SEM-DIC experiment rather than the conventional scheme of using macroscopic responses at different loading directions. Subsequently, the information which is available using CPFE, such as the critical resolved shear stress (CRSS) and relative slip activity, was used to study the effects of heat treatment on the response of WE43 Mg alloy. The contributions of different strengthening mechanisms on the CRSS were addressed. The results show that effects of heat treatment can be captured using the predominant mechanisms of the grain size effect and the influence of precipitates. Finally, it has been shown that classical Hall-Petch in which one constant can capture the size effects, should be modified. To do so, each deformation mode should have a unique Hall-Petch constant, which are calculated here for the WE43 Mg alloy.

36 MATERIALS SCIENCE↗

Tensile and compressive plastic deformation behavior of medium-entropy Cr-Co-Ni single crystals from cryogenic to elevated temperatures

The equiatomic Cr-Co-Ni medium-entropy alloy has the face-centered cubic (FCC) structure. Bulk single crystals of this alloy were grown and tested in tension and compression between 14 K and 1373 K with the loading axis parallel to [23]. At room temperature, the critical resolved shear stress (CRSS) for {111}<10> slip is 65 ± 5 MPa and does not exhibit a tension-compression asymmetry. It does, however, increase significantly as the test temperature decreases. A dulling of this temperature dependence occurs below 50 K, which may be due to the inertia effect. When the measured values above 50 K are extrapolated to lower temperatures, a value of 225 MPa is estimated for the CRSS at 0 K. This is larger than that (168 MPa) previously determined for the equiatomic Cr-Mn-Fe-Co-Ni high-entropy alloy using a similar procedure. The stacking fault energy of the present Cr-Co-Ni is estimated to be about 14 mJm-2, which is sufficiently low to account for deformation twinning both at 77 K and room temperature. Twinning at 77 K occurs on conjugate (1) planes at an onset shear stress of 482 MPa after primary slip and propagates in the form of Lüders deformation. At room temperature, twinning occurs uniformly throughout the gauge section on primary (111) planes at an onset shear stress of 381 MPa after primary and subsequent conjugate slip. Thin layers with the hexagonal close-packed stacking are observed in association with twinning both at 77 K and room temperature.

36 MATERIALS SCIENCE↗

Hydrogen effects on the deformation and slip localization in a single crystal austenitic stainless steel

Hydrogen is known to embrittle austenitic stainless steels, which are widely used in high-pressure hydrogen storage and delivery systems, but the mechanisms that lead to such material degradation are still being elucidated. The current work investigates the deformation behavior of single crystal austenitic stainless steel 316L through combined uniaxial tensile testing, characterization and atomistic simulations. Thermally precharged hydrogen is shown to increase the critical resolved shear stress (CRSS) without previously reported deviations from Schmid’s law. Molecular dynamics simulations further expose the statistical nature of the hydrogen and vacancy contributions to the CRSS in the presence of alloying. Slip distribution quantification over large in-plane distances (> 1 mm), achieved via atomic force microscopy (AFM), highlights the role of hydrogen increasing the degree of slip localization in both single and multiple slip configurations. The most active slip bands accumulate significantly more deformation in hydrogen precharged specimens, with potential implications for damage nucleation. For $\langle$110$\rangle$ tensile loading, slip localization further enhances the activity of secondary slip, increases the density of geometrically necessary dislocations and leads to a distinct lattice rotation behavior compared to hydrogen-free specimens, as evidenced by electron backscatter diffraction (EBSD) maps. Finally, the results of this study provide a more comprehensive picture of the deformation aspect of hydrogen embrittlement in austenitic stainless steels.