Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “CERAMIC MELTERS”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 19 records

Numerical modeling of Joule heated ceramic melter

Computational fluid dynamics and heat transfer models of waste glass melters are being developed to support the vitrification campaign at the Waste Treatment and Immobilization Plant (WTP) as part of the United States nuclear waste stewardship and environmental protection programs. The WTP mission aims to achieve the stable and durable processing of vitrified waste in the safest, most efficient, and economical manner possible. Hanford’s tank waste is far more complex and varied than the waste treated by other vitrification facilities and both startup and long-term operational challenges are likely to be even greater than prior experience has shown. There are thousands of different waste compositions, which makes processing the waste a complex and challenging task. Models of test melters, pilot-scale, and full-scale melters have been developed to provide understanding and insight into the various physical and chemical phenomena occurring during vitrification. So the results of these modeling activities will be used to support the WTP operations to process legacy nuclear waste into a stable form for disposal.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Predictive modeling of crystal accumulation in high-level waste glass melters processing radioactive waste

The effectiveness of HLW vitrification is limited by precipitation/accumulation of spinel crystals [(Fe, Ni, Mn, Zn)(Fe, Cr)2O4] in the glass discharge riser of Joule-heated ceramic melters during idling. These crystals do not affect glass durability; however, if accumulated in thick layer, they can clog the melter and prevent discharge of molten glass into canisters. To address this problem, an empirical model was developed that can predict thicknesses of accumulated layers as a function of glass composition. This model predicts well the accumulation of single crystals and/or small-scale agglomerates, but, excessive agglomeration observed in high-Ni-Fe glass resulted in an under-prediction of accumulated layers, which gradually worsen over time as an increased number of agglomerates formed. Accumulation rate of ~53.8 ± 3.7 µm/h determined for this glass will result in ~26 mm thick layer in 20 days of melter idling.

Crystal accumulation↗

Investigation of processing advanced waste forms in Cold Crucible Induction Melter systems

The Cold Crucible Induction Melter (CCIM) technology has been identified in several independent reviews and studies as a potential alternative or supplemental vitrification technology for specific U.S. Department of Energy (DOE) high level radioactive waste (HLW) streams. These inventories have unique chemistries, such as high alumina, high iron, high chromium, etc., that are not amenable to efficient immobilization in conventional borosilicate glass (BSG) matrices. Advanced waste forms, such as iron phosphate glass (FePG), high crystalline BSG (HC-BSG), and alumino-silicate glass-ceramic (GC) have been shown to provide significantly improved immobilization matrices for these challenging waste streams, including dramatically improved waste loadings; however, they are difficult to efficiently process in the baseline joule-heated ceramic melters (JHCMs). The CCIM technology can effectively process these advanced waste forms at the desired high waste loadings. This paper describes the most recent collaborative activities between the DOE Office of Environmental Management (DOE EM) and various Russian institutions in modeling, development and testing of advanced waste forms in CCIMs, including FePG and HC-BSG formulations. Additionally, past interactions with other international partners, including France and Korea, are described. Finally, recent enhancements to CCIM processing related to modeling, draining techniques and automated control, which were collaboratively developed, will be discussed. (authors)

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Water Cleaning System for the Exhaust Pipe of HLW Glass Melter (LFCM) - 17180

Vitrification technology has been generally applied to stabilize High-Level Radioactive Waste (HLW) generated from spent fuel reprocessing. In Japan, Joule Heated Liquid Fed Ceramic Melter (LFCM) system is selected for HLW vitrification and the recent active test has been successfully demonstrated its stable operation. The higher reliability of off-gas treatment system (OGTS) which consists of wet scrubber, absorbers and filters connected to the LFCM is also important to ensure long term system operation. The OGTS removes radioactive gases, mists and dust generated by LFCM and maintains radioactive containments by keeping negative pressure inside. In the past active and inactive tests, it was observed that differential pressure in the exhaust pipe attached to LFCM gradually increased during continuous operation and some deposits were observed inside the off-gas pipe. So the cleaning operation needs to be improved and more frequent in order to avoid the exhaust pipe clogging. Therefore we investigated several cleaning systems and operational methods for the exhaust pipe of LFCM. As a result, we have successfully developed the modified water cleaning system. In this presentation we will introduce our water cleaning system. In addition, we will present the result of inactive mock-up tests for the visualization of this water cleaning system. (authors)

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Advanced waste form and Melter development for treatment of troublesome high-level wastes

A number of waste components in US defense high level radioactive wastes (HLW) have proven challenging for current Joule heated ceramic melter (JHCM) operations and have limited the ability to increase waste loadings beyond already realized levels. Many of these “troublesome" waste species cause crystallization in the glass melt that can negatively impact product quality or have a deleterious effect on melter processing. Recent efforts at US Department of Energy laboratories have focused on understanding crystallization behavior within HLW glass melts and investigating approaches to mitigate the impacts of crystallization so that increases in waste loading can be realized. Advanced glass formulations have been developed to highlight the unique benefits of next-generation melter technologies such as the Cold Crucible Induction Melter (CCIM). Crystal-tolerant HLW glasses have been investigated to allow sparingly soluble components such as chromium to crystallize in the melter but pass out of the melter before accumulating.The Hanford site AZ-101 tank waste composition represents a waste group that is waste loading limited primarily due to high concentrations of Fe 2 O 3 (also with high Al 2 O 3 concentrations). Systematic glass formulation development utilizing slightly higher process temperatures and higher tolerance to spinel crystals demonstrated that an increase in waste loading of more than 20% could be achieved for this waste composition, and by extension higher loadings for wastes in the same group. An extended duration CCIM melter test was conducted on an AZ-101 waste simulant using the CCIM platform at the Idaho National Laboratory (INL). The melter was continually operated for approximately 80 hours demonstrating that the AZ-101 high waste loading glass composition could be readily processed using the CCIM technology. The resulting glass was close to the targeted composition and exhibited excellent durability in both the as poured state and after being slowly cooled according to the canister centerline cooling (CCC) profile. Glass formulation development was also completed on other Hanford tank wastes that were identified to further challenge waste loading due to the presence of appreciable quantities (>750 g) of plutonium in the waste tanks. In addition to containing appreciable Pu quantities, the C-102 waste tank and the 244-TX waste tank contain high concentrations of aluminum and iron, respectively that will further challenge vitrification processing. Glass formulation testing also demonstrated that high waste loadings could be achieved with these tank compositions using the attributes afforded by the CCIM technology.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

NEXT GENERATION MELTER(S) FOR VITRIFICATION OF HANFORD WASTE STATUS AND DIRECTION

Vitrification technology has been selected to treat high-level waste (HLW) at the Hanford Site, the West Valley Demonstration Project and the Savannah River Site (SRS), and low activity waste (LAW) at Hanford. In addition, it may potentially be applied to other defense waste streams such as sodium bearing tank waste or calcine. Joule-heated melters (already in service at SRS) will initially be used at the Hanford Site's Waste Treatment and Immobilization Plant (WTP) to vitrify tank waste fractions. The glass waste content and melt/production rates at WTP are limited by the current melter technology. Significant reductions in glass volumes and mission life are only possible with advancements in melter technology coupled with new glass formulations. The Next Generation Melter (NGM) program has been established by the U.S. Department of Energy's (DOE's), Environmental Management Office of Waste Processing (EM-31) to develop melters with greater production capacity (absolute glass throughput rate) and the ability to process melts with higher waste fractions. Advanced systems based on Joule-Heated Ceramic Melter (JHCM) and Cold Crucible Induction Melter (CCIM) technologies will be evaluated for HLW and LAW processing. Washington River Protection Solutions (WRPS), DOE's tank waste contractor, is developing and evaluating these systems in cooperation with EM-31, national and university laboratories, and corporate partners. A primary NGM program goal is to develop the systems (and associated flowsheets) to Technology Readiness Level 6 by 2016. Design and testing are being performed to optimize waste glass process envelopes with melter and balance of plant requirements. A structured decision analysis program will be utilized to assess the performance of the competing melter technologies. Criteria selected for the decision analysis program will include physical process operations, melter performance, system compatibility and other parameters.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

MODELING THE IMPACT OF ELEVATED MERCURY IN DEFENSE WASTE PROCESSING FACILITY MELTER FEED ON THE MELTER OFF-GAS SYSTEM-PRELIMINARY REPORT

The Defense Waste Processing Facility (DWPF) is currently evaluating an alternative Chemical Process Cell (CPC) flowsheet to increase throughput. It includes removal of the steam-stripping step, which would significantly reduce the CPC processing time and lessen the sampling needs. However, its downside would be to send 100% of the mercury that comes in with the sludge straight to the melter. For example, the new mercury content in the Sludge Batch 5 (SB5) melter feed is projected to be 25 times higher than that in the SB4 with nominal steam stripping of mercury. This task was initiated to study the impact of the worst-case scenario of zero-mercury-removal in the CPC on the DWPF melter offgas system. It is stressed that this study is intended to be scoping in nature, so the results presented in this report are preliminary. In order to study the impact of elevated mercury levels in the feed, it is necessary to be able to predict how mercury would speciate in the melter exhaust under varying melter operating conditions. A homogeneous gas-phase oxidation model of mercury by chloride was developed to do just that. The model contains two critical parameters pertaining to the partitioning of chloride among HCl, Cl, Cl{sub 2}, and chloride salts in the melter vapor space. The values for these parameters were determined at two different melter vapor space temperatures by matching the calculated molar ratio of HgCl (or Hg{sub 2}Cl{sub 2}) to HgCl{sub 2} with those measured during the Experimental-Scale Ceramic Melter (ESCM) tests run at the Pacific Northwest National Laboratory (PNNL). The calibrated model was then applied to the SB5 simulant used in the earlier flowsheet study with an assumed mercury stripping efficiency of zero; the molar ratio of Cl-to-Hg in the resulting melter feed was only 0.4, compared to 12 for the ESCM feeds. The results of the model run at the indicated melter vapor space temperature of 650 C (TI4085D) showed that due to excessive shortage of chloride, only 6% of the mercury fed is expected to get oxidized, mostly as HgCl, while the remaining mercury would exist either as elemental mercury vapor (90%) or HgO (4%). Noting that the measured chloride level in the SB5 qualification sample was an order of magnitude lower than that used in the SB5 simulant, the degree of chloride shortage will be even greater. As a result, the projected level of HgCl in the actual SB5 melter exhaust will be even lower than 6% of the total mercury fed, while that of elemental mercury is likely to be greater than 90%. The homogeneous oxidation of mercury in the off-gas was deemed to be of primary importance based on the postulation that mercury and other volatile salts form submicron sized aerosols upon condensation and thus remain largely in the gas stream downstream of the quencher where they can deposit in the off-gas lines, Steam-Atomized Scrubbers (SAS), and High-Efficiency Mist Eliminator (HEME). Formation of these submicron semi-volatile salts in the condensate liquid is considered to be unlikely, so the liquid phase reactions were considered to be less important. However, subsequent oxidation of mercury in the liquid phase in the off-gas system was examined in a simplified model of the off-gas condensate. It was found that the condensate chemistry was consistent with further oxidation of elemental mercury to Hg{sub 2}Cl{sub 2} and conversion of HgO to chlorides. The results were consistent with the available experimental data. It should also be noted that the model predictions presented in this report do not include any physically entrained solids, which typically account for much of the off-gas carryover on a mass basis. The high elemental mercury vapor content predicted at the DWPF Quencher inlet means that physically entrained solids could provide the necessary surface onto which elemental mercury vapor could condense, thereby coating the solids as well as the internal surfaces of the off-gas system with mercury. Clearly, there are many process benefits to be gained by removing the steam-stripping step from the CPC cycle. The goal of this task was to study what adverse impact the zero-mercury-removal scenario would have on the DWPF melter off-gas system operation. It is stressed again that this study was intended to be scoping in nature, so the results presented in this report are preliminary. Any further substantiation of these results for actual implementation into the DWPF flowsheet would require an in-depth modeling study of all three reaction zones, including the aqueous-phase reactions in the quencher, OGCT, Steam Atomized Scrubber (SAS), and off-gas condenser with recirculated condensate, and the proof-of-principle experiments.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

DEVELOPMENT OF GLASS MATRICES FOR HLW RADIOACTIVE WASTES

Vitrification is currently the most widely used technology for the treatment of high level radioactive wastes (HLW) throughout the world. Most of the nations that have generated HLW are immobilizing in either borosilicate glass or phosphate glass. One of the primary reasons that glass has become the most widely used immobilization media is the relative simplicity of the vitrification process, e.g. melt waste plus glass forming frit additives and cast. A second reason that glass has become widely used for HLW is that the short range order (SRO) and medium range order (MRO) found in glass atomistically bonds the radionuclides and governs the melt properties such as viscosity, resistivity, sulphate solubility. The molecular structure of glass controls contaminant/radionuclide release by establishing the distribution of ion exchange sites, hydrolysis sites, and the access of water to those sites. The molecular structure is flexible and hence accounts for the flexibility of glass formulations to waste variability. Nuclear waste glasses melt between 1050-1150 C which minimizes the volatility of radioactive components such as Tc{sup 99}, Cs{sup 137}, and I{sup 129}. Nuclear waste glasses have good long term stability including irradiation resistance. Process control models based on the molecular structure of glass have been mechanistically derived and have been demonstrated to be accurate enough to control the world's largest HLW Joule heated ceramic melter in the US since 1996 at 95% confidence.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Vitrification of Sellafield Wastes with High Metallic Magnesium Alloy Content - 17495

The Sellafield nuclear complex, located in northwest England, is the largest such site in the United Kingdom. Sellafield Limited, which is the operating contractor for the Nuclear Decommissioning Authority, is evaluating thermal treatment technologies for a potential future facility to process a variety of Intermediate Level Waste sludges and slurries accumulated from historical site operations. In support of that effort, Atkins and the Vitreous State Laboratory (VSL) of The Catholic University of America conducted studies to evaluate the feasibility and implications of installing a joule-heated ceramic melter (JHCM) vitrification system to process a variety of sludge and slurry radioactive wastes at the Sellafield site. These sludges have the potential to contain a significant proportion of reactive metals in localized regions. The metallic fraction derives from unreacted Magnox spent fuel cladding. Thus, an important objective of this work was to investigate the performance of JHCM technology for the treatment of streams with localized regions of high reactive metal contents. The present work was focused on Site Ion Exchange Effluent Plant (SIXEP) Magnox sludges, investigated previously. Suitable waste simulants were developed for the SIXEP Magnox sludge waste stream, which included surrogates for all important radionuclides. High waste-loading, fully compliant glass formulations were designed using a combination of previous experience, extensive waste glass data bases, and small-scale crucible melts. Glasses from the test melts were characterized for properties that are important for processability and product quality. The most viable compositions were then selected for small-scale melter trials to collect information on processing rates and behavior, off-gas and secondary waste compositions, and overall system mass balance. These data were used to support the technology evaluation, which considered such factors as minimization of inactive additions, waste volume reduction, retention of radionuclides, minimization of secondary wastes, and overall process efficiency and effectiveness. The data were also used to develop sizing estimates for the full-scale facility and to estimate treatment durations under various treatment scenarios. A series of tests was then performed with partial replacement of the magnesium hydroxide with a metallic magnesium alloy that is close in composition to Magnox alloy. A commercially available magnesium alloy, Elecktron AZ31B, which has a nominal magnesium content of 95.7%, was used for this purpose. The testing was performed on a DuraMelter 10 (DM10) JHCM system to characterize the melter off-gas, glass product, and the effects of magnesium alloy particle size on feed processing. Data on processing rate and any processing issues, product glass composition, off-gas composition including hydrogen, and system operating parameters, including flows, temperatures, pressures, etc., were collected and analyzed to evaluate the effects of magnesium alloy on the vitrification process. (authors)

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

DETERMINATION OF STOKES SHAPE FACTOR FOR SINGLE PARTICLES AND AGGLOMERATES

The large octahedral crystals of spinel can precipitate from glass during the high-level waste vitrification process and potentially block the glass discharge riser of electrically heated ceramic melters. To help predict the settling behavior of spinel in the riser, the settling of single particles and agglomerates was studied in stagnant and transparent viscosity oils at room temperature with developed optical particle-dynamics-analyzer. Determined dimensions and terminal settling velocities of particles were used for calculation of their Stokes shape factors. Calculated shape factor for the glass beads was almost identical with the theoretical shape factor of 2/9 for a perfect sphere. The shape factor for single spinel crystal was about 7.6 % higher compare to the theoretically predicted value for octahedron. Stokes shape factor of irregularly shaped multi-particle agglomerates was lower than that of the glass beads and individual spinel crystals because of the higher surface drag caused by the larger surface area to volume ratio.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Ruthenium Behavior at Phase Separation of Borosilicate Glass-12259

The Rokkasho reprocessing plant (RRP) located in Aomori, Japan, vitrifies high level waste (HLW) into a borosilicate glass. The HLW is generated from the reprocessing of spent fuel and contains ruthenium (Ru) and other platinum group metals (PGMs). Based on the recent consequences after a huge earthquake that occurred in Japan, a hypothetical blackout was postulated for the RRP to address additional safety analysis requirements. During a prolonged blackout, the borosilicate glass could phase separate due to cooling of the glass in the melter. The Ru present in the glass matrix could migrate into separate phases and impact the durability of the borosilicate glass. The durability of the glass is important for quality assurance and performance assessment of the vitrified HLW. A fundamental study was performed at an independent university to understand the impact of a prolonged blackout. Simulated HLW glasses were prepared for the RRP, and the Ru behavior in phase separated glasses was studied. The simulated HLW glasses contained nonradioactive elements and PGMs. The glass compositions were then altered to enhance the formation of the phase-separated glasses when subjected to thermal treatment at 700 deg. C for 24 hours. The synthesized simulated glasses contained 1.1 % Ru by weight as ruthenium dioxide (RuO{sub 2}). A portion of the RuO{sub 2} formed needle-shaped crystals in the glass specimens. After the thermal treatment, the glass specimen had separated into two phases. One of the two phases was a B{sub 2}O{sub 3} rich phase, and the other phase was a SiO{sub 2} rich phase. The majority of the chemical species in the B{sub 2}O{sub 3} rich phase was leached away with the Material Characterization Center-3 (MCC-3) protocol standardized by the Pacific Northwest National Laboratory using an aqueous low-concentrated nitric acid solution, but the leaching of the Ru fraction was very limited; less than 1% of the original Ru content. The Ru leaching was much less than those of the other elements, and the needle-shaped crystals of RuO{sub 2} were observed in the B{sub 2}O{sub 3} rich phase in the specimen after the leaching test. Another experiment was performed using another glass specimen which had been prepared with the same frits, but used reagent RuO{sub 2} of granular shape at lower content (0.0073% by weight as RuO{sub 2}). The leached fractions of elements for the latter specimen increased to almost the same fraction (more than 10% of the original Ru content) as observed for boron and sodium, when the phase separated glass was leached using the MMC-3 protocol with non-acidic de-ionized water. Based on the results of this study, it was concluded that needle-shaped RuO{sub 2} crystals are contained in the B{sub 2}O{sub 3}-rich phase after phase separation of the borosilicate glass after a hypothetical blackout. The leaching fraction for the needle-shaped RuO{sub 2} present in the phase separated glass is much lower than those for boron or sodium. Ruthenium behavior has been studied for a hypothetical loss of cooling in the liquid fed ceramic melter for high level waste by taking into account the phase separation of borosilicate glass. The needle-shaped crystal of ruthenium dioxide after bi-nodal-type phase separation of the borosilicate glass at 700 deg. C migrated into the B{sub 2}O{sub 3} rich phase, but remained without dissolution by an acidic aqueous solution. Additionally, granular ruthenium dioxide can be a morphological form of ruthenium after bimodal-type phase separation of the vitrified high level waste with borosilicate glass media. After the phase separation of the borosilicate glass, the crystal shape of the ruthenium dioxide is either needle-shaped or granular, and the leachable fraction of ruthenium is relatively much lower than those of major components (boron and sodium) in the vitrified borosilicate glass. The fraction of leached ruthenium increased to almost the same fraction as observed for boron and sodium when the phase-separated glass was leached with ultrapure water. (authors)

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Glass Formulation for Next Generation Melters

This report describes glass formulation work performed at the Vitreous State Laboratory (VSL) to support the development and testing of next generation advanced joule-heated ceramic melters (NG AJHCMs). The principal objective was to develop and test new glass formulations to take advantage of the enhanced processing capabilities of the NG AJHCMs. New glass formulations were designed to maximize waste loadings while meeting all processing and product quality requirements. The increase in waste loadings, together with the improvements afforded by the NG AJHCMs, will potentially reduce the glass volumes while increasing the throughput rates. Newly developed glass formulations will be needed in melter testing to demonstrate the feasibility of NG AJHCM technologies. This work builds on previous work performed at VSL to increase waste loading and processing rates for Hanford high-iron and high-chromium high level waste (HLW) streams.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Advanced Waste Form and Melter Development for Treatment of Troublesome High-level Wastes

A number of waste components in US defense high level radioactive wastes (HLW) have proven challenging for current Joule heated ceramic melter (JHCM) operations and have limited the ability to increase waste loadings beyond already realized levels. Many of these “troublesome" waste species cause crystallization in the glass melt that can negatively impact product quality or have a deleterious effect on melter processing. Recent efforts at US Department of Energy laboratories have focused on understanding crystallization behavior within HLW glass melts and investigating approaches to mitigate the impacts of crystallization so that increases in waste loading can be realized. Advanced glass formulations have been developed to highlight the unique benefits of next-generation melter technologies such as the Cold Crucible Induction Melter (CCIM). Crystal-tolerant HLW glasses have been investigated to allow sparingly soluble components such as chromium to crystallize in the melter but pass out of the melter before accumulating. The Hanford site AZ-101 tank waste composition represents a waste group that is waste loading limited primarily due to high concentrations of Fe 2 O 3 (with higher Al 2 O 3 ). Systematic glass formulation development utilizing slightly higher process temperatures and higher tolerance to spinel crystals demonstrated that an increase in waste loading of more than 20% could be achieved for this waste composition, and by extension higher loadings for wastes in the same group.

Marra, James↗

Advanced Waste Form and Melter Development for Treatment of Troublesome High-level Wastes

A number of waste components in US defense high level radioactive wastes (HLW) have proven challenging for current Joule heated ceramic melter (JHCM) operations and have limited the ability to increase waste loadings beyond already realized levels. Many of these "troublesome" waste species cause crystallization in the glass melt that can negatively impact product quality or have a deleterious effect on melter processing. Recent efforts at US Department of Energy laboratories have focused on understanding crystallization behavior within HLW glass melts and investigating approached to mitigate the impacts of crystallization so that increases in waste loading can be realized. Advanced glass formulations have been developed to highlight the unique benefits of next-generation melter technologies such as the Cold Crucible Induction Melter (CCIM). Crystal-tolerant HLW glasses have been investigated to allow sparingly soluble components such as chromium to crystallize in the melter but pass out of the melter before accumulating.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Melter Testing for Technetium Removal Using Goethite Precipitation

During vitrification of low activity waste (LAW) at the Hanford Tank Waste Treatment and Immobilization Plant (WTP), liquid effluents are produced in the primary off-gas treatment system that processes the exhaust gases from the LAW melters. That effluent stream, which contains captured hazardous and radioactive species from the melter exhaust, is then recycled and eventually becomes part of subsequent melter feed batches. Other constituents, such as sulfur and halides, are also recycled in this process and this can impact the LAW glass loadings that are achievable. Thus, breaking the melter recycle loop could have advantages with respect to reducing LAW glass volumes. However, this recycle stream cannot currently be diverted to liquid secondary waste treatment because of the levels of several constituents in the scrub solutions, particularly technetium. Researchers at Pacific Northwest National Laboratory (PNNL) have been investigating a process whereby the technetium could be precipitated from the off-gas recycle stream in the mineral goethite ((Tc, Fe)OOH). It could then be diverted to the high level waste (HLW) stream through the WTP pretreatment facility and the decontaminated liquid stream could be sent to secondary waste treatment. As part of the test program to develop the goethite precipitation process, it is necessary to assess the impacts of including this material in the HLW melter feed and the extent to which the captured technetium is volatilized during HLW vitrification. To support such testing, sufficiently large batches of material were prepared at PNNL using rhenium as a surrogate for technetium. These materials were shipped to the Vitreous State Laboratory (VSL) of the Catholic University of America (CUA) for testing on a DuraMelter 10 (DM10) small-scale joule-heated ceramic melter system. This report describes the testing that was performed with those materials.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Cold crucible induction melter studies for making glass ceramic waste forms: A feasibility assessment

Glass ceramics are being developed to immobilize fission products, separated from used nuclear fuel by aqueous reprocessing, into a stable waste form suitable for disposal in a geological repository. This work documents the glass ceramic formulation at bench scale and for a scaled melter test performed in a pilot-scale (approximately 1/4 scale) cold crucible induction melter (CCIM). Melt viscosity, electrical conductivity, and crystallization behavior upon cooling were measured on a small set of compositions to select a formulation for melter testing. Property measurements also identified a temperature range for melter operation and cooling profiles necessary to crystallize the targeted phases in the waste form. Bench scale and melter run results successfully demonstrate the processability of the glass ceramic using the CCIM melter technology.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Vitrification Process for Idaho HLW Calcine - 18433

The majority of the liquid wastes produced from reprocessing of several types of spent nuclear fuel at the Department of energy's (DOE) Idaho site have been volume reduced by calcination. The resulting ∼155,600 ft{sup 3} of calcined waste is stored in 43 shielded stainless steel bins, which have a 500-year design life. The calcined material is both a high-level waste and a RCRA hazardous waste, which complicates treatment and disposal options. In addition to a potential direct disposal option, treatment options that have been considered include steam reforming, hot isostatic pressing (HIP), and vitrification. This paper describes testing and evaluation of a vitrification option for the calcine. Vitrification to produce a borosilicate glass has the advantage that it is the only treatment that provides a waste form that meets the current HLW repository waste acceptance criteria. It is therefore the lowest risk option in terms of regulatory and legislative concerns. The present work addressed several key questions: (i) Calcine waste loadings in glass, which determine the number of HLW canisters produced and the required glass production rate (throughput) for the system design; (ii) Melt rate per unit glass pool surface area of the melter, which determines the sizing of the vitrification system; and (iii) The ability to meet waste form acceptance requirements (PCT and TCLP) while achieving reasonable waste loadings. These are issues of fundamental importance to the sizing estimates for the unit operations and overall flow-sheet and they, therefore, directly impact the cost and schedule estimates. Fully compliant, high-waste-loading glasses were developed for two of the four Idaho calcine wastes. The results demonstrate that waste loadings of 35 wt% waste oxides are achievable for the two alumina calcines and about 30 wt% is achievable for the two zirconia calcines. Testing of these formulations in a joule-heated ceramic melter showed glass production rates of over 5000 kg/(m2/d) for the Alumina calcine and over 8500 kg/(m{sup 2}/d) for the Zirconium-Na Blend calcine. These extremely high production rates translate directly into smaller system size and shorter mission duration and, therefore, reduced costs. Based on these results, a preliminary design for the full-scale vitrification system was developed. The system consists of waste receipt, vitrification, off-gas treatment, and canister sealing and decontamination equipment. The calcine is blended with the appropriate glass forming chemicals (or glass frit) and fed to the melter as a solid stream. The melter has a glass pool surface area of about 2.5 m{sup 2} and is equipped with a bubbling system to increase processing rates. Glass production rates of about 6 metric tons per day are projected. The vitrification system would be installed into the existing Idaho Waste Treatment Unit Facility (IWTU) so that no new facilities are required to house the treatment system, thus greatly reducing overall cost, duration, and risk. The system would be designed to treat all of the calcine waste within a period of 12 years at an operating efficiency of 80%, producing a total of about 8500 canisters each weighing two metric tons. (authors)

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

The effects of glass doping, temperature and time on the morphology, composition, and iron redox of spinel crystals

Precipitation of large crystals/agglomerates of spinel and their accumulation in the pour spout riser of a Joule-heated ceramic melter during idling can plug the melter and prevent pouring of molten glass into canisters. Thus, there is a need to understand the effects of spinel-forming components, temperature, and time on the growth of crystals in connection with an accumulation rate. In our study, crystals of spinel [Fe, Ni, Mn, Zn, Sn][Fe, Cr]₂O₄ were precipitated from simulated high-level waste borosilicate glasses containing different concentrations of Ni, Fe, and Cr by heat treating at 850 and 900°C for different times. These crystals were extracted from the glasses and analyzed with scanning electron microscopy and image analysis for size and shape, with inductively coupled plasma-atomic emission spectroscopy and atom probe tomography for concentration of spinel-forming components, and with wet colorimetry and Mössbauer spectroscopy for Fe²⁺/Fe total ratio. High concentrations of Ni, Fe, and Cr in glasses resulted in the precipitation of crystals larger than 100 µm in just two days. Crystals were a solid solution of NiFe₂O₄, NiCr₂O₄, and -Fe₂O₃ (identified only in the high-Ni-Fe glass) and also contained small concentrations of less than 1 at% of Li, Mg, Mn, and Al.

chemical analysis↗